Lithium dendrite growth analysis method and device and electronic equipment

By establishing evolution equations and deposition system models of phase field parameters, including separators and phase field regions, the problem of inaccurate growth analysis of lithium dendrites in the prior art is solved, and the performance and safety of lithium batteries are improved.

CN119066909APending Publication Date: 2024-12-03ZHEJIANG ZEEKR INTELLIGENT TECH CO LTD +2
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202410995802.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-24
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

In the simulation analysis of lithium dendrites, the prior art usually only considers the phase field region, which leads to a large difference between the simulation results and the actual situation, affecting the performance of lithium batteries.

Method used

Simulation calculations are performed to improve the analytical accuracy of lithium dendrites by establishing evolution equations of phase field parameters and deposition models of deposition systems, including separators and phase field regions.

Benefits of technology

It improves the analytical accuracy of lithium dendrites, reveals the microscopic mechanism of lithium dendrites, guides separator design and optimization, and improves the performance and safety of lithium-ion batteries.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119066909A_ABST
    Figure CN119066909A_ABST
Patent Text Reader

Abstract

The invention provides a lithium dendrite growth analysis method and device and electronic equipment, and relates to the technical field of batteries. The method comprises the following steps: determining phase field parameters for performing phase field simulation on lithium dendrite growth, and establishing an evolution equation of the phase field parameters; a deposition model of a deposition system is established, and the deposition system comprises a diaphragm and a phase field region; defining each region of the sedimentary model according to the evolution equation of the phase field parameters; simulation calculation conditions are determined according to the defined sedimentary model, an evolution equation of the phase field parameters is solved based on the simulation calculation conditions, and a result that the phase field parameters change along with time is obtained; and obtaining an analysis result of lithium dendrite growth according to a time-varying result of the phase field parameters. According to the technical scheme, compared with the prior art, definition and modeling of the diaphragm phase are added, simulation analysis is conducted on lithium dendrite growth by integrating the diaphragm and the phase field area, and the accuracy of lithium dendrite growth analysis is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of battery technology, and in particular to a lithium dendrite growth analysis method, device and electronic equipment. Background Art

[0002] Irregular deposition of lithium metal on the anode will form lithium dendrites, which will lead to a decrease in the reversible capacity of the battery and internal short circuits. The growth of lithium dendrites is the result of the combined action of multiple physical fields, including ion concentration field, electric field, stress field, and temperature field. Due to the complexity of the lithium dendrite problem under multi-physical field conditions, simulation analysis is currently commonly used to study the lithium dendrite growth process.

[0003] Existing methods usually use the phase field method to simulate lithium dendrites, that is, combining thermodynamics, kinetics and electrochemistry to construct a phase field model of lithium deposition, and then predicting the lithium dendrite morphology based on the phase field model. However, this method usually only considers the influence of the phase field area on the growth of lithium dendrites, but the growth process of lithium dendrites is determined by many factors, which may cause the simulation results to differ greatly from the actual situation, affecting the simulation design of lithium batteries, and may further affect the performance of lithium batteries. Summary of the invention

[0004] The problem solved by the present invention is how to improve the analysis accuracy of lithium dendrite growth.

[0005] In order to solve the above problems, the present invention provides a lithium dendrite growth analysis method, device and electronic equipment.

[0006] In a first aspect, the present invention provides a lithium dendrite growth analysis method, comprising:

[0007] Determining phase field parameters for phase field simulation of lithium dendrite growth, and establishing an evolution equation of the phase field parameters;

[0008] Establishing a deposition model of a deposition system, wherein the deposition system includes a diaphragm and a phase field region;

[0009] Defining each region of the deposition model according to the evolution equation of the phase field parameter;

[0010] Determining simulation calculation conditions according to the defined deposition model, solving the evolution equation of the phase field parameter based on the simulation calculation conditions, and obtaining the result of the phase field parameter changing with time;

[0011] The analysis result of lithium dendrite growth is obtained according to the result of the phase field parameter changing with time.

[0012] Optionally, the lithium dendrite growth analysis method further includes:

[0013] Establishing a plurality of deposition models of different deposition systems, wherein the diaphragms in the respective deposition systems are different;

[0014] Solving the evolution equations of the phase field parameters based on the deposition models of the deposition systems respectively, and obtaining the results of the phase field parameters corresponding to the deposition models of the deposition systems respectively changing with time;

[0015] Analyzing the results of the phase field parameters corresponding to the deposition models of each deposition system over time, and obtaining analysis results of the effects of multiple different separators on the generation of lithium dendrites;

[0016] The separator with the best effect of inhibiting the growth of lithium dendrites is determined based on the analysis results of the effects of multiple different separators on the generation of lithium dendrites.

[0017] Optionally, the phase field parameters include phase field order parameters, lithium ion concentration and electric potential, and the evolution equations for establishing the phase field parameters include:

[0018] Establish the phase field sequence parameter evolution equation;

[0019] Establish the lithium ion concentration distribution control equation;

[0020] Establish the governing equations for the electric potential distribution.

[0021] Optionally, establishing the phase field sequence parameter evolution equation includes:

[0022] Determining a total free energy function of the deposition system according to a chemical free energy density function, a gradient free energy density function, and an electrochemical free energy density function, wherein the chemical free energy density function is related to the phase field order parameter, the lithium ion concentration, and the electric potential, the gradient free energy density function is related to the phase field order parameter, and the electrochemical free energy density function is related to the lithium ion concentration and the electric potential;

[0023] Establishing the Allen-Kahn equation based on the total free energy function and the interface migration coefficient;

[0024] The phase field order parameter evolution equation is established according to the Allen-Kahn equation and the Butler-Volmer equation.

[0025] Optionally, establishing a lithium ion concentration distribution control equation includes:

[0026] Determining an effective diffusion coefficient according to a solid-phase diffusion coefficient and a liquid-phase diffusion coefficient, wherein the solid-phase diffusion coefficient is used to describe the migration behavior of lithium ions in lithium metal, and the liquid-phase diffusion coefficient is used to describe the migration behavior of lithium ions in the electrolyte;

[0027] The lithium ion concentration distribution control equation is established according to the effective diffusion coefficient and the deposition reaction consumption term.

[0028] Optionally, the control equation for establishing the potential distribution includes:

[0029] Determine the effective conductivity according to the solid phase conductivity and the liquid phase conductivity, wherein the solid phase conductivity is used to describe the conductivity characteristics in lithium metal, and the liquid phase conductivity is used to describe the conductivity characteristics in the electrolyte;

[0030] A governing equation for the potential distribution is established according to the effective conductivity.

[0031] Optionally, determining simulation calculation conditions according to the defined deposition model includes:

[0032] The parameters of the evolution equation of the phase field parameters are set, a grid is divided based on the defined deposition model, and boundary conditions for simulation calculations are set.

[0033] Optionally, establishing a deposition model of the deposition system includes:

[0034] generating an initial region of the deposition system, and defining the initial region according to the phase field parameter to respectively establish an electrolyte deposition model, a lithium metal negative electrode deposition model, and a diaphragm deposition model;

[0035] A deposition model of the deposition system is established according to the electrolyte deposition model, the lithium metal negative electrode deposition model and the diaphragm deposition model.

[0036] Optionally, establishing a deposition model of the deposition system further comprises: establishing the diaphragm deposition model by a parameterized modeling method.

[0037] In a second aspect, the present invention provides a lithium dendrite growth analysis device, comprising:

[0038] The first module is used to determine the phase field parameters for phase field simulation of lithium dendrite growth and establish the evolution equation of the phase field parameters;

[0039] A second module is used to establish a deposition model of a deposition system, wherein the deposition system includes a diaphragm and a phase field region;

[0040] A third module is used to define each region of the deposition model according to the evolution equation of the phase field parameter;

[0041] The fourth module is used to determine the simulation calculation conditions according to the defined deposition model, solve the evolution equation of the phase field parameter based on the simulation calculation conditions, and obtain the result of the phase field parameter changing with time;

[0042] The fifth module is used to obtain the analysis result of lithium dendrite growth according to the result of the phase field parameter changing with time.

[0043] In a third aspect, the present invention provides an electronic device, including a memory and a processor;

[0044] The memory is used to store computer programs;

[0045] The processor is used to implement the lithium dendrite growth analysis method as described in the first aspect when executing the computer program.

[0046] The beneficial effect of the lithium dendrite growth analysis method of the present invention is: by establishing an evolution equation of phase field parameters and a deposition model of a deposition system including a diaphragm and a phase field region, defining each region of the deposition model according to the evolution equation of the phase field parameters, determining simulation calculation conditions according to the defined deposition model, and then solving the evolution equation of the phase field parameters based on the simulation calculation conditions, and obtaining the analysis result of lithium dendrite growth according to the result of the solved phase field parameters changing with time. Compared with the prior art, the definition and modeling of the diaphragm phase are added, and the simulation analysis of the lithium dendrite growth is performed by combining the diaphragm and the phase field region, thereby improving the analysis accuracy of the lithium dendrite growth. On this basis, a lithium dendrite growth phase field model including three phases of diaphragm, electrode and electrolyte can be established, the influence of different diaphragm types on the growth of lithium dendrites is studied, and the microscopic mechanism of lithium dendrite growth is revealed, which can further guide the design and optimization of the diaphragm, and ultimately improve the performance and safety of lithium-ion batteries. BRIEF DESCRIPTION OF THE DRAWINGS

[0047] Figure 1 Schematic diagram of the process of the lithium dendrite growth analysis method according to an embodiment of the present invention;

[0048] Figure 2 Schematic diagram of the process of analyzing the growth of lithium dendrites of different separators according to an embodiment of the present invention;

[0049] Figure 3 A schematic diagram of a flow chart for establishing an evolution equation of phase field parameters according to an embodiment of the present invention;

[0050] Figure 4 A schematic diagram of a flow chart for establishing a phase field sequence parameter evolution equation according to an embodiment of the present invention;

[0051] Figure 5 A schematic diagram of a flow chart for establishing a lithium ion concentration distribution control equation according to an embodiment of the present invention;

[0052] Figure 6 A schematic diagram of a flow chart of establishing a control equation for electric potential distribution according to an embodiment of the present invention;

[0053] Figure 7This is a system architecture diagram of a lithium dendrite growth analysis device according to an embodiment of the present invention;

[0054] Figure 8 A system architecture diagram of an electronic device according to an embodiment of the present invention;

[0055] Fig. 9 A schematic diagram of modeling of a diaphragm and a deposition system according to an embodiment of the present invention;

[0056] Fig.10 Schematic diagram of the growth morphology of lithium dendrites according to an embodiment of the present invention. DETAILED DESCRIPTION

[0057] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the specific embodiments of the present invention are described in detail below in conjunction with the accompanying drawings. Although certain embodiments of the present invention are shown in the accompanying drawings, it should be understood that the present invention can be implemented in various forms and should not be interpreted as being limited to the embodiments described herein. On the contrary, these embodiments are provided to provide a more thorough and complete understanding of the present invention. It should be understood that the drawings and embodiments of the present invention are only for exemplary purposes and are not intended to limit the scope of protection of the present invention.

[0058] It should be understood that the various steps described in the method embodiments of the present invention may be performed in different orders and / or in parallel. In addition, the method embodiments may include additional steps and / or omit the steps shown. The scope of the present invention is not limited in this respect.

[0059] The term "including" and its variations used in this document are open inclusions, that is, "including but not limited to"; the term "based on" means "based at least in part on"; the term "one embodiment" means "at least one embodiment"; the term "another embodiment" means "at least one other embodiment"; the term "some embodiments" means "at least some embodiments"; the term "optionally" means "optional embodiments". The relevant definitions of other terms will be given in the following description. It should be noted that the concepts of "first", "second", etc. mentioned in the present invention are only used to distinguish different devices, modules or units, and are not used to limit the order or interdependence of the functions performed by these devices, modules or units.

[0060] It should be noted that the modifications of "one" and "plurality" mentioned in the present invention are illustrative rather than restrictive, and those skilled in the art should understand that, unless otherwise clearly indicated in the context, it should be understood as "one or more".

[0061] The names of the messages or information exchanged between multiple devices in the embodiments of the present invention are only used for illustrative purposes, and are not used to limit the scope of these messages or information.

[0062] like Figure 1 As shown, a lithium dendrite growth analysis method provided by an embodiment of the present invention includes:

[0063] S100: Determine phase field parameters for phase field simulation of lithium dendrite growth, and establish evolution equations of the phase field parameters.

[0064] Specifically, the phase field parameters for phase field simulation of lithium dendrite growth are first determined, such as phase field order parameters, lithium ion concentration and electric potential, and then the phase field parameter evolution equation is derived based on thermodynamics to provide a mathematical model basis that needs to be input into the finite element simulation software, thereby converting the physical problem into a mathematical model that can be processed in the finite element software.

[0065] Among them, the evolution equations of phase field parameters usually include multiple PDE equations (Partial Differential Equations), and the PDE equations are established by corresponding physical laws.

[0066] S200: Establishing a deposition model of a deposition system, wherein the deposition system includes a diaphragm and a phase field region.

[0067] Specifically, a geometric model can be created in CAD software and then imported into finite element simulation software, or it can be created in integrated software (integrated CAD and finite element simulation functions) to establish a deposition model of the deposition system, that is, a lithium dendrite growth phase field model including three phases of diaphragm, electrode and electrolyte, wherein the deposition system includes a diaphragm and a phase field region, and the phase field region includes an electrolyte and an electrode.

[0068] Among them, Fig. 9 The deposition model shown in Figure 1 is used to define the scope of the PDE equation. That is, the deposition model plays an important role in defining the scope of the physical problem space in the process of modeling and solving the PDE equation, and determines the physical domain on which the PDE equation acts. In addition, the deposition model is also used to visualize the PDE calculation results, that is, the deposition model is used to display the following Fig.10 The growth morphology image of lithium dendrites is shown. Therefore, the deposition model plays a fundamental supporting role in the subsequent visualization of results, providing a spatial framework and structure for the visualization of calculation results, making the display of results intuitive and easy to understand.

[0069] Among them, the effect of the diaphragm on the growth of lithium dendrites cannot be ignored. The diaphragm with functional coating can inhibit the growth of lithium dendrites through different ways such as physical blocking, lithium ion redistribution, or piezoelectric effect of piezoelectric ceramics. When the diaphragm is present, the lithium dendrites are hindered by the diaphragm and grow along the pores of the diaphragm. If the deposition time is long enough or the deposition driving force is large enough, the dendrites are likely to pass through the diaphragm to reach the counter electrode, thereby short-circuiting the battery.

[0070] S300: defining each region of the deposition model according to the evolution equation of the phase field parameter.

[0071] Specifically, the evolution equation of the simplified phase field parameters can be simplified according to the specific problem. For example, some items may be ignored when assuming uniform material and steady-state conditions. The simplified evolution equation of the phase field parameters is input into the finite element simulation software to clarify the physical properties and boundary conditions of each region, such as the phase field region, diaphragm region and boundary type (fixed, free, etc.), so as to realize the definition of each region in the deposition model.

[0072] S400: Determine simulation calculation conditions according to the defined deposition model, solve the evolution equation of the phase field parameter based on the simulation calculation conditions, and obtain the result of the phase field parameter changing with time.

[0073] Specifically, the simulation calculation conditions are determined according to the defined deposition model, such as determining the relevant parameters in the phase field parameter evolution equation, meshing the deposition model, and defining boundary conditions, etc., providing all the details and settings required for the solution, and then running the finite element simulation software to solve the phase field parameter evolution equation to obtain the result of the phase field parameter changing with time.

[0074] S500: Obtaining analysis results of lithium dendrite growth according to the results of the phase field parameters changing with time.

[0075] Specifically, the analysis results of lithium dendrite growth are obtained based on the results of the phase field parameters changing with time, such as Fig.10 The growth morphology image of lithium dendrites shown in the figure can be used to study the effects of different separator types on the growth of lithium dendrites in the future.

[0076] In this embodiment, by establishing the evolution equation of phase field parameters and the deposition model of the deposition system including the diaphragm and the phase field area, after defining each area of ​​the deposition model according to the evolution equation of the phase field parameters, the simulation calculation conditions are determined according to the defined deposition model, and then the evolution equation of the phase field parameters is solved based on the simulation calculation conditions. The analysis results of lithium dendrite growth are obtained according to the results of the solved phase field parameters changing with time. Compared with the prior art, the definition and modeling of the diaphragm phase are added, and the analysis accuracy of lithium dendrite growth is improved. On this basis, a lithium dendrite growth phase field model including the three phases of diaphragm, electrode and electrolyte can be established, the influence of different diaphragm types on lithium dendrite growth can be studied, and the microscopic mechanism of lithium dendrite growth can be revealed, which can further guide the design and optimization of the diaphragm, and ultimately improve the performance and safety of lithium-ion batteries.

[0077] Optionally, the lithium dendrite growth analysis method further includes:

[0078] S201: establishing a plurality of deposition models of different deposition systems, wherein the diaphragms in the respective deposition systems are different.

[0079] Specifically, combined Figure 2 As shown, the type of diaphragm is adjusted to establish deposition models for different deposition systems.

[0080] S401: Solving the evolution equations of the phase field parameters based on the deposition models of the deposition systems respectively, and obtaining the results of the phase field parameters corresponding to the deposition models of the deposition systems respectively changing with time.

[0081] Specifically, combined Figure 2 As shown, based on the deposition models of each deposition system, the evolution equations of the phase field parameters are solved respectively, and the results of the phase field parameters corresponding to the deposition models of each deposition system changing with time are obtained, such as the growth morphology images of different lithium dendrites.

[0082] S501: Analyze the results of the phase field parameters corresponding to the deposition models of each deposition system over time, and obtain analysis results of the effects of multiple different separators on the generation of lithium dendrites.

[0083] Specifically, combined Figure 2 As shown, the results of the changes in the phase field parameters corresponding to the deposition models of each deposition system over time are analyzed, and the analysis results of the effects of multiple different membranes on the formation of lithium dendrites are obtained, that is, the growth morphology images of different lithium dendrites are analyzed, and the analysis results of the effects of the corresponding membranes on the formation of lithium dendrites are obtained.

[0084] S601: Determine the separator with the best effect on inhibiting the growth of lithium dendrites based on the analysis results of the effects of multiple different separators on the generation of lithium dendrites.

[0085] Specifically, combined Figure 2 As shown in the figure, selecting the diaphragm with the best effect on inhibiting the growth of lithium dendrites from the analysis results of the effects of multiple different diaphragms on the formation of lithium dendrites can further guide the design and optimization of the diaphragm, and ultimately improve the performance and safety of lithium-ion batteries.

[0086] In this optional embodiment, a deposition model of a deposition system including different diaphragms is established to perform a lithium dendrite growth analysis method, from which a diaphragm with the best lithium dendrite growth inhibition effect can be selected, which can further guide the design and optimization of the diaphragm, ultimately improving the performance and safety of lithium-ion batteries.

[0087] Optionally, the phase field parameters include phase field order parameters, lithium ion concentration and electric potential, and the evolution equations for establishing the phase field parameters include:

[0088] S110: Establish phase field sequence parameter evolution equation.

[0089] Specifically, combined Figure 3 As shown, the phase field parameters include the phase field order parameter ξ, the lithium ion concentration c i and potential For the phase field order parameter ξ, its evolution over time can be described by the Allen-Kahn equation:

[0090]

[0091] Among them, L i represents the interface migration coefficient, F represents the total free energy of the system, and ξ represents the phase field order parameter.

[0092] Among them, for the phase field sequence parameters ξ, φ, ξ = 0 represents a certain phase, ξ = 1 represents another phase, and the value between 0 and 1 represents the diffusion interface between the two phases. The number of phase field sequence parameters is determined according to the phases included in the phase field model; for example, combined with Fig. 9 As shown, ξ=0 and φ=0 represent electrolyte, ξ=0 and φ=1 represent separator, ξ=1 and φ=0 represent lithium metal negative electrode, wherein the separator is usually composed of Fig. 9 Polymer materials and pore composition shown.

[0093] S120: Establishing a lithium ion concentration distribution control equation.

[0094] Specifically, combined Figure 3 As shown, the evolution of lithium ion concentration over time can be described by the Kahn-Hilliard equation and Fick's second law, where the expression of the Kahn-Hilliard equation is:

[0095]

[0096] Among them, M i represents the interfacial migration coefficient, c i Indicates the lithium ion concentration.

[0097] The lithium ion concentration distribution control equation can be established based on the Kahn-Hilliard equation and Fick's second law. The details are shown below.

[0098] S130: Establish the control equation of electric potential distribution.

[0099] Specifically, combined Figure 3 As shown, the potential distribution of the deposition system can be described by the Nernst-Planck equation, thereby establishing the control equation of the potential distribution. The details are described later.

[0100] In this optional embodiment, by establishing the phase field sequence parameter evolution equation, the lithium ion concentration distribution control equation and the potential distribution control equation, the phase field parameter evolution equation can be established, and the physical problem can be converted into a mathematical model that can be processed in the finite element software, which is conducive to solving.

[0101] Optionally, establishing the phase field sequence parameter evolution equation includes:

[0102] S111: Determine the total free energy function of the deposition system according to a chemical free energy density function, a gradient free energy density function and an electrochemical free energy density function, wherein the chemical free energy density function is related to the phase field order parameter, the lithium ion concentration and the electric potential, the gradient free energy density function is related to the phase field order parameter, and the electrochemical free energy density function is related to the lithium ion concentration and the electric potential.

[0103] Specifically, combined Figure 4 As shown, the total free energy function of the system is a function of the phase field parameters, and its expression is:

[0104]

[0105] The chemical free energy density is a function of order parameter, concentration and potential, and its expression is:

[0106]

[0107] Among them, f 0 represents the double-well potential function, f ion represents the interaction energy function between ions and the field, W represents the potential barrier height, represents the concentration of the i-th ion, i represents any ion in the deposition system, c о represents the initial concentration of liquid lithium ions, R represents the gas constant, T represents the ambient temperature, is the Hamiltonian operator.

[0108] In addition, the chemical free energy density It can also be expressed as:

[0109]

[0110] Among them, W 01 , W 02 , W 12 represents the potential barrier height.

[0111] Among them, the gradient free energy density The expression is:

[0112]

[0113] Among them, k ξ represents the interface energy anisotropy function, in this embodiment:

[0114] k ξ =κ 0 [1+δcosωθ];

[0115] Among them, κ 0 represents the interface energy coefficient, δ represents the anisotropy strength, ω represents the anisotropy modulus, and θ represents the angle between the interface normal and the coordinate axis.

[0116] In addition, the gradient free energy density It can also be expressed as:

[0117]

[0118] Among them, k ξ , k φ represents the interface energy anisotropy function, and the two are collectively referred to as k ξ、φ , in this embodiment:

[0119] k ξ、φ =κ 0 [1+δcosωθ];

[0120] The electrochemical free energy density The expression is:

[0121]

[0122] Among them, z i represents the number of electron transfers of different components, and F represents the Faraday constant.

[0123] S112: Establishing the Allen-Kahn equation according to the total free energy function and the interface migration coefficient.

[0124] S113: Establishing the phase field order parameter evolution equation according to the Allen-Kahn equation and the Butler-Volmer equation.

[0125] Specifically, combined Figure 4 As shown, the equations in step S111 are introduced into the Allen-Kahn equation, and the phase field order parameter evolution equation is established in combination with the Butler-Volmer equation. The expression of the phase field order parameter evolution equation is:

[0126]

[0127] Among them, L σ , L φ represents the interface mobility coefficient; gξ)=Wξ 2 (1-ξ)2 , g(φ)=Wφ 2 (1-φ) 2 , that is, the double-well potential function; κ, κ φ represents the gradient energy coefficient; L η Represents the reaction constant; h(ξ)=ξ 3 910-15ξ+6ξ 2 ), that is, the interpolation function established, is used to ensure the effectiveness and continuity of the diffusion interface.

[0128] In this optional embodiment, after determining the total free energy function based on the chemical free energy density function, the gradient free energy density function and the electrochemical free energy density function, the phase field order parameter evolution equation is established by combining the Allen-Kahn equation and the Butler-Volmer equation, and the physical problem is converted into a mathematical model that can be processed in the finite element software, which is conducive to solving the problem.

[0129] Optionally, establishing a lithium ion concentration distribution control equation includes:

[0130] S121: determining an effective diffusion coefficient according to a solid-phase diffusion coefficient and a liquid-phase diffusion coefficient, wherein the solid-phase diffusion coefficient is used to describe the migration behavior of lithium ions in lithium metal, and the liquid-phase diffusion coefficient is used to describe the migration behavior of lithium ions in an electrolyte.

[0131] S122: Establishing the lithium ion concentration distribution control equation according to the effective diffusion coefficient and the deposition reaction consumption term.

[0132] Specifically, combined Figure 5 As shown, the expression of the lithium ion concentration distribution control equation is:

[0133]

[0134] Among them, D eff represents the effective diffusion coefficient. To ensure that it is effective at the diffusion interface, D eff =D m h(ξ)+D e (1-h(ξ)),D m represents the solid phase diffusion coefficient, which is used to describe the migration behavior of lithium ions in lithium metal. e represents the liquid phase diffusion coefficient, which is used to describe the migration behavior of lithium ions in the electrolyte; the last term of the lithium ion concentration distribution control equation represents the lithium ions consumed by the deposition reaction.

[0135] In this optional embodiment, after determining the effective diffusion coefficient based on the solid-phase diffusion coefficient and the liquid-phase diffusion coefficient, a lithium ion concentration distribution control equation is established in combination with the deposition reaction consumption term, and the physical problem is converted into a mathematical model that can be processed in finite element software, which is conducive to solving the problem.

[0136] Optionally, the control equation for establishing the potential distribution includes:

[0137] S131: determining effective conductivity according to solid-phase conductivity and liquid-phase conductivity, wherein the solid-phase conductivity is used to describe the conductivity characteristics in lithium metal, and the liquid-phase conductivity is used to describe the conductivity characteristics in the electrolyte.

[0138] S132: Establishing a control equation for the potential distribution according to the effective conductivity.

[0139] Specifically, combined Figure 6 As shown, the potential distribution of the deposition system can be described by the Nernst-Planck equation, and the governing equation of the potential distribution is:

[0140]

[0141] Among them, σ eff represents the effective conductivity. To ensure that it is effective at the diffusion interface, σ eff =σ m h(ξ)+σ e (1-h(ξ)),σ m represents the solid phase conductivity, which is used to describe the conductivity characteristics in lithium metal, σ e It represents liquid phase conductivity and is used to describe the conductivity characteristics in the electrolyte.

[0142] in, I R represents the current density, c s represents the site density of lithium metal, and n represents the number of electrons involved in the electrode reaction.

[0143] In this optional embodiment, after the effective conductivity is determined based on the solid phase conductivity and the liquid phase conductivity, a control equation for the potential distribution is established to convert the physical problem into a mathematical model that can be processed in finite element software, which is conducive to solving the problem.

[0144] Optionally, determining simulation calculation conditions according to the defined deposition model includes:

[0145] The parameters of the evolution equation of the phase field parameters are set, a grid is divided based on the defined deposition model, and boundary conditions for simulation calculations are set.

[0146] Specifically, the parameters of the phase field parameter evolution equation are set, the grid is divided based on the defined deposition model, and the phase field parameter evolution equation is solved after the boundary conditions are set. By refining and setting the deposition model, it is ensured that the deposition model and physical parameters are sufficiently refined and accurate, and the necessary details (such as grids and boundary conditions) are provided for the solution steps, so that the simulation can proceed smoothly.

[0147] In this optional embodiment, the phase field parameter evolution equation is solved by setting the simulation calculation conditions, providing necessary details for the solution step so that the simulation can proceed smoothly.

[0148] Optionally, establishing a deposition model of the deposition system includes:

[0149] An initial region of the deposition system is generated, and the initial region is defined according to the phase field parameters to respectively establish an electrolyte deposition model, a lithium metal negative electrode deposition model, and a diaphragm deposition model.

[0150] Specifically, combined Fig. 9 As shown, the initial region of the deposition system can be generated by CAD software. For example, a square region of appropriate size can be generated in the CAD software as the initial region of the electrolyte and the electrode, and the initial region of the diaphragm can be generated according to the morphology of the diaphragm. That is, the geometric model established in the CAD software is used as the initial region of the deposition system, and the initial region is defined according to the phase field parameters, thereby establishing the electrolyte deposition model, the lithium metal negative electrode deposition model and the diaphragm deposition model respectively.

[0151] For example, when ξ=0 and φ=0, an electrolyte deposition model is established, when ξ=1 and φ=0, a lithium metal negative electrode deposition model is established, and when ξ=0 and φ=1, a diaphragm deposition model is established.

[0152] A deposition model of the deposition system is established according to the electrolyte deposition model, the lithium metal negative electrode deposition model and the diaphragm deposition model.

[0153] Specifically, after establishing an electrolyte deposition model, a lithium metal negative electrode deposition model and a diaphragm deposition model, a deposition model of a deposition system is formed according to the above three deposition models.

[0154] In this optional embodiment, the initial region is defined according to the phase field parameters to establish a deposition model of the deposition system, which is conducive to finite element simulation and thus improves the accuracy of the lithium dendrite growth analysis results.

[0155] Optionally, establishing a deposition model of the deposition system further comprises: establishing the diaphragm deposition model by a parameterized modeling method.

[0156] Specifically, any modeling method can be adopted for modeling the membrane deposition model, such as direct geometric modeling, random reconstruction algorithm modeling based on microscopic images, or parametric modeling with adjustable pore structure. In order to reflect the pore size and pore tortuosity characteristics of the membrane, the parametric modeling method is preferred.

[0157] In this optional embodiment, the diaphragm deposition model is geometrically modeled by a parametric modeling method, which can reflect the pore size and pore tortuosity characteristics of the diaphragm and improve the accuracy of the lithium dendrite growth analysis results.

[0158] like Figure 7 As shown, a lithium dendrite growth analysis device 700 provided in an embodiment of the present invention includes:

[0159] The first module 710 is used to determine the phase field parameters for phase field simulation of lithium dendrite growth and establish the evolution equation of the phase field parameters;

[0160] A second module 720 is used to establish a deposition model of a deposition system, wherein the deposition system includes a diaphragm and a phase field region;

[0161] The third module 730 is used to define each region of the deposition model according to the evolution equation of the phase field parameter;

[0162] The fourth module 740 is used to determine simulation calculation conditions according to the defined deposition model, solve the evolution equation of the phase field parameter based on the simulation calculation conditions, and obtain the result of the phase field parameter changing with time;

[0163] The fifth module 750 is used to obtain the analysis result of lithium dendrite growth according to the result of the phase field parameter changing with time.

[0164] like Figure 8 As shown, an electronic device 800 provided by an embodiment of the present invention includes a memory 820 and a processor 810; the memory 820 is used to store a computer program; the processor 810 is used to implement the lithium dendrite growth analysis method as described above when executing the computer program.

[0165] In other words, an electronic device 800 includes a memory 820 and a processor 810 coupled to the memory 820; the memory 820 is configured to store a computer program; and the processor 810 is configured to perform the following operations when executing the computer program:

[0166] Determining phase field parameters for phase field simulation of lithium dendrite growth, and establishing an evolution equation of the phase field parameters;

[0167] Establishing a deposition model of a deposition system, wherein the deposition system includes a diaphragm and a phase field region;

[0168] Defining each region of the deposition model according to the evolution equation of the phase field parameter;

[0169] Determining simulation calculation conditions according to the defined deposition model, solving the evolution equation of the phase field parameter based on the simulation calculation conditions, and obtaining the result of the phase field parameter changing with time;

[0170] The analysis result of lithium dendrite growth is obtained according to the result of the phase field parameter changing with time.

[0171] An embodiment of the present invention provides a computer-readable storage medium, on which a computer program is stored. When the computer program is executed by a processor, the lithium dendrite growth analysis method as described above is implemented.

[0172] In other words, a non-volatile computer-readable storage medium stores a computer program, and when the computer program is executed by a processor, the processor performs the following operations:

[0173] Determining phase field parameters for phase field simulation of lithium dendrite growth, and establishing an evolution equation of the phase field parameters;

[0174] Establishing a deposition model of a deposition system, wherein the deposition system includes a diaphragm and a phase field region;

[0175] Defining each region of the deposition model according to the evolution equation of the phase field parameter;

[0176] Determining simulation calculation conditions according to the defined deposition model, solving the evolution equation of the phase field parameter based on the simulation calculation conditions, and obtaining the result of the phase field parameter changing with time;

[0177] The analysis result of lithium dendrite growth is obtained according to the result of the phase field parameter changing with time.

[0178] An electronic device 800 that can be used as a server or client of the present invention will now be described, which is an example of a hardware device that can be applied to various aspects of the present invention. The electronic device 800 is intended to represent various forms of digital electronic computer equipment, such as laptop computers, desktop computers, workbenches, personal digital assistants, servers, blade servers, mainframe computers, and other suitable computers. The electronic device 800 can also represent various forms of mobile devices, such as personal digital processing, cellular phones, smart phones, wearable devices, and other similar computing devices. The components shown herein, their connections and relationships, and their functions are merely examples, and are not intended to limit the implementation of the present invention described herein and / or required.

[0179] The electronic device 800 includes a computing unit, which can perform various appropriate actions and processes according to a computer program stored in a read-only memory (ROM) or a computer program loaded from a storage unit into a random access memory (RAM). In the RAM, various programs and data required for the operation of the device can also be stored. The computing unit, ROM, and RAM are connected to each other via a bus. An input / output (I / O) interface is also connected to the bus.

[0180] A person of ordinary skill in the art can understand that all or part of the processes in the above-mentioned embodiment method can be completed by instructing the relevant hardware through a computer program, and the program can be stored in a computer-readable storage medium. When the program is executed, it can include the processes of the embodiments of the above-mentioned methods. Among them, the storage medium can be a disk, an optical disk, a read-only memory (ROM) or a random access memory (RAM), etc. In the present application, the unit described as a separate component may or may not be physically separated, and the component displayed as a unit may or may not be a physical unit, that is, it may be located in one place, or it may be distributed on multiple network units. Some or all of the units can be selected according to actual needs to achieve the purpose of the embodiment of the present invention. In addition, each functional unit in each embodiment of the present invention can be integrated in a processing unit, or each unit can exist physically separately, or two or more units can be integrated in one unit. The above-mentioned integrated unit can be implemented in the form of hardware or in the form of a software functional unit.

[0181] Although the present invention is disclosed as above, the protection scope of the present invention is not limited thereto. Those skilled in the art may make various changes and modifications without departing from the spirit and scope of the present invention, and these changes and modifications will fall within the protection scope of the present invention.

Claims

1. A lithium dendrite growth analysis method, characterized in that: include: Determining phase field parameters for phase field simulation of lithium dendrite growth, and establishing an evolution equation of the phase field parameters; Establishing a deposition model of a deposition system, wherein the deposition system includes a diaphragm and a phase field region; Defining each region of the deposition model according to the evolution equation of the phase field parameter; Determining simulation calculation conditions according to the defined deposition model, solving the evolution equation of the phase field parameter based on the simulation calculation conditions, and obtaining the result of the phase field parameter changing with time; The analysis result of lithium dendrite growth is obtained according to the result of the phase field parameter changing with time.

2. The lithium dendrite growth analysis method according to claim 1, characterized in that: Also includes: Establishing a plurality of deposition models of different deposition systems, wherein the diaphragms in the respective deposition systems are different; Solving the evolution equations of the phase field parameters based on the deposition models of the deposition systems respectively, and obtaining the results of the phase field parameters corresponding to the deposition models of the deposition systems respectively changing with time; Analyzing the results of the phase field parameters corresponding to the deposition models of each deposition system over time, and obtaining analysis results of the effects of multiple different separators on the generation of lithium dendrites; The separator with the best effect of inhibiting the growth of lithium dendrites is determined based on the analysis results of the effects of multiple different separators on the generation of lithium dendrites.

3. The lithium dendrite growth analysis method according to claim 1, characterized in that: The phase field parameters include phase field sequence parameters, lithium ion concentration and electric potential, and the evolution equations for establishing the phase field parameters include: Establish the phase field sequence parameter evolution equation; Establish the lithium ion concentration distribution control equation; Establish the governing equations for the electric potential distribution.

4. The lithium dendrite growth analysis method according to claim 3, characterized in that: The establishment of the phase field sequence parameter evolution equation comprises: Determining a total free energy function of the deposition system according to a chemical free energy density function, a gradient free energy density function, and an electrochemical free energy density function, wherein the chemical free energy density function is related to the phase field order parameter, the lithium ion concentration, and the electric potential, the gradient free energy density function is related to the phase field order parameter, and the electrochemical free energy density function is related to the lithium ion concentration and the electric potential; Establishing the Allen-Kahn equation based on the total free energy function and the interface migration coefficient; The phase field order parameter evolution equation is established according to the Allen-Kahn equation and the Butler-Volmer equation.

5. The lithium dendrite growth analysis method according to claim 3, characterized in that: The establishment of the lithium ion concentration distribution control equation comprises: Determining an effective diffusion coefficient according to a solid-phase diffusion coefficient and a liquid-phase diffusion coefficient, wherein the solid-phase diffusion coefficient is used to describe the migration behavior of lithium ions in lithium metal, and the liquid-phase diffusion coefficient is used to describe the migration behavior of lithium ions in the electrolyte; The lithium ion concentration distribution control equation is established according to the effective diffusion coefficient and the deposition reaction consumption term.

6. The lithium dendrite growth analysis method according to claim 3, characterized in that: The control equations for establishing the potential distribution include: Determine the effective conductivity according to the solid phase conductivity and the liquid phase conductivity, wherein the solid phase conductivity is used to describe the conductivity characteristics in lithium metal, and the liquid phase conductivity is used to describe the conductivity characteristics in the electrolyte; A governing equation for the potential distribution is established according to the effective conductivity.

7. The lithium dendrite growth analysis method according to claim 1, characterized in that: Determining the simulation calculation conditions according to the defined deposition model includes: The parameters of the evolution equation of the phase field parameters are set, a grid is divided based on the defined deposition model, and boundary conditions for simulation calculations are set.

8. The lithium dendrite growth analysis method according to any one of claims 1 to 7, characterized in that: The establishment of a deposition model of the deposition system comprises: generating an initial region of the deposition system, and defining the initial region according to the phase field parameter to respectively establish an electrolyte deposition model, a lithium metal negative electrode deposition model, and a diaphragm deposition model; A deposition model of the deposition system is established according to the electrolyte deposition model, the lithium metal negative electrode deposition model and the diaphragm deposition model.

9. The lithium dendrite growth analysis method according to claim 8, characterized in that: The establishing of the deposition model of the deposition system further comprises: establishing the diaphragm deposition model by a parameterized modeling method.

10. A lithium dendrite growth analysis device, characterized in that: include: The first module is used to determine the phase field parameters for phase field simulation of lithium dendrite growth and establish the evolution equation of the phase field parameters; A second module is used to establish a deposition model of a deposition system, wherein the deposition system includes a diaphragm and a phase field region; A third module is used to define each region of the deposition model according to the evolution equation of the phase field parameter; The fourth module is used to determine the simulation calculation conditions according to the defined deposition model, solve the evolution equation of the phase field parameter based on the simulation calculation conditions, and obtain the result of the phase field parameter changing with time; The fifth module is used to obtain the analysis result of lithium dendrite growth according to the result of the phase field parameter changing with time.

11. An electronic device, characterized in that: including memory and processor; The memory is used to store computer programs; The processor is used to implement the lithium dendrite growth analysis method as described in any one of claims 1 to 9 when executing the computer program.

Citation Information

Cited By

  • Automatic control method and system for precious metal purification process

    CN121386364A