Semiconductor light-emitting element and light-emitting device
By using the AlaGa1-aN material layer and the Al-free nitride material layer in the semiconductor light emitting element, the light absorption problem in the traditional gallium nitride epitaxial structure is solved, and the luminescence efficiency and electron-hole recombination efficiency are improved.
Patent Information
- Application Number
- CN202411086304.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-08
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2044-08-08
AI Technical Summary
The thicker p-type gallium nitride material in the traditional gallium nitride epitaxial structure has obvious light absorption on light below 370nm, seriously affecting the light output efficiency of the light emitting element.
By using the AlaGa1-aN material layer as the P-type layer in the semiconductor light emitting element, its thickness and doping concentration are controlled, the absorption of light is reduced, and the ohmic contact layer is formed using a layer of nitride material without Al, if necessary, to ensure that Light output efficiency.
The light-emitting efficiency of the light emitting element is improved, the light absorption by the p-type gallium nitride material is reduced, and the electron-hole recombination efficiency is enhanced.
Smart Images

Figure CN119069588A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of semiconductor devices and apparatuses, and in particular to a semiconductor light-emitting element and a light-emitting apparatus. Background Art
[0002] Due to its high luminous efficiency, GaN-based LEDs are now widely used in various light source fields such as backlight, lighting, car lights, and decoration. From a technical perspective, further improving the luminous efficiency of LED chips is still the focus of current industry development. The luminous efficiency is mainly determined by two factors. The first is the radiation recombination efficiency of electron holes in the active region, that is, the internal quantum efficiency; the second is the light extraction efficiency.
[0003] For nitride light-emitting diodes, in order to improve their luminous efficiency, various epitaxial structures are usually used to improve their internal quantum efficiency. One of the factors that affect the internal quantum efficiency is the light absorption characteristics of the gallium nitride material itself. In order to obtain better ohmic contact and good material quality, the traditional gallium nitride epitaxial structure uses thicker p-type gallium nitride materials to grow p-type layers. However, thicker p-type gallium nitride materials have obvious light absorption below 370nm, which seriously affects the light output efficiency of the light-emitting element. Summary of the invention
[0004] In view of the above-mentioned defects of nitride light-emitting diodes in the prior art, the present invention provides a semiconductor light-emitting element and a light-emitting device, which solve one or more of the above-mentioned problems by improving the material selection and thickness setting of the P-type layer.
[0005] In a first aspect of the present application, a semiconductor light emitting element is provided, which comprises at least an epitaxial structure, wherein the epitaxial structure comprises at least a first semiconductor layer structure, an active layer and a second semiconductor layer structure stacked from bottom to top, wherein the active layer comprises Al y Ga 1-y N barrier layer and Al x Ga 1-x N potential well layer, wherein 0<x<1, 0<y<1, the second semiconductor layer structure includes Al a Ga 1-a N material layer, wherein 0<a<1.
[0006] According to another embodiment of the present invention, a light emitting device is provided, which includes the semiconductor light emitting element described in the present invention.
[0007] As described above, the semiconductor light emitting element and light emitting device of the present application have the following beneficial effects:
[0008] In the semiconductor light emitting element of the present application, the active layer includes Al y Ga 1-y N barrier layer and Alx Ga 1-x N potential well layer, wherein 0<x<1, 0<y<1, the second semiconductor layer structure includes Al a Ga 1-a N material layer, wherein 0<a<1. As mentioned above, the P-type layer of the present application selects Al a Ga 1-a In addition, the P-type layer may include an ohmic contact layer formed by a nitride material layer that does not contain Al, and the thickness of the ohmic contact layer is controlled to be less than 10nm to reduce the p-type gallium nitride material, thereby reducing the absorption of light and improving the light extraction efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0009] Figure 1 Shown is a schematic structural diagram of a light-emitting element provided in Embodiment 1 of the present invention.
[0010] Figure 2 Display as Figure 1 Schematic diagram of the structure of the circled part A.
[0011] Figure 3 Shown as an optional embodiment Figure 1 Schematic diagram of the structure of the circled part A.
[0012] Figure 4 Display as Figure 1 Schematic diagram of the concentration distribution of different elements in each layer of the epitaxial structure.
[0013] Figure 5 Shown is a schematic diagram of the concentration distribution of different elements in each layer of the epitaxial structure in an optional embodiment.
[0014] Figure 6 Shown is a schematic diagram of a light-emitting device provided in the second embodiment of the present application.
[0015] Component number description
[0016] 100, light-emitting element; 110, substrate; 120, epitaxial structure; 121, first semiconductor layer structure; 122, active layer; 1221, barrier layer; 1222, well layer; 123, second semiconductor layer structure; 1231, first layer structure; 1232, second layer structure; 130, protective layer; 140, first electrode; 150, second electrode; 200, light-emitting device; 201, circuit substrate; 202, light-emitting element. DETAILED DESCRIPTION
[0017] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.
[0018] The composition of each layer included in the present application can be analyzed by any suitable method, such as secondary ion mass spectrometry (SIMS); the thickness of each layer can be analyzed by any suitable method, such as transmission electron microscopy (TEM) or scanning electron microscopy (SEM), to match the depth position of each layer on the SIMS map.
[0019] According to one embodiment of the present application, a semiconductor light emitting element is provided, which includes at least an epitaxial structure, wherein the epitaxial structure includes at least a first semiconductor layer structure, an active layer and a second semiconductor layer structure stacked from bottom to top, wherein the active layer includes Al y Ga 1-y N barrier layer and Al x Ga 1-x N potential well layer, wherein 0<x<1, 0<y<1, the second semiconductor layer structure includes Al a Ga 1-a N material layer, wherein 0<a<1.
[0020] As mentioned above, the second semiconductor layer structure in the epitaxial structure is used as a P-type layer, and Al a Ga 1-a The N material layer reduces the light absorption of the P-type layer and improves the light emitting effect of the light emitting element.
[0021] Optionally, the second semiconductor layer structure is a P-type doped layer, wherein the concentration of the P-type dopant is greater than 1×10 17 atom / cm 3 .
[0022] Optionally, the thickness of the second semiconductor layer structure is less than or equal to 200 nm.
[0023] Optionally, the Al a Ga 1-a The thickness of the N material layer is less than or equal to 200 nm.
[0024] By controlling the doping concentration of the P-type dopant in the second semiconductor layer structure and the Al a Ga 1-aThe thickness of the N material layer and the second semiconductor layer structure can not only provide sufficient holes for recombination, but also ensure that the P-type dopants therein will not diffuse into the active layer, thereby reducing the damage to the active layer and ensuring the electron-hole recombination efficiency.
[0025] Optionally, the Al a Ga 1-a The thickness of the N material layer accounts for 60%-100% of the thickness of the second semiconductor layer structure.
[0026] By controlling the Al content in the second semiconductor layer a Ga 1-a The thickness ratio of the N material layer is to reduce the p-type gallium nitride material as much as possible, thereby reducing the absorption of light by the p-type gallium nitride material, thereby improving the light extraction efficiency of the light-emitting element.
[0027] Optionally, the second semiconductor layer structure may include a nitride material layer that does not contain Al, and the thickness of the nitride material layer that does not contain Al is less than or equal to 10 nm.
[0028] Optionally, the thickness of the Al-free nitride material layer is less than or equal to 5 nm. Optionally, in the Al-free nitride material layer, the concentration of the P-type dopant is greater than 5×10 17 atom / cm 3 .
[0029] Optionally, the Al-free nitride material layer is located on the Al a Ga 1-a N material layer.
[0030] The second semiconductor layer structure may include a nitride material layer not containing Al formed on the Al a Ga 1-a The thickness of the nitride material layer not containing Al in the second semiconductor layer structure is controlled on the N material layer, such as the GaN material layer or the InGaN material layer. The ohmic contact layer formed by the nitride material layer not containing Al can, on the one hand, still ensure good ohmic contact capability; on the other hand, it can also reduce the p-type gallium nitride material as much as possible, thereby reducing the absorption of light and improving the light extraction efficiency.
[0031] Optionally, the Al a Ga 1-a The thickness of the N material layer is greater than the thickness of the nitride material layer not containing Al.
[0032] Optionally, the Al a Ga 1-a The thickness of the N material layer is at least twice the thickness of the Al-free nitride material layer.
[0033] As described above, the present application strictly controls the occupancy rate of the Al-free gallium nitride material layer in the second semiconductor layer structure by controlling the position and thickness of the Al-free gallium nitride material layer, thereby ensuring that it does not produce obvious light absorption and ensuring the light emitting effect of the light emitting element.
[0034] Optionally, the quantum well of the active layer is a material layer that does not contain In.
[0035] Optionally, the light emission wavelength of the active layer is between 220nm and 410nm.
[0036] Optionally, the light emission wavelength of the active layer is between 240nm and 370nm.
[0037] Since p-type gallium nitride materials absorb light significantly in the ultraviolet wavelength range of light-emitting diodes, especially in the wavelength range below 370nm, the light extraction efficiency of the light-emitting element is seriously affected. Therefore, in ultraviolet light-emitting diodes radiating the above wavelength range, by increasing the Al content in the second semiconductor layer structure, a Ga 1-a The proportion of N material layer can effectively reduce the absorption of light and improve the light output efficiency.
[0038] According to another embodiment of the present invention, a light emitting device is provided, which includes the semiconductor light emitting element of the present invention. The light emitting device includes the light emitting element of the present application, and thus has good light emitting effect and reliability.
[0039] Embodiment 1
[0040] This embodiment provides a semiconductor light emitting element (also called LED, light emitting diode), such as Figure 1 As shown, the light emitting element 100 includes at least an epitaxial structure 120, and the epitaxial structure 120 includes at least a first semiconductor layer structure 121, an active layer 122 and a second semiconductor layer structure 123 stacked in sequence from bottom to top. The epitaxial structure 120 can be any epitaxial structure that can radiate light under the action of voltage, for example, it can be an AlGaInN-based epitaxial structure, an AlGaN-based epitaxial structure or an AlGaInP-based epitaxial structure. In this embodiment, the epitaxial structure 120 is an AlGaN-based epitaxial structure that can provide ultraviolet light. Optionally, the light emitting element 100 can be a light emitting element of a face-up, flip-down or vertical structure. In this embodiment, a light emitting element of a flip-down structure is used as an example for description.
[0041] The first semiconductor layer structure 121 may be an N-type layer, and correspondingly, the second semiconductor layer structure 123 may be a P-type layer, or vice versa. This embodiment takes the first semiconductor layer structure 121 as an N-type layer, and correspondingly, the second semiconductor layer structure 123 as a P-type layer as an example.
[0042] In this embodiment, the N-type semiconductor layer is an N-type AlGaN layer, which is used to provide electrons and serves as an ohmic contact layer when the first electrode 140 is subsequently formed. The N-type AlGaN layer provides electrons by doping with n-type impurities, and the n-type impurities may be, for example, Si, Ge, Sn, Se, and Te. In this embodiment, the n-type impurity is preferably Si. The thickness of the N-type AlGaN layer is about 1 μm to 4 μm, and the Si doping concentration is 5×10 18 atoms / cm 3 ~2×10 20 atoms / cm 3 The N-type AlGaN layer is the layer with the highest N-type doping concentration in the epitaxial structure 120, and the N-type AlGaN layer can be a single layer structure or a super lattice structure. The N-type AlGaN layer is formed as a highly doped layer, which can reduce the contact resistance.
[0043] like Figure 1 As shown, an active layer 122 is formed on the first semiconductor layer structure 121. The active layer 122 is a region that provides light radiation for the recombination of electrons and holes. Different materials can be selected according to different luminescent wavelengths. The active layer 122 can be a periodic structure of a single quantum well or multiple quantum wells composed of a quantum well layer 1222 and a barrier layer 1221. By adjusting the composition ratio of the semiconductor material in the active layer 122, it is expected to radiate light of different wavelengths. In some embodiments, the active layer 122 is a material layer that does not contain In, for example, it can be an AlGaN / AlGaN multiple quantum well with 5 to 15 periods. Furthermore, the active layer 122 can be doped with Si, and the doping concentration of Si is between 1×10 17 Atoms / cm 3 ~1×10 19 Atoms / cm 3 .
[0044] In this embodiment, Figure 2 As shown, preferably, the active layer 122 includes p Al y Ga 1-y N barrier layer 1221 and q Al x Ga 1-x N potential well layer 1222, Al y Ga 1-y N barrier layer 1221 and Al x Ga 1-xThe N potential well layers 1222 are arranged alternately, wherein 0<x<1, 0<y<1, 1≤p≤20, 1≤q≤20, the values of p and q can be the same or different, and the barrier layer 1221 has a larger band gap than the potential well layer 1222. The barrier layer 1221 and the potential well layer 1222 in the active layer 122 are arranged alternately, which can realize the recombination of electrons and holes in the active layer 122, Al y Ga 1-y N barrier layer 1221 and Al x Ga 1-x The alternating arrangement of the N potential well layers 1222 can ensure that the light radiated after the recombination of electrons and holes is ultraviolet light with a wavelength of about 220nm to 410nm. In addition, the barrier layer 1221 and the potential well layer 1222 in the active layer 122 of the present application are both AlGaN material layers, and the lattice constants of the two are similar, the crystal growth quality is good, and there are few dislocations or micro-pit defects in the active layer 122, which is also beneficial to prevent Mg atoms from diffusing into the active layer 122. In an optional embodiment, the Al content in the active layer 122 is controlled to be above 30%, and further, above 50%. The control of the Al content and the selection of the constituent materials of the active layer 122 can ensure the effective recombination of electrons and holes in the active layer 122, ensure the luminous effect of the ultraviolet light-emitting diode, and make the active layer 122 radiate ultraviolet light with a wavelength of about 300nm. Optionally, the wavelength of the light radiated by the active layer 122 is between 220 nm and 410 nm, and further, the wavelength is between 240 nm and 370 nm.
[0045] Refer again Figure 1 In this embodiment, the second semiconductor layer structure 123 is a P-type layer, and holes are provided by doping P-type impurities, and the P-type impurities can be Mg, Zn, Ca, Sr and Ba. In this embodiment, the P-type impurity is preferably Mg. In an optional embodiment, the second semiconductor layer structure 123 includes an Al-containing gallium nitride material layer, and the thickness H of the second semiconductor layer structure 123 is less than or equal to 200nm, and further, H≤100nm. The thickness of the Al-containing gallium nitride material layer accounts for 60% to 100% of the thickness of the second semiconductor layer structure 123, and further, 70% to 100%, 80% to 100%, 90% to 100%, 95% to 100%. The thickness setting of the second semiconductor layer structure 123 and the thickness ratio setting of the gallium nitride material layer without Al can reduce the p-type gallium nitride material as much as possible, which can effectively reduce the light absorption phenomenon of the P-type gallium nitride material, thereby improving the light extraction efficiency of the light-emitting element. The doping concentration of Mg in the second semiconductor layer structure 123 is greater than or equal to 1×10 17 atom / cm 3 , further, the Mg doping concentration is greater than or equal to 1×10 17 atom / cm 3and less than or equal to 1×10 21 atom / cm 3 .
[0046] In an optional embodiment of this embodiment, the second semiconductor layer structure 123 is a single material layer structure, that is, Figure 2 As shown, the second semiconductor layer structure 123 includes a first layer structure 1231, and the first layer structure 1231 is Al a Ga 1-a N material layer, 0<a<1. In this embodiment, the thickness H1 of the first layer structure 1231 is less than or equal to 200nm. a Ga 1-a The first layer structure 1231 formed by the N material layer, namely Al a Ga 1-a The thickness H1 of the N material layer 1231 accounts for 100% of the thickness H of the second semiconductor layer 123, so there is basically no light absorption phenomenon, which is beneficial to improving the light extraction efficiency of the light-emitting element. In addition, the above-mentioned first layer structure 1231 is formed above the active layer 122 and is arranged adjacent to the active layer 122. Since the first layer structure 1231 is a material layer containing Al, it can play a role in blocking electrons from entering the second semiconductor layer structure 123 to a certain extent. Therefore, the electron blocking layer may not be separately provided in the epitaxial structure 120 of the light-emitting element of this embodiment, which reduces the thickness of the epitaxial structure to a certain extent and reduces the light absorption phenomenon.
[0047] In another optional embodiment of the present application, the second semiconductor layer structure 123 is a multilayer structure formed of different materials, optionally, such as Figure 3 As shown, a second layer structure 1232 may also be included, and the second layer structure 1232 is a nitride material layer that does not contain Al. The nitride material layer that does not contain Al may be a GaN material layer or an InGaN material layer, but the embodiment of the present invention is not limited thereto. The second layer structure 1232 is located above the first layer structure 1231, that is, the second layer structure 1232 is located on the side of the first layer structure 1231 away from the active layer 122. In the second layer structure 1232, the doping concentration of the P-type dopant is greater than 5×10 17 atom / cm 3 .
[0048] In this optional embodiment, in order to minimize the light absorption phenomenon of the above-mentioned second layer structure 1232 that does not contain Al, the thickness H2 of the above-mentioned second layer structure 1232 is controlled to be smaller than the thickness H1 of the first layer structure 1231, and H1≥2H2, further, H1≥3H2, H1≥4H2 or H1≥9H2. Further, the thickness H2 of the second layer structure 1232 is controlled to be less than or equal to 10nm, and further, H2 is less than or equal to 5nm. The second layer structure 132 is a material layer that does not contain Al, which can enable the subsequently formed metal electrode to form a good ohmic contact with the second semiconductor layer structure 123, thereby ensuring the electrical performance of the light-emitting element; at the same time, through the above-mentioned control of the thickness of the second layer structure 1232, its light absorption phenomenon is greatly reduced, and the light output rate of the light-emitting element is improved.
[0049] The P-type dopant in the second semiconductor layer structure 123 having the above structural features of this embodiment can have a variety of different diffusion forms. Figure 4 As shown, in an optional embodiment, the position of the depth of the horizontal axis in the figure is 0 μm as the reference point, that is, the upper surface of the second semiconductor layer structure 123 of the epitaxial structure 120 is used as the reference point, and the thickness of the second semiconductor layer structure 123 is within the range of 0nm to 60nm from the reference point, more specifically, within the range of 0nm to 55nm. The thickness of the active layer 122 is within the range of 50nm to 130nm from the reference point, more specifically, within the range of 55nm to 125nm. Within the above-mentioned depth range of the second semiconductor layer structure 123, along the diffusion direction of the P-type dopant, the concentration of the P-type dopant shows a trend of first decreasing and then increasing. The concentration of the P-type dopant first forms a first sudden drop zone L1, a slow rise zone L2 is formed at the rear end of the first sudden drop zone L1, and a steep rise zone L3 is formed at the rear end of the slow rise zone L2. The thickness of the first sudden drop zone L1 ranges from 0 to 20 nm, the thickness of the slow drop zone L2 ranges from 15 nm to 45 nm, and the thickness of the steep rise zone L3 ranges from 40 nm to 55 nm. In the first sudden drop zone L1, the concentration of the P-type dopant is between 1×10 17 atom / cm 3 ~1×10 21 atom / cm 3 , that is, the concentration of P-type dopants is from 1×10 21 atom / cm 3 It dropped to 1×10 17 atom / cm 3 After the first sudden drop zone L1, the P-type dopant shows a slow rising trend, forming a slow drop zone L2. In the slow drop zone L2, the concentration of the P-type dopant is between 1×10 17 atom / cm 3 ~1×10 18 atom / cm 3, that is, the concentration of P-type dopants is from 1×10 17 atom / cm 3 Slowly increase to 1×10 18 atom / cm 3 A concentration trough of the P-type dopant is formed between the first sudden drop region L1 and the slow rise region L2. The concentration trough is formed at a depth of 15nm to 25nm in the second semiconductor layer structure. Then the concentration rises rapidly to form a steep rise region L3. In the steep rise region L3, the concentration of the P-type dopant is between 5×10 17 atom / cm 3 ~1×10 19 atom / cm 3 , that is, the concentration of P-type dopants is from 5×10 17 atom / cm 3 Rapidly rise to 1×10 19 atom / cm 3 After the steep rise region L3, the Mg atoms enter the depth range of the active layer 122. Figure 4 As shown in FIG. 1 , the concentration of Mg atoms drops sharply to form a second sudden drop region L4. The Mg atomic concentration drop slope of the second sudden drop region L4 is greater than the Mg atomic concentration drop slope of the first sudden drop region L1 in the second semiconductor layer structure 123. In the second sudden drop region L4, the concentration of P-type dopants (Mg atoms) is between 1×10 16 atom / cm 3 ~1×10 19 atom / cm 3 , that is, the concentration of P-type dopants is from 1×10 19 atom / cm 3 Rapidly dropped to 1×10 16 atom / cm 3 , that is, the active layer 122 behind the second semiconductor layer structure 123 contains almost no diffused P-type dopants, such as Mg atoms.
[0050] The concentration control of the P-type dopant in the second semiconductor layer structure 123 can ensure that there are sufficient P-type dopants in the second semiconductor layer structure 123, ensuring sufficient hole supply. At the same time, it is ensured that there are almost no Mg atoms in the above-mentioned depth range of the active layer 122, reducing damage to the active layer and ensuring the recombination efficiency of electrons and holes.
[0051] In another optional embodiment of this embodiment, if Figure 5As shown, the position with a depth of 0 μm on the horizontal axis in the figure is used as the reference point, that is, the upper surface of the second semiconductor layer structure 123 of the epitaxial structure 120 is used as the reference point. The thickness of the second semiconductor layer structure 123 is in the range of 0 nm to 80 nm from the reference point, more specifically, in the range of 0 nm to 70 nm. The thickness of the active layer 122 is in the range of 60 nm to 130 nm from the reference point, more specifically, in the range of 65 nm to 120 nm. Within the above-mentioned depth range of the second semiconductor layer structure 123, along the diffusion direction of the P-type dopant, the concentration of the P-type dopant forms a third sudden drop zone L5, and a slow drop zone L6 is formed at the rear end of the third sudden drop zone L5. In the third sudden drop zone L5, the concentration of the P-type dopant is between 1×10 19 atom / cm 3 ~1×10 21 atom / cm 3 That is, in the third sudden drop region L5, the concentration of P-type dopants is from 1×10 21 atom / cm 3 Rapidly dropped to 1×10 19 atom / cm 3 In the slow-down zone L6, the concentration of P-type dopants is between 1×10 18 atom / cm 3 ~1×10 19 atom / cm 3 That is, in the slow-down zone L6, the concentration of P-type dopants increases from 1×10 19 atom / cm 3 Slowly decrease to 1×10 18 atom / cm 3 . Also refer to Figure 5 The third sudden drop region L5 is formed in the thickness range of 0 to 10 nm of the second semiconductor layer structure 123 , and the gradual drop region L6 is formed in the thickness range of 10 to 50 nm of the second semiconductor layer structure 123 .
[0052] In this optional embodiment, after the above-mentioned slow-down zone L6, the concentration of the P-type dopant forms a fourth sudden-down zone L7 and a buffer zone L8 located after the fourth sudden-down zone L7. Figure 5 It can be seen that the concentration decrease slope of the P-type dopant in the fourth sudden drop region L7 is greater than the concentration decrease slope in the third sudden drop region L5. Specifically, in the fourth sudden drop region L7, the concentration of the P-type dopant is between 1×10 16 atom / cm 3 ~5×10 18 atom / cm 3 That is, in the fourth sudden drop region L7, the concentration of P-type dopants is from 5×10 18 atom / cm 3 It dropped to 1×1016 atom / cm 3 In the buffer zone L8, the concentration of P-type dopants is between 1×10 16 atom / cm 3 ~5×10 17 atom / cm 3 , that is, in the buffer zone L8, the concentration of P-type dopants is from 5×10 17 atom / cm 3 Slowly decrease to 1×10 16 atom / cm 3 .
[0053] As described above, by controlling the above-mentioned diffusion characteristics of Mg atoms in the second semiconductor layer structure 123, it is ensured that the active layer 122 after the second semiconductor layer structure 123 contains almost no diffused P-type dopants, which effectively reduces the influence of Mg atoms on MQW and improves the quality of MQW. Therefore, the recombination efficiency of electrons and holes in the active layer 123 is guaranteed, which is beneficial to improving the luminous efficiency.
[0054] Likewise Figure 1 As shown, the light emitting element 100 further includes a protective layer 130 formed on the surface of the epitaxial structure 120, the protective layer 130 covers the upper surface of the epitaxial structure 120, and optionally covers the sidewalls of the epitaxial structure 120 at the same time, so as to protect the epitaxial structure 120 from damage by impurities such as water vapor and dust. An electrode structure is also formed above the epitaxial structure 120, and the protective layer 130 covers the sidewalls of the electrode structure at the same time, or covers part of the upper surface of the electrode structure at the same time, so as to protect the electrode structure while exposing the upper surface of the electrode structure to realize the subsequent welding of the light emitting element 100. Figure 1 As shown, the electrode structure includes a first electrode 140 and a second electrode 150. The first electrode 140 is electrically connected to the first semiconductor layer structure 121, for example, forming an ohmic contact with the N-type AlGaN layer, and the second electrode 150 is electrically connected to the second semiconductor layer structure 123, for example, electrically connected to the second semiconductor layer structure 123 through an ohmic contact layer 1231.
[0055] Refer again Figure 1, the light emitting element 100 of this embodiment may also include a substrate 110, and the epitaxial structure 120 is located above the substrate. The epitaxial structure 120 may be formed by growing directly from the substrate 110, or may be transferred to the top of the substrate after growing on the growth substrate. The above-mentioned substrate 110 may be an insulating substrate or a conductive substrate. In an optional embodiment, the substrate 110 is a growth substrate for epitaxial growth of a semiconductor epitaxial stack, including sapphire (Al2O3), SiC substrate, Si substrate, etc. The substrate 110 includes a first surface and a second surface arranged opposite to each other. The substrate 110 is a patterned substrate having a micro-pattern on the first surface, and the patterned substrate is conducive to the growth of the epitaxial structure 120, and can reduce the number of dislocations in the epitaxial structure 120, and improve the crystal quality of the epitaxial structure 120.
[0056] In an optional embodiment of this embodiment, the first semiconductor layer structure 121 may also include a bottom layer located between the N-type AlGaN layer and the substrate, the bottom layer including a u-type AlN layer and a u-type AlGaN layer, the AlN layer and the AlGaN layer can effectively relieve the stress generated when growing the above-mentioned N-type AlGaN layer, which is conducive to obtaining a high-crystal quality epitaxial structure 120. It can be understood that in order to realize the flip-chip light-emitting diode of this embodiment to emit light from the substrate side, a reflective structure, such as a DBR structure, is also formed on one side of the P-type semiconductor layer. The above-mentioned protective layer 130 can also be a reflective insulating material layer.
[0057] Embodiment 2
[0058] This embodiment provides a light emitting device, such as Figure 6 As shown, the light emitting device 200 includes a substrate 201 and a light emitting element 202 disposed on the substrate 201, wherein the light emitting element 202 may be the light emitting element provided in the first embodiment of the present application. The substrate 201 may be a packaging substrate or a circuit substrate connected to an external power supply. The light emitting device 200 may be formed as a sterilization and disinfection device.
[0059] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.
Claims
1. A semiconductor light emitting element, characterized in that: The semiconductor light emitting element comprises at least one epitaxial structure, and the epitaxial structure comprises at least a first semiconductor layer structure, an active layer and a second semiconductor layer structure stacked from bottom to top, wherein the active layer comprises Al y Ga 1-y N barrier layer and Al x Ga 1-x N potential well layer, wherein 0<x<1, 0<y<1, the second semiconductor layer structure includes Al a Ga 1-a N material layer, wherein 0<a<1.
2. The semiconductor light emitting element according to claim 1, characterized in that The second semiconductor layer structure is a P-type doped layer, wherein the concentration of the P-type dopant is greater than 1×10 17 atom / cm 3 .
3. The semiconductor light emitting element according to claim 1, characterized in that The thickness of the second semiconductor layer structure is less than or equal to 200 nm.
4. The semiconductor light emitting element according to claim 1, characterized in that The Al a Ga 1-a The thickness of the N material layer is less than or equal to 200 nm.
5. The semiconductor light emitting element according to claim 1, characterized in that The Al a Ga 1-a The thickness of the N material layer accounts for 60%-100% of the thickness of the second semiconductor layer structure.
6. The semiconductor light emitting element according to claim 1, characterized in that The second semiconductor layer structure may include a nitride material layer not containing Al, and a thickness of the nitride material layer not containing Al is less than or equal to 10 nm.
7. The semiconductor light emitting element according to claim 6, characterized in that: The thickness of the nitride material layer not containing Al is less than or equal to 5 nm.
8. The semiconductor light emitting element according to claim 6, characterized in that In the Al-free nitride material layer, the concentration of the P-type dopant is greater than 5×10 17 atom / cm 3 .
9. The semiconductor light emitting element according to claim 6, characterized in that: The Al-free nitride material layer is located on the Al a Ga 1-a N material layer.
10. The semiconductor light emitting element according to claim 6, characterized in that The Al a Ga 1-a The thickness of the N material layer is greater than the thickness of the nitride material layer not containing Al.
11. The semiconductor light emitting element according to claim 6, characterized in that: The Al a Ga 1-a The thickness of the N material layer is at least twice the thickness of the Al-free nitride material layer.
12. The semiconductor light emitting element according to claim 1, characterized in that The quantum well of the active layer is a material layer that does not contain In.
13. The semiconductor light emitting element according to claim 1, characterized in that The P-type dopant is magnesium atoms.
14. The semiconductor light emitting element according to claim 1, characterized in that: The light emission wavelength of the active layer is between 220nm and 410nm.
15. The semiconductor light emitting element according to claim 1, characterized in that: The light emission wavelength of the active layer is between 240nm and 370nm.
16. A light emitting device, characterized in that: The invention comprises a circuit substrate and a light emitting element arranged on the circuit substrate, wherein the light emitting element comprises the semiconductor light emitting element according to any one of claims 1 to 15.
Citation Information
Patent Citations
UV-LED with quantum dot p-region structure
CN105355736A
Group iii nitride semiconductor light emitting element and method for producing same
CN110462851A
Deep ultraviolet LED with gradient transparent electrode contact layer and preparation method thereof
CN115377269A
Ultraviolet light emitting diode and preparation method thereof
CN116053370A
Semiconductor light-emitting element and light-emitting device
CN116565084A