Electronic equipment manufacturing method, electronic equipment and wireless charging system
By embedding magnets in the housing of the electronic device and using the transition layer and contact section for magnetization, the problem of increasing the thickness of the entire machine caused by the introduction of magnets is solved, and the thinning and portability of the electronic device is improved, while enhancing magnetic fixation Effect.
Patent Information
- Application Number
- CN202310636251.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-31
- Publication Date
- 2024-12-03
AI Technical Summary
When existing electronic devices introduce magnets to achieve magnetic suction connections, they lead to an increase in the thickness of the entire machine stack, reducing user experience and portability.
By providing a magnet on the housing of the electronic device and embedding it at least partially within the housing, or opening a groove on the housing and embedding the magnet portion therein, a combination of isotropic or pre-oriented transition layer and contact section, Magnetization is carried out to achieve magnetic fixation, while optimizing the connection structure between the magnet and the housing to reduce the overall thickness.
It effectively reduces the stacking thickness of electronic devices, realizes a thin and light design, improves portability, and enhances the magnetic absorption fixation strength, reducing interference from magnetic leakage to circuits and components.
Smart Images

Figure CN119072040A_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to the field of magnetic attraction technology, and in particular, to an electronic device manufacturing method, an electronic device and a wireless charging system. Background Art
[0002] Wireless charging technology is a charging technology that transmits energy between the charger and the power device through a magnetic field. Because it gets rid of the connection of wires, it greatly improves the convenience of user operation. At present, in order to ensure the fixing effect, the charger and the power device are connected and fixed by magnetic attraction.
[0003] Taking mobile phones and other electrical devices as an example, magnets need to be introduced into the stacking of the whole device to achieve magnetic adsorption with the TX end of the charger. However, the introduction of magnets in the mobile phone will increase the stacking thickness of the whole device, thereby reducing the user experience. Summary of the invention
[0004] The present disclosure aims to solve one of the technical problems in the related art at least to some extent.
[0005] The disclosed embodiment provides a method for manufacturing an electronic device, which can reduce the stacking thickness of the electronic device, thereby facilitating the electronic device to be made thinner and lighter.
[0006] The disclosed embodiment also provides an electronic device.
[0007] The disclosed embodiment also provides a wireless charging system.
[0008] In a first aspect, a method for manufacturing an electronic device according to an embodiment of the present disclosure, the electronic device comprises a shell and a magnetic part, and the manufacturing method comprises: arranging a magnet on the shell; and at least partially embedding the magnetic part into the shell.
[0009] The electronic device manufacturing method of the disclosed embodiment can reduce the stacking thickness of the electronic device, which is conducive to making the electronic device lighter and thinner.
[0010] In some embodiments, the method further includes: opening a groove on the shell; and embedding the magnet portion at least partially into the groove.
[0011] In some embodiments, the method further includes: disposing a transition layer in the groove and / or outside the magnet portion, the transition layer being an isotropic magnetic transition layer or the transition layer being a pre-oriented anisotropic transition layer; and magnetizing the transition layer and / or the magnet portion.
[0012] In some embodiments, the isotropic magnetic transition layer includes a binder and magnetic powder, the binder is a thermoplastic resin and / or nylon, and the magnetic powder is neodymium iron boron and / or ferrite.
[0013] In some embodiments, the mass percentage of the binder is 5% to 20%, and the mass percentage of the magnetic powder is 80% to 95%.
[0014] In some embodiments, the method further includes: integrally forming the magnet portion and the shell.
[0015] In some embodiments, the magnetic portion is an isotropic magnet / a pre-oriented anisotropic magnet; the magnetic portion has a contact segment, and the contact segment is used to contact with a charging device to magnetize the shell and / or the contact segment.
[0016] In some embodiments, the magnetism in the contact section is greater than the magnetism in other parts of the housing.
[0017] In some embodiments, the magnet portion includes a binder and magnetic powder, the binder is a thermoplastic resin and / or nylon, and the magnetic powder is neodymium iron boron and / or ferrite.
[0018] In some embodiments, the magnetic powder content in the contact section is greater than the magnetic powder content in other parts of the shell.
[0019] In a second aspect, an electronic device according to an embodiment of the present disclosure is an electronic device prepared by any of the electronic device manufacturing methods described above, and comprises: a housing; and a magnetic portion, wherein the magnetic portion is at least partially embedded in the housing.
[0020] In some embodiments, the electronic device also includes a transition layer, which is arranged between the shell and the magnet, and the transition layer is an isotropic magnetic transition layer / pre-oriented anisotropic magnetic transition layer, and the transition layer has a first surface and a second surface in the thickness direction of the shell, and the first surface is arranged adjacent to the shell relative to the second surface. The transition has an S pole and an N pole, and is bent or bent in the magnetization direction from the S pole to the N pole and protrudes toward the second surface.
[0021] In some embodiments, the magnetization direction from the S pole to the N pole is an arc, and the curvature of the magnetization direction first decreases and then increases along the direction from the S pole to the N pole.
[0022] In a third aspect, the charging system of the embodiment of the present disclosure includes an electronic device and a charging device that can be magnetically fixed, the electronic device is the electronic device described in any one of the above embodiments, the charging device includes a second magnet, the electronic device and the charging device are magnetically fixed through the magnetic attraction of the magnetic part and the second magnet, or the electronic device and the charging device are magnetically fixed through the contact section on the magnetic part and the magnetic attraction of the second magnet. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 It is a flowchart of the method for manufacturing an electronic device according to an embodiment of the present disclosure.
[0024] Figure 2 It is a flowchart of a method for manufacturing an electronic device according to another embodiment of the present disclosure.
[0025] Figure 3 It is a flowchart of a method for manufacturing an electronic device according to another embodiment of the present disclosure.
[0026] Figure 4 It is a flowchart of a method for manufacturing an electronic device according to another embodiment of the present disclosure.
[0027] Figure 5 is a cross-sectional view of an electronic device in the related art.
[0028] Figure 6 It is a cross-sectional view of a charging system in the related art.
[0029] Figure 7 is a cross-sectional view of an electronic device according to an embodiment of the present disclosure.
[0030] Figure 8 is a cross-sectional view of an electronic device according to another embodiment of the present disclosure.
[0031] Fig. 9 is a cross-sectional view of a charging system according to an embodiment of the present disclosure.
[0032] Fig.10 is a cross-sectional view of a charging system according to another embodiment of the present disclosure.
[0033] Reference numerals:
[0034] Electronic device 100, charging device 200,
[0035] Shell 1 , magnet portion 2 , contact section 21 , transition layer 3 , first surface 31 , second surface 32 , magnetic flux lines 4 , second magnet 5 . DETAILED DESCRIPTION
[0036] Embodiments of the present disclosure are described in detail below, and examples of the embodiments are shown in the accompanying drawings. The embodiments described below with reference to the accompanying drawings are exemplary and are intended to be used to explain the present disclosure, but should not be understood as limiting the present disclosure.
[0037] First, as Figure 1 As shown, the electronic device manufacturing method of the embodiment of the present disclosure,
[0038] S101 . Set the magnet part 2 on the housing 1 .
[0039] It should be noted that the magnet part 2 and the shell 1 can be integrally formed or separately formed. When the magnet part 2 and the shell 1 are separately formed, the magnet part 2 and the shell 1 can be connected by bonding, clamping or bolting.
[0040] S102 , embedding the magnet portion 2 at least partially into the housing 1 .
[0041] It should be noted that the magnet portion 2 may be partially embedded in the housing 1 , or the magnet portion 2 may be completely embedded in the housing 1 .
[0042] The electronic device manufacturing method of the disclosed embodiment embeds the magnetic part 2 into the shell 1. On the one hand, the magnetic part 2 and the shell 1 can overlap in the thickness direction of the shell 1, thereby reducing the overall thickness and reducing the distance between the magnetic part 2 and the magnetic attraction component in the charging device 200, thereby reducing the magnetic resistance and enhancing the strength of the magnetic attraction fixation. On the other hand, the reduction in thickness can reduce the overall volume of the electronic device 100, thereby facilitating the thin and light design of the electronic device 100 and improving portability.
[0043] In some embodiments, Figure 2 As shown, the electronic device manufacturing method further includes:
[0044] S201 , forming a groove on the housing 1 .
[0045] It should be noted that a groove is provided on the inner side of the shell 1 , the depth of the groove is less than the thickness of the shell 1 , and the groove may be an annular groove, or there may be multiple grooves which are distributed in an annular shape.
[0046] S202, embedding the magnet part 2 at least partially into the groove.
[0047] For example, the magnet portion 2 may be partially embedded in the groove, or the magnet portion 2 may be fully embedded in the groove.
[0048] The electronic device manufacturing method of the disclosed embodiment can also enhance the fixing effect of the magnet part 2 by means of the stopping and limiting of the groove.
[0049] In some embodiments, Figure 3 As shown, the electronic device manufacturing method further includes:
[0050] S301 , a transition layer 3 is arranged in the groove and / or outside the magnet part 2 , wherein the transition layer 3 is an isotropic magnetic transition layer.
[0051] It should be noted that a transition layer 3 is provided at the bottom of the groove, or a transition layer 3 is provided on the side of the magnet part 2 facing the housing 1, or a transition layer 3 is provided at the bottom of the groove and on the side of the magnet part 2 facing the housing 1. For example, the transition layer 3 can be integrally formed with the housing 1, or the transition layer 3 can be integrally formed with the magnet part 2.
[0052] Alternatively, the transition layer 3 is a pre-oriented anisotropic magnetic transition layer 3. In other words, the transition layer 3 is made of a pre-oriented anisotropic magnetic material.
[0053] It should be noted that the magnet part 2 can be an isotropic magnet, which is a magnet with the same magnetic properties in any direction, for example, the magnet part 2 is bonded NdFeB or bonded ferrite or other magnetic materials. Alternatively, the magnet part 2 is also an anisotropic magnet, which is a magnet with different magnetic properties in different directions, for example, the magnet part 2 is sintered NdFeB or sintered ferrite.
[0054] S302, the transition layer 3 and / or the magnetic body part 2 are magnetized.
[0055] It should be noted that the transition layer 3 and / or the magnet part 2 may be magnetized first and then embedded into the shell 1, or the transition layer 3 and / or the magnet part 2 may be embedded into the shell 1 first and then magnetized.
[0056] For example, a groove is formed on the shell, and then the magnet part 2 and / or transition layer 3 made of isotropic bonded magnetic material which are not magnetized are embedded, and the magnet part 2 and / or transition layer 3 which have been embedded are magnetized.
[0057] Alternatively, a groove is firstly made on the shell, and then the magnet part 2 and / or the transition layer 3 are magnetized, and finally the magnetized magnet part 2 and / or the transition layer 3 are embedded into the groove on the shell.
[0058] Alternatively, when the magnet portion 2 and / or the transition layer 3 is a pre-oriented anisotropic magnetic material.
[0059] A groove may be firstly formed on the shell 1, and then an anisotropic bonded magnet with a bent orientation may be manufactured using a bent orientation magnetic field. The magnet may then be embedded into the groove on the shell 1, and the pre-oriented magnet may be bent magnetized.
[0060] Alternatively, a groove may be firstly formed on the shell 1, and then an anisotropic bonded magnet with a curved orientation may be manufactured using a curved orientation magnetic field, and then the pre-oriented magnet may be curvedly magnetized to ensure that the magnetization direction of the magnet is curved, and finally the magnetized magnet may be embedded in the groove;
[0061] Alternatively, a groove can be first opened on the shell 1 and used as the position for making the magnet mold. A bending orientation field can be arranged at the position of the mold, and an anisotropic bonded magnet can be injected into the mold at high temperature. When the magnet is cooled to room temperature, the magnet at this position completes the bending orientation, and finally the entire shell with the magnet is bent and magnetized.
[0062] For example, the transition layer 3 is magnetized by an external magnetic field, or the magnet part 2 is magnetized by an external magnetic field, or the transition layer 3 and the magnet part 2 are magnetized simultaneously by an external magnetic field. It should be noted that since the transition layer 3 is an isotropic magnetic material or a pre-oriented anisotropic magnetic material, the required magnetic field can be designed according to the needs and can be magnetized in an oriented direction in any direction. Therefore, the magnetization direction 4 in the transition layer 3 and the magnet part 2 can be designed to be arc-shaped through magnetization design, and the magnetization direction 4 is convex in the direction away from the shell 1. It should be noted that the magnetization design can be adjusted according to actual needs, so as to obtain magnetization directions 4 in different directions in the transition layer 3.
[0063] By providing a transition layer 3 between the magnet part 2 and the shell 1, not only can the magnetic conductivity be improved, the magnetic resistance and magnetic leakage be reduced, but also the connection strength between the magnet part 2 and the shell 1 can be improved, and since the transition layer 3 is provided in the groove, the adverse effect of the strength of the shell 1 caused by the groove on the shell 1 is reduced. In some embodiments, the transition layer 3 includes a binder and magnetic powder, the binder is a thermoplastic resin and / or nylon, and the magnetic powder is neodymium iron boron and / or ferrite.
[0064] It should be noted that the transition layer 3 is made of a bonded magnetic material, and each bonded magnetic material includes a binder and magnetic powder. The binder can be a thermoplastic resin, or the binder is nylon, or the binder is a thermoplastic resin and nylon configured in a certain ratio, for example, the mass ratio of the thermoplastic resin is 50%, the mass ratio of the nylon is 50%, or the mass ratio of the thermoplastic resin is 40%, and the mass ratio of the nylon is 40%. The magnetic powder can be neodymium iron boron, or the magnetic powder is ferrite, or the magnetic powder is a mixture of neodymium iron boron and ferrite in a certain ratio, for example, the magnetic powder includes 50% neodymium iron boron and 50% ferrite, or the magnetic powder includes 40% neodymium iron boron and 60% ferrite.
[0065] In some embodiments, the mass percentage of the binder is 5% to 20%, and the mass percentage of the magnetic powder is 80% to 95%.
[0066] For example, if the mass percentage of the binder is 5%, the mass percentage of the magnetic powder is 95%, or if the mass percentage of the binder is 10%, the mass percentage of the magnetic powder is 90%, or if the mass percentage of the binder is 15%, the mass percentage of the magnetic powder is 85%, or if the mass percentage of the binder is 20%, the mass percentage of the magnetic powder is 80%. It should be noted that when the content of the magnetic powder increases, the magnetism of the transition layer 3 increases, and conversely, when the content of the magnetic powder decreases, the magnetism of the transition layer 3 decreases. For example, the magnetism of the transition layer 3 can be adjusted according to actual needs.
[0067] In some embodiments, Figure 4 As shown, the electronic device manufacturing method further includes:
[0068] S401 , integrally forming the magnet part 2 and the housing 1 .
[0069] In the method for manufacturing an electronic device of the disclosed embodiment, the magnet part 2 is embedded in the housing 1, or the housing 1 is made of magnetic material, and the magnet part 2 does not need to be installed, which can further reduce the overall size thickness, and can make the distance between the magnet part 2 and the magnetic attraction component in the charging device 200 reduce the magnetic resistance and enhance the strength of magnetic attraction fixation. On the other hand, the reduction in thickness can achieve a reduction in the overall volume of the electronic device 100, which is conducive to realizing a lightweight design of the electronic device 100 and improving portability. In addition, the fixing effect of the magnet part 2 can also be enhanced by the stop limit of the assembly groove.
[0070] In some embodiments, Figure 4 As shown, the magnet part is an isotropic magnet, and the electronic device manufacturing method further includes:
[0071] S402 , a contact section 21 is provided on the magnet portion 2 , and the contact section 21 is used for contacting a charging device.
[0072] S403 , magnetizing the housing 1 and / or the contact section 21 .
[0073] It should be noted that the portion of the housing 1 that contacts the charging device 200 is configured as a contact section 21 . For example, the contact section 21 is entirely made of a bonded magnetic material.
[0074] For example, the entire shell 1 is magnetized by an external magnetic field, so that the transition layer 3 and the magnetic part 2 inside the shell 1 are magnetized, or, when the entire shell 1 is made of a bonded magnetic material, the entire shell 1 is magnetized so that the shell 1 has magnetism, or, only the contact section 21 is magnetized so that the transition layer 3 and the magnetic part 2 inside the contact section 21 have magnetism.
[0075] In some embodiments, the magnetic energy in the contact section 21 is greater than the magnetic energy in other parts of the housing 1 .
[0076] For example, when manufacturing the shell 1, the contact segment 21 is manufactured first, and then the other parts of the shell 1 are integrally formed with the contact segment 21. The other parts of the shell 1 can be made completely of non-magnetic materials. In other words, only the contact segment 21 on the shell 1 is magnetic. When the magnetism of the contact segment 21 is greater than the magnetism of other parts of the shell 1, the connection stability between the electronic device 100 and the charging device 200 is guaranteed.
[0077] In some embodiments, the content of magnetic powder in the contact section 21 is greater than the content of magnetic powder in the transition layer 3 at other locations of the housing 1 .
[0078] For example, the content of magnetic powder in the contact section 21 can be 95%, and the content of magnetic powder in the transition layer 3 of other parts of the shell 1 can be 5%. It should be noted that the greater the content of magnetic powder, the greater the magnetism, and vice versa, the smaller the content of magnetic powder, the smaller the magnetism. Alternatively, the content of binder in the contact section 21 is 5%, and the content of binder in the transition layer 3 of other parts of the shell 1 can be 95%. It should be noted that the greater the content of binder, the smaller the magnetism, and vice versa, the greater the magnetism.
[0079] When the contact segment 21 or the entire shell 1 is made of isotropic bonded magnetic material, the contact segment 21 can be prepared first, and then other parts of the shell 1 are manufactured around the contact segment 21, and finally only the contact segment 21 is magnetized.
[0080] Alternatively, the contact segment 21 is made of isotropic bonded magnetic material, and the other parts of the shell 1 are made of non-magnetic material. The contact segment 21 can be prepared first, and then the other parts of the shell 1 are manufactured around the contact segment 21, and finally only the contact segment 21 is magnetized.
[0081] like Figure 5 and Figure 6 As shown, in the electronic device 100 in the related art, the magnets are directly stacked on the inner side of the shell 1, the overall thickness of the shell 1 is relatively large, and the magnets occupy the internal space of the shell 1, occupying the installation space of other components, which is not conducive to the lightweight of the electronic device 100.
[0082] Second, as Figure 6 As shown, the electronic device 100 of the embodiment of the present disclosure includes a housing 1 and a magnetic part 2, wherein the magnetic part 2 is at least partially embedded in the housing 1. In some embodiments, the electronic device further includes a transition layer 3, which is disposed between the housing 1 and the magnetic part 2. The transition layer 3 is an isotropic transition layer 3, and the transition layer 3 has a first surface 31 and a second surface 32 in the thickness direction of the housing 1. The first surface 31 is arranged adjacent to the housing 1 relative to the second surface 32. The transition layer 3 has an S pole and an N pole, and the magnetization direction 4 from the S pole to the N pole is bent or curved and extends and protrudes toward the second surface 32.
[0083] It should be noted that during use, the first surface 31 forms a magnetic working surface, that is, the magnetic flux lines 4 of the magnet part 2 will come out from the N pole and enter the S pole, thereby realizing the magnetic fixation of other components by the magnet part 2. The second surface 32 forms a non-magnetic working surface of the magnet part 2, that is, there are fewer or no magnetic flux lines 4 outside the second surface 32, thereby avoiding magnetic leakage on the non-magnetic working surface.
[0084] The electronic device 100 of the embodiment of the present disclosure designs the magnetization direction 4 to be curved so that the distribution density of the magnetic flux lines 4 on the side of the non-magnetic working surface of the magnetic part 2 is low, thereby reducing the leakage magnetic flux of the magnetic part 2, avoiding the interference of the leakage magnetic flux on the circuits, components, etc., and improving the constraints and restrictions on the placement of the components, circuits, etc. of the electronic device 100 caused by the leakage magnetic flux, thereby reducing the difficulty of the design process.
[0085] Secondly, it also avoids the need to make more avoidance in the internal space of the electronic device 100 and other electrical devices to reduce the impact of magnetic interference, which is beneficial to reducing the overall volume of the electronic device 100 and achieving lightness and thinness, thereby improving the portability of the electronic device 100.
[0086] In some embodiments, the magnetizing direction 4 from the S pole to the N pole is an arc, and the curvature of the magnetizing direction 4 first decreases and then increases along the direction from the S pole to the N pole, that is, the magnetizing direction 4 is along the direction from left to right, and the curvature of the magnetizing direction 4 at the S pole and the N pole is relatively large, while the curvature of the magnetizing direction 4 in the middle (that is, the position adjacent to the second surface 32) is relatively small, thereby ensuring the constraint effect on the magnetizing direction 4 and avoiding magnetic leakage.
[0087] Second, as Fig. 9 and Fig.10 As shown, in the electronic device 100 of the embodiment of the present disclosure, the shell 1 and the magnetic part 2 of the electronic device 100 are integrally formed, which can further reduce the thickness of the electronic device 100. Moreover, since there is no need to install a magnet on the inner side of the shell 1, the interference effect of leakage magnetic field on circuits, components, etc. is further reduced.
[0088] In a third aspect, the charging system of the embodiment of the present disclosure is characterized in that it includes an electronic device 100 and a charging device 200 that can be fixed by magnetic attraction, the electronic device 100 is the electronic device 100 of the second aspect, and the shell 1 and the magnetic part 2 in the electronic device 100 are formed separately, the charging device 200 includes a second magnet, and the electronic device 100 and the charging device 200 are magnetically fixed by the magnetic attraction of the magnetic part 2 and the second magnet.
[0089] It should be noted that the second magnet 5 is installed inside the shell 1 of the charging device 200, and the position of the second magnet 5 corresponds to the position of the magnetic part 2. When the electronic device 100 and the charging device 200 are in contact, the magnetic conductive part 2 and the second magnet 5 are adsorbed to achieve magnetic fixation of the electronic device 100 and the charging device 200.
[0090] Alternatively, the electronic device 100 is the electronic device 100 of any one of the embodiments of the second aspect described above, and the shell 1 and the magnetic part 2 in the electronic device 100 are integrally formed, and the electronic device 100 and the charging device 200 are magnetically fixed by the contact section 21 of the shell 1 and the magnetic attraction of the second magnet.
[0091] It should be noted that, for the electronic device 100 manufactured by the manufacturing method of the second aspect, when the electronic device 100 contacts the charging device 200 , the contact section 21 and the second magnet 5 are attracted to each other to achieve magnetic fixation of the electronic device 100 and the charging device 200 .
[0092] In the description of the present invention, it is to be understood that the terms “center”, “longitudinal”, “lateral”, “length”, “width”, “thickness”, “up”, “down”, “front”, “back”, “left”, “right”, “vertical”, “horizontal”, “top”, “bottom”, “inside”, “outside”, “clockwise”, “counterclockwise”, “axial”, “radial”, “circumferential”, etc., indicating orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the present invention.
[0093] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In the description of the present invention, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.
[0094] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral one; it can be a mechanical connection, an electrical connection, or communication with each other; it can be a direct connection, or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0095] In the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may mean that the first and second features are in direct contact, or the first and second features are in indirect contact through an intermediate medium. Moreover, a first feature being "above", "above" or "above" a second feature may mean that the first feature is directly above or obliquely above the second feature, or simply means that the first feature is higher in level than the second feature. A first feature being "below", "below" or "below" a second feature may mean that the first feature is directly below or obliquely below the second feature, or simply means that the first feature is lower in level than the second feature.
[0096] In the present invention, the terms "one embodiment", "some embodiments", "examples", "specific examples", or "some examples" etc. mean that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the described specific features, structures, materials or characteristics may be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art may combine and combine the different embodiments or examples described in this specification and the features of the different embodiments or examples, without contradiction.
[0097] Although the embodiments of the present invention have been shown and described above, it is to be understood that the above embodiments are exemplary and are not to be construed as limitations of the present invention. A person skilled in the art may change, modify, replace and vary the above embodiments within the scope of the present invention.
Claims
1. A method for manufacturing an electronic device, characterized in that: The electronic device comprises a housing and a magnetic part, and the manufacturing method comprises: A magnet portion is provided on the housing; The magnet portion is at least partially embedded in the housing.
2. The method for manufacturing an electronic device according to claim 1, wherein: The method further comprises: A groove is formed on the housing; The magnet portion is at least partially embedded in the groove.
3. The method for manufacturing an electronic device according to claim 2, wherein: The method further comprises: A transition layer is arranged in the groove and / or outside the magnet part, wherein the transition layer is an isotropic magnetic transition layer or a pre-oriented anisotropic transition layer; The transition layer and / or the magnetic body portion are magnetized.
4. The method for manufacturing an electronic device according to claim 3, wherein: The magnet portion and the transition layer are integrally formed.
5. The method for manufacturing an electronic device according to claim 3, wherein: The isotropic magnetic transition layer comprises a binder and magnetic powder, wherein the binder is a thermoplastic resin and / or nylon, and the magnetic powder is neodymium iron boron and / or ferrite.
6. The method for manufacturing an electronic device according to claim 5, characterized in that: The mass percentage of the binder is 5% to 20%, and the mass percentage of the magnetic powder is 80% to 95%.
7. The method for manufacturing an electronic device according to claim 1, wherein: The method further includes: integrally forming the magnet portion and the housing.
8. The method for manufacturing an electronic device according to claim 7, wherein: The magnet part is an isotropic magnet or a pre-oriented anisotropic magnet; A contact section is provided on the magnetic part, and the contact section is used for contacting a charging device. The method further comprises: magnetizing the housing and / or the contact section.
9. The method for manufacturing an electronic device according to claim 8, characterized in that: The magnetism in the contact section is greater than the magnetism in other parts of the shell.
10. The method for manufacturing an electronic device according to claim 8 or 9, characterized in that: The magnet part includes a binder and magnetic powder, the binder is thermoplastic resin and / or nylon, and the magnetic powder is neodymium iron boron and / or ferrite.
11. The method for manufacturing an electronic device according to claim 10, characterized in that: The content of magnetic powder in the contact section is greater than the content of magnetic powder in other parts of the shell.
12. An electronic device, wherein the electronic device is an electronic device manufactured according to the electronic device manufacturing method according to any one of claims 1 to 6, or the electronic device is an electronic device manufactured according to the electronic device manufacturing method according to any one of claims 7 to 11, characterized in that: include: case; A magnet portion is at least partially embedded in the housing.
13. The electronic device according to claim 12, characterized in that: It also includes a transition layer, which is arranged between the shell and the magnet part. The transition layer is an isotropic magnetic material / pre-oriented anisotropic magnetic material. The transition layer has a first surface and a second surface in the thickness direction of the shell. The first surface is arranged adjacent to the shell relative to the second surface. The transition layer has an S pole and an N pole, and is bent or bent in the magnetization direction from the S pole to the N pole and protrudes toward the second surface.
14. The electronic device according to claim 13, characterized in that: The magnetization direction from the S pole to the N pole is an arc, and the curvature of the magnetization direction first decreases and then increases along the direction from the S pole to the N pole.
15. A charging system, characterized in that: It includes an electronic device and a charging device that can be magnetically fixed, the electronic device is the electronic device described in claim 12 or 14, the charging device includes a second magnet, the electronic device and the charging device are magnetically fixed through the magnetic attraction of the magnetic part and the second magnet, or the electronic device and the charging device are magnetically fixed through the contact section on the magnetic part and the magnetic attraction of the second magnet.