Transparent aqueous suspension oil droplet composition with protective effect and preparation method thereof
By forming a transparent water agent suspended oil bead composition in cosmetics, the oil-soluble actives are locked with castor oil/IPDI copolymer and hydrogenated castor oil/sebic acid copolymer, combining the acrylate cross-linked polymer and xanthan gum to enhance the oil-soluble actives by forming a transparent water agent in cosmetics. Thickener solves the stability of oil-soluble active substances in water agents, and achieves efficient skin care effects and safety.
Patent Information
- Application Number
- CN202411288425.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-14
- Publication Date
- 2024-12-06
AI Technical Summary
When oil-soluble active substances are directly present in aqueous agents, they are easily decomposed by water and oxygen, reducing their skin care efficiency. The prior art has not effectively solved this stability problem.
By forming a transparent water agent suspended oil bead composition, an oil gel is formed using castor oil/IPDI copolymer and hydrogenated castor oil/sebic acid copolymer to lock the oil-soluble active substance inside the oil beads and isolate the contact between water and oxygen. Acrylate (esters)/C10-30 alkanol acrylate cross-linked polymer and xanthan gum are used as thickening agents to achieve stable suspension of the oil gel.
It effectively improves the stability of oil-soluble active substances, improves its utilization rate in water-based products, avoids the stimulation of emulsifiers, meets the stability and aesthetic needs of the product, and ensures the safety of use.
Smart Images

Figure BDA0005043761860000051 
Figure BDA0005043761860000061 
Figure HDA0005043761870000011
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of cosmetics (A61K8), and in particular to a transparent aqueous suspension oil droplet composition with protective effect and a preparation method thereof. Background Art
[0002] With the improvement of national standards and quality of life, consumers' skin care requirements for cosmetics have further increased. Some oil-soluble active substances such as retinol and its derivatives, dimethylmethoxybenzodihydropyranol and phenethyl resorcinol are of great significance to the skin. Retinol and its derivatives are converted into retinoic acid under the action of enzymes on the skin surface, and have significant efficacy in anti-aging, anti-photoaging, acne removal and whitening. Dimethylmethoxybenzodihydropyranol is a scavenger of ROS (oxygen free radicals) and RNS (nitrogen free radicals), which can prevent biological molecules and cells from being damaged by air pollutants, ultraviolet radiation and active reactants produced in the human body, thereby preventing premature aging of the skin. Phenethyl resorcinol can effectively inhibit the synthesis of melanin, improve uneven skin color, and reduce skin coloration caused by ultraviolet radiation. It is also an excellent antioxidant and has anti-wrinkle ability. However, when the above-mentioned oil-soluble active ingredients exist directly in aqueous solutions, water and the oxygen in the water will accelerate their degradation and reduce their skin care efficiency; therefore, it is very necessary to isolate these oil-soluble raw materials from water to protect their activity and enable them to act smoothly on the skin to exert their efficacy.
[0003] Chinese patent CN118490539A discloses an oil gel dispersion and a preparation method thereof, wherein an oil gel having a particle size greater than 1 μm and a viscosity of 0-300000 mPa.s is independently and stably suspended in a continuous phase solution having a viscosity of 0-300000 mPa.s to obtain a stable oil gel dispersion. Chinese patent CN117017878A discloses an oil droplet essence and a preparation method thereof, wherein the essence is prepared by using a solvent, a moisturizer, an oil droplet, an emollient, a suspending agent, and a skin conditioner in a mass ratio of (80-90): (10-20): (15-25): (0.5-1): (0.2-0.4): (0.05-0.2), thereby solving the problem of poor stability of the active ingredients in the existing water-oil essence; however, none of these prior arts effectively solve the above technical problems. Summary of the invention
[0004] In view of the above technical problems, the first aspect of the present invention provides a transparent aqueous suspended oil droplet composition with protective effect, the composition at least comprising an oil gel and water; the oil gel is composed of an oil-soluble active substance, a castor oil / IPDI copolymer and / or a hydrogenated castor oil / sebacic acid copolymer, and oils.
[0005] Preferably, the oil-soluble active ingredient includes at least one of retinol and its derivatives, dimethylmethoxychromanol, phenethylresorcinol, and 4-butylresorcinol.
[0006] Preferably, castor oil / IPDI copolymer and / or hydrogenated castor oil / sebacic acid copolymer can adopt Estogel series products; for example, Estogel M (a mixture of castor oil / IPDI copolymer and caprylic acid / capric acid triglyceride), EstogelGreen (hydrogenated castor oil / sebacic acid copolymer), or ESTOGEL MAX (a mixture of castor oil / IPDI copolymer, caprylic acid / capric acid triglyceride, hydrogenated castor oil / sebacic acid copolymer).
[0007] Preferably, the composition does not contain an emulsifier.
[0008] Preferably, the amount of the oil gel added to the composition is 0.1-70 wt %.
[0009] Preferably, the oil comprises a combination of one or more of C12-15 alcohol benzoate, triethylhexanoin, coconut oil caprylate / caprate, oily plant extracts, polysiloxanes, and squalane.
[0010] The effect of skin care products depends largely on the action of active ingredients, and the stability of oil-soluble active ingredients in water will decrease, making them ineffective in water-based products. If such active ingredients can be isolated from water, the stability of the active ingredients can be effectively improved. The present invention obtains a transparent aqueous suspended oil droplet composition through exploration, and it is particularly preferred that 1-50% of oil and 0.1-5% of castor oil / IPDI copolymer form oil droplets, and the oil and castor oil / IPDI copolymer self-assemble to form a layered structure gel through supramolecular chemistry; the oil-soluble active ingredients are further locked inside the oil droplets, effectively isolating the oil-soluble active ingredients from contact with moisture and oxygen in water, so that the stability of the oil-soluble active ingredients is effectively improved, and its utilization rate is further improved.
[0011] Preferably, the composition comprises, by weight percentage: 0-10% thickener, 0.1-60% oil gel, 0-10% auxiliary agent, and deionized water to make up the balance; the added amount of thickener and auxiliary agent is not zero.
[0012] Preferably, based on the total mass of the composition, the components of the oil gel include 0-5% oil-soluble active ingredients, 0.1-5% castor oil / IPDI copolymer, and 1-50% oil; and the added amount of the oil-soluble active ingredients is not zero.
[0013] Preferably, based on the total mass of the composition, the composition further comprises 0-20% polyol and 0-10% humectant; the added amount of the polyol and humectant is not zero.
[0014] Preferably, based on the total weight of the composition, the auxiliary agent includes 0.1-5% preservative and 0-1% pH regulator.
[0015] Preferably, the thickener includes one or more combinations of acrylic acid (esters) / C10-30 alkyl acrylate crosspolymer, xanthan gum, polyacrylate crosspolymer-6, sodium polyacrylate, cellulose and its derivatives, polysaccharides, and carbomer.
[0016] Preferably, the thickener includes a combination of one or more of acrylic acid (esters) / C10-30 alkyl acrylate crosspolymer, xanthan gum, polyacrylate crosspolymer-6, and sodium polyacrylate.
[0017] On the basis of the oil gel, the present invention further selects to add acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer and xanthan gum as thickeners in the aqueous solution, effectively suspends oil droplets in the aqueous solution, and further improves the stability of the oil gel containing specific oil-soluble active substances; and the appearance of the composition is ornamental, meeting the aesthetic needs of consumers; further, the system can achieve reliable stability without adding an emulsifier, and effectively avoids the irritation of the emulsifier to the skin.
[0018] Examples of the polyol include glycerin, butanediol, and the like.
[0019] Preferably, the moisturizing agent includes a combination of one or more of betaine, polyglycerol-3, hyaluronic acid and its salts, ceramide, urea, amino acid, methyl gluceth-10, and diglycerin.
[0020] More preferably, the moisturizing agent includes a combination of one or more of betaine, polyglycerol-3, hyaluronic acid and salts thereof.
[0021] Preferably, the oily plant extract includes at least one of meadowfoam seed oil, olive oil, shea butter, avocado oil, sweet almond oil and jojoba oil.
[0022] Preferably, the auxiliary agent may also include a skin conditioner, especially a plant extract, which may be exemplified by ocimum basilicum flower / leaf extract, coralline algae (corallina officinalis) extract, ocimum sanctum leaf extract, neem (melia azadirachta) flower extract, neem (melia azadirachta) leaf extract, and the like.
[0023] Examples of the pH adjuster include sodium hydroxide and arginine.
[0024] Examples of the preservative include p-hydroxyacetophenone, 1,2-hexanediol, and 1,2-pentanediol.
[0025] The second aspect of the present invention provides a method for preparing a transparent aqueous suspension oil droplet composition having a protective effect, the preparation steps comprising:
[0026] S1. Mix the thickener, polyol, humectant and water evenly, heat to 70-85°C for 10 min, and then cool to 30-40°C to obtain mixture A;
[0027] S2. The raw materials in the oil gel are mixed uniformly to obtain a mixture B;
[0028] S3. Add mixed material B to mixed material A, keep warm and stir slowly for 0.5-2h, then add additives and mix.
[0029] Preferably, the step S2 is specifically as follows: heating the components in the oil gel except the oil-soluble active substance to 95-105° C. to melt evenly, keeping the temperature for 30 minutes and then cooling to 70-75° C. to obtain a mixture B1; then adding the oil-soluble active substance to the mixture B1 and stirring evenly to obtain a mixture B2.
[0030] In order to improve the stability of the oil gel, the present invention optimizes the preparation method of the oil gel. During the preparation, the oil and the castor oil / IPDI copolymer are firstly melted evenly at 95-105° C., and then cooled to 70-75° C.; before the oil gel is added to the aqueous phase raw material, the oil-soluble active substance is added to the oil droplets constructed by the oil and the castor oil / IPDI copolymer; thereby, the suspension stability of the oil-soluble active substance in the oil gel system and the oil gel in the aqueous agent is improved to the greatest extent.
[0031] Beneficial effects:
[0032] The present invention provides a protective transparent aqueous suspension oil droplet composition and a preparation method thereof, which has the following advantages:
[0033] (1) The present invention preferably uses 1-50% of oil and 0.1-5% of castor oil / IPDI copolymer to form oil droplets. The oil and castor oil / IPDI copolymer form a layered gel structure, which locks the oil-soluble active substance inside the oil droplets, effectively isolating the oil-soluble active substance from contact with moisture and oxygen in water, thereby effectively improving the stability of the oil-soluble active substance.
[0034] (2) The present invention adds acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer and xanthan gum as thickeners in the aqueous solution to effectively suspend oil droplets in the aqueous solution, thereby further improving the stability of the oil gel containing specific oil-soluble active ingredients; and the appearance of the composition is ornamental, meeting the aesthetic needs of consumers.
[0035] (3) This system can achieve reliable stability without adding emulsifiers, and can effectively avoid the irritation of emulsifiers to the skin, ensuring safety of use while effectively exerting its efficacy.
[0036] (4) When preparing the composition of the present invention, the oil and the castor oil / IPDI copolymer are first mixed, and the oil-soluble active substance is added to the oil droplets constructed by the oil and the castor oil / IPDI copolymer before the oil gel is added to the aqueous phase raw material; thereby maximizing the suspension stability of the oil-soluble active substance in the oil gel system and the oil gel in the aqueous solution.
[0037] (5) The raw materials of the present invention are easily available, the process is simple, and the efficacy, safety, and feasibility of the cosmetic can be met at the same time, and the application prospect is broad. BRIEF DESCRIPTION OF THE DRAWINGS
[0038] Figure 1 . Physical picture of the composition of Example 1;
[0039] Figure 2 . Actual picture of the composition of Comparative Example 1. DETAILED DESCRIPTION
[0040] Example 1.
[0041] This embodiment provides a transparent aqueous suspension oil droplet composition with protective effect, and the raw materials are shown in Table 1 below.
[0042] Table 1
[0043]
[0044]
[0045] The preparation steps of the transparent aqueous suspension oil droplet composition include:
[0046] S1. Mix the phase A materials evenly, heat to 80°C for 10 min, and then cool to 35°C to obtain a mixture A;
[0047] S2. The components of phase B (oleogel) except the oil-soluble active ingredient are heated to 100°C and melted uniformly, kept at this temperature for 30 minutes and then cooled to 70°C to obtain a mixture B1; the oil-soluble active ingredient is then added to the mixture B1 and stirred uniformly to obtain a mixture B2;
[0048] S3. Add mixed material B2 to mixed material A, keep warm and stir slowly for 1 hour, then add phase C raw materials and mix.
[0049] Note: Some of the raw materials in Table 1 need to be pre-dissolved before mixing, so they are divided into A1, A2, C1, C2, and C3. The raw materials in each sub-phase are first mixed and pre-dissolved before mixing with other raw materials.
[0050] Example 2.
[0051] This embodiment provides a transparent aqueous suspension oil droplet composition with protective effect. The specific implementation method is the same as that of Example 1; the difference is that Estogel M is replaced by ESTOGEL MAX (composed of 48wt% castor oil / IPDI copolymer, 32wt% caprylic / capric triglyceride, and 20wt% hydrogenated castor oil / sebacic acid copolymer).
[0052] Example 3.
[0053] This example provides a transparent aqueous suspension oil droplet composition with protective effect. The specific implementation method is the same as that of Example 1; the difference is that Estogel M is replaced by Estogel Green (hydrogenated castor oil / sebacic acid copolymer).
[0054] Comparative Example 1.
[0055] A common emulsion, the specific implementation manner is the same as that of Example 1; the difference is that no castor oil / IPDI copolymer is added to the raw materials, and the difference is supplemented by deionized water of phase A1.
[0056] Performance Testing
[0057] 1. Oil-soluble active ingredient content
[0058] The samples prepared in Example 1 and Comparative Example 1 were placed in an environment of 4°C for 1 month, and then the content of dimethylmethoxychromanol was measured respectively (the initial content of dimethylmethoxychromanol was 0.1%); three groups of parallel samples were set for each sample, the test item was dimethylmethoxychromanol, and the detection method referred to the SOP-QC014-01 dimethylmethoxychromanol test standard operating procedures; the test results are shown in Table 2 below. The P value of the test results of the three groups of samples was 0.00455, showing significant statistical differences.
[0059] It can be seen from Table 2 that after Example 1 and Comparative Example 1 were placed at 4° C. for 1 month, the content of dimethylmethoxychromanol in Example 1 was above 0.09 wt %, while the content of dimethylmethoxychromanol in Comparative Example 1 decreased to below 0.09 wt %; that is, the composition of the present invention exhibits an effective protective effect on dimethylmethoxychromanol.
[0060] Table 2
[0061] Sample name Test results (wt%) The first group of samples: Example 1 0.0934% The first group of samples: Comparative Example 1 0.0837% The second group of samples: Example 1 0.0939% The second group of samples: Comparative Example 1 0.0884% The third group of samples: Example 1 0.0945% The third group of samples: Comparative Example 1 0.0853%
[0062] 2. Appearance
[0063] The product pictures of Example 1 and Comparative Example 1 are shown in Figure 1 , Figure 2 ; It can be seen from the figure that in the transparent aqueous suspension oil droplet composition prepared by the present invention, the oil gel appears as small particles and is evenly dispersed in the aqueous solution; while Comparative Example 1 does not show a similar effect.
[0064] The test results of Examples 2 and 3 are similar to those of Example 1.
Claims
1. A transparent aqueous suspension oil droplet composition having protective effect, characterized in that: The composition includes at least an oleogel and water; The oil gel is composed of oil-soluble active substances, castor oil / IPDI copolymer and / or hydrogenated castor oil / sebacic acid copolymer, and oil.
2. The protective transparent aqueous suspension oil drop composition according to claim 1, characterized in that: The composition does not contain an emulsifier.
3. The protective transparent aqueous suspension oil drop composition according to claim 1, characterized in that: The oil gel is added in an amount of 0.1-70 wt % in the composition.
4. The protective transparent aqueous suspension oil drop composition according to claim 1, characterized in that: Calculated by weight percentage, the composition includes: 0-10% thickener, 0.1-60% oil gel, 0-10% auxiliary agent, and deionized water to make up the balance; the added amount of thickener and auxiliary agent is not zero.
5. The protective transparent aqueous suspension oil drop composition according to claim 4, characterized in that: Based on the total weight of the composition, the components of the oil gel include 0-5% oil-soluble active substances, 0.1-5% castor oil / IPDI copolymer, and 1-50% oil; the added amount of the oil-soluble active substances is not zero.
6. The protective transparent aqueous suspension oil drop composition according to claim 4, characterized in that: Based on the total mass of the composition, the composition further comprises 0-20% polyol and 0-10% moisturizer; the added amount of the polyol and moisturizer is not zero.
7. The protective transparent aqueous suspension oil drop composition according to claim 6, characterized in that: The auxiliary agent includes at least one of a preservative, a pH adjuster and a fragrance.
8. The protective transparent aqueous suspension oil drop composition according to claim 1, characterized in that: The oil-soluble active substance includes at least one of retinol and its derivatives, dimethylmethoxychromanol, phenethylresorcinol and 4-butylresorcinol.
9. A method for preparing the protective transparent aqueous suspension oil droplet composition according to claim 6, characterized in that: The preparation steps include: S1. Mix the thickener, polyol, humectant and water evenly, heat to 70-85°C for 10 min, and then cool to 30-40°C to obtain mixture A; S2. The raw materials in the oil gel are mixed uniformly to obtain a mixture B; S3. Add mixed material B to mixed material A, keep warm and stir slowly for 0.5-2h, then add additives and mix.
10. The method for preparing the transparent aqueous suspension oil droplet composition with protective effect according to claim 9, characterized in that: The step S2 is specifically as follows: heating the components in the oil gel except the oil-soluble active substance to 95-105° C. to melt evenly, keeping the temperature for 30 minutes and then cooling to 70-75° C. to obtain a mixture B1; then adding the oil-soluble active substance to the mixture B1 and stirring evenly to obtain a mixture B2.
Citation Information
Patent Citations
Oil bead essence and preparation method thereof
CN117017878A
Oil gel dispersion liquid and preparation method thereof
CN118490539A
Cited By
Whitening composition and preparation method thereof
CN120131472A
Composition with whitening effect as well as preparation method and application thereof
CN121512870A
A composition with whitening efficacy and a preparation method and application thereof
CN121512870B