Production process for preparing iron phosphate from phosphated residues

Through the pretreatment, pickling and water washing steps of phosphating slag, iron phosphate was successfully purified, the problem of phosphating waste slag pollution was solved, resource reuse and environmental protection were realized, and engineering costs and operational complexity were reduced.

CN119079958APending Publication Date: 2024-12-06ANHUI CHAOYUE ENVIRONMENTAL TECH CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202411242975.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-05
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

The phosphated waste slag produced during the phosphating process causes pollution to the environment. The existing neutralization treatment methods consume a large amount of neutralizing agents and may cause secondary pollution, making it difficult to achieve harmless treatment of hazardous waste and reuse of resources.

Method used

The pretreatment, pickling, water washing and drying steps of phosphating slag are adopted to remove acid molten substances and soluble impurities through the reaction of acid solution to obtain pure iron phosphate, realizing the purification of iron phosphate and reuse of resources.

Benefits of technology

The harmless treatment of hazardous waste has been achieved, environmental pollution has been reduced, resource reuse has been achieved, and the investment and operational complexity of engineering projects has been reduced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119079958A_ABST
    Figure CN119079958A_ABST
Patent Text Reader

Abstract

The invention discloses a production process for preparing iron phosphate from phosphated residues, which comprises the following steps: crushing phosphated residue raw materials to disperse the phosphated residues into smaller particles, pickling the crushed phosphated residues to remove acid melting substances in the phosphated residues, washing the pickled phosphated residues for multiple times, and drying the washed phosphated residues to obtain iron phosphate. According to the method, phosphoric acid residues are subjected to acid pickling, acid-soluble substances are removed, then washing and drying are carried out, purified iron phosphate is obtained, and therefore comprehensive utilization of hazardous waste is achieved, and the method is suitable for industrial production. Harmless treatment of hazardous waste can be achieved, pollution to the environment is reduced, and recycling of resources can be achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of chemical industry, and in particular to a production process for preparing ferric phosphate from phosphating slag. Background Art

[0002] Phosphating is one of the important pretreatment methods before metal coating, and is widely used in the fields of chemical industry, metallurgy, automobile, aerospace, shipbuilding, etc. However, the phosphating process will inevitably produce solid waste phosphating slag with iron phosphate and zinc phosphate as the main components. In addition, it also contains impurity ions such as Na+, Mg2+, Mn2+, etc. If discharged arbitrarily, it will inevitably cause serious pollution to water, atmosphere and soil. At present, neutralization methods are mostly used to neutralize them, which not only consumes a large amount of neutralizers, but also causes secondary pollution to the environment.

[0003] Therefore, those skilled in the art provide a production process for preparing iron phosphate from phosphating slag to solve the problems raised in the above background technology. Summary of the invention

[0004] The purpose of the present invention is to solve the shortcomings of the prior art and to propose a production process for preparing iron phosphate from phosphating slag.

[0005] The composition of phosphating slag varies greatly due to the different types of metals treated, phosphating processes and types of phosphating solutions. Taking the zinc phosphating solution of a steel plant as an example, the composition of phosphating slag is roughly: 3-6% zinc content, 15-20% iron content, and about 50% phosphoric acid and phosphate content. In addition, some phosphating slags also contain a small amount of manganese, nickel, copper and other components. The test and analysis using inductively coupled plasma (ICP) show that the content of iron phosphate in phosphating waste slag is generally 75% to 80%. If iron phosphate can be extracted from solid phosphating waste slag and used as raw materials for industrial and agricultural production, it can not only achieve the harmless treatment of hazardous wastes and reduce pollution to the environment, but also achieve the reuse of resources.

[0006] In order to achieve the above object, the present invention adopts the following technical solutions:

[0007] A production process for preparing ferric phosphate from phosphating slag, comprising the following steps:

[0008] S1. Phosphating slag pretreatment: crushing the phosphating slag raw material to disperse it into smaller particles;

[0009] S2, pickling treatment: pickling the crushed phosphating slag to remove acid-fusible substances in the phosphating slag;

[0010] S3, water washing: washing the phosphating slag after pickling for multiple times to remove residual acid and soluble impurities;

[0011] S4. Drying: Dry the washed phosphating slag to remove excess water and obtain pure iron phosphate.

[0012] Preferably, the specific operation method of step S2 is:

[0013] S2.1, mixing the phosphating slag with an acid solution of appropriate concentration for reaction;

[0014] S2.2. Control the temperature and time of pickling treatment to ensure sufficient reaction and remove acid-fusible impurities in the phosphating slag;

[0015] S2.3. After pickling, solid-liquid separation is carried out and the pickling residue and pickling liquid are collected.

[0016] Preferably, the acid solution in step S2.1 is one of hydrochloric acid and sulfuric acid.

[0017] Preferably, the specific operation method of step S3 is:

[0018] S3.1. Wash the acid leaching residue several times with deionized water to remove residual acid and soluble impurities;

[0019] S3.2, control the washing temperature and solid-liquid ratio to improve washing efficiency;

[0020] S3.3, after washing, perform solid-liquid separation and collect the filter residue after washing.

[0021] Compared with the prior art, the present invention has the following beneficial effects:

[0022] In the present invention, the phosphoric acid residue is pickled to remove acid-soluble substances, and then washed with water and dried to obtain purified iron phosphate, thereby realizing comprehensive utilization of hazardous wastes, which can not only realize harmless treatment of hazardous wastes and reduce pollution to the environment, but also realize the reuse of resources;

[0023] The equipment required for this process is common equipment for chemical enterprises. The project requires low investment, is easy to operate and manage, and has no secondary pollution. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] In order to more specifically and intuitively illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art are briefly introduced below.

[0025] Figure 1 A production process flow chart of preparing iron phosphate from phosphating slag proposed by the present invention; DETAILED DESCRIPTION

[0026] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments.

[0027] Reference Figure 1 A production process for preparing iron phosphate from phosphating slag comprises the following steps:

[0028] S1. Phosphating slag pretreatment: crushing the phosphating slag raw material to disperse it into smaller particles;

[0029] S2, pickling treatment: pickling the crushed phosphating slag to remove acid-fusible substances in the phosphating slag;

[0030] S3, water washing: washing the phosphating slag after pickling for multiple times to remove residual acid and soluble impurities;

[0031] S4. Drying: Dry the washed phosphating slag to remove excess water and obtain pure iron phosphate.

[0032] The specific operation method of step S2 is:

[0033] S2.1, mixing the phosphating slag with an acid solution of appropriate concentration for reaction;

[0034] S2.2. Control the temperature and time of pickling treatment to ensure sufficient reaction and remove acid-fusible impurities in the phosphating slag;

[0035] S2.3. After pickling, solid-liquid separation is carried out and the pickling residue and pickling liquid are collected.

[0036] The acid solution in step S2.1 is one of hydrochloric acid and sulfuric acid.

[0037] The specific operation method of step S3 is:

[0038] S3.1. Wash the acid leaching residue several times with deionized water to remove residual acid and soluble impurities;

[0039] S3.2, control the washing temperature and solid-liquid ratio to improve washing efficiency;

[0040] S3.3, after washing, perform solid-liquid separation and collect the filter residue after washing.

[0041] Example:

[0042] The process of the present invention is to firstly pickle the phosphoric acid residue to remove acid-soluble substances, then wash with water, and dry to obtain purified iron phosphate;

[0043] In the process of phosphating slag pickling, temperature control has an important influence on the reaction rate and film quality. The ideal working temperature range is usually 40-60 degrees Celsius. Too high a temperature will accelerate the decomposition of dihydrogen phosphate, rapidly increase the free acid, and increase the formation of sediment, while too low a temperature will slow down the phosphating reaction rate and affect the film quality. In order to control the temperature, a water tank temperature control mold temperature controller can be used. This equipment can provide uniform heating, reduce the temperature difference between the heat source and the solution, and reduce the decomposition rate of the solution.

[0044] Controlling the pickling time is crucial to removing the oxide layer and iron scale on the metal surface. Generally speaking, the pickling time should be controlled within 5-10 minutes. Too short a time may lead to incomplete treatment, while too long a time may cause excessive corrosion or hydrogen embrittlement. In actual operation, appropriate adjustments should be made according to the specific conditions of the workpiece and the concentration of the pickling solution.

[0045] The main purpose of washing phosphating slag is to remove impurities in the phosphating slag, especially metal ions. These impurities in the phosphating slag can be effectively removed through the water washing process.

[0046] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.

Claims

1. A production process for preparing iron phosphate from phosphating slag, characterized in that: The following steps are involved: S1. Phosphating slag pretreatment: crushing the phosphating slag raw material to disperse it into smaller particles; S2, pickling treatment: pickling the crushed phosphating slag to remove acid-fusible substances in the phosphating slag; S3, water washing: washing the phosphating slag after pickling for multiple times to remove residual acid and soluble impurities; S4. Drying: Dry the washed phosphating slag to remove excess water and obtain pure iron phosphate.

2. The process for preparing ferric phosphate from phosphating slag according to claim 1, characterized in that: The specific operation method of step S2 is: S2.1, mixing the phosphating slag with an acid solution of appropriate concentration for reaction; S2.

2. Control the temperature and time of pickling treatment to ensure sufficient reaction and remove acid-fusible impurities in the phosphating slag; S2.

3. After pickling, solid-liquid separation is carried out and the pickling residue and pickling liquid are collected.

3. The production process for preparing ferric phosphate from phosphating slag according to claim 2, characterized in that: The acid solution in step S2.1 is one of hydrochloric acid and sulfuric acid.

4. The production process for preparing ferric phosphate from phosphating slag according to claim 2, characterized in that: The specific operation method of step S3 is: S3.

1. Wash the acid leaching residue several times with deionized water to remove residual acid and soluble impurities; S3.2, control the washing temperature and solid-liquid ratio to improve washing efficiency; S3.3, after washing, solid-liquid separation is performed and the filter residue after washing is collected.

Citation Information

Patent Citations

  • Method for extracting and preparing iron phosphate with phosphorization slag

    CN105776165A