Performance optimization method of carbon fiber composite material for aerospace equipment

Through plasma treatment and hot-pressing tank molding technology, combined with nano-scale silicon carbide reinforced particles and annealing treatment, the performance of carbon fiber composite materials is optimized, and the problem of insufficient binding effect and thermal stability of carbon fiber surface impurities is solved, and the mechanics of the material is improved Performance and thermal stability meet the complex needs of aerospace equipment.

CN119081350AInactive Publication Date: 2024-12-06GUILIN UNIV OF AEROSPACE TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411177770.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-26
Publication Date
2024-12-06
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The impurities on the surface of carbon fiber in the preparation method of traditional carbon fiber composites affect their binding effect with the resin matrix, resulting in the inability to meet the higher requirements of mechanical properties, and the thermal stability is not enough to cope with the demands of aerospace equipment in high temperature environments, production process efficiency and Quality consistency also needs to be improved.

Method used

Plasma treatment technology is used to remove impurities on the surface of carbon fiber, and mixed with high-temperature epoxy resin matrix, nano-scale silicon carbide reinforced particles are added, and the performance of carbon fiber composite materials is optimized through the hot-pressing tank molding process and annealing process.

Benefits of technology

It significantly improves the tensile strength, bending strength and thermal stability of carbon fiber composite materials, ensures that they can better withstand mechanical loads and extreme temperature changes in aerospace equipment, and improves the consistency of production efficiency and product quality.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention provides a performance optimization method of a carbon fiber composite material for aerospace equipment, and belongs to the technical field of material scientificity, according to the performance optimization method, plasma with specific power and time is adopted to treat carbon fibers, surface impurities can be removed, activity can be improved, the bonding effect with a resin matrix can be enhanced, product quality consistency can be improved, and the defective rate and cost can be reduced. The treated carbon fibers and a specific resin matrix are mixed in proportion, and nano-scale silicon carbide particles are added, so that the mechanical property is enhanced, the tensile strength is improved by at least 30%, the bending strength is improved by at least 25%, the mechanical load of a spacecraft can be better borne, an autoclave forming process and subsequent annealing treatment can be better carried out, and the service life of the spacecraft is prolonged. The thermal stability of the composite material is improved by at least 20% at 500 DEG C, reliable operation of aerospace equipment under complex working conditions such as high temperature is ensured, in short, the performance of the carbon fiber composite material is effectively improved, and the optimization method is of great significance to development of the aerospace technology.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of material science and technology, and specifically relates to a method for optimizing the performance of a carbon fiber composite material for aerospace equipment. Background Art

[0002] With the continuous development of aerospace technology, the performance requirements for aerospace equipment materials are increasing. Carbon fiber composites have been widely used in the aerospace field because of their excellent properties such as high specific strength, high specific modulus, fatigue resistance, and corrosion resistance. However, in actual production and use, carbon fiber composites still have some aspects that need to be improved. The traditional preparation method of carbon fiber composites has limitations in certain properties. For example, impurities on the surface of carbon fiber may affect its bonding effect with the resin matrix, resulting in the overall performance of the composite material being affected. The interface bonding force between the carbon fiber and the resin matrix that has not been fully treated is weak, making it difficult for the mechanical properties of the composite material to meet higher requirements. For example, tensile strength and bending strength may not meet the increasingly stringent aerospace equipment use standards. In the aerospace environment, the equipment needs to withstand extreme temperature changes and various mechanical loads. The existing carbon fiber composites also have room for improvement in thermal stability. When facing a high temperature environment, their performance may decline, and the reliable operation of aerospace equipment under complex working conditions such as high temperature cannot be guaranteed. In addition, in actual production, how to optimize the preparation process of carbon fiber composites to improve production efficiency and product quality consistency is also an urgent problem to be solved.

[0003] With the diversification and complexity of space missions, higher requirements are placed on the performance of carbon fiber composite materials used in aerospace equipment. Not only do they need to have significant improvements in mechanical properties, but they also need to have better performance in thermal stability and other aspects to adapt to the special needs of the space environment. Therefore, the development of a new method for optimizing the performance of carbon fiber composite materials is of great significance to improving the performance and reliability of aerospace equipment. The performance optimization method of carbon fiber composite materials for aerospace equipment in this case came into being in this context. Summary of the invention

[0004] The purpose of the present invention is to provide a method for optimizing the performance of carbon fiber composite materials for aerospace equipment, aiming to solve the problems in the prior art.

[0005] To achieve the above object, the present invention provides the following technical solutions:

[0006] A method for optimizing the performance of a carbon fiber composite material for aerospace equipment comprises the following steps:

[0007] The carbon fiber is surface treated by plasma treatment technology to remove impurities on the surface of the carbon fiber and increase its surface activity within a specific power range and treatment time, wherein the plasma treatment power is 50W to 100W and the treatment time is 15 minutes to 30 minutes.

[0008] The surface-treated carbon fiber is mixed with a specific resin matrix, which is a high-temperature resistant epoxy resin. The temperature during mixing is controlled at 80° C. to 100° C., and the mass ratio of the carbon fiber to the resin matrix is ​​3:7.

[0009] The mixed material is molded using a specific molding process, wherein the molding process is autoclave molding, the pressure of the autoclave is set at 2MPa to 4MPa, the temperature is set at 150°C to 180°C, and the molding time is 3 hours to 5 hours.

[0010] As a preferred solution of the present invention, when the carbon fiber is subjected to surface treatment, the gas atmosphere of the plasma treatment is a mixed gas of argon and oxygen, wherein the volume ratio of argon to oxygen is 3:1.

[0011] As a preferred solution of the present invention, during the process of mixing the carbon fibers with the resin matrix, nano-scale reinforcing particles are added. The nano-scale reinforcing particles are silicon carbide, and their mass accounts for 2% to 5% of the total mass of the carbon fibers and the resin matrix.

[0012] As a preferred solution of the present invention, after the autoclave molding, the molded composite material is post-processed, and the post-processing includes annealing at a specific temperature and time, the annealing temperature is 200°C to 250°C, and the annealing time is 1 hour to 2 hours.

[0013] As a preferred solution of the present invention, the carbon fiber composite material optimized by this method has a tensile strength increased by at least 30% compared with before optimization, a bending strength increased by at least 25%, and a thermal stability increased by at least 20% compared with before optimization when the temperature reaches 500°C.

[0014] Compared with the prior art, the present invention has the following beneficial effects:

[0015] First, by using plasma treatment technology with a specific power range (50W to 100W) and treatment time (15 minutes to 30 minutes) to treat the surface of carbon fiber, impurities on the surface of carbon fiber can be effectively removed and its surface activity can be improved, which significantly enhances the bonding effect between carbon fiber and resin matrix, and fundamentally solves the problem of impurities on the surface of carbon fiber affecting the bonding effect in traditional preparation methods. In actual production, this improvement can improve the consistency of product quality, reduce the defective rate caused by poor bonding, and reduce production costs. Secondly, the treated carbon fiber is mixed with a specific high-temperature resistant epoxy resin matrix at a mass ratio of 3:7 at a temperature of 80°C to 100°C, and nano-scale silicon carbide reinforcing particles with a mass ratio of 2% to 5% are added, which greatly enhances the mechanical properties of the composite material. Compared with before optimization, the tensile strength is increased by at least 30% and the bending strength is increased by at least 25%, which means that in the actual application of aerospace equipment, the material can better withstand various Mechanical loads, such as vibration and impact during the launch and flight of spacecraft, can ensure the structural integrity and reliability of the equipment even in the face of increasingly diverse and complex aerospace missions. Furthermore, in the autoclave molding process, a pressure of 2MPa to 4MPa, a temperature of 150℃ to 180℃ and a molding time of 3 to 5 hours are set, and an annealing treatment of 1 to 2 hours at a temperature of 200℃ to 250℃ is performed after molding, so that the thermal stability of the composite material is at least 20% higher than that before optimization when the temperature reaches 500℃. In the aerospace environment, equipment often faces extreme temperature changes. This improvement in thermal stability can ensure that aerospace equipment can operate reliably under complex working conditions such as high temperature, and avoid the degradation of material performance due to temperature changes, which affects the normal function and service life of the equipment. In short, this optimization method provides a practical and effective way to improve the performance of carbon fiber composite materials used in aerospace equipment, which is of great significance to promoting the development of aerospace technology. DETAILED DESCRIPTION

[0016] The technical solutions in the embodiments of the present invention will be described clearly and completely below in combination with the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0017] Example 1

[0018] The present invention provides the following technical solution: a method for optimizing the performance of a carbon fiber composite material for aerospace equipment, characterized in that it comprises the following steps:

[0019] The carbon fiber is surface treated by plasma treatment technology to remove impurities on the surface of the carbon fiber and increase its surface activity within a specific power range and treatment time, wherein the plasma treatment power is 50W to 100W and the treatment time is 15 minutes to 30 minutes.

[0020] The surface-treated carbon fiber is mixed with a specific resin matrix, which is a high-temperature resistant epoxy resin. The temperature during mixing is controlled at 80° C. to 100° C., and the mass ratio of the carbon fiber to the resin matrix is ​​3:7.

[0021] The mixed material is molded using a specific molding process, wherein the molding process is autoclave molding, the pressure of the autoclave is set at 2MPa to 4MPa, the temperature is set at 150°C to 180°C, and the molding time is 3 hours to 5 hours.

[0022] In a specific embodiment of the present invention, firstly, by setting a plasma treatment power of 50W to 100W and a treatment time of 15 minutes to 30 minutes, impurities on the surface of the carbon fiber can be removed just right, just like carefully wiping a precious object to thoroughly remove the dirt on its surface. In actual production, carbon fiber will inevitably be contaminated with some impurities during production, storage and transportation. If these impurities are not removed, they will form weak points when combined with the resin matrix later, affecting the overall performance of the composite material. After this plasma treatment, the impurities are effectively removed, making the surface of the carbon fiber purer, creating ideal conditions for good combination with the resin matrix. At the same time, this treatment method can also increase the surface activity of the carbon fiber, which It is like injecting new vitality into the surface of carbon fiber, making it easier to react chemically with the resin matrix to form a stronger bonding force. In actual production life, the enhanced surface activity means that when mixed with the resin matrix later, the two can be more closely combined. This close combination can not only improve the mechanical properties of the composite material, but also enhance its stability in various environments. For example, in aerospace equipment, composite materials need to withstand extreme temperature changes in the space environment, micrometeorite impacts and other complex situations. When carbon fiber and resin matrix are well combined, they can better transfer stress, making the composite material less prone to delamination and cracking when facing these complex situations, thereby improving the reliability and service life of aerospace equipment, and in terms of production efficiency. This treatment method also has a positive impact, because it can improve the bonding effect between carbon fiber and resin matrix and reduce the defective rate caused by poor bonding. In actual production, the production of defective products not only wastes raw materials, but also increases production costs and production time. After improving the bonding effect through plasma treatment, the quality of the composite materials produced is more stable, reducing rework and waste treatment due to quality problems, thereby improving the overall production efficiency. At the same time, the surface characteristics of the treated carbon fiber are more consistent, making it easier to control the process parameters in the subsequent processing process, further ensuring the consistency of product quality, which is of great significance for the large-scale production of high-performance carbon fiber composite materials, and can meet the large-scale demand for high-quality materials in the aerospace field. The second step of claim 1 is to mix the treated carbon fiber with a specific resin matrix, and mix the carbon fiber and the high-temperature resistant epoxy resin matrix at a mass ratio of 3:7 at a temperature of 80°C to 100°C. This operation also brings many beneficial effects. First, the mixing temperature of 80°C to 100°C is carefully selected. Within this temperature range, the high-temperature resistant epoxy resin matrix can maintain appropriate fluidity, which can fully infiltrate the carbon fiber without causing the resin matrix to decompose or other adverse chemical reactions due to excessive temperature. In actual production life, when the resin matrix can well infiltrate the carbon fiber, it is like cement that can fully fill the gaps between bricks, making the bond between the carbon fiber and the resin matrix tighter.This close combination can effectively transfer stress and improve the mechanical properties of the composite material. Secondly, the mass ratio of 3:7 is determined based on a comprehensive consideration of the performance of the composite material. The carbon fiber plays a role in enhancing the mechanical properties of the composite material, while the resin matrix plays a role in bonding and transferring stress. When the carbon fiber and the resin matrix are mixed in a mass ratio of 3:7, it can ensure that the composite material has sufficient strength while also having good toughness and processability. In the actual application of aerospace equipment, composite materials with this mass ratio can better adapt to the various mechanical loads faced by spacecraft in different stages such as launch, flight and landing. For example, when a spacecraft is launched, it will be subjected to huge acceleration and vibration, and this mass ratio of composite materials It can effectively absorb and disperse these stresses to ensure the integrity of the spacecraft structure. In addition, the use of a high-temperature resistant epoxy resin matrix is ​​of great significance. In the aerospace environment, the equipment will face high temperatures. Ordinary resin matrices may soften and decompose at high temperatures, thereby causing the performance of the composite material to deteriorate. The high-temperature resistant epoxy resin matrix can maintain the stability of its performance at higher temperatures, so that the composite material can still maintain good mechanical properties and structural stability in a high-temperature environment. This has important adaptability to the high-temperature environment faced by aerospace equipment in the process of crossing the atmosphere and entering space orbit, and can ensure the reliable operation of aerospace equipment under various extreme working conditions. The third step of claim 1 is to use a hot autoclave molding process to mold the mixed material. For molding, set the pressure of 2MPa to 4MPa, the temperature of 150℃ to 180℃ and the molding time of 3 hours to 5 hours. This molding process has many advantages. First, the pressure of 2MPa to 4MPa can make the components in the mixed material more closely combined. Under this pressure, the carbon fiber, resin matrix and nano-scale reinforcing particles can better fill and compact each other, reducing the pores and defects inside the material. In actual production, the presence of pores and defects will reduce the mechanical properties and thermal stability of the composite material. Through the appropriate pressure for autoclave molding, these unfavorable factors can be effectively reduced and the quality of the composite material can be improved. Secondly, the temperature range of 150℃ to 180℃ is precisely controlled. At this temperature, the resin matrix can be fully cured and form a good bond with the carbon fiber and nano-scale reinforcing particles. At the same time, this temperature will not be too high to cause adverse phenomena such as thermal decomposition of the material. In actual production life, the appropriate curing temperature can ensure that the composite material has good mechanical properties and chemical stability. For example, in aerospace equipment, composite materials need to maintain the stability of their performance in various harsh environments. The appropriate curing temperature can make the resin matrix form a uniform and dense structure during the curing process, thereby improving the fatigue resistance and corrosion resistance of the composite material. Furthermore, the molding time of 3 to 5 hours can ensure the full progress of the autoclave molding process. During this period of time, the material can gradually take shape under the action of pressure and temperature.There is enough time for the components to diffuse and react with each other, making the structure of the composite material more stable and uniform. In actual production, if the molding time is too short, the material may not be fully cured and the performance may not meet the requirements; if the molding time is too long, it will waste energy and increase production costs. By reasonably setting the molding time of 3 to 5 hours, efficient production can be achieved while ensuring the performance of the composite material. This autoclave molding process is of great significance for improving the overall performance and production efficiency of composite materials, and can meet the needs of aerospace equipment for high-performance materials.

[0023] Specifically, when the carbon fiber is subjected to surface treatment, the gas atmosphere of the plasma treatment is a mixed gas of argon and oxygen, wherein the volume ratio of argon to oxygen is 3:1.

[0024] In this embodiment: First, argon plays an important role in plasma treatment. Argon is an inert gas that can produce a stable plasma state in a plasma environment. When carbon fiber is in this argon plasma, the high-energy particles of argon can gently and effectively impact the surface of the carbon fiber to remove impurities on the surface. This is like a group of meticulous "cleaners" who will not react chemically with the carbon fiber, but can clean the dust and dirt on the surface through physical action. In actual production, this gentle cleaning method can protect the main structure of the carbon fiber to the greatest extent and avoid damage to the carbon fiber due to excessive chemical reactions. At the same time, the addition of oxygen brings new advantages to plasma treatment. Oxygen can react chemically with the surface of the carbon fiber in the plasma, further oxidize and remove some stubborn impurities, and can form some active oxidative groups on the surface of the carbon fiber. These active oxidative groups are like building many "bridges" on the surface of the carbon fiber, so that the carbon fiber can react more easily with the chemical groups in the resin matrix when it is subsequently combined with the resin matrix, thereby enhancing the bonding force between the carbon fiber and the resin matrix. In actual production and life, this enhanced bonding force is crucial to improving the performance of composite materials. For example, in aerospace equipment, composite materials need to withstand a variety of complex situations such as aerodynamic pressure and extreme temperature changes during high-speed flight. Stronger bonding can ensure that composite materials will not have problems such as delamination and debonding under these harsh conditions, thereby improving the reliability and safety of aerospace equipment. In addition, the mixing of argon and oxygen in a volume ratio of 3:1 is carefully optimized. This ratio can fully exert the oxidation and activation effects of oxygen while ensuring the stable plasma state of argon. If the oxygen ratio is too high, it may cause excessive oxidation of carbon fibers and destroy their structural integrity; if the oxygen ratio is too low, it may not fully exert its oxidation and activation effects. By precisely controlling the volume ratio of argon to oxygen to 3:1, the best effect of carbon fiber surface treatment can be achieved. In actual production, this precise gas ratio control can improve the stability and repeatability of the production process, ensure that each batch of processed carbon fibers has similar surface characteristics, and further improve the quality consistency of composite materials. This is of great significance for the large-scale production of high-performance carbon fiber composites and meeting the demand for high-quality materials in the aerospace field.

[0025] Specifically, in the process of mixing the carbon fibers with the resin matrix, nano-scale reinforcing particles are added. The nano-scale reinforcing particles are silicon carbide, and the mass of the nano-scale reinforcing particles accounts for 2% to 5% of the total mass of the carbon fibers and the resin matrix.

[0026] In this embodiment: the addition of nano-scale silicon carbide reinforced particles can significantly improve the mechanical properties of the composite material. Silicon carbide itself has high hardness and strength. When it is evenly dispersed in the carbon fiber and resin matrix in the form of nano-scale particles, it can effectively hinder the crack propagation inside the composite material. In actual production and life, when the composite material is subjected to external forces, cracks are often one of the main causes of material damage. Nano-scale silicon carbide particles are like tiny "shields" that can prevent further crack expansion, thereby improving the tensile strength and bending strength of the composite material. For example, in aerospace equipment, the structural components of the spacecraft need to withstand various mechanical loads, such as the huge thrust during launch, the aerodynamic force during flight, etc. The composite material with nano-scale silicon carbide reinforced particles added can better cope with these mechanical loads and ensure the stability and safety of the spacecraft structure. Secondly, the nano-scale silicon carbide reinforced particles can also improve the interface bonding between the carbon fiber and the resin matrix. Because silicon carbide particles have unique surface properties, they can act as a "bridge" at the interface between the carbon fiber and the resin matrix to enhance the bonding between the two. In actual production, good interface bonding can more effectively transfer stress and avoid the occurrence of stress concentration. When the composite material is subjected to external force, the stress can be more evenly distributed throughout the material, rather than concentrated in a weak area, thereby further improving the mechanical properties and reliability of the composite material. In addition, the range of 2% to 5% by mass is scientifically researched and verified by practice. Adding nano-scale silicon carbide reinforcing particles within this range can not only give full play to its role in enhancing mechanical properties and improving interface bonding, but also will not affect the fluidity and processability of the resin matrix due to excessive addition. If too much silicon carbide particles are added, the resin matrix may be too viscous, making it difficult to fully infiltrate the carbon fiber, affecting the molding quality of the composite material. Within the range of 2% to 5% by mass, the mechanical properties of the composite material can be maximized while ensuring good processing performance. In the actual production process, this reasonable addition ratio can optimize the production process, improve production efficiency and product quality. At the same time, for fields such as aerospace equipment that have extremely high requirements for material performance, this optimized composite material can better meet its strict requirements in mechanical properties and provide strong support for the development of aerospace technology.

[0027] Specifically, after the autoclave molding, the molded composite material is post-processed, and the post-processing includes annealing at a specific temperature and time, the annealing temperature is 200° C. to 250° C., and the annealing time is 1 hour to 2 hours.

[0028] In this embodiment: First, annealing can eliminate the residual stress generated by the composite material during the autoclave molding process. During autoclave molding, residual stress will inevitably be generated due to the difference in thermal expansion coefficients of different components inside the material and the changes in temperature and pressure. Through annealing, the atoms inside the material can have enough time to rearrange, thereby reducing the residual stress level and improving the dimensional stability of the composite material. In aerospace equipment, dimensional accuracy is crucial, and even small dimensional changes may affect the assembly and performance of the equipment. For example, in the precision parts of a spacecraft, if the composite material is dimensionally unstable, it may cause deviations in the connection between the parts, affecting the structural integrity and operational reliability of the entire spacecraft. Secondly, annealing helps to further improve the thermal stability of the composite material. When the composite material is annealed at a temperature of 200°C to 250°C for 1 to 2 hours, the molecular structure inside the material will undergo certain adjustments and optimizations. This optimization enables the composite material to better maintain its performance when facing a higher temperature environment. During space flight, the spacecraft may enter or pass through high temperature areas, such as the high temperature generated by passing through the atmosphere when returning to the earth. After annealing, carbon fiber composite materials can still maintain good mechanical properties and structural integrity in this extreme high temperature environment, reducing problems such as material deformation and performance degradation caused by high temperature. At the same time, annealing can also improve the uniformity of the microstructure of the composite material. During the annealing process, the components inside the material can be more evenly distributed, avoiding large local performance differences. This is of great significance for aerospace equipment, because uneven material properties may lead to local failure when certain key parts are subjected to stress, while a uniform microstructure can improve the overall performance and service life of the entire material, ensuring that aerospace equipment can operate reliably in long-term space missions.

[0029] Specifically, the carbon fiber composite material optimized by this method has a tensile strength increased by at least 30% compared with that before optimization, a bending strength increased by at least 25%, and a thermal stability increased by at least 20% when the temperature reaches 500°C compared with that before optimization.

[0030] In this embodiment: In terms of tensile strength, the tensile strength is increased by at least 30%, making the application of carbon fiber composite materials in aerospace equipment more reliable. In the structural components of spacecraft, such as the fuselage frame, solar panel bracket, etc., it is necessary to withstand various tensile forces. The optimized material can better resist these tensile forces, ensuring that the structure of the spacecraft will not be damaged by tensile stress during launch, flight and various dynamic changes in the space environment. For example, during the launch of the spacecraft, it will experience strong acceleration and vibration. Composite materials with higher tensile strength can ensure that the structural components will not be broken or deformed due to these external forces, thereby ensuring the safe flight of the spacecraft. Moreover, in space In the environment, there may be unexpected situations such as micrometeorite impacts. The improvement of tensile strength can also increase the spacecraft's resistance to external impacts and reduce the risk of structural damage caused by impacts. In terms of bending strength, at least 25% improvement has an important impact on the structural design and performance of aerospace equipment. Some parts of the spacecraft, such as wings and antennas, need to have good bending properties to adapt to different flight attitudes and mechanical loads in the space environment. Higher bending strength means that these parts are less likely to break or be damaged when subjected to bending forces. For example, when the spacecraft adjusts its attitude, parts such as wings will be subjected to bending forces in different directions. The optimized composite material can ensure that these parts The parts maintain structural integrity and stability under various bending conditions. In addition, some unexpected bending conditions may occur during the assembly and transportation of the spacecraft. The improvement of bending strength can reduce material damage caused by these conditions, reduce maintenance costs, and improve the overall reliability of aerospace equipment. In terms of thermal stability, when the temperature reaches 500°C, the performance improvement of at least 20% compared to before optimization is crucial for the operation of aerospace equipment in extremely high temperature environments. When the spacecraft re-enters the atmosphere, the intense friction with the air will generate extremely high temperatures. The improvement of thermal stability can ensure that the material still maintains good performance in this high temperature environment, for example, the heat shield of the spacecraft The use of this optimized carbon fiber composite material in key components such as spacecraft can better withstand high temperatures, prevent heat from being transferred to the internal structure, and protect the electronic equipment and other key components inside the spacecraft from being affected by high temperatures. At the same time, in some aerospace equipment such as satellites, local temperatures may rise due to factors such as solar radiation. The improvement of thermal stability can ensure that the material's performance will not drop sharply due to temperature increase in this case, thereby ensuring the normal operation of the satellite and the reliability of functions such as communication. In addition, the improvement of thermal stability can also extend the service life of aerospace equipment, reduce material aging and damage caused by high temperature, reduce the cost of frequent material replacement, and provide strong support for the long-term implementation of space missions.

[0031] The working principle and use process of the present invention:

[0032] First, the surface treatment of carbon fiber is carried out. The carbon fiber is placed in a plasma treatment device, the power is set to 50W to 100W, the treatment time is 15 minutes to 30 minutes, and a mixed gas of argon and oxygen in a volume ratio of 3:1 is used as the gas atmosphere for plasma treatment. In this process, the high-energy particles of the plasma can effectively remove impurities on the surface of the carbon fiber, just like a deep cleaning of the carbon fiber, making its surface look brand new. At the same time, it can also increase the surface activity of the carbon fiber, laying the foundation for the subsequent good combination with the resin matrix. After the treatment is completed, the carefully "cleaned" and activated carbon fiber is ready to be mixed with the resin matrix. Then, under the environment of temperature control at 80℃ to 100℃, the carbon fiber is mixed with the high-temperature resistant epoxy resin matrix in a mass ratio of 3:7. At the same time, nano-scale silicon carbide reinforcing particles with a mass of 2% to 5% of the total mass of the carbon fiber and the resin matrix are added. At this time, it is like modulating a high-performance "alloy". The components are fused with each other. During the mixing process, it is necessary to stir continuously to ensure that the carbon fiber, resin matrix and silicon carbide particles are evenly distributed to form a tightly combined whole. Then, the hot press molding process is used to mix the mixture. The combined materials are placed in an autoclave, the pressure is set to 2MPa to 4MPa, the temperature is 150℃ to 180℃, and the molding time is 3 hours to 5 hours. At this stage, the autoclave is like a magical "magic furnace". Under the action of appropriate pressure and temperature, the materials are gradually formed, and the components are further fused and solidified to form a composite material with a specific shape and performance. Finally, after the autoclave is formed, the composite material is post-processed, and the formed composite material is placed in an annealing device and annealed at a temperature of 200℃ to 250℃ for 1 hour to 2 hours. This step is like "finishing" the composite material to further improve the stability and uniformity of its performance. After this series of operation processes, the final carbon fiber composite material has been significantly improved in terms of tensile strength, bending strength and thermal stability, which can better meet the use requirements of aerospace equipment in complex space environments and provide solid material guarantees for the development of aerospace technology. In actual production and life, this strict and precise operation process can ensure the stability and reliability of product quality, and bring higher performance products to the aerospace field and other fields where the material may be applied.

[0033] Finally, it should be noted that the above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art can still modify the technical solutions described in the aforementioned embodiments or replace some of the technical features therein by equivalents. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.

Claims

1. A method for optimizing the performance of carbon fiber composite materials for aerospace equipment, characterized in that: The following steps are involved: The carbon fiber is surface treated by plasma treatment technology to remove impurities on the surface of the carbon fiber and increase its surface activity within a specific power range and treatment time, wherein the plasma treatment power is 50W to 100W and the treatment time is 15 minutes to 30 minutes. The surface-treated carbon fiber is mixed with a specific resin matrix, which is a high-temperature resistant epoxy resin. The temperature during mixing is controlled at 80° C. to 100° C., and the mass ratio of the carbon fiber to the resin matrix is ​​3:

7. The mixed material is molded using a specific molding process, wherein the molding process is autoclave molding, the pressure of the autoclave is set at 2MPa to 4MPa, the temperature is set at 150°C to 180°C, and the molding time is 3 hours to 5 hours.

2. The method for optimizing the performance of a carbon fiber composite material for aerospace equipment according to claim 1, characterized in that: When the carbon fiber is surface treated, the gas atmosphere of the plasma treatment is a mixed gas of argon and oxygen, wherein the volume ratio of argon to oxygen is 3:

1.

3. The method for optimizing the performance of a carbon fiber composite material for aerospace equipment according to claim 2, characterized in that: In the process of mixing the carbon fiber and the resin matrix, nano-scale reinforcing particles are also added. The nano-scale reinforcing particles are silicon carbide, and the mass of the nano-scale reinforcing particles accounts for 2% to 5% of the total mass of the carbon fiber and the resin matrix.

4. The method for optimizing the performance of a carbon fiber composite material for aerospace equipment according to claim 3, characterized in that: After the autoclave molding, the molded composite material is post-processed, and the post-processing includes annealing at a specific temperature and time, the annealing temperature is 200° C. to 250° C., and the annealing time is 1 hour to 2 hours.

5. The method for optimizing the performance of a carbon fiber composite material for aerospace equipment according to claim 4, characterized in that: The carbon fiber composite material optimized by this method has a tensile strength increased by at least 30% and a bending strength increased by at least 25% compared with before optimization, and a thermal stability increased by at least 20% when the temperature reaches 500°C compared with before optimization.