Organic silicon pressure-sensitive adhesive removing solution and application process thereof

By using the synergistic effect of polyols, fatty amines and phosphate/ketone complexes, an efficient silicone pressure-sensitive adhesive removal solution was developed, solving the problem of difficult removal of silicone pressure-sensitive adhesive residues in the prior art. , achieves rapid and thorough removal effect, ensuring the cleanliness and smoothness of the substrate surface.

CN119081796AActive Publication Date: 2024-12-06HUBEI SINOPHORUS ELECTRONIC MATERIALS CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202410999109.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-24
Publication Date
2024-12-06
Estimated Expiration
2044-07-24

AI Technical Summary

Technical Problem

In the prior art, there are fewer methods for removing silicone pressure-sensitive adhesive residues, which leads to the impact of the electrical properties of the substrate and it is difficult for existing cleaning agents to completely remove residues after high-temperature curing.

Method used

Using a degluing solution including polyols, fatty amines and phosphate/ketone complexes, provides alkaline conditions through fatty amines, and the synergistic action of phosphate and ketones accelerates the peeling rate of silicone pressure-sensitive glue, and improves polyols The wetting properties of the liquid ensure that there is no residue on the surface of the substrate after removal.

Benefits of technology

It realizes efficient and rapid removal of silicone pressure-sensitive adhesive residues, shortens the glue removal time, and ensures that the removed substrate surface is smooth and without residue. It is especially suitable for sample sheets after multiple high-temperature baking and vacuum processes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
  • Figure SMS_2
    Figure SMS_2
Patent Text Reader

Abstract

The invention provides an organosilicone pressure-sensitive adhesive removing solution and an application process thereof, the organosilicone pressure-sensitive adhesive removing solution comprises the following components in percentage by weight: 8-15% of polyol, 3-7% of fatty amine, 4-20% of a cosolvent and the balance of a solvent, and the cosolvent is a compound of phosphate and ketone; according to the invention, fatty amine is added into the adhesive removing solution, so that the stripping rate of the organic silicon pressure-sensitive adhesive can be accelerated; a phosphate group and a ketone group in the cosolvent cooperate with each other and are combined with active end groups at two ends of a siloxane adhesive in the organosilicone pressure-sensitive adhesive to promote removal of the organosilicone pressure-sensitive adhesive, the aliphatic amine and the cosolvent form a'stripping and pulling 'effect on the organosilicone pressure-sensitive adhesive, stubborn residual adhesive falls off and is dissolved in the solvent, the polyhydric alcohol reduces the surface tension of a solution, and the adhesion of the organosilicone pressure-sensitive adhesive is improved. And the surface of the sample is kept flat and smooth. The photoresist removing liquid is reasonable in formula, is not easy to volatilize, and can completely remove the organic silicon pressure-sensitive residual adhesive, so that a sample wafer subjected to photoresist removal has good roughness.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of cleaning agents for semiconductor industry, and in particular to an organic silicon pressure-sensitive adhesive degumming liquid and an application process thereof. Background Art

[0002] With the promotion of applications such as high-performance computing, data centers, in-vehicle displays, and business conferences, the demand for displays used to display large amounts of information in various industries is increasing. The semiconductor display field is developing rapidly and has attracted social attention. Among them, micro-light-emitting diodes (Micro-LEDs) are traditional LEDs that are miniaturized to form an array with micron-level spacing to achieve ultra-high resolution, which can be used in the display field. Compared with traditional liquid crystal displays (LCDs) and organic light-emitting displays (OLEDs), Micro-LED displays have the advantages of long luminous life, high brightness, thin and light volume, low power consumption, and high pixel density, becoming the representative of the third generation of displays with high authenticity, interactive and personalized displays as the main features.

[0003] Currently, Micro-LED is limited by the mass transfer technology of lamp beads, and most displays are small in size. Glass front and back wiring screen splicing technology is one of the solutions. Silicone pressure-sensitive adhesive protective film will be used for wiring on the front and back of the glass. Silicone pressure-sensitive adhesive protective film has strong adhesion. After the substrate has been subjected to multiple high-temperature baking and vacuum processes, a large amount of silicone pressure-sensitive adhesive will remain after the protective film is torn off, and it is stubborn and difficult to remove, affecting the electrical properties of the substrate and subsequent processes.

[0004] In the prior art, the preparation and performance of organosilicon pressure-sensitive adhesives have been studied extensively and in depth, but the research on the removal method of organosilicon pressure-sensitive adhesive residues is relatively rare. Therefore, it is very necessary to provide a degumming solution that can effectively remove the organosilicon pressure-sensitive adhesive residues on the surface of the substrate without affecting the performance of the substrate. Summary of the invention

[0005] The main purpose of the present invention is to overcome the shortcomings of the prior art and provide a silicone pressure-sensitive adhesive degumming liquid which is not easy to volatilize, has a fast degumming rate and a good degumming effect.

[0006] To achieve the above object, the technical solution adopted by the present invention is: A silicone pressure-sensitive adhesive debonding solution comprises, by weight percentage, 8-15% of polyol, 3-7% of fatty amine, 4-20% of co-solvent, and the balance being solvent.

[0007] Wherein, the polyol is one or more of ethylene glycol, 1,2-propylene glycol, 1,4-butanediol, 1,6-hexanediol, neopentyl glycol, and glycerol. The polyol reduces the surface tension of the solution and improves the wettability of the liquid medicine.

[0008] The fatty amine is at least one of ethylenediamine, isopropylamine, 1,4-butylenediamine, tert-butylamine and 2-ethylhexylamine. The fatty amine substance can provide alkaline conditions for removing the organic silicon pressure sensitive adhesive, promote the dissolution of the organic silicon pressure sensitive adhesive on the substrate, and accelerate the stripping rate of the organic silicon pressure sensitive adhesive.

[0009] The cosolvent is a compound of phosphate ester and ketone, and the weight ratio of phosphate ester to ketone is 1:2-1:5; preferably, the weight ratio of phosphate ester to ketone is 1:3. The synergistic effect of the compound of phosphate ester and ketone improves the surface activity of the substrate and accelerates the removal speed of the silicone pressure-sensitive adhesive.

[0010] Furthermore, the phosphate ester is at least one of trimethyl phosphate, triethyl phosphate, tripropyl phosphate, tributyl phosphate, tri(2-ethylhexyl) phosphate, tricresyl phosphate, dimethyl phosphate, diethyl phosphate, dibutyl phosphate, di(2-ethylhexyl) phosphate, and tetraethylmethylene diphosphate.

[0011] Furthermore, the ketone is at least one of dicyclopropyl ketone, cyclopentyl ethyl ketone and dicyclohexyl methyl ketone.

[0012] Furthermore, the solvent is at least one of dimethyl sulfoxide, sulfolane, dimethyl sulfone, N,N-dimethylformamide, N-methylpiperazine, N-ethylpiperazine, diethyl sulfone and tetramethylene sulfone, and dimethyl sulfoxide is more preferred. The organic solvent has good water solubility and can effectively dissolve the silicone pressure-sensitive adhesive and promote the removal of the silicone pressure-sensitive adhesive.

[0013] The degumming liquid of the present invention can fully spread and penetrate on the surface of the substrate; the fatty amine can provide alkaline conditions for removing the silicone pressure-sensitive adhesive, promote the dissolution of the silicone pressure-sensitive adhesive on the substrate, and accelerate the stripping rate of the silicone pressure-sensitive adhesive; a cosolvent of a compound of phosphate and ketone is used, wherein the phosphate group (O=P-ORx) and the ketone group (O=C-Ry) cooperate with each other and combine with the active end groups at both ends of the siloxane adhesive in the silicone pressure-sensitive adhesive to promote the removal of the silicone pressure-sensitive adhesive, and the fatty amine and the cosolvent form a "peeling and pulling" effect on the silicone pressure-sensitive adhesive, so that the stubborn residual adhesive falls off and dissolves in the solvent; the polyol organic matter can improve the wettability of the liquid, can clean the surface particles and residues, keep the sample surface after degumming without residue, and have good roughness; the water-soluble organic solvent promotes the dissolution and removal of the residual film. The synergistic effect of all components of the present invention accelerates the degumming speed and enhances the degumming effect.

[0014] The present invention also provides the use of the above-mentioned adhesive removal solution in removing the organic silicon pressure-sensitive adhesive remaining on the semiconductor sample after high-temperature curing.

[0015] Furthermore, the application process of the adhesive remover in removing the high-temperature cured organic silicon pressure-sensitive adhesive remaining on the semiconductor sample specifically comprises the following steps: S1: Pour the silicone pressure-sensitive adhesive debonding liquid into the debonding tank, and after heating, vertically place the sample to be debonded with the silicone pressure-sensitive adhesive into the debonding tank for soaking; S2: After soaking for a certain period of time, first vertically place the sample in a cleaning tank filled with N-methylpyrrolidone and soak it at room temperature for 5-10 minutes, then vertically place the sample in deionized water for cleaning and drying; S3: Observe the sample after debonding under a microscope to confirm whether the silicone pressure-sensitive adhesive remains and the roughness of the sample surface.

[0016] Furthermore, in S1, the soaking is pulling or ultrasonic soaking to obtain a better removal effect.

[0017] Furthermore, in S1, the degumming solution is immersed in the solution at a temperature of 50-80°C for a time of 5-10 minutes.

[0018] Further preferably, the degumming solution immersion temperature is 60-70°C.

[0019] Furthermore, in S2, N-methylpyrrolidone is first used to clean the degumming liquid remaining on the surface of the sample, and then deionized water is used to clean it, so as to achieve a thorough cleaning effect.

[0020] Compared with the prior art, the present invention has the following beneficial effects: 1. The degumming liquid of the present invention enhances the permeability and solubility of the degumming liquid through the synergistic effect of fatty amine, phosphate group (O=P-ORx) and ketone group (O=C-Ry), so that the organic silicon pressure-sensitive adhesive layer remaining on the sample after high-temperature curing can be peeled off, and the stubborn residual adhesive can be removed and dissolved into the degumming liquid; the addition of polyol can remove surface particles and residues, so that the surface of the sample after degumming is clean and has good roughness.

[0021] 2. The degumming liquid prepared by the present invention can efficiently and quickly strip the silicone pressure-sensitive adhesive by adjusting the content of each component in the degumming liquid, greatly shortening the degumming time, and the surface of the substrate after stripping is smooth and free of residue; the degumming liquid of the present invention is particularly capable of removing the silicone pressure-sensitive adhesive remaining on the sample after multiple high-temperature baking and vacuum processes. DETAILED DESCRIPTION

[0022] In order to better understand the present invention, the present invention is further described in detail below in conjunction with tables and examples, but the scope of protection claimed in the present invention is not limited to the following examples.

[0023] The degumming solution of the present invention can be obtained by simply mixing the components described in the following examples and comparative examples.

[0024] Table 1 Components and contents of degumming solutions of Examples 1-14 and Comparative Examples 1-6

[0025] The present invention also provides a process for applying the above-mentioned adhesive removal solution to remove the organic silicon pressure-sensitive adhesive remaining on the semiconductor sample after high-temperature curing, which specifically comprises the following steps: S1: Pour the silicone pressure-sensitive adhesive debonding liquid into the debonding tank, heat it to 70°C, and vertically place the sample to be debonded with the silicone pressure-sensitive adhesive into the debonding tank for ultrasonic immersion; S2: After soaking for a certain period of time, the sample is first placed vertically in a cleaning tank filled with N-methylpyrrolidone and left to soak at room temperature for 5 minutes, and then the sample is placed vertically in deionized water for cleaning and drying; S3: Observe the sample after debonding under an optical microscope to confirm whether the silicone pressure-sensitive adhesive remains. Observe the sample after debonding under an atomic force microscope to confirm the surface roughness after debonding.

[0026] S4: According to the removal effect, if it is confirmed under an optical microscope that the residual glue is completely removed, stop immersing and record the immersion time and surface roughness; if it is confirmed under an optical microscope that the residual glue is not cleaned, repeat steps S1-S3 and increase the immersion time of the glue removal solution by 5 minutes each time. The immersion time shall not exceed 40 minutes until it is completely removed or stop at 40 minutes, and record the immersion time and surface roughness.

[0027] Performance Test: The sample sheets (3*3cm in size) of the organic silicone pressure-sensitive adhesive to be removed were immersed in the organic silicone pressure-sensitive adhesive degumming solution described in the embodiment and the comparative example, respectively, at a soaking temperature of 70°C and a soaking time of 5 minutes. The soaking time was increased by 5 minutes each time according to the removal effect, and the soaking time did not exceed 40 minutes until the removal was complete or stopped at 40 minutes. The soaking time was recorded. After the stripping was completed, the samples were washed with N-methylpyrrolidone and deionized water in turn and dried, and the removal effect of the degumming solution was observed under a microscope. The test results are shown in Table 2.

[0028] Evaluation criteria for silicone pressure-sensitive adhesive removal: Advantages: The surface after degumming is smooth and has no residue; Good: There is no residue on the surface after degumming, but there are slight ups and downs; Poor: There is no residue on the surface after degumming, but there are obvious ups and downs or there is residue on the surface.

[0029] Table 2 Removal of silicone pressure-sensitive adhesive on samples in Examples and Comparative Examples

[0030] According to the results of the above-mentioned embodiments and comparative examples, it can be seen that the degumming solutions provided in embodiments 1-14 can completely remove the silicone pressure-sensitive adhesive on the surface of the sample within 5 minutes, and keep the surface of the sample flat and smooth. Compared with comparative example 1, the embodiment shows that adding polyols to the degumming solution can keep the surface of the sample flat and smooth; compared with the embodiment, comparative examples 2 and 4-6 show that adding fatty amines or co-solvents to the degumming solution can quickly and efficiently remove the silicone pressure-sensitive adhesive; compared with the embodiment, comparative example 3 shows that adding a certain amount of fatty amines to the degumming solution can achieve an efficient and fast degumming effect. It can be seen that the three components in the degumming solution of the present invention have a synergistic effect on the removal of the silicone pressure-sensitive adhesive remaining on the sample after multiple high-temperature baking and vacuum processes.

[0031] The above embodiments are only preferred technical solutions of the present invention and should not be regarded as limiting the present invention. The protection scope of the present invention shall be the technical solutions recorded in the claims, including equivalent replacement solutions of the technical features in the technical solutions recorded in the claims. That is, equivalent replacement improvements within this scope are also within the protection scope of the present invention.

Claims

1. A silicone pressure-sensitive adhesive degumming liquid, characterized in that: The invention comprises the following components in weight percentage: 8-15% of polyol, 3-7% of fatty amine, 4-20% of auxiliary solvent and the balance of solvent.

2. The silicone pressure-sensitive adhesive remover according to claim 1, characterized in that: The polyol is one or more of ethylene glycol, 1,2-propylene glycol, 1,4-butanediol, 1,6-hexanediol, neopentyl glycol and glycerol.

3. The silicone pressure-sensitive adhesive remover according to claim 1, characterized in that: The fatty amine is at least one of ethylenediamine, isopropylamine, 1,4-butanediamine, tert-butylamine and 2-ethylhexylamine.

4. The silicone pressure-sensitive adhesive remover according to claim 1, characterized in that: The cosolvent is a compound of phosphate ester and ketone, and the weight ratio of the phosphate ester to the ketone is 1:2-1:

5.

5. The silicone pressure-sensitive adhesive remover according to claim 4, characterized in that: The phosphate ester is at least one of trimethyl phosphate, triethyl phosphate, tripropyl phosphate, tributyl phosphate, tri(2-ethylhexyl) phosphate, tricresyl phosphate, dimethyl phosphate, diethyl phosphate, dibutyl phosphate, di(2-ethylhexyl) phosphate or tetraethylmethylene diphosphate.

6. The silicone pressure-sensitive adhesive remover according to claim 4, characterized in that: The ketone is at least one of dicyclopropyl ketone, cyclopentyl ethyl ketone or dicyclohexyl methyl ketone.

7. The silicone pressure-sensitive adhesive remover according to claim 1, characterized in that: The solvent is at least one of dimethyl sulfoxide, sulfolane, dimethyl sulfone, N,N-dimethylformamide, N-methylpiperazine, N-ethylpiperazine, diethyl sulfone or tetramethylene sulfone.

8. Use of the organic silicon pressure sensitive adhesive remover according to claim 1 in removing organic silicon pressure sensitive adhesive remaining on semiconductor samples after high temperature curing.

9. The use according to claim 8, characterized in that: The process of the application comprises the following steps: S1: Pour the silicone pressure-sensitive adhesive debonding liquid into the debonding tank, and after heating, vertically place the sample to be debonded with the silicone pressure-sensitive adhesive into the debonding tank for soaking; S2: After soaking, first vertically place the sample in a cleaning tank filled with N-methylpyrrolidone and soak it at room temperature for 5-10 minutes, then vertically place the sample in deionized water for cleaning and drying; S3: Observe the sample after debonding under a microscope to confirm whether there is any glue residue and the roughness of the sample surface.

10. The use according to claim 9, characterized in that: In S1, the degumming solution is immersed in the solution at a temperature of 50-80°C for a period of 5-10 minutes.

Citation Information

Patent Citations

  • Degumming agent and method for recovering IC from electronic device

    CN104745334A

  • Positive photo-resist stripping solution for semiconductor bump processing

    CN106154772A

  • Process solution composition for treating polymers

    CN115074189A

  • Degumming liquid as well as preparation method and application thereof

    CN115895802A

  • Label removal solution for returnable beverage bottles