Concrete bridge deck-asphalt pavement base interface indentation machine and indentation parameter design method
By designing the interface indentation machinery and indentation parameter design methods for concrete bridge deck-asphalt paving base, the problems of insufficient interface roughness and low construction efficiency in traditional interface disposal methods are solved, and efficient interface processing and interlayer bonding are achieved. Improve performance to meet the needs of large-area mechanized construction.
Patent Information
- Application Number
- CN202411295395.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-14
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2044-09-14
AI Technical Summary
The interface disposal method of traditional concrete bridge deck-asphalt paving base has problems such as insufficient interface roughness, low construction efficiency, large noise pollution and high material costs, which cannot meet the needs of large-area mechanized construction.
A concrete bridge deck-asphalt paving base interface indentation machinery and indentation parameters design method was designed. The three-steel wheel roller frame was equipped with indentation rollers and steel or iron indentation teeth, which was realized through the cockpit and positioning antenna. Constant-speed linear indentation, combined with 3D printing and experiment optimization of indentation parameters, improve interface roughness and interlayer bonding performance.
It achieves rapid and convenient improvement of the roughness of the concrete base interface, improves the bonding performance between asphalt paving layers, meets the needs of large-area mechanized construction, has high construction efficiency, does not damage the integrity of concrete aggregates, and no additional material costs.
Smart Images

Figure CN119083268A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of concrete bridge deck construction machinery, in particular to a concrete bridge deck-asphalt pavement base interface indentation machinery and an indentation parameter design method. Background Art
[0002] In the process of concrete bridge deck-asphalt pavement construction, in order to improve the bonding performance between the concrete base and the asphalt pavement layer, the concrete interface needs to be roughened to remove the slurry on the concrete surface, thereby improving the interlayer bonding performance of the concrete bridge deck. However, the traditional concrete bridge deck-asphalt pavement base interface treatment method has certain defects, such as:
[0003] The roughening process of the concrete interface is to pull out a simple rough texture by a roughening tool before the initial setting of the concrete. The roughness of the concrete interface formed by this method is not high, and the structural depth TD is only about 0.5mm, which cannot meet the needs of the industry. The roughening process of the concrete interface is to remove the interface slurry after the strength is formed by using tools such as a roughening hammer. This process is applied to bridge deck paving, and the construction efficiency is too low to meet the large-scale construction of concrete bridge decks. The existing mainstream bridge deck shot blasting construction process is often accompanied by large noise pollution during the interface treatment process, and the material cost of the shot loss must be borne. Therefore, the present invention designs a concrete bridge deck-asphalt pavement base interface indentation machine and an indentation parameter design method, wherein the indentation machine can quickly and conveniently improve the roughness of the concrete base interface, and the machine can meet the needs of large-scale mechanized construction of bridge decks, and will not destroy the integrity of concrete aggregates during the construction process. The construction efficiency is high, there is no dust, the construction quality is better, and there is no additional material cost, thereby solving the problems caused by the existing concrete bridge deck-asphalt pavement base interface treatment construction. The indentation parameter design method can determine the construction time of the indentation machine and further improve the indentation tooth parameters of the indentation machine, so as to better improve the interlayer bonding performance between the base concrete indentation treatment interface and the asphalt pavement layer. Summary of the invention
[0004] In view of the problems existing in the above-mentioned traditional concrete bridge deck-asphalt pavement base interface treatment method, the present invention designs a concrete bridge deck-asphalt pavement base interface indentation machine and indentation parameter design method, which is specifically implemented through the following technical solutions:
[0005] A concrete bridge deck-asphalt pavement base interface indentation machine and an indentation parameter design method, wherein the indentation machine includes a machine body, an indentation roller, an indentation tooth, a cockpit, a speed control panel, a positioning antenna, a steering wheel, and the like.
[0006] The creasing machine uses a three-steel wheel roller frame as the mechanical body, and the mechanical body is equipped with three creasing rollers in the form of one in front and two in the back. The driving paths between the creasing rollers do not overlap each other, and a layer of creasing teeth is connected to the outer side of each creasing roller.
[0007] A cockpit is fixed on the top surface of the mechanical body. A steering wheel, a speed control panel and a display terminal are arranged inside the cockpit. A positioning antenna is arranged at the rear of the cockpit and is connected to the display terminal.
[0008] The indentation teeth on the indentation roller are made of steel, iron or the like, which can bear the weight of the indentation machine without deformation, and a large amount of cement concrete material will not adhere during the indentation process.
[0009] The connection between the indentation teeth and the indentation roller is achieved by welding, bonding, etc., which can ensure that the indentation teeth are tightly fitted on the indentation roller without slipping.
[0010] When the creasing machine is driving, the display terminal in the cockpit reflects the driving speed and direction through the positioning antenna, and the driving speed and direction of the creasing machine are adjusted through the speed control panel and the steering wheel. The creasing teeth on the creasing roller are used to creasing the surface of the base cement concrete, ensuring that the creasing machine produces uniform pit-shaped grooves on the cement concrete surface in a uniform and linear manner.
[0011] The indentation parameter design method of the indentation machine may include the following steps:
[0012] Step 1, pouring cement concrete into a concrete mold, and taking out the cement concrete after solidifying for 1h, 2h, 3h, and 4h under standard curing conditions;
[0013] Step 2: prefabricate the initial concrete interface indentation plate by 3D printing or other technologies, penetrate and indent the cement concrete at different setting times, and stop and remove the indentation plate when the penetration depth reaches about 5 mm;
[0014] Step 3, after the cement concrete is indented, the cement concrete specimen is demoulded after being cured under standard conditions for 1-2 days, and then taken out after continuing to be cured for 7 days, and the cement concrete interface slurry after indentation is brushed off with a wire brush, and the weight change of the cement concrete before and after brushing is weighed as the slurry weight, and then the difficulty of brushing off the cement concrete slurry under different setting times is compared;
[0015] Step 4: Apply asphalt and spread gravel on the cement concrete specimen after indentation treatment, and then spread asphalt mixture to make a cement concrete + asphalt mixture composite structure specimen. Perform a 45° oblique shear test on the composite specimen to measure the interlayer failure load F of the composite structure specimen under different setting times. Combined with the cross-sectional area A of the composite specimen, the interlayer shear strength is calculated by the following formula:
[0016]
[0017] Step 5, determining the indentation timing parameters by comprehensively considering the ease of brushing off the slurry at the indentation interface of cement concrete at different setting times and the change in interlayer shear strength;
[0018] Step 6: Keep the indentation area of the indentation plate unchanged and adjust the indentation density. When the cement concrete is cured under standard conditions to the determined indentation time, perform concrete penetration indentation and repeat the oblique shear test to compare the changes in interlayer shear strength of different indentation densities and determine a reasonable indentation density.
[0019] Step 7, keep the indentation area and density of the indentation plate unchanged, adjust the indentation section inclination angle, when the cement concrete is cured under standard conditions to the determined indentation time, perform concrete penetration indentation and repeat the oblique shear test, compare the change of interlayer shear strength with different indentation section inclination angles, and determine a reasonable indentation section inclination angle;
[0020] Step 8. Keep the indentation area, density and cross-sectional inclination of the indentation plate unchanged, and adjust the indentation shape. When the cement concrete is cured under standard conditions to the determined indentation time, conduct concrete penetration indentation and repeat the oblique shear test. Use a steel brush and a roughening hammer to set control specimens under traditional interface treatment methods such as roughening, brushing and chiseling. By comparing the shear strength between layers under different interface treatment methods, a more reasonable indentation shape is determined, and the determined indentation area, density, cross-sectional inclination and shape are used as the shape parameters of the indentation teeth equipped with the indentation machine.
[0021] Beneficial effects:
[0022] Compared with the traditional concrete bridge deck-asphalt pavement base interface treatment method, the advantages of the concrete bridge deck-asphalt pavement base interface indentation machine and indentation parameter design method designed in the present invention are specifically manifested in:
[0023] 1. The concrete indentation operation can be completed by indentation machinery and equipment, which can quickly and conveniently improve the roughness of the concrete base interface and better enhance the interlayer bonding between it and the asphalt pavement layer. In addition, the indentation machinery can save more manpower, thereby improving construction efficiency and meeting the needs of large-scale mechanized construction of bridge decks.
[0024] 2. The indentation teeth equipped with the indentation machine can press out pit-shaped grooves during construction. Compared with traditional strip grooves, it can cope with shear stress in different directions. At the same time, the indentation machine can also control the speed and direction of the indentation operation, making the pressed grooves more uniform and beautiful.
[0025] 3. The invented indentation parameter design method can determine the construction timing of the indentation machine and continuously improve the indentation tooth shape parameters of the indentation machine, thereby greatly enhancing the interlayer bonding performance of the concrete bridge deck-asphalt pavement indentation treatment interface. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1 This is a schematic diagram of the mechanical structure of the concrete bridge deck-asphalt pavement base interface indentation of the present invention.
[0027] Figure 2 yes Figure 1 Left View
[0028] Figure 3 This is a flow chart of the indentation parameter design method of the present invention.
[0029] Figure 4 This is a bar graph of the weight of the slurry removed from the indentation interface under different setting times of the present invention.
[0030] Figure 5 This is a graph showing the change in interlayer shear strength under initial concrete interface indentation plate interface treatment at different setting times of the present invention.
[0031] Figure 6 Schematic diagram of shape parameters of indentation teeth on the indentation plate of the present invention
[0032] Figure 7 This is a bar graph of shear strength between concrete bridge deck and asphalt pavement layers of different interface types of the present invention.
[0033] Figure 8 This is a schematic diagram of the shape parameters of the indentation teeth equipped with the indentation machine for the concrete bridge deck-asphalt pavement base interface of the present invention.
[0034] Fig. 9 This is a schematic diagram of the indentation roller equipped with the concrete bridge deck-asphalt pavement base interface indentation machine of the present invention
[0035] The meanings of the marks in the accompanying drawings are as follows: 1: mechanical body; 2: indentation roller; 3: indentation teeth; 4: cockpit; 5: speed control panel; 6: positioning antenna; 7: steering wheel; 8: display terminal. DETAILED DESCRIPTION
[0036] The technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. However, the embodiments given are not intended to limit the present invention. All other embodiments obtained by ordinary technicians in the field based on the embodiments of the present invention without making any creative work shall fall within the scope of protection of the present invention.
[0037] Schematic diagram of the mechanical structure of the indentation at the interface between concrete bridge deck and asphalt pavement base Figure 1 As shown, it mainly includes a mechanical body, an indentation roller, an indentation tooth, a cockpit, a speed control panel, a positioning antenna and a steering wheel.
[0038] The left side view of the indentation machine of the concrete bridge deck-asphalt pavement base interface is as follows Figure 2 As shown, the creasing machine uses a three-steel wheel roller frame as the mechanical body, and the mechanical body is equipped with three creasing rollers in the form of one in front and two in the back. The driving paths between the creasing rollers do not overlap each other, and a layer of creasing teeth is connected to the outer side of each creasing roller.
[0039] A cockpit is fixed on the top surface of the mechanical body, and inside the cockpit are provided with a steering wheel, a speed control panel and a display terminal. A positioning antenna is arranged at the rear of the cockpit, and the positioning antenna is connected to the display terminal.
[0040] The process of the indentation parameter design method of the indentation machine is as follows Figure 3 As shown, the specific steps include:
[0041] Step 1, pour cement concrete into a cylindrical cement concrete mold with a diameter of 10 cm and a height of 5 cm according to a C40 cement concrete mix ratio of cement: sand: gravel: water = 398: 667: 1240: 195, then place the cement concrete specimen in a constant temperature curing box for curing under standard conditions, and take out the cement concrete after it solidifies for 1h, 2h, 3h, and 4h respectively;
[0042] Step 2: Prefabricate an initial concrete interface indentation plate (right angle - 7) with a rectangular cross-section, no inclination, and 7 indentation teeth by 3D printing technology, and then use a universal testing machine to penetrate the cement concrete with the indentation plate, and stop and remove the plate when the penetration depth reaches about 5 mm;
[0043] Step 3: After the cement concrete is indented, the cement concrete specimen is placed in a constant temperature curing box and cured under standard conditions for 1-2 days before demoulding. It is then taken out after continuing to be cured for 7 days, and the cement concrete interface slurry after indentation is brushed off with a wire brush. Figure 4 The weight of cement concrete slurry removed at different setting times is measured, and it is found that the weight of cement concrete slurry removed after setting for 3-4 hours is smaller, and the slurry is easier to brush off;
[0044] Step 4: Preferably, apply 1.6 kg / m2 of water to the cement concrete interface after indentation treatment. 2 SBS modified asphalt was used, and crushed stone with a particle size of 4.75-9.5 mm was spread with a coverage rate of about 65%. After the asphalt crushed stone was completely cooled, a 5 cm high C40 cement concrete + 5 cm high AC-13 asphalt mixture composite structure specimen was formed by Marshall compaction. The asphalt mixture oil-stone ratio was 5.0%, and the gradation design was shown in Table 1. The composite structure specimen was subjected to a 45° inclined shear test with a loading rate of 10 mm / min by a universal testing machine. The interlayer failure load F of the composite structure specimen under different setting times was measured, and combined with the cross-sectional area A of the composite specimen, the interlayer shear strength τ was obtained by the following formula:
[0045]
[0046] Table 1AC-13 asphalt mixture synthetic gradation
[0047]
[0048] The interlayer shear strength of the initial concrete interface indentation plate (right angle -7) interface treatment changes under different setting times. Figure 5 As shown, it is concluded that the shear strength of cement concrete is better after setting for about 3-4 hours;
[0049] Step 5: Determine the timing of concrete indentation at about 3-4 hours based on the ease of brushing off the slurry at the cement concrete indentation interface under different setting times and the change in interlayer shear strength;
[0050] Step 6, keeping the indentation area of the indentation plate unchanged, adjusting the number of indentation teeth to four and prefabricating the indentation plate (right angle - 4), curing the cement concrete under standard conditions for about 3-4 hours, performing cement concrete penetration indentation and repeating the oblique shear test, comparing the changes in interlayer shear strength of different indentation densities, and finding that the shear strength of the right angle - 4 indentation plate is higher;
[0051] Step 7, keeping the indentation area and density of the indentation plate unchanged, changing the rectangular cross-section indentation teeth of the right-angle-4 indentation plate into trapezoidal cross-section indentation teeth with a cross-section inclination angle of 60° and prefabricating the indentation plate (trapezoidal-4), curing the cement concrete under standard conditions for about 3-4 hours, performing cement concrete penetration indentation and repeating the oblique shear test, comparing the changes in interlayer shear strength of different indentation cross-section inclination angles, and finding that the shear strength of the trapezoidal-4 indentation plate is higher;
[0052] Step 8: Keep the indentation area, density and cross-sectional inclination of the indentation plate unchanged, change the shape of the indentation teeth to a circle and prefabricate the indentation plate (cone-4), cure the cement concrete under standard conditions for about 3-4 hours, perform cement concrete penetration indentation and repeat the oblique shear test, compare the changes in interlayer shear strength, and find that the shear strength of the trapezoid-4 indentation plate is still higher. Combine steel brushes and chiseling hammers to set control specimens under traditional interface treatment methods such as roughening, brushing, and chiseling. Take three groups of parallel specimens for each interface treatment method. The diameter of the designed indentation plates of different shapes is 5 cm. The schematic diagram of the shape parameters of the indentation teeth on the indentation plate is as follows: Figure 6 As shown in the figure, the shear strength bar graph of different interface types between concrete bridge deck and asphalt pavement is as follows Figure 7 shown.
[0053] The interlayer shear strength under different indentation shapes and traditional interface treatment methods was compared through the indentation parameter design method, and the reasonable indentation parameters of the indentation machine were obtained:
[0054] (1) The indentation timing parameters should be selected when the cement concrete solidifies for about 3-4 hours under standard curing conditions.
[0055] (2) Figure 8 The schematic diagram of the shape parameters of the indentation teeth is shown. The indentation shape parameters are selected as follows: the long side of the upper bottom surface is 25 mm, the short side is 14 mm, the cross section is a trapezoidal indentation tooth with an inclination angle of 60°, and the indentation tooth height is preferably set to 5 mm.
[0056] like Fig. 9 The schematic diagram of the indentation roller structure shown in the figure adopts steel indentation tooth material, and the indentation teeth with the above-mentioned indentation shape parameters are tightly fitted on the indentation roller by welding.
[0057] When cement concrete solidifies for about 3-4 hours under standard curing conditions, the indentation construction work of cement concrete is carried out by means of an indentation machine. During the driving process of the indentation machine, the display terminal in the cockpit reflects the driving speed and direction through the positioning antenna, and adjusts the driving speed and direction of the indentation machine through the speed control panel and the steering wheel. The surface of the base cement concrete is indented by the indentation teeth on the indentation roller, so that the indentation machine produces uniform pit-shaped grooves on the surface of the cement concrete in a uniform and linear indentation manner.
[0058] Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions of the aforementioned embodiments, or to make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A concrete bridge deck-asphalt pavement interface indentation machine and indentation parameter design method, characterized in that The concrete bridge deck-asphalt pavement base interface indentation machine used comprises a machine body (1), an indentation roller (2), indentation teeth (3), a cockpit (4), a speed control panel (5), a positioning antenna (6), a steering wheel (7), and a display terminal (8). The indentation machine uses a three-steel wheel roller frame as the machine body (1). The machine body (1) is equipped with three indentation rollers (2) in the form of one in front and two in the back. The driving paths between the indentation rollers (2) do not overlap each other. A layer of indentation teeth (3) is connected to the outer side of each indentation roller (2). A cockpit (4) is fixed on the top surface of the machine body (1). The cockpit (4) is provided with a steering wheel (7), a speed control panel (5) and a display terminal (8). A positioning antenna (6) is arranged at the rear of the cockpit (4). The positioning antenna (6) is connected to the display terminal (8).
2. The concrete bridge deck-asphalt pavement base interface indentation construction machine according to claim 1, characterized in that The construction timing of the indentation machine and the shape parameters of the indentation teeth (3) are determined by an indentation parameter design method, and the design method includes the following steps: Step 1, pouring cement concrete into a concrete mold, and taking out the cement concrete after solidifying for 1h, 2h, 3h, and 4h under standard curing conditions; Step 2, prefabricate an initial concrete interface indentation plate, penetrate and indent the cement concrete at different setting times through the concrete interface indentation plate, and stop and remove the indentation plate when the penetration depth reaches about 5 mm; Step 3, after the cement concrete is indented, the cement concrete specimen is demoulded after curing for 1-2 days under standard conditions, and then taken out after continuing to cure for 7 days. The cement concrete interface slurry after indentation is brushed off with a wire brush to compare the ease of brushing off the cement concrete slurry under different setting times; Step 4: Apply asphalt and spread gravel on the cement concrete specimen after indentation treatment, and then spread asphalt mixture to make a cement concrete + asphalt mixture composite structure specimen. Perform a 45° oblique shear test on the composite specimen to measure the interlayer failure load F of the composite structure specimen under different setting times, and combine the cross-sectional area A of the composite specimen to obtain the interlayer shear strength τ by the following formula: Step 5, determining the indentation timing parameters by comprehensively considering the ease of brushing off the slurry at the cement concrete indentation interface under different setting times and the change in interlayer shear strength; Step 6: Keep the indentation area of the indentation plate unchanged and adjust the indentation density. When the cement concrete is cured under standard conditions to the determined indentation time, perform concrete penetration indentation and repeat the oblique shear test to compare the changes in interlayer shear strength of different indentation densities and determine a reasonable indentation density. Step 7, keep the indentation area and density of the indentation plate unchanged, and then adjust the indentation section inclination angle. When the cement concrete is cured under standard conditions to the determined indentation time, perform concrete penetration indentation and repeat the oblique shear test, compare the change of interlayer shear strength of different indentation section inclination angles, and determine a reasonable indentation section inclination angle. Step 8: Keep the indentation area, density and cross-sectional inclination of the indentation plate unchanged, and then change the indentation shape. When the cement concrete is cured under standard conditions to the determined indentation time, perform concrete penetration indentation and repeat the oblique shear test. Use a steel brush and a roughening hammer to set control specimens under traditional interface treatment methods such as roughening, brushing and roughening. By comparing the interlayer shear strength under different interface treatment methods, determine a more reasonable indentation shape, and use the determined indentation area, density, cross-sectional inclination and shape as the shape parameters of the indentation teeth (3) equipped with the indentation machine.
3. The concrete bridge deck-asphalt pavement interface indentation machine according to claim 1 is characterized in that The indentation teeth (3) on the indentation roller (2) can be made of steel, iron or other materials that can bear the weight of the indentation machine without deformation and will not adhere to a large amount of cement concrete during the indentation process.
4. The concrete bridge deck according to claim 1. Asphalt pavement base interface indentation machine, characterized in that The connection between the indentation teeth (3) and the indentation roller (2) can be achieved by welding, bonding or the like, which can ensure that the indentation teeth (3) are tightly fitted on the indentation roller (2) and do not slip.
5. The concrete bridge deck-asphalt pavement interface indentation machine according to claim 1, characterized in that During the driving process of the creasing machine, the display terminal (8) in the cockpit (4) reflects the driving speed and direction through the positioning antenna (6), and adjusts the driving speed and direction of the creasing machine through the speed control panel (5) and the steering wheel (7). The creasing teeth (3) on the creasing roller (2) are used to perform creasing treatment on the base cement concrete surface, ensuring that the creasing machine produces uniform pit-shaped grooves on the cement concrete surface in a uniform and linear creasing manner.
6. The indentation parameter design method according to claim 2, characterized in that In step 2, the indentation plate can be prefabricated by using 3D printing and other technologies to accurately prefabricate the indentation plate with specific shape parameters.
7. The indentation parameter design method according to claim 2, characterized in that The difficulty of brushing off the cement concrete slurry in step 3 is evaluated by the difference in weight before and after brushing off the cement concrete, i.e., the slurry weight.
Citation Information
Patent Citations
Rubber powder modified asphalt macadam bridge surface waterproof layer and construction method
CN101220579A
Cement pavement embossing device for road construction
CN115262333A
Ultra-thin overlay one-time paving forming device
CN214168675U
Paving construction method, pavement structure, and longitudinal groove forming instrument for pavement
US20170159250A1