Manufacturing method of double-sided photovoltaic cell
By textured processing and transparent conductive oxide deposition of silicon wafers of double-sided photovoltaic cells, tiny pits are formed, which solves the problem of poor surface absorption and refractive effects after cutting, and improves the photoelectric conversion efficiency and battery performance.
Patent Information
- Application Number
- CN202411270347.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-11
- Publication Date
- 2024-12-06
AI Technical Summary
In the production of double-sided photovoltaic cells, after the silicon wafer is cut through diamond wire or laser, the cut surface has poor absorption and refractive effect on light, affecting the photoelectric conversion efficiency.
Using single crystal silicon material, a randomly distributed tiny pits are formed through textured treatment and transparent conductive oxide deposition technology, which increases the absorption and reflection of light. Specific steps include: cleaning and etching the surface of the silicon wafer, depositing transparent conductive oxides, and improving its surface flatness through chemical or mechanical treatment.
It improves the photoelectric conversion efficiency, enhances the absorption and reflection ability of light, and improves the performance of the battery.
Smart Images

Figure CN119092598A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of battery manufacturing, and in particular to a method for manufacturing a double-sided photovoltaic cell. Background Art
[0002] Bifacial photovoltaic cells, also known as double-sided solar cells, are photovoltaic cells that can receive sunlight from two directions and convert it into electrical energy. Unlike traditional single-sided photovoltaic cells, the back of bifacial photovoltaic cells also has photoelectric conversion capabilities, thanks to their special design and manufacturing process.
[0003] In the production of bifacial photovoltaic cells, silicon is basically used as the main material for the production of cells. Silicon is made into silicon wafers, which are then installed on both sides of the cell. A layer of transparent oxide is attached to the silicon wafer on the back of the cell as a backplane, allowing light to shine from the back of the photovoltaic cell to the silicon wafer.
[0004] In the process of making silicon wafers, silicon wafers are cut into silicon wafers by diamond wire or laser, and then the cut surface of the silicon wafer is used to absorb and refract light. However, the effect of only using the cut surface of the silicon wafer to absorb and refract light is poor. Summary of the invention
[0005] The purpose of the present application is to solve the problem raised in the above-mentioned background technology that in the process of manufacturing silicon wafers, silicon wafers are cut into silicon wafers by diamond wire or laser, and then the surface of the silicon wafers after cutting is used to absorb and refract light, but only the surface of the silicon wafers after cutting is used to absorb and refract light, and the effect is poor. The present application provides a method for manufacturing double-sided photovoltaic cells.
[0006] In order to achieve the above-mentioned purpose, this application specifically adopts the following technical solutions:
[0007] A method for manufacturing a double-sided photovoltaic cell, the manufacturing method comprising:
[0008] S1: Select silicon as the main material, the selected silicon material is single crystal silicon, select transparent conductive oxide as the backplane of the battery, and make the single crystal silicon into silicon wafers;
[0009] S2: After the single crystal silicon is made into a silicon wafer, the surface of the silicon wafer is textured;
[0010] S3: depositing a transparent conductive oxide on the back side of the silicon wafer and treating the transparent oxide;
[0011] S4: Making electrodes on the front and back of the battery, and encapsulating the manufactured battery cell between two layers of plastic film;
[0012] S5: Finished cells are tested for efficiency and classified according to performance.
[0013] By adopting the above technical methods, the surface of the silicon wafer is cleaned and processed, and then the surface of the cabinet is textured, and then a transparent conductive oxide is deposited on the back of the silicon wafer, so that randomly distributed tiny pits can be formed on the surface of the silicon wafer to increase light absorption and reflection.
[0014] Furthermore, the single crystal silicon is grown into silicon crystal using a Czochralski process.
[0015] Furthermore, the silicon crystal is cut into thin slices using a slicing technique, and the slicing technique is diamond wire cutting or laser cutting.
[0016] Furthermore, the silicon wafer is subjected to texturing treatment, and the texturing treatment adopts a wet chemical etching method.
[0017] Furthermore, a transparent conductive oxide is deposited on the back of the silicon wafer, and the transparent conductive oxide is TCO. The TCO layer is deposited on the back of the silicon wafer using physical vapor deposition or chemical vapor deposition technology.
[0018] Furthermore, the TCO layer is subjected to surface treatment, and the surface treatment is chemical etching or mechanical polishing.
[0019] Furthermore, the silicon wafer is coated with a photoresist, and the photoresist is used to define an area to be etched during exposure and development processes.
[0020] In summary, the present application includes at least one of the following beneficial effects:
[0021] 1. In the present application, after a silicon rod formed of single crystal silicon is cut into silicon wafers, the silicon wafers are thoroughly cleaned, cleaned with an organic solvent such as acetone or ethanol and deionized water, and the natural oxide layer is removed by pickling, and then the silicon wafers are placed in an etching solution. Common etching solutions include a mixture of hydrofluoric acid (HF), nitric acid (HNO3), acetic acid (CH3COOH) and deionized water. The surface of the silicon wafer can produce tiny pits on the surface under the action of these etching solutions, thereby increasing the absorption and reflection of light and improving the photoelectric conversion effect of the silicon wafer under light. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 It is a first three-dimensional structural schematic diagram of the toolbox in this application. DETAILED DESCRIPTION
[0023] The following is combined with Figure 1 This application is described in further detail.
[0024] The embodiment of the present application discloses a method for manufacturing a double-sided photovoltaic cell.
[0025] Reference Figure 1 , a method for manufacturing a double-sided photovoltaic cell, the manufacturing method comprising:
[0026] S1: Select silicon as the main material, the selected silicon material is single crystal silicon, select transparent conductive oxide as the backplane of the battery, and make the single crystal silicon into silicon wafers;
[0027] S2: After the single crystal silicon is made into a silicon wafer, the surface of the silicon wafer is textured;
[0028] S3: depositing a transparent conductive oxide on the back side of the silicon wafer and treating the transparent oxide;
[0029] S4: Making electrodes on the front and back of the battery, and encapsulating the manufactured battery cell between two layers of plastic film;
[0030] S5: Finished cells are tested for efficiency and classified according to performance.
[0031] When supporting a group of bifacial photovoltaic cells, first select single crystal silicon, then make the single crystal silicon into silicon wafers, then clean and process the surface of the silicon wafers, then texture the surface of the cabinet, then deposit transparent conductive oxide on the back of the silicon wafers, then place the silicon wafers between layers of plastic film to form a cell, then install electrodes on the cell, and complete the production of bifacial photovoltaic cells. After the single crystal silicon is made into silicon wafers, the surface of the silicon wafers is processed by texturing, so that randomly distributed tiny pits can be formed on the surface of the silicon wafers to increase light absorption and reflection.
[0032] Specifically, the single crystal silicon is grown into silicon crystal using a Czochralski process.
[0033] First, high-purity polysilicon raw materials are placed in a quartz crucible. The polysilicon is melted by induction heating or resistance heating at a high temperature (about 1420°C). A small single crystal silicon seed is immersed in the molten silicon, and then slowly rotated and pulled upward. By precisely controlling the temperature gradient and pulling speed, the silicon is gradually crystallized from the molten state to form a single crystal silicon rod. The Czochralski method can grow large-diameter single crystal silicon rods, which are suitable for large-scale production.
[0034] Specifically, the silicon crystal is cut into thin slices using a slicing technique, and the slicing technique is diamond wire cutting or laser cutting.
[0035] After the single crystal silicon rods are produced, they are cut using a diamond wire cutting machine or a laser cutting machine to improve the efficiency of silicon wafer production.
[0036] Specifically, the silicon wafer is subjected to texturing treatment, and the texturing treatment adopts a wet chemical etching method.
[0037] First, the silicon wafer needs to be thoroughly cleaned, using organic solvents such as acetone or ethanol and deionized water for cleaning, and acid pickling to remove the natural oxide layer. Then the silicon wafer is placed in an etching solution. Common etching solutions are a mixture of hydrofluoric acid (HF), nitric acid (HNO3), acetic acid (CH3COOH) and deionized water. These etching solutions can create tiny pits on the surface of the silicon wafer, increasing the absorption and reflection of light.
[0038] Specifically, a transparent conductive oxide is deposited on the back of the silicon wafer, and the transparent conductive oxide is TCO. The TCO layer is deposited on the back of the silicon wafer using a physical vapor deposition or chemical vapor deposition technique.
[0039] Commonly used TCO materials include indium tin oxide (ITO), zinc oxide (ZnO), aluminum zinc oxide (AZO), etc. The deposition process requires precise control of parameters such as temperature, pressure, gas flow and deposition time. After deposition, the silicon wafer usually needs to be annealed to improve the crystallinity and conductivity of the TCO layer so that light can pass normally through the back of the silicon wafer.
[0040] Specifically, the TCO layer is subjected to surface treatment, and the surface treatment is chemical etching or mechanical polishing.
[0041] After the TCO layer is attached to the back of the silicon wafer, it is chemically etched or mechanically polished to improve its surface flatness and light transmittance, thereby further improving the efficiency of light passing through the TCO layer.
[0042] Specifically, the silicon wafer is coated with a photoresist, and the photoresist is used to define the area to be etched during the exposure and development process.
[0043] Photoresist is coated on the silicon wafer, and then the area to be etched is defined through exposure and development processes, so that the photoresist can protect the unexposed area during the etching process.
Claims
1. A method for manufacturing a bifacial photovoltaic cell, characterized in that: The method for manufacturing a double-sided photovoltaic cell comprises: S1: Select silicon as the main material, the selected silicon material is single crystal silicon, select transparent conductive oxide as the backplane of the battery, and make the single crystal silicon into silicon wafers; S2: After the single crystal silicon is made into a silicon wafer, the surface of the silicon wafer is textured; S3: depositing a transparent conductive oxide on the back side of the silicon wafer and treating the transparent oxide; S4: Making electrodes on the front and back of the battery, and encapsulating the manufactured battery cell between two layers of plastic film; S5: Finished batteries are tested for efficiency and classified according to performance.
2. A method for manufacturing a double-sided photovoltaic cell according to claim 1, characterized in that: The single crystal silicon is grown as a silicon crystal using a Czochralski process.
3. A method for manufacturing a double-sided photovoltaic cell according to claim 2, characterized in that: The silicon crystal is cut into thin slices using a slicing technique, such as diamond wire cutting or laser cutting.
4. A method for manufacturing a double-sided photovoltaic cell according to claim 3, characterized in that: The silicon wafer is subjected to texturing treatment, and the texturing treatment adopts a wet slip etching method.
5. A method for manufacturing a double-sided photovoltaic cell according to claim 1, characterized in that: A transparent conductive oxide is deposited on the back of the silicon wafer. The transparent conductive oxide is TCO. The TCO layer is deposited on the back of the silicon wafer using a physical vapor deposition or chemical vapor deposition technique.
6. A method for manufacturing a double-sided photovoltaic cell according to claim 5, characterized in that: The TCO layer is subjected to surface treatment, wherein the surface treatment is chemical etching or mechanical polishing.
7. A method for manufacturing a double-sided photovoltaic cell according to claim 3, characterized in that: The silicon wafer is coated with a photoresist, and the photoresist is used to define the area to be etched during the exposure and development process.