Oil sludge viscosity reduction and dehydration biological agent suitable for oil sludge treatment
By using biological matrix agents, modified hydroxyapatite additives and tablet additives in sludge treatment, the problems of low dehydration efficiency, poor separation rate and poor viscosity reduction effects are solved, and more efficient sludge treatment effects are achieved.
Patent Information
- Application Number
- CN202411912598.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-12-24
- Publication Date
- 2025-03-21
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The low dehydration efficiency of oil sludge, poor separation rate and poor viscosity reduction effects in the existing sludge treatment technology limit the efficiency of the product.
A sludge viscosity-reducing and dehydrating biological agent is used, including biological matrix agent, hydroxyapatite additive and tablet additive, with a mass ratio of (5-7):3:1. Among them, the biological matrix agent is microorganisms such as Bacillus, and the hydroxyapatite additive is improved by the modification liquid and ball milling treatment, and the sheet additive is improved by the combination of heat treatment and ball milling fluid.
Through the coordination and coordination between raw materials, the dehydration efficiency of sludge, sludge separation rate and viscosity reduction effect are optimized, and the efficiency of product usage is significantly improved.
Smart Images

Figure BDA0005206092540000111 
Figure BDA0005206092540000121
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of oil sludge treatment, and in particular to an oil sludge viscosity reducing and dehydrating biological agent suitable for oil sludge treatment. Background Art
[0002] At present, in the process of oil field development, the crude oil produced fluid is often subject to corrosion, scaling, waxing and viscosity changes during its transportation and treatment from formation-wellbore-ground gathering and transportation pipeline network-centralized processing station-oil-water treatment due to changes in the properties of the produced fluid and the physical and chemical parameters of the process system, which has a serious impact on oil field production.
[0003] In the prior art, the sludge treatment has poor sludge dehydration efficiency, low sludge separation rate and poor viscosity reduction effect, which limits the use efficiency of the product. Based on this, the present invention further improves the treatment thereof. Summary of the invention
[0004] In view of the defects of the prior art, the purpose of the present invention is to provide a biological agent for reducing viscosity and dehydrating oil sludge suitable for oil sludge treatment, so as to solve the problems raised in the above background technology.
[0005] The present invention solves the technical problem by adopting the following technical scheme: The present invention provides a biological agent for reducing sludge viscosity and dehydrating sludge suitable for sludge treatment, wherein the biological agent for reducing sludge viscosity and dehydrating sludge comprises a bio-matrix agent, a hydroxyapatite additive and a flaky auxiliary agent; wherein the material mass ratio of the bio-matrix agent, the hydroxyapatite additive and the flaky auxiliary agent is (5-7):3:1.
[0006] Preferably, the biological matrix agent is prepared by mixing Bacillus, Alcaligenes faecalis, Gram-positive bacteria and Pseudomonas aeruginosa in a weight ratio of 2:1:1:1.
[0007] Preferably, the preparation method of the hydroxyapatite additive is:
[0008] S1: immersing aluminum borate whiskers into a sufficient amount of sodium silicate solution and stirring evenly, then filtering and drying to obtain an aluminum borate whisker agent;
[0009] 2-5 parts of nano carbon powder and 1-3 parts of silane coupling agent KH550 are added to 5-8 parts of sodium citrate solution, and then 2-4 parts of aluminum borate whisker agent are added and stirred to obtain a modified solution;
[0010] S2: immersing the hydroxyapatite in a modification liquid of 3-5 times the total amount of the hydroxyapatite and stirring the liquid, after the stirring is completed, filtering and drying are performed to obtain modified hydroxyapatite;
[0011] S3: ball-milling 5-8 parts of modified hydroxyapatite, 1-2 parts of stearic acid, 3-5 parts of 5% chitosan solution by mass and 3-6 parts of 4% yttrium nitrate solution by mass, filtering and drying after the ball-milling is completed to obtain a hydroxyapatite additive.
[0012] Preferably, the mass fraction of the sodium silicate solution is 4-6%; the mass fraction of the sodium citrate solution is 5-8%.
[0013] Preferably, the stirring speed of the immersion stirring treatment is 450-500 r / min, and the stirring is for 1-2 hours; the ball milling speed of the ball milling treatment is 1000-1500 r / min, and the ball milling is for 45-55 minutes.
[0014] Preferably, the preparation method of the flaky auxiliary agent is:
[0015] S11: heat treating the flaky talc at 210-220° C. for 10-15 min, cooling to 55° C. at a rate of 2-5° C. / min, and keeping the temperature to obtain a flaky talc agent;
[0016] S12: mixing talcum powder flakes and ball milling liquid in a weight ratio of 5:3 and subjecting them to ball milling. After the ball milling is completed, filtering and drying are performed to obtain a flake auxiliary agent.
[0017] Preferably, the mixing and ball milling treatment is carried out at a ball milling speed of 1500 r / min and the ball milling is carried out for 1 hour.
[0018] Preferably, the preparation method of the ball milling liquid is:
[0019] 1-3 parts of nano-silica sol, 2-4 parts of dopamine hydrochloride solution and 3-6 parts of nano-titanium dioxide are uniformly mixed, and then 2-4 parts of boron nitride are added and stirred thoroughly to obtain a ball milling solution.
[0020] Preferably, the mass fraction of the dopamine hydrochloride solution is 2-5%.
[0021] Compared with the prior art, the present invention has the following beneficial effects:
[0022] The viscosity reducing and dehydrating biological agent of the present invention adopts a biological matrix agent, a hydroxyapatite additive and a flaky auxiliary agent, and optimizes the oil sludge dehydration efficiency of the product through the blending and coordination between the raw materials, and coordinates and improves the oil sludge separation rate effect and the viscosity reducing effect; the hydroxyapatite additive adopts hydroxyapatite improved by a modified liquid, and then ball milled with stearic acid, chitosan solution and 4% by mass yttrium nitrate solution, and the performance effect of the product is enhanced through the blending and coordination between the raw materials and the coordination and synergy between the raw materials; at the same time, the flaky auxiliary agent adopts flaky talcum powder, which is heat-treated at 210-220 DEG C for 10-15 minutes, and then cooled to 55 DEG C at a rate of 2-5 DEG C / min, and heat-insulated, so as to optimize the stability of the flaky talcum powder, and the flaky auxiliary agent obtained by ball milling with a specific ball milling liquid and the hydroxyapatite additive have a more significant effect, thereby further improving the product performance. DETAILED DESCRIPTION
[0023] The following is a clear and complete description of the technical solutions in the embodiments of the present invention in conjunction with specific embodiments. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0024] The present embodiment provides a biological agent for reducing sludge viscosity and dehydrating sludge suitable for sludge treatment to solve the problems raised in the above-mentioned background technology.
[0025] The present invention solves the technical problem by adopting the following technical scheme: The present invention provides a biological agent for reducing sludge viscosity and dehydrating sludge suitable for sludge treatment, wherein the biological agent for reducing sludge viscosity and dehydrating sludge comprises a bio-matrix agent, a hydroxyapatite additive and a flaky auxiliary agent; wherein the material mass ratio of the bio-matrix agent, the hydroxyapatite additive and the flaky auxiliary agent is (5-7):3:1.
[0026] The biological matrix agent of this embodiment is prepared by mixing Bacillus, Alcaligenes faecalis, Gram-positive bacteria, and Pseudomonas aeruginosa in a weight ratio of 2:1:1:1.
[0027] The preparation method of the hydroxyapatite additive of this embodiment is:
[0028] S1: immersing aluminum borate whiskers into a sufficient amount of sodium silicate solution and stirring evenly, then filtering and drying to obtain an aluminum borate whisker agent;
[0029] 2-5 parts of nano carbon powder and 1-3 parts of silane coupling agent KH550 are added to 5-8 parts of sodium citrate solution, and then 2-4 parts of aluminum borate whisker agent are added and stirred to obtain a modified solution;
[0030] S2: immersing the hydroxyapatite in a modification liquid of 3-5 times the total amount of the hydroxyapatite and stirring the liquid, after the stirring is completed, filtering and drying are performed to obtain modified hydroxyapatite;
[0031] S3: ball-milling 5-8 parts of modified hydroxyapatite, 1-2 parts of stearic acid, 3-5 parts of 5% chitosan solution by mass and 3-6 parts of 4% yttrium nitrate solution by mass, filtering and drying after the ball-milling is completed to obtain a hydroxyapatite additive.
[0032] The mass fraction of the sodium silicate solution in this embodiment is 4-6%; the mass fraction of the sodium citrate solution is 5-8%.
[0033] The stirring speed of the immersion stirring treatment in this embodiment is 450-500 r / min, and the stirring is 1-2 hours; the ball milling speed of the ball milling treatment is 1000-1500 r / min, and the ball milling is 45-55 minutes.
[0034] The preparation method of the flaky auxiliary agent of this embodiment is:
[0035] S11: heat treating the flaky talc at 210-220° C. for 10-15 min, cooling to 55° C. at a rate of 2-5° C. / min, and keeping the temperature to obtain a flaky talc agent;
[0036] S12: mixing talcum powder flakes and ball milling liquid in a weight ratio of 5:3 and subjecting them to ball milling. After the ball milling is completed, filtering and drying are performed to obtain a flake auxiliary agent.
[0037] The mixing ball milling process in this embodiment has a ball milling speed of 1500 r / min and a ball milling time of 1 h.
[0038] The preparation method of the ball milling liquid of this embodiment is:
[0039] 1-3 parts of nano-silica sol, 2-4 parts of dopamine hydrochloride solution and 3-6 parts of nano-titanium dioxide are uniformly mixed, and then 2-4 parts of boron nitride are added and stirred thoroughly to obtain a ball milling solution.
[0040] The mass fraction of the dopamine hydrochloride solution in this embodiment is 2-5%.
[0041] Example 1.
[0042] The present embodiment provides a biological agent for reducing sludge viscosity and dehydrating sludge suitable for sludge treatment to solve the problems raised in the above-mentioned background technology.
[0043] The present invention solves the technical problem by adopting the following technical scheme: The present invention provides a biological agent for reducing sludge viscosity and dehydrating sludge suitable for sludge treatment, wherein the biological agent for reducing sludge viscosity and dehydrating sludge comprises a biological matrix agent, a hydroxyapatite additive and a flaky auxiliary agent; wherein the material mass ratio of the biological matrix agent, the hydroxyapatite additive and the flaky auxiliary agent is 5:3:1.
[0044] The biological matrix agent of this embodiment is prepared by mixing Bacillus, Alcaligenes faecalis, Gram-positive bacteria, and Pseudomonas aeruginosa in a weight ratio of 2:1:1:1.
[0045] The preparation method of the hydroxyapatite additive of this embodiment is:
[0046] S1: immersing aluminum borate whiskers into a sufficient amount of sodium silicate solution and stirring evenly, then filtering and drying to obtain an aluminum borate whisker agent;
[0047] 2 parts of nano carbon powder and 1 part of silane coupling agent KH550 are added to 5 parts of sodium citrate solution, and then 2 parts of aluminum borate whisker agent are added and stirred to obtain a modified solution;
[0048] S2: immersing the hydroxyapatite in a modification liquid of 3 times the total amount of the hydroxyapatite and stirring the liquid, after the stirring is completed, filtering and drying are performed to obtain modified hydroxyapatite;
[0049] S3: 5 parts of modified hydroxyapatite, 1 part of stearic acid, 3 parts of 5% by mass chitosan solution and 3 parts of 4% by mass yttrium nitrate solution are ball-milled. After the ball-milling is completed, the mixture is filtered and dried to obtain a hydroxyapatite additive.
[0050] The mass fraction of the sodium silicate solution in this embodiment is 4%; the mass fraction of the sodium citrate solution is 5%.
[0051] The stirring speed of the immersion stirring treatment in this embodiment is 450 r / min, and the stirring is for 1 hour; the ball milling speed of the ball milling treatment is 1000 r / min, and the ball milling is for 45 minutes.
[0052] The preparation method of the flaky auxiliary agent of this embodiment is:
[0053] S11: heat treating the flaky talc at 210° C. for 10 min, cooling to 55° C. at a rate of 2° C. / min, and keeping the temperature, to obtain a flaky talc agent;
[0054] S12: mixing talcum powder flakes and ball milling liquid in a weight ratio of 5:3 and subjecting them to ball milling. After the ball milling is completed, filtering and drying are performed to obtain a flake auxiliary agent.
[0055] The mixing ball milling process in this embodiment has a ball milling speed of 1500 r / min and a ball milling time of 1 h.
[0056] The preparation method of the ball milling liquid of this embodiment is:
[0057] 1 part of nano-silica sol, 2 parts of dopamine hydrochloride solution and 3 parts of nano-titanium dioxide were mixed evenly, and then 2 parts of boron nitride were added and stirred thoroughly to obtain a ball milling solution.
[0058] The mass fraction of the dopamine hydrochloride solution in this embodiment is 2%.
[0059] Example 2.
[0060] The present embodiment provides a biological agent for reducing sludge viscosity and dehydrating sludge suitable for sludge treatment to solve the problems raised in the above-mentioned background technology.
[0061] The present invention solves the technical problem by adopting the following technical scheme: The present invention provides a biological agent for reducing sludge viscosity and dehydrating sludge suitable for sludge treatment, wherein the biological agent for reducing sludge viscosity and dehydrating sludge comprises a biological matrix agent, a hydroxyapatite additive and a flaky auxiliary agent; wherein the material mass ratio of the biological matrix agent, the hydroxyapatite additive and the flaky auxiliary agent is 7:3:1.
[0062] The biological matrix agent of this embodiment is prepared by mixing Bacillus, Alcaligenes faecalis, Gram-positive bacteria, and Pseudomonas aeruginosa in a weight ratio of 2:1:1:1.
[0063] The preparation method of the hydroxyapatite additive of this embodiment is:
[0064] S1: immersing aluminum borate whiskers into a sufficient amount of sodium silicate solution and stirring evenly, then filtering and drying to obtain an aluminum borate whisker agent;
[0065] 5 parts of nano carbon powder and 3 parts of silane coupling agent KH550 are added to 8 parts of sodium citrate solution, and then 4 parts of aluminum borate whisker agent are added and stirred to obtain a modified solution;
[0066] S2: immersing the hydroxyapatite in a modification liquid of 5 times the total amount of the hydroxyapatite and stirring the liquid, after the stirring is completed, filtering and drying are performed to obtain modified hydroxyapatite;
[0067] S3: 8 parts of modified hydroxyapatite, 2 parts of stearic acid, 5 parts of 5% by mass chitosan solution and 6 parts of 4% by mass yttrium nitrate solution are ball-milled, and after the ball-milling is completed, the mixture is filtered and dried to obtain a hydroxyapatite additive.
[0068] The mass fraction of the sodium silicate solution in this embodiment is 6%; the mass fraction of the sodium citrate solution is 8%.
[0069] The stirring speed of the immersion stirring treatment in this embodiment is 500 r / min, and the stirring is for 2 hours; the ball milling speed of the ball milling treatment is 1500 r / min, and the ball milling is for 55 minutes.
[0070] The preparation method of the flaky auxiliary agent of this embodiment is:
[0071] S11: heat treating the flaky talc at 220° C. for 15 min, cooling to 55° C. at a rate of 5° C. / min, and keeping the temperature, to obtain a flaky talc agent;
[0072] S12: mixing talcum powder flakes and ball milling liquid in a weight ratio of 5:3 and subjecting them to ball milling. After the ball milling is completed, filtering and drying are performed to obtain a flake auxiliary agent.
[0073] The mixing ball milling process in this embodiment has a ball milling speed of 1500 r / min and a ball milling time of 1 h.
[0074] The preparation method of the ball milling liquid of this embodiment is:
[0075] 3 parts of nano-silica sol, 4 parts of dopamine hydrochloride solution and 6 parts of nano-titanium dioxide were mixed evenly, and then 4 parts of boron nitride were added and stirred thoroughly to obtain a ball milling solution.
[0076] The mass fraction of the dopamine hydrochloride solution in this embodiment is 5%.
[0077] Example 3.
[0078] The present embodiment provides a biological agent for reducing sludge viscosity and dehydrating sludge suitable for sludge treatment to solve the problems raised in the above-mentioned background technology.
[0079] The present invention solves the technical problem by adopting the following technical scheme: The present invention provides a biological agent for reducing sludge viscosity and dehydrating sludge suitable for sludge treatment, wherein the biological agent for reducing sludge viscosity and dehydrating sludge comprises a biological matrix agent, a hydroxyapatite additive and a flaky auxiliary agent; wherein the material mass ratio of the biological matrix agent, the hydroxyapatite additive and the flaky auxiliary agent is 6:3:1.
[0080] The biological matrix agent of this embodiment is prepared by mixing Bacillus, Alcaligenes faecalis, Gram-positive bacteria, and Pseudomonas aeruginosa in a weight ratio of 2:1:1:1.
[0081] The preparation method of the hydroxyapatite additive of this embodiment is:
[0082] S1: immersing aluminum borate whiskers into a sufficient amount of sodium silicate solution and stirring evenly, then filtering and drying to obtain an aluminum borate whisker agent;
[0083] 3.5 parts of nano carbon powder and 2 parts of silane coupling agent KH550 are added to 6.5 parts of sodium citrate solution, and then 3 parts of aluminum borate whisker agent are added and stirred to obtain a modified solution;
[0084] S2: immersing the hydroxyapatite in a modification liquid of 4 times the total amount of the hydroxyapatite and stirring the liquid, after the stirring is completed, filtering and drying are performed to obtain modified hydroxyapatite;
[0085] S3: 6.5 parts of modified hydroxyapatite, 1.5 parts of stearic acid, 4 parts of 5% by mass chitosan solution and 4.5 parts of 4% by mass yttrium nitrate solution are ball-milled, and after the ball-milling is completed, the mixture is filtered and dried to obtain a hydroxyapatite additive.
[0086] The mass fraction of the sodium silicate solution in this embodiment is 5%; the mass fraction of the sodium citrate solution is 6.5%.
[0087] The stirring speed of the immersion stirring treatment in this embodiment is 470 r / min, and the stirring is 1.5 hours; the ball milling speed of the ball milling treatment is 1250 r / min, and the ball milling is 50 minutes.
[0088] The preparation method of the flaky auxiliary agent of this embodiment is:
[0089] S11: heat treating the flaky talc at 215° C. for 12.5 min, cooling to 55° C. at a rate of 3.5° C. / min, and keeping the temperature, to obtain a flaky talc agent;
[0090] S12: mixing talcum powder flakes and ball milling liquid in a weight ratio of 5:3 and subjecting them to ball milling. After the ball milling is completed, filtering and drying are performed to obtain a flake auxiliary agent.
[0091] The mixing ball milling process in this embodiment has a ball milling speed of 1500 r / min and a ball milling time of 1 h.
[0092] The preparation method of the ball milling liquid of this embodiment is:
[0093] 2 parts of nano-silica sol, 3 parts of dopamine hydrochloride solution and 4.5 parts of nano-titanium dioxide were mixed evenly, and then 3 parts of boron nitride were added and stirred thoroughly to obtain a ball milling solution.
[0094] The mass fraction of the dopamine hydrochloride solution in this embodiment is 3.5%.
[0095] Example 4.
[0096] The present embodiment provides a biological agent for reducing sludge viscosity and dehydrating sludge suitable for sludge treatment to solve the problems raised in the above-mentioned background technology.
[0097] The present invention solves the technical problem by adopting the following technical scheme: The present invention provides a biological agent for reducing sludge viscosity and dehydrating sludge suitable for sludge treatment, wherein the biological agent for reducing sludge viscosity and dehydrating sludge comprises a biological matrix agent, a hydroxyapatite additive and a flaky auxiliary agent; wherein the material mass ratio of the biological matrix agent, the hydroxyapatite additive and the flaky auxiliary agent is 6:3:1.
[0098] The biological matrix agent of this embodiment is prepared by mixing Bacillus, Alcaligenes faecalis, Gram-positive bacteria, and Pseudomonas aeruginosa in a weight ratio of 2:1:1:1.
[0099] The preparation method of the hydroxyapatite additive of this embodiment is:
[0100] S1: immersing aluminum borate whiskers into a sufficient amount of sodium silicate solution and stirring evenly, then filtering and drying to obtain an aluminum borate whisker agent;
[0101] 3 parts of nano carbon powder and 2 parts of silane coupling agent KH550 are added to 6 parts of sodium citrate solution, and then 3 parts of aluminum borate whisker agent are added and stirred to obtain a modified solution;
[0102] S2: immersing the hydroxyapatite in a modification liquid of 4 times the total amount of the hydroxyapatite and stirring the liquid, after the stirring is completed, filtering and drying are performed to obtain modified hydroxyapatite;
[0103] S3: 6 parts of modified hydroxyapatite, 1 part of stearic acid, 4 parts of 5% by mass chitosan solution and 4 parts of 4% by mass yttrium nitrate solution are ball-milled, and after the ball-milling is completed, the mixture is filtered and dried to obtain a hydroxyapatite additive.
[0104] The mass fraction of the sodium silicate solution in this embodiment is 5%; the mass fraction of the sodium citrate solution is 6%.
[0105] The stirring speed of the immersion stirring treatment in this embodiment is 470 r / min, and the stirring is 1.2 hours; the ball milling speed of the ball milling treatment is 1200 r / min, and the ball milling is 48 minutes.
[0106] The preparation method of the flaky auxiliary agent of this embodiment is:
[0107] S11: heat treating the flaky talc at 212° C. for 12 min, cooling to 55° C. at a rate of 3° C. / min, and keeping the temperature, to obtain a flaky talc agent;
[0108] S12: mixing talcum powder flakes and ball milling liquid in a weight ratio of 5:3 and subjecting them to ball milling. After the ball milling is completed, filtering and drying are performed to obtain a flake auxiliary agent.
[0109] The mixing ball milling process in this embodiment has a ball milling speed of 1500 r / min and a ball milling time of 1 h.
[0110] The preparation method of the ball milling liquid of this embodiment is:
[0111] 2 parts of nano-silica sol, 3 parts of dopamine hydrochloride solution and 4 parts of nano-titanium dioxide were mixed evenly, and then 3 parts of boron nitride were added and stirred thoroughly to obtain a ball milling solution.
[0112] The mass fraction of the dopamine hydrochloride solution in this embodiment is 3%.
[0113] Example 5.
[0114] The present embodiment provides a biological agent for reducing sludge viscosity and dehydrating sludge suitable for sludge treatment to solve the problems raised in the above-mentioned background technology.
[0115] The present invention solves the technical problem by adopting the following technical scheme: The present invention provides a biological agent for reducing sludge viscosity and dehydrating sludge suitable for sludge treatment, wherein the biological agent for reducing sludge viscosity and dehydrating sludge comprises a biological matrix agent, a hydroxyapatite additive and a flaky auxiliary agent; wherein the material mass ratio of the biological matrix agent, the hydroxyapatite additive and the flaky auxiliary agent is 6:3:1.
[0116] The biological matrix agent of this embodiment is prepared by mixing Bacillus, Alcaligenes faecalis, Gram-positive bacteria, and Pseudomonas aeruginosa in a weight ratio of 2:1:1:1.
[0117] The preparation method of the hydroxyapatite additive of this embodiment is:
[0118] S1: immersing aluminum borate whiskers into a sufficient amount of sodium silicate solution and stirring evenly, then filtering and drying to obtain an aluminum borate whisker agent;
[0119] 4 parts of nano carbon powder and 2 parts of silane coupling agent KH550 are added to 7 parts of sodium citrate solution, and then 3 parts of aluminum borate whisker agent are added and stirred to obtain a modified solution;
[0120] S2: immersing the hydroxyapatite in a modification liquid of 4 times the total amount of the hydroxyapatite and stirring the liquid, after the stirring is completed, filtering and drying are performed to obtain modified hydroxyapatite;
[0121] S3: 6 parts of modified hydroxyapatite, 2 parts of stearic acid, 4 parts of 5% by mass chitosan solution and 5 parts of 4% by mass yttrium nitrate solution are ball-milled, and after the ball-milling is completed, the mixture is filtered and dried to obtain a hydroxyapatite additive.
[0122] The mass fraction of the sodium silicate solution in this embodiment is 5%; the mass fraction of the sodium citrate solution is 7%.
[0123] The stirring speed of the immersion stirring treatment in this embodiment is 490 r / min, and the stirring is for 2 hours; the ball milling speed of the ball milling treatment is 1480 r / min, and the ball milling is for 52 minutes.
[0124] The preparation method of the flaky auxiliary agent of this embodiment is:
[0125] S11: heat treating the flaky talc at 212° C. for 14 min, cooling to 55° C. at a rate of 4° C. / min, and keeping the temperature, to obtain a flaky talc agent;
[0126] S12: mixing talcum powder flakes and ball milling liquid in a weight ratio of 5:3 and subjecting them to ball milling. After the ball milling is completed, filtering and drying are performed to obtain a flake auxiliary agent.
[0127] The mixing ball milling process in this embodiment has a ball milling speed of 1500 r / min and a ball milling time of 1 h.
[0128] The preparation method of the ball milling liquid of this embodiment is:
[0129] 3 parts of nano-silica sol, 4 parts of dopamine hydrochloride solution and 5 parts of nano-titanium dioxide were mixed evenly, and then 3 parts of boron nitride were added and stirred thoroughly to obtain a ball milling solution.
[0130] The mass fraction of the dopamine hydrochloride solution in this embodiment is 4%.
[0131] Comparative Example 1.
[0132] The difference from Example 3 is that no hydroxyapatite additive is added.
[0133] Comparative Example 2.
[0134] The difference from Example 3 is that no modifying liquid is added to the hydroxyapatite additive.
[0135] Comparative Example 3.
[0136] The difference from Example 3 is that no S3 treatment is added to the hydroxyapatite additive.
[0137] Comparative Example 4.
[0138] The difference from Example 3 is that no aluminum borate whisker agent is added to the modified solution.
[0139] Comparative Example 5.
[0140] The difference from Example 3 is that no flake auxiliary agent is added.
[0141] Comparative Example 6.
[0142] The difference from Example 3 is that no ball milling liquid is added to the flaky auxiliary agent.
[0143] Comparative Example 7.
[0144] The difference from Example 3 is that nano titanium dioxide and boron nitride are not added to the ball milling liquid.
[0145] The product performances of Examples 1-5 and Comparative Examples 1-7 of the present invention were tested under conventional conditions, and the test results are as follows.
[0146]
[0147]
[0148] It can be seen from Examples 1-5 and Comparative Examples 1-7 that the products of Examples 1-5 of the present invention have excellent sludge dehydration efficiency, and at the same time, the sludge separation rate effect and the viscosity reduction effect are significant;
[0149] If neither hydroxyapatite additive nor flake additive is added to the product, the performance of the product will be significantly deteriorated. The combination of the two will have a synergistic effect and the product performance effect will be significant.
[0150] When no modifying liquid is added to the hydroxyapatite additive, no S3 treatment is added to the hydroxyapatite additive, no aluminum borate whisker agent is added to the modifying liquid, no ball milling liquid is added to the flaky auxiliary agent, and no nano titanium dioxide and boron nitride are added to the ball milling liquid, the performance of the products tends to deteriorate. Only the hydroxyapatite additive and flaky auxiliary agent obtained by the method of the present invention have the most significant performance effect of the product, and other methods are not as obvious as the effect of the present invention.
[0151] It will be apparent to those skilled in the art that the present invention is not limited to the details of the exemplary embodiments described above and that the present invention can be implemented in other specific forms without departing from the spirit or essential features of the present invention. Therefore, the embodiments should be considered exemplary and non-restrictive in all respects, and the scope of the present invention is defined by the appended claims rather than the above description, and it is intended that all changes falling within the meaning and scope of the equivalent elements of the claims be included in the present invention.
[0152] In addition, it should be understood that although the present specification is described according to implementation modes, not every implementation mode contains only one independent technical solution. This description of the specification is only for the sake of clarity. Those skilled in the art should regard the specification as a whole. The technical solutions in each embodiment may also be appropriately combined to form other implementation modes that can be understood by those skilled in the art.
Claims
1. A biological agent for reducing sludge viscosity and dehydrating sludge suitable for sludge treatment, characterized in that: The oil sludge viscosity reduction and dehydration biological agent comprises a biological matrix agent, a hydroxyapatite additive and a flaky auxiliary agent; wherein the material mass ratio of the biological matrix agent, the hydroxyapatite additive and the flaky auxiliary agent is (5-7):3:
1.
2. According to claim 1, a biological agent for reducing sludge viscosity and dehydrating sludge suitable for sludge treatment, characterized in that: The biological matrix agent is prepared by mixing Bacillus, Alcaligenes faecalis, Gram-positive bacteria and Pseudomonas aeruginosa in a weight ratio of 2:1:1:
1.
3. According to claim 1, a biological agent for reducing sludge viscosity and dehydrating sludge suitable for sludge treatment, characterized in that: The preparation method of the hydroxyapatite additive is: S1: immersing aluminum borate whiskers into a sufficient amount of sodium silicate solution and stirring evenly, then filtering and drying to obtain an aluminum borate whisker agent; 2-5 parts of nano carbon powder and 1-3 parts of silane coupling agent KH550 are added to 5-8 parts of sodium citrate solution, and then 2-4 parts of aluminum borate whisker agent are added and stirred to obtain a modified solution; S2: immersing the hydroxyapatite in a modification liquid of 3-5 times the total amount of the hydroxyapatite and stirring the liquid, after the stirring is completed, filtering and drying are performed to obtain modified hydroxyapatite; S3: ball-milling 5-8 parts of modified hydroxyapatite, 1-2 parts of stearic acid, 3-5 parts of 5% chitosan solution by mass and 3-6 parts of 4% yttrium nitrate solution by mass, filtering and drying after the ball-milling is completed to obtain a hydroxyapatite additive.
4. The biological agent for reducing sludge viscosity and dehydrating sludge suitable for sludge treatment according to claim 3, characterized in that: The mass fraction of the sodium silicate solution is 4-6%; the mass fraction of the sodium citrate solution is 5-8%.
5. The biological agent for reducing sludge viscosity and dehydrating sludge suitable for sludge treatment according to claim 3, characterized in that: The stirring speed of the immersion stirring treatment is 450-500 r / min, and the stirring is 1-2 hours; the ball milling speed of the ball milling treatment is 1000-1500 r / min, and the ball milling is 45-55 minutes.
6. The biological agent for reducing sludge viscosity and dehydrating sludge suitable for sludge treatment according to claim 3, characterized in that: The preparation method of the flaky auxiliary agent is: S11: heat treating the flaky talc at 210-220° C. for 10-15 min, cooling to 55° C. at a rate of 2-5° C. / min, and keeping the temperature to obtain a flaky talc agent; S12: mixing talcum powder flakes and ball milling liquid in a weight ratio of 5:3, and subjecting the mixture to ball milling. After the ball milling is completed, the mixture is filtered and dried to obtain a flake auxiliary agent.
7. The biological agent for reducing sludge viscosity and dehydrating sludge suitable for sludge treatment according to claim 6, characterized in that: The mixing and ball milling process was performed at a ball milling speed of 1500 r / min and the ball milling was performed for 1 hour.
8. The biological agent for reducing sludge viscosity and dehydrating sludge suitable for sludge treatment according to claim 6, characterized in that: The preparation method of the ball milling liquid is: 1-3 parts of nano-silica sol, 2-4 parts of dopamine hydrochloride solution and 3-6 parts of nano-titanium dioxide are uniformly mixed, and then 2-4 parts of boron nitride are added and stirred thoroughly to obtain a ball milling solution.
9. The biological agent for reducing sludge viscosity and dehydrating sludge suitable for sludge treatment according to claim 8, characterized in that: The mass fraction of the dopamine hydrochloride solution is 2-5%.