A metal-organic chemical vapor deposition apparatus and method
The centrally integrated MOCVD equipment design solves the problems of low thin film deposition uniformity, low equipment integration and low uptime of existing equipment, and realizes a high-efficiency and stable wafer growth process, reducing operation and maintenance costs and pollution risks.
Patent Information
- Application Number
- CN202611519052.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-29
- Publication Date
- 2026-11-10
AI Technical Summary
Existing MOCVD equipment suffers from problems such as poor uniformity of thin film deposition, low equipment integration, low degree of automation, high operation and maintenance costs, low uptime, and insufficient control over defects and particulate contamination in the reaction chamber structure design.
The equipment is a centrally integrated metal-organic chemical vapor deposition system for mass production, including fixtures, jigs, conveying mechanisms and reaction chambers. It is designed as a single-clamp, single-wafer mode without a base or spindle. Combined with a gas supply system and a robotic arm, it achieves unmanned operation. The jig is equipped with gas pipelines and guide plates to ensure uniform gas distribution and wafer rotation.
It improves the temperature uniformity of the reaction chamber, reduces equipment maintenance costs, increases uptime, ensures machine stability, reduces production costs and wafer contamination risks, and improves the consistency of wafer growth.
Smart Images

Figure CN123063740A_ABST
Abstract
Description
Technical Field
[0001] This application belongs to the field of semiconductor component fabrication technology, and specifically relates to a metal-organic chemical vapor deposition apparatus and method. Background Technology
[0002] Metal-organic chemical vapor deposition (MOCVD) is a key technology that uses metal-organic compounds as precursors to grow thin film materials on the substrate surface through gas-phase chemical reactions. It is widely used in high-tech fields such as semiconductors, optoelectronics, and new energy. In the fabrication of compound semiconductor devices such as gallium nitride and gallium arsenide, light-emitting diodes, and solar cells, it is the core equipment technology foundation supporting the development of related industries.
[0003] Current MOCVD equipment primarily comprises six core modules: the reaction chamber, the precursor delivery system, the heating system, the vacuum system, the exhaust gas treatment system, and the control system. With the rapid development of emerging fields such as Mini-LED, Micro-LED, and third-generation semiconductor power devices, the performance shortcomings of existing MOCVD equipment are becoming increasingly apparent, specifically manifested in the following deficiencies or problems: ① The unreasonable design of the reaction chamber structure leads to poor uniformity of thin film deposition, making it difficult to adapt to the fabrication requirements of large-size substrates and complex structures.
[0004] ② The equipment has low integration, low automation, high maintenance costs, and low utilization rate.
[0005] ③ Insufficient control over defects and particulate contamination affects product quality. Summary of the Invention
[0006] Based on the above analysis, the embodiments of the present invention aim to provide a metal-organic chemical vapor deposition (MOCVD) apparatus and method to solve one or more of the aforementioned problems existing in the prior art. The present invention can improve growth uniformity, effectively increase utilization rate, and enhance machine stability.
[0007] The objective of this invention is achieved as follows: A metal-organic chemical vapor deposition apparatus, comprising: A jig with loading space; The fixtures, each holding a wafer, are stacked longitudinally within the loading space of the fixture. A conveying mechanism having a conveyor belt and multiple transfer bins, wherein the conveyor belt is configured to transport the fixture to the corresponding transfer bin; The reaction chamber is configured as the site for the deposition reaction; there are multiple reaction chambers, each equipped with a transfer chamber.
[0008] Furthermore, the fixture is connected to a gas supply system configured to supply inert gas into the loading space of the fixture to ensure the cleanliness of the loading space.
[0009] Furthermore, the loading space is provided with an air inlet at the top and an air outlet at the bottom. The gas supply system introduces inert gas into the loading space through the air inlet at the top and the gas flows out through the air outlet at the bottom. Preferably, the loading space is maintained under positive gas pressure.
[0010] Furthermore, each of the fixtures is provided with a barcode, and the conveyor belt is provided with a barcode scanning device. The barcode scanning device is configured to scan the barcodes on the fixtures and upload the scanned information to the control system. The control system controls the conveyor belt to transfer each fixture to the transfer chamber of the corresponding reaction chamber based on the scanning information.
[0011] Furthermore, the reaction chamber is equipped with a rotatable carrier for mounting multiple clamps; The transfer chamber is equipped with a robotic arm and a transfer chamber door. The robotic arm is used to sequentially remove the fixtures and wafers from the reaction chamber after growth is completed, during the cooling stage, and place them in an empty fixture for cooling. It is also used to load new fixtures and wafers into the reaction chamber before the reaction chamber cools down to room temperature.
[0012] Furthermore, the reaction chamber is equipped with a heating wire, a baffle plate is provided above the heating wire, and the clamp is located above the baffle plate.
[0013] Furthermore, the barrier plate is made of any one of quartz, graphite, and silicon carbide.
[0014] Furthermore, the clamp is fixed to the side wall of the reaction chamber by a concave-convex interlocking structure.
[0015] Furthermore, the fixture is provided with a single wafer slot, a gas supply line is provided at the bottom of the wafer slot, and three first gas outlets are provided on the bottom surface of the wafer slot, which are connected to the gas supply line. The wafer trench has three second vent holes on its sidewall, which are connected to the gas supply pipeline through an internal airflow channel.
[0016] Furthermore, the interior of the reaction chamber is also equipped with a spray structure, which includes a spray head and a guide plate. The spray head is cylindrical and is connected to the top cover of the reaction chamber. Furthermore, the material of the deflector includes any one of quartz, graphite, and silicon carbide.
[0017] Odd-numbered spray heads are used to expel ammonia gas, while even-numbered spray heads are used to expel metal-organic sources carried by hydrogen / nitrogen gas.
[0018] On the other hand, a metal-organic chemical vapor deposition method is provided, using the aforementioned metal-organic chemical vapor deposition equipment, the method comprising the following steps: First, place the wafer on the fixture, and then load the multiple fixtures containing the wafer into the jig; The fixture containing the wafer and jig is placed on a conveyor belt and then transported to the transfer chamber via the conveyor belt. The robotic arm inside the transfer chamber transfers the fixture containing the wafers from the jig and places it in the reaction chamber, where the first batch of wafers begins to react and grow. After the first batch of wafers has completed reaction growth, the program ends. During the cooling phase, the door is opened, and the robotic arm inside the transfer chamber transfers the wafers and fixtures from the reaction chamber and places them in the hollow fixture inside the transfer chamber. By rotating the carrier inside the reaction chamber, all the first batch of wafers and fixtures after the reaction are taken out in sequence. Subsequently, before the reaction chamber cools down to room temperature, a new batch of wafers and fixtures is transferred to the reaction chamber via a robotic arm in the transfer chamber. At this time, the temperature inside the reaction chamber has not yet dropped to room temperature and still has a certain temperature. After the transfer is completed, the door is closed; the program is started, and the second batch of wafers begins growth. Repeat the above steps until all batches of wafer reaction growth are completed.
[0019] Furthermore, during the reaction process, the gas supply line delivers gas to the wafer through the first gas outlet at the bottom of the wafer tank and the second gas outlet on the side wall of the tank, thereby regulating its temperature and speed.
[0020] Compared with the prior art, the metal-organic chemical vapor deposition equipment and method provided by the present invention can achieve at least one of the following beneficial effects: a) This invention effectively improves the temperature uniformity of the reaction chamber; reduces equipment maintenance costs, shortens maintenance time, and increases uptime; reduces the impact of by-products and ensures machine stability.
[0021] b) This invention differs from the current mainstream. The designed metal-organic chemical vapor deposition equipment has the characteristics of being baseless, spindleless, and single-clip single-wafer. The designed central integrated system has the characteristics of unmanned operation, stability and high efficiency, and can effectively solve problems such as wafer contamination, difficulty in process traceability and consistency in the production process. Attached Figure Description
[0022] To more clearly illustrate the technical solutions in the embodiments of this specification or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments recorded in the embodiments of this specification. For those skilled in the art, other drawings can be obtained based on these drawings.
[0023] Figure 1 A schematic diagram of the centrally integrated production process for mass production of the metal-organic chemical vapor deposition equipment provided by the present invention. Figure 2 This is a schematic diagram of the overall structure of the fixture provided by the present invention; Figure 3 This is a schematic diagram of the internal structure of the fixture provided by the present invention; Figure 4 This is a schematic diagram of the structure of the fixture provided by the present invention, in which multiple clamps are installed. Figure 5 This is a schematic diagram of the structure of the reaction chamber provided by the present invention; Figure 6 This is a schematic diagram of the structure of the clamp provided by the present invention; Figure 7 This is a top view of the mounting fixture inside the reaction chamber provided by the present invention; Figure 8 This is a schematic diagram of the spray head structure provided by the present invention.
[0024] Figure label: 1. Workbench; 2. Conveyor belt; 3. Transfer chamber; 4. Transfer chamber door; 5. Fixture; 6. Heating wire; 7. Baffle plate; 8. Side wall; 9. Clamp; 10. Guide plate; 11. Spray head; 12. Top cover; 13. First vent; 14. Wafer tank; 15. Second vent; 16. Reaction chamber; 17. Gas pipeline. Detailed Implementation
[0025] To make the objectives, technical solutions, and advantages of the embodiments of this application clearer, the technical solutions of the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this application, not all embodiments. It should be noted that, unless otherwise specified, the implementation methods and features in the implementation methods in this disclosure can be combined, separated, interchanged, and / or rearranged. Based on the embodiments of this application, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of this application.
[0026] In the accompanying drawings, the dimensions and relative dimensions of components may be exaggerated for clarity and / or descriptive purposes. When exemplary embodiments can be implemented differently, a specific process sequence may be performed in a different order than that described. For example, two consecutively described processes may be performed substantially simultaneously or in the reverse order of their description. Furthermore, the same reference numerals denote the same components.
[0027] The terminology used herein is for the purpose of describing particular embodiments and is not intended to be limiting. As used herein, unless the context clearly indicates otherwise, the singular forms “a” and “the” are intended to include the plural forms as well. Furthermore, when the terms “comprising” and / or “including” and variations thereof are used in this specification, it indicates the presence of the stated features, integrals, steps, operations, parts, components, and / or groups thereof, but does not exclude the presence or addition of one or more other features, integrals, steps, operations, parts, components, and / or groups thereof. It should also be noted that, as used herein, the terms “substantially,” “about,” and other similar terms are used as approximate terms rather than as terms of degree, thus explaining the inherent biases in measurements, calculated values, and / or provided values that would be recognized by one of ordinary skill in the art.
[0028] Example 1 One specific embodiment of the present invention discloses a metal-organic chemical vapor deposition (MOCVD) apparatus, employing a centralized design concept for mass production. Multiple fixtures 9 can be placed within the reaction chamber 16, with each fixture 9 holding one wafer. The number of fixtures 9 inside the reaction chamber 16 can be adjusted according to specific product production requirements. Furthermore, the fixtures 9 and wafers are detachable, eliminating the need for manual operation. The production process involves the production personnel placing the wafer on the fixture 9 on the workbench 1, then using a jig 5 to secure the fixture 9 containing the wafer and place it on the conveyor belt 2. This application designs a "fully sealed jig 5" independent of the reaction chamber 16 and the conveying environment. The sealed environment provided by the jig 5 ensures that the wafer is not contaminated by external factors (even the cleanroom environment) during transport and waiting.
[0029] Specifically, such as Figures 1 to 8As shown, a metal-organic chemical vapor deposition (MOCVD) apparatus includes a fixture 5, clamps 9, a conveying mechanism, and a reaction chamber 16. Each fixture 5 provides a loading space, and each clamp 9 loads a wafer. Multiple clamps 9 loaded with wafers are stacked longitudinally within the loading space of the fixture 5. The fixture 5 is fully sealed to prevent contamination of the clamps 9 and wafers during conveying and waiting processes. The conveying mechanism has a conveyor belt 2 and multiple transfer chambers 3. The conveyor belt 2 is configured to transport the fixture 5 to the corresponding transfer chamber 3. The reaction chamber 16 is configured as the site for the deposition reaction. There are multiple reaction chambers 16, and each reaction chamber 16 is equipped with a transfer chamber 3.
[0030] In this embodiment, a rotatable carrier is provided in the reaction chamber 16, which is used to place multiple clamps 9; a robotic arm is provided in the transfer chamber 3, and the transfer chamber 3 is provided with a transfer chamber door 4; the robotic arm is used to take out the clamps 9 and wafers in the reaction chamber 16 after growth is completed in sequence during the cooling stage, and place them in an empty fixture 5 for cooling; and before the reaction chamber 16 cools down to room temperature, a new clamp 9 and wafer are loaded into the reaction chamber 16.
[0031] In one alternative embodiment, the clamp 9 is fixed to the side wall 8 of the reaction chamber 16 by a pin, and the fixing and releasing actions of the pin are pneumatically controlled. For example, compression control is provided by a cylinder, and a pneumatic valve controls the inflow and outflow of compressed nitrogen. By controlling the opening and closing of the pneumatic valve, the compressed nitrogen acts on the pin, causing it to press upward against the clamp 9 and fix it to the side wall 8 of the reaction chamber 16. By closing the pneumatic valve, the compressed air is released, the pin is released downward, and the clamp 9 is thus dislodged from the side wall 8.
[0032] After the growth process in reaction chamber 16 is complete, the internal temperature drops below 300°C. According to the program settings, transfer chamber door 4 opens, and the carrier containing fixtures 9 inside reaction chamber 16 begins to rotate, sequentially rotating fixtures 9 to the transfer door. When fixtures 9 reach the transfer door, a robotic arm inside transfer chamber 3 extends and clamps them. Once fixtures 9 are clamped, air is released by controlling a pneumatic valve (controlling the pin to push upwards or release downwards), causing the pins securing fixtures 9 to release downwards, thus detaching fixtures 9 from the side wall 8 of reaction chamber 16. The robotic arm places the removed fixtures 9 in an empty fixture 5 for cooling. The carrier then continues to rotate, sequentially removing all fixtures 9 + wafers. After all fixtures 9 are removed, the robotic arm sequentially removes new fixtures 9 + wafers and fixes them to the side wall 8 of reaction chamber 16 by controlling the pins via a pneumatic valve. After this process is completed, transfer chamber door 4 closes. The program resumes, and reaction chamber 16 begins the next growth cycle.
[0033] Traditional epitaxial growth involves placing a graphite disk containing the wafer in a reaction chamber for cooling after growth is complete. Once the temperature drops to 80°C, the top cover of the reaction chamber is opened to allow for wafer removal and replacement. The top cover is then closed, and the chamber is heated again to resume growth. In contrast, this embodiment uses a "clamp 9 + wafer" unit as a rapidly replaceable unit. Before the reaction chamber 16 has fully cooled, the wafer is "heat-exchanged" out via a robotic arm in the transfer chamber 3. The reaction chamber 16 itself maintains a certain temperature and is not exposed to the atmosphere. Once the new "clamp 9 + wafer" unit is installed, the temperature can be quickly raised to begin the next batch of production. This process reduces the cooling time of the wafer in the reaction chamber 16, shortening the overall growth time. This represents the ultimate embodiment of "centralized integration" in terms of production efficiency and is an effective solution to the current pain point of heating / cooling operations encroaching on operational capacity in epitaxial growth. This not only effectively improves equipment utilization but also significantly reduces material usage and production costs. After the wafer growth is complete and it cools to room temperature, conveyor belt 2 transports it to workbench 1. Production personnel remove the wafer from fixture 9. The wafer continues to flow for other processes, while fixture 9 and jig 5 are cleaned. The entire system can operate unmanned, greatly reducing uncontrollable risks caused by human factors, increasing production uptime, and reducing the requirements of the MOCVD system on the carrier. Furthermore, there is no need to open the reaction chamber 16, greatly maintaining the stability of the reaction chamber 16.
[0034] It should be noted that the reaction chamber 16 can form a sealed space. The transfer chamber 3 and the reaction chamber 16 are integrated. After the transfer chamber 3 enters the fixture 5 containing the clamp 9, the transfer chamber 3 will be evacuated to maintain the same pressure as the reaction chamber 16. Throughout the entire process, the top cover 12 of the reaction chamber 16 will not be opened.
[0035] In one alternative embodiment, the clamp 9 is placed horizontally within the fixture 5. The fixture 5 has a gas supply system at its top, configured to supply inert gas into the loading space of the fixture 5 to ensure the cleanliness of the loading space. The inert gas includes, but is not limited to, nitrogen and helium. The fixture 5 is connected to the gas supply system, and inert gas is blown downwards from the top of the fixture 5, filling the entire fixture 5 with inert gas, maintaining positive pressure, and ensuring the cleanliness of the interior of the fixture 5.
[0036] Specifically, the fixture 5 has a loading space inside, with an air inlet at the top and an air outlet at the bottom. The pure nitrogen supply system introduces inert gas into the loading space through the air inlet at the top and flows out through the air outlet at the bottom, thereby ensuring the cleanliness of the fixture 5. Preferably, the loading space maintains a positive gas pressure.
[0037] Furthermore, each fixture 5 is equipped with a barcode, and the conveyor belt 2 is equipped with a barcode scanning device. The barcode scanning device is configured to scan the barcodes on the fixtures 5 and upload the scanned information to the control system. Based on the scanned information, the control system controls the conveyor belt 2 to transfer each fixture 5 to the transfer chamber 3 of the corresponding reaction chamber 16. During operation, the barcode scanning device on the conveyor belt 2 scans the barcodes on the fixtures 5 and transfers the corresponding fixtures 5 to the transfer chamber 3 of the corresponding reaction chamber 16 to await processing. This process not only ensures the smooth operation of the entire production process but also enables real-time production tracking. Once a production anomaly is detected, the anomaly can be located and resolved immediately, ensuring the stability of the production line and improving utilization.
[0038] In this embodiment, the reaction chamber 16 is provided with a heating wire 6, and a baffle plate 7 is provided above the heating wire 6 to prevent gas from contacting the heating wire 6, causing wear and tear on the heating wire 6, and affecting the heating efficiency. The baffle plate 7 is made of materials including but not limited to quartz, graphite, and silicon carbide, and the clamp 9 is located above the baffle plate 7. Optionally, the heating wire 6 is made of tungsten wire and is fixed to the bottom of the reaction chamber 16.
[0039] Currently, mainstream MOCVD production carriers use graphite disks without fixture 9. In this embodiment, fixture 9 is located above the baffle plate 7, which differs from the current mainstream design (which uses graphite disks, or a large graphite disk + small graphite disk design, without fixture 9). The fixture 9 in this embodiment adopts a single-clamp, single-piece mode. Compared to the currently used large graphite disk / large disk-within-a-small-disk mode, this effectively reduces the stringent requirements on carrier materials, precision, and lifespan, greatly improving equipment uptime (facilitating replacement).
[0040] In other words, the fixture 9 is designed to clamp a single wafer, and the number of fixtures 9 can be determined according to the actual design. For example, the entire reaction chamber 16 contains a total of 4 sets of fixtures 9, which can realize the rotation and temperature control of the wafer. The fixture 9 is provided with a single wafer groove 14 (i.e., a recess), the bottom of which is empty to ensure that the heat energy output by the heating wire 6 can be directly transferred to the substrate; the bottom of the groove has a shrinkage design to prevent the substrate from falling; there is a gas supply pipe 17 in the middle of the bottom of the groove, and the gas exits from the three first gas outlets 13 of the gas supply pipe, which allows the substrate to be suspended.
[0041] Furthermore, the wafer trench 14 has three second vent holes 15 on its sidewall, which enable the wafer to rotate and ensure the uniformity of material deposition.
[0042] Compared to the current mainstream graphite disk or large disk + small disk design, the fixture 9 in this embodiment, by setting up a gas supply pipe 17, not only has a simple structure that is easy to manufacture, but also facilitates later maintenance and upkeep. There is a gas supply pipe 17 at the bottom of the groove, and the gas exits from three first gas outlets 13, ensuring that the wafer is in a suspended state and that the temperature is controlled in real time. There are three second gas outlets 15 on the side wall of the wafer tank 14 to ensure the wafer's self-rotation capability.
[0043] Secondly, each fixture 9 is independent, with better independence and less susceptibility to the influence of surrounding wafers; the single-wafer-single-clamp system offers high flexibility, enabling independent and precise control of the growth temperature and rotation speed of a single wafer, which is beneficial for controlling the stress and uniformity of wafer growth.
[0044] In this embodiment, each clamp 9 is mechanically fixed in the reaction chamber 16. Optionally, the clamp 9 can be fixed to the side wall 8 of the reaction chamber 16 by means of a tongue-and-groove interlocking structure and a pin.
[0045] In this embodiment, the reaction chamber 16 is further equipped with a spray structure, which includes a spray head 11 and a guide plate 10. The spray head 11 is cylindrical and is connected to the top cover of the reaction chamber 16, which is installed on the top of the chamber. A temperature reflectivity monitor is installed on the top of the top cover to detect the wafer temperature and reflectivity. The guide plate 10 directs the gas, such as ammonia and hydrogen / nitrogen, flowing from the spray head 11 directly to the wafer on the fixture 9, preventing eddies between the spray head 11 and the wafer / fixture 9 and ensuring the uniformity of epitaxial growth. The material of the guide plate 10 includes, but is not limited to, quartz, graphite, and silicon carbide.
[0046] The structure of the spray head 11 is designed with the appropriate number of layers (e.g., 3, 5, 7 layers, etc.) according to the actual product (e.g., LED, power device, laser, etc.), and is equipped with multi-layer guide plates 10. Among them, the odd-numbered spray heads 11 mainly carry ammonia gas, while the even-numbered spray heads 11 mainly carry the metal-organic source carried by hydrogen / nitrogen gas. Specifically, the number of spray heads 11 is multi-layered; the odd-numbered spray heads 11 are used to guide the outflowing ammonia gas directly to the wafer, while the even-numbered spray heads 11 are used to guide the outflowing hydrogen / nitrogen gas carried by the metal-organic source directly to the wafer.
[0047] Currently, mainstream MOCVD uses a large disk or a large disk + small disk structure. The large disk acts as a flow guide 10 for the gas from the vent to the wafer surface, requiring no additional flow guide. However, this embodiment uses a single-wafer, single-clamp fixture 9 production method. A gap exists between the vent and the wafer, which can cause airflow collapse within the cavity, resulting in uneven airflow and affecting epitaxial growth. Therefore, the flow guide 10 in this embodiment is designed to directly guide the gas flowing from the spray head 11 to the wafer, preventing eddies between the spray head 11 and the wafer and ensuring uniform epitaxial growth.
[0048] This embodiment also provides a metal-organic chemical vapor deposition method using the aforementioned metal-organic chemical vapor deposition equipment. The method includes the following steps: First, place the wafer on the fixture 9, and then load the multiple fixtures 9 containing the wafer into the jig 5; The fixture 5 containing the wafer and jig 9 is placed on the conveyor belt 2, and the fixture 5 is transported to the transfer chamber 3 via the conveyor belt 2. The robotic arm inside transfer chamber 3 transfers the wafer-containing fixture 9 from jig 5 and places it in reaction chamber 16. By controlling the pneumatic valve, compressed nitrogen gas in the cylinder is released, causing the pin fixing fixture 9 to push upwards, thus fixing fixture 9 to the side wall 8 of reaction chamber 16. The gas tubing is connected, and the gas flow is tested; the first batch of wafers begins to react and grow in reaction chamber 16. After the first batch of wafers has completed reaction growth, the program ends. During the cooling stage, the transfer chamber door is opened, and the robotic arm in the transfer chamber 3 transfers the wafers and fixtures 9 from the reaction chamber 16 and places them in the hollow fixture 5 in the transfer chamber 3. By rotating the carrier in the reaction chamber 16, all the first batch of wafers and fixtures 9 after the reaction are taken out in sequence. Subsequently, before the reaction chamber 16 cools down to room temperature, the next batch of new wafers and fixtures 9 are transferred to the reaction chamber 16 via a robotic arm in the transfer chamber 3. At this time, the temperature inside the reaction chamber 16 has not yet dropped to room temperature and still has a certain temperature. After the transfer is completed, the chamber door is closed. The program is started, and the second batch of wafers begins growth. Repeat the above steps until all batches of wafer reaction growth are completed.
[0049] During the reaction process, the gas supply line 17 delivers gas to the wafer through the first vent 13 at the bottom of the wafer tank 14 of the fixture 9 and the second vent 15 on the side wall of the tank, thereby regulating its temperature and speed. The working principle is as follows: When the growth temperature is set to 1080°C, the temperature reflectivity monitor on the top cover monitors the wafer temperature in real time during epitaxial layer growth. When the monitored wafer temperature reaches 1060°C, the monitor feeds this value back to the software. The software uses an algorithm to regulate the gas flow meter of the wafer at the monitoring position, reducing the gas output from the three first vent 13, thus lowering the wafer's suspension height. The reduced distance between the wafer and the bottom heating wire 6 increases the thermal radiation received, causing the wafer temperature to rise, and vice versa.
[0050] After the grown wafer and fixture 9 have cooled to room temperature, they are conveyed to workbench 1 via conveyor belt 2. The workers then remove the wafer, fixture 9, and jig 5 in sequence, and the wafer moves to the next process.
[0051] Compared with the prior art, the metal-organic chemical vapor deposition equipment and method provided in this embodiment can achieve the following beneficial effects: 1. Employing a centrally integrated production model, suitable for large-scale production. The entire production system is fully automated, eliminating the impact of human factors. This reduces stringent requirements on the production vehicle and lowers production costs. 2. No need to open the reaction chamber, thus ensuring chamber stability; 3. The clamp adopts a single-clamp, single-wafer design, which is fixed to the side wall of the reaction chamber for easy disassembly and maintenance. The single-clamp, single-wafer design offers advantages such as simple gas delivery piping, facilitating later maintenance; furthermore, it provides a relatively independent system, less susceptible to interference from surrounding wafers, and exhibits better independence. 4. The use of rotation and temperature control can effectively improve the quality of grown crystals and enhance wafer uniformity.
[0052] 5. Add a flow guide plate design to prevent eddies between the spray head and the wafer, ensuring the uniformity of epitaxial growth.
[0053] The specific embodiments described above further illustrate the purpose, technical solution, and beneficial effects of this application. It should be understood that the above description is only a specific embodiment of this application and is not intended to limit the scope of protection of this application. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of this application should be included within the scope of protection of this application.
Claims
1. A metal-organic chemical vapor deposition apparatus, characterized in that, include: A jig with loading space; The fixtures, each holding a wafer, are stacked longitudinally within the loading space of the fixture. A conveying mechanism having a conveyor belt and multiple transfer bins, wherein the conveyor belt is configured to transport the fixture to the corresponding transfer bin; The reaction chamber is configured as the site for the deposition reaction; there are multiple reaction chambers, each equipped with a transfer chamber.
2. The metal-organic chemical vapor deposition apparatus according to claim 1, characterized in that, The fixture is connected to a gas supply system configured to supply inert gas into the loading space of the fixture to ensure the cleanliness of the loading space.
3. The metal-organic chemical vapor deposition apparatus according to claim 1, characterized in that, The loading space has an air inlet at the top and an air outlet at the bottom. The gas supply system introduces inert gas into the loading space through the air inlet at the top and the gas flows out through the air outlet at the bottom. Preferably, the loading space is maintained under positive gas pressure.
4. The metal-organic chemical vapor deposition apparatus according to claim 1, characterized in that, Each fixture is equipped with a barcode, and the conveyor belt is equipped with a barcode scanning device. The barcode scanning device is configured to scan the barcodes on the fixtures and upload the scanned information to the control system. The control system controls the conveyor belt to transfer each fixture to the transfer chamber of the corresponding reaction chamber based on the scanning information.
5. The metal-organic chemical vapor deposition apparatus according to claim 1, characterized in that, The reaction chamber is equipped with a rotatable carrier for mounting multiple clamps. The transfer chamber is equipped with a robotic arm and a transfer chamber door. The robotic arm is used to sequentially remove the fixtures and wafers from the reaction chamber after growth is completed, during the cooling stage, and place them in an empty fixture for cooling. It is also used to load new fixtures and wafers into the reaction chamber before the reaction chamber cools down to room temperature.
6. The metal-organic chemical vapor deposition apparatus according to claim 1, characterized in that, The reaction chamber is equipped with a heating wire, and a baffle plate is provided above the heating wire. The clamp is located above the baffle plate. Preferably, the barrier plate is made of any one of quartz, graphite, and silicon carbide.
7. The metal-organic chemical vapor deposition apparatus according to claim 1, characterized in that, The clamp is fixed to the side wall of the reaction chamber by a concave-convex interlocking structure.
8. The metal-organic chemical vapor deposition apparatus according to claim 1, characterized in that, The fixture is provided with a single wafer slot, a gas supply line is provided at the bottom of the wafer slot, and three first gas outlets are provided on the bottom surface of the wafer slot, which are connected to the gas supply line. The wafer trench has three second vent holes on its sidewall, which are connected to the gas supply pipeline through an internal airflow channel.
9. The metal-organic chemical vapor deposition apparatus according to claim 1, characterized in that, The reaction chamber is also equipped with a spray structure, which includes a spray head and a guide plate. The spray head is cylindrical and is connected to the top cover of the reaction chamber. Preferably, the material of the guide plate includes any one of quartz, graphite, and silicon carbide; Odd-numbered spray heads are used to expel ammonia gas, while even-numbered spray heads are used to expel metal-organic sources carried by hydrogen / nitrogen gas.
10. A method for metal-organic chemical vapor deposition, characterized in that, Using the metal-organic chemical vapor deposition apparatus according to any one of claims 1 to 9, the method comprises the following steps: First, place the wafer on the fixture, and then load the multiple fixtures containing the wafer into the jig; The fixture containing the wafer and jig is placed on a conveyor belt and then transported to the transfer chamber via the conveyor belt. The robotic arm inside the transfer chamber transfers the fixture containing the wafers from the jig and places it in the reaction chamber, where the first batch of wafers begins to react and grow. After the first batch of wafers has completed reaction growth, the program ends. During the cooling phase, the door is opened, and the robotic arm inside the transfer chamber transfers the wafers and fixtures from the reaction chamber and places them in the hollow fixture inside the transfer chamber. By rotating the carrier inside the reaction chamber, all the first batch of wafers and fixtures after the reaction are taken out in sequence. Subsequently, before the reaction chamber cools down to room temperature, a new batch of wafers and fixtures is transferred to the reaction chamber via a robotic arm in the transfer chamber. At this time, the temperature inside the reaction chamber has not yet dropped to room temperature and still has a certain temperature. After the transfer is completed, the door is closed; the program is started, and the second batch of wafers begins growth. Repeat the above steps until all batches of wafer reaction growth are completed.