A clamp for thermocouple welding
By employing a clamp with elastic clamping arms and ceramic clamping blocks, combined with the design of arc grooves and fluorescent marking rings, the problems of clamping damage and unquantifiable parameters during welding were solved, achieving stability and consistency in welding quality, reducing precious metal loss and training costs, and improving production efficiency.
Patent Information
- Application Number
- CN202611422603.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-14
- Publication Date
- 2026-11-17
AI Technical Summary
Existing technologies for welding precious metal thermocouples suffer from problems such as clamping damage, misalignment, inaccurate length control, reliance on manual experience, unquantifiable parameters, and high maintenance costs, resulting in unstable welding quality and low production efficiency.
The fixture, consisting of elastic clamping arms and ceramic clamping blocks, combined with an arc groove and detachable design, along with a fluorescent marking ring and hinge structure, enables precise positioning and visual control of the coupling wire, avoids mechanical damage, quantifies process parameters, and reduces maintenance costs.
It improved the stability and consistency of welding quality, reduced precious metal loss, shortened the training cycle, and increased production efficiency and product qualification rate.
Smart Images

Figure CN123103109A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of thermocouples, and more specifically to a clamp for thermocouple welding. Background Technology
[0002] Precious metal thermocouples, such as platinum-rhodium series thermocouples like the S, B, and R types, are key temperature-sensing elements in high-temperature measurement. Due to their excellent high-temperature resistance, oxidation resistance, and temperature measurement stability, they are widely used in industries such as metallurgy, aerospace, energy, and metrology. The forming quality of the welding tip of a precious metal thermocouple directly determines its temperature measurement accuracy, response rate, and long-term service stability. Currently, oxyhydrogen flame welding, with its advantages of pure flame without carbon pollution and controllable temperature range, has become the mainstream process for forming precious metal thermocouple welding tips.
[0003] In existing technologies, when welding the measuring ends of precious metal thermocouples, it is usually done manually by holding ordinary tweezers and clamping them 10mm from the ends of the thermocouple wires to fix the two parallel wires (the diameter of a single wire is usually 0.5mm). The ends of the wires are then placed into an oxyhydrogen flame, causing the ends of the two wires to melt and form the weld head. This welding method has the following problems:
[0004] 1. The gripping ends of ordinary tweezers are mostly flat or sharp-edged, which can easily cause mechanical damage such as indentations and scratches (i.e., mottled appearance) on the surface of the thermocouple wire when gripping it. This damages the surface microstructure of the platinum-rhodium thermocouple wire, easily inducing grain coarsening and localized oxidation and corrosion under high-temperature conditions, and exacerbating thermoelectric potential drift. Furthermore, it is difficult to ensure that the two thermocouple wires are aligned side by side during gripping, resulting in a flattened weld head with an irregular outline. This leads to uneven heat conduction and distribution at the temperature measuring end, and a decrease in temperature measurement stability. It is difficult to meet the high precision and high stability requirements of thermocouples.
[0005] 2. Traditional processes rely entirely on the operator's subjective experience to judge the length of the welding wire inserted into the flame. If the insertion length is too long, excessive molten material results in an oversized welding head, increasing the heat capacity of the temperature measuring end, altering heat conduction characteristics, and causing thermal response lag and excessive dynamic temperature measurement errors. If the insertion length is too short, it easily leads to defects such as an undersized welding head, incomplete welds, and weld detachment, and is prone to breakage failure during actual use. Furthermore, due to the dynamic fluctuations in the temperature and flame size of the oxyhydrogen flame, and the fact that the operator's goggles obstruct the view during fusion welding, it is impossible to accurately control the amount of molten material. This makes welding quality highly dependent on manual experience, resulting in large product size variations, poor batch consistency, and difficulty in quality control during large-scale production.
[0006] 3. The required length of welding wire to be fed into the flame varies depending on the diameter and flame conditions. However, traditional clamping tools lack positioning and parameter recording functions, making it impossible to quantify and solidify process parameters suitable for different working conditions. These process parameters rely entirely on the operator's individual practical experience, lacking standardized and replicable operating procedures. This not only results in a learning cycle of several months for new employees and high process training costs, but also leads to significant differences in welding processes between different operators and different production batches. Standardized mass production is impossible, severely restricting stable product quality output and process iteration upgrades.
[0007] 4. Traditional welding processes require multi-dimensional inspection of the weld head dimensions using a micrometer after welding. Defective products necessitate secondary clamping and welding or removal and re-welding. This secondary clamping process easily causes secondary mechanical damage to the weld head root and intact thermocouple wires. On one hand, this leads to the scrapping and waste of expensive platinum-rhodium materials, significantly increasing production costs. On the other hand, repeated welding, inspection, and rework increase the number of processes, reduce production efficiency, and further deteriorate the thermocouple forming quality and service performance, making it difficult to effectively improve the product qualification rate.
[0008] Chinese utility model patent with authorization announcement number CN205996371U discloses a thermocouple welding clamp. The clamp is a wire cutter body structure. On the upper and lower planes of the opening and closing jaws, there are semi-circular pre-compression grooves with straight lines arranged perpendicular to the jaws and spaced parallel to each other. The width of the pre-compression groove is adapted to the diameter of the thermocouple wire. The thermocouple wire is embedded and limited by the semi-circular pre-compression groove, so as to reduce the contact resistance and prevent the thermocouple wire from slipping. However, this technical solution is designed for capacitor discharge thermocouple welding machines, where the clamping clamp also serves as a conductive component in the welding circuit. It is not suitable for the process of welding precious metal thermocouples using an oxyhydrogen flame, and has the following shortcomings: First, the clamping jaws and semi-circular pre-compression groove are both rigid metal structures. When clamping platinum-rhodium precious metal thermocouple wires, indentations or scratches will form on the wire surface, damaging the surface structure. Furthermore, the semi-circular pre-compression groove can only circumferentially limit the position of a single wire, failing to ensure that two wires are aligned side-by-side, leading to defects such as flattening and irregular contours in the weld head. Second, this solution only addresses the clamping process. The solution suffers from several drawbacks. First, it lacks contact resistance and anti-slip mechanisms. Second, it fails to quantify and position the length of the welding wire extending into the flame, making it impossible to control the welding head's forming size and requiring operators to rely on subjective experience to judge the insertion length. Third, it lacks real-time observation methods during welding. When operators wear goggles to obstruct their vision during oxyhydrogen flame welding, they cannot observe the melting state of the welding wire's end, making it difficult to accurately control the amount of melt. Fourth, the semi-circular pre-compression groove is directly formed on the clamp body, with a fixed and non-replaceable groove diameter. This makes it unsuitable for welding wires of different diameters, and the clamp must be scrapped entirely after the pre-compression groove wears out, resulting in high maintenance costs.
[0009] According to the national standard GB / T16701-2010 "Method for Measurement of Thermoelectric Potential of Precious and Base Metal Thermocouple Wires", the diameter of the thermocouple welding head must be controlled to be 2 to 3 times the diameter of the thermocouple wire. For example, the standard welding head diameter for a 0.5mm thermocouple wire is 1.0 to 1.5mm. For standard thermocouples used in precision metrology calibration, the standards are even more stringent. Specifically, the verification procedures JJG75-2022 "Standard Platinum-Rhodium 10 - Platinum Thermocouple" and JJG167-1995 "Standard Platinum-Rhodium 30 - Platinum-Rhodium 6 Thermocouple" clearly require that the welding head diameter of a 0.5mm thermocouple wire be precisely controlled within a narrow range of 1.1 to 1.3mm.
[0010] Existing traditional manual clamping welding processes are constrained by the aforementioned shortcomings, failing to consistently meet the precision dimensional requirements of high-end metrology-grade thermocouples, and making it difficult to guarantee product qualification rates and batch stability. Therefore, the industry urgently needs to develop a specialized welding fixture and corresponding calibration method that allows for quantifiable adjustment of the thermocouple wire flame feed length, supports real-time monitoring of the welding process, and enables iterative optimization of process parameters. This will address the industry pain points of poor accuracy, low consistency, lack of standardized processes, and severe wear and tear associated with existing technologies. Summary of the Invention
[0011] The purpose of this invention is to address the shortcomings of existing technologies by providing a fixture for thermocouple welding.
[0012] The objective of this invention is achieved through the following solution: a clamp for thermocouple welding, comprising an elastic clamping structure consisting of two clamping arms, with ceramic clamping blocks detachably fixed at the clamping ends of both clamping arms. Arc-shaped grooves are provided on the facing surfaces of both ceramic clamping blocks. A hinge seat is fixedly mounted on the outer side of one clamping arm, and the hinge seat is provided with a hinge shaft, a first limiting shaft, a second limiting shaft, a first positioning hole, and a second positioning hole. One end of a connecting rod is hinged and fixed to the hinge seat via the hinge shaft. A positioning pin can be selectively inserted into either the first or second positioning hole, cooperating with the positioning hole on the connecting rod to position and fix the connecting rod. The first and second limiting shafts are used to limit the rotation angle of the connecting rod. An observation rod is fixedly mounted on the other end of the connecting rod, and the observation rod is perpendicular to the connecting rod. A fluorescent marking ring is sleeved on the observation rod, and the fluorescent marking ring frictionally engages with the observation rod. A scale is provided on the observation rod for observing the position of the fluorescent marking ring.
[0013] Preferably, the clamping end of the clamping arm is provided with a slot, and the rear end of the ceramic clamping block is provided with a square protrusion. After the square protrusion is inserted into the slot, the ceramic clamping block and the clamping arm are locked and fixed by a locking screw.
[0014] Preferably, the angle formed between the line connecting the center of the first positioning hole and the center of the hinge shaft and the line connecting the center of the second positioning hole and the center of the hinge shaft is 45°.
[0015] Preferably, the cross-section of the arc-shaped groove is a minor arc or a semi-circular arc.
[0016] Preferably, the fluorescent marking ring is made of strontium aluminate long afterglow phosphor and high-temperature resistant silicone rubber, and the inner diameter of the fluorescent marking ring is smaller than the outer diameter of the observation rod.
[0017] Preferably, the hinge base includes a connecting base and two upright plates, the two upright plates are arranged parallel to each other on the connecting base, and a gap is left between the two upright plates for clamping the connecting rod. The connecting base is fixed to the clamping arm by bolts, adhesive, or welding.
[0018] The ceramic clamping block is made of zirconia ceramic or silicon nitride ceramic.
[0019] The axial length of the fluorescent marking ring is 0.3–0.5 mm.
[0020] The beneficial effects of this invention are as follows:
[0021] 1. This invention employs a detachable ceramic clamping block in conjunction with an arc-shaped groove to clamp precious metal thermocouple wires. The ceramic material has high hardness, a smooth surface without sharp edges, and does not wet the molten precious metal, preventing contamination of the welding head by the clamping head. When clamping platinum-rhodium precious metal thermocouple wires, it effectively prevents mechanical damage such as indentations and scratches on the wire surface, protecting the surface metallographic structure of the wire, preventing grain coarsening and localized oxidation corrosion under high-temperature operating conditions, and reducing thermocouple thermoelectric potential drift. The opposing arc-shaped grooves can simultaneously achieve circumferential restraint on two thermocouple wires, ensuring that the two wires remain aligned side-by-side after clamping. After the welding head is molten and formed, its shape is round and will not collapse or misalign, ensuring uniform and stable heat conduction at the temperature measuring end and improving the temperature measurement accuracy of the finished thermocouple. Furthermore, the ceramic clamping block is detachable and replaceable, allowing for the replacement of clamping blocks with corresponding groove specifications according to different wire diameters, resulting in strong tooling versatility. When the working surface wears down, only the clamping block needs to be replaced, eliminating the need to scrap the entire fixture and effectively reducing maintenance costs.
[0022] 2. This invention utilizes a hinged structure between a hinged seat and a connecting rod, relying on a limiting shaft, positioning holes, and positioning pins to reliably switch between the observation rod's positioning and observation states, and to achieve repeated positioning. When positioning the coupling wire, the observation rod is flipped to the positioning state (i.e., the connecting rod is rotated parallel to the clamping arm, the second limiting shaft restricts further rotation of the connecting rod, and the positioning pin is inserted into the second positioning hole and the positioning hole on the connecting rod to achieve limiting and fixing of the connecting rod). When welding the coupling wire, the observation rod is flipped to the observation state (i.e., the connecting rod is rotated at 45° to the clamping arm, the first limiting shaft restricts further rotation of the connecting rod, and the positioning pin is inserted into the first positioning hole and the positioning hole on the connecting rod to achieve limiting and fixing of the connecting rod). The positioning holes and limiting shafts work together to ensure a consistent reference position for the observation rod after each deployment, eliminating reference deviations caused by manual placement and providing a stable structural foundation for quantitatively controlling the length of the coupling wire extending into the flame.
[0023] 3. This invention features a sliding, friction-positioned fluorescent marker ring on a graduated observation rod, creating a visualized length reference system. Operators can pre-adjust the position of the fluorescent marker ring on the observation rod's scale according to the target weld head size, thereby quantifying and limiting the weld head size during thermocouple wire welding. This changes the traditional operation mode that relies entirely on the operator's subjective judgment based on experience, enabling quantifiable and replicable welding process parameters. It reduces dependence on operator experience, shortens the training cycle for new employees, and improves the consistency of weld head sizes across different operators and production batches. The fluorescent marker ring possesses long afterglow self-luminescence properties, allowing operators to clearly identify the marker position even when wearing dark goggles or under strong light interference from an oxyhydrogen flame. This enables real-time observation of the melting state at the thermocouple wire end, precise control of the melting amount, and reduction of defects such as excessive weld head size, incomplete welds, and weld detachment. It also reduces the need for rework and scrapping of precious metal thermocouple wires, lowers the consumption of expensive platinum and rhodium materials, and improves product qualification rates. It is particularly suitable for the mass production of metrology-grade high-precision precious metal thermocouples. Attached Figure Description
[0024] Figure 1 This is a schematic diagram of the structure of the present invention in its free state;
[0025] Figure 2 This is a schematic diagram of the structure of the present invention when clamping the coupling wire;
[0026] Figure 3 for Figure 2 A schematic diagram of the structure along direction A;
[0027] Figure 4 This is a schematic diagram of the structure during the welding of the coupling wires according to the present invention;
[0028] Figure 5 for Figure 4 A schematic diagram of the B-direction structure;
[0029] Figure 6 for Figure 4 CC section view;
[0030] Figure 7 for Figure 4 DD sectional view;
[0031] Figure 8 This is a schematic diagram of the structure of the clamping block of the present invention;
[0032] Figure 9 for Figure 8 Schematic diagram of the E-direction structure;
[0033] Figure 10 for Figure 8 A schematic diagram of the F-direction structure. Detailed Implementation
[0034] like Figures 1 to 10As shown, a clamp for thermocouple welding includes an elastic clamping structure composed of two clamping arms 1 made of TC4 titanium alloy. Ceramic clamping blocks 2 are detachably fixed at the clamping ends of both clamping arms 1. Specifically, the clamping ends of the clamping arms 1 are provided with slots, and the rear end of the ceramic clamping block 2 is provided with a square protrusion 22. After the square protrusion 22 is inserted into the slot, the ceramic clamping block 2 is locked and fixed to the clamping arms 1 by locking screws. The insertion and positioning structure of the slot and the square protrusion 22, combined with the locking screws, ensures the installation and positioning accuracy of the ceramic clamping block 2, preventing displacement and misalignment during clamping operations and ensuring the alignment accuracy of the double arc grooves. It also enables rapid disassembly and replacement of the ceramic clamping block 2, shortening the changeover and debugging time. The surface contact between the square protrusion and the slot can withstand greater clamping reaction force, resulting in strong shear resistance and preventing loosening and deformation over long-term use. The ceramic clamping block 2 is made of zirconia ceramic or silicon nitride ceramic. Both ceramic clamping blocks 2 have arc-shaped grooves 21 on their facing surfaces. The cross-section of the arc-shaped grooves 21 is a minor arc or a semi-circular arc. This arrangement can form a semi-enclosed limiting of the coupling wires 8, which not only ensures the centering accuracy of the two wires side by side, but also avoids the groove walls from fully covering and squeezing the coupling wires 8, reducing the pressure area of the coupling wires 8 and further reducing the risk of mechanical damage. Moreover, the arc surface has a high degree of fit with the outer surface of the coupling wires 8, and the clamping force is evenly distributed, which can achieve stable clamping under a smaller clamping force and better protect the precious metal coupling wires 8. A hinge seat 3 is fixedly installed on the outer side of one of the clamping arms 1. The hinge seat 3 includes a connecting base 36 and two upright plates 37. The two upright plates 37 are arranged parallel to each other on the connecting base 36, and a gap is left between the two upright plates 37 for clamping the connecting rod 4. The connecting base 36 is fixed to the clamping arm 1 by bolts, adhesive, or welding. Hinges 31, first limiting shafts 32, second limiting shafts 33, first positioning holes 34, and second positioning holes 35 are installed at corresponding positions on the two upright plates 37. One end of a connecting rod 4 is hinged and fixed to the hinge seat 3 via the hinge shafts 31. A positioning pin 5 can be selectively inserted into the first positioning hole 34 or the second positioning hole 35, cooperating with the positioning holes on the connecting rod 4 to position and fix the connecting rod 4. The included angle between the line connecting the center of the first positioning hole 34 and the center of the hinge shaft 31 and the line connecting the center of the second positioning hole 35 and the center of the hinge shaft 31 is 45°. The purpose of this setting is that when the operator holds this device to clamp the precious metal thermocouple wire for welding, the 45° angle facilitates the operator's line of sight when welding the thermocouple wire 8.The first limiting shaft 32 and the second limiting shaft 33 are used to limit the rotation angle of the connecting rod 4. An observation rod 6 is fixedly installed at the other end of the connecting rod 4. The observation rod 6 is perpendicular to the connecting rod 4 and has a scale. A fluorescent marking ring 7 is sleeved on the observation rod 6. The axial length of the fluorescent marking ring 7 is 0.3-0.5 mm. The fluorescent marking ring 7 is made of strontium aluminate long afterglow phosphor and high-temperature resistant silicone rubber. The inner diameter of the fluorescent marking ring 7 is slightly smaller than the outer diameter of the observation rod 6, so that the fluorescent marking ring 7 is tightly attached to the observation rod 6 by the elasticity of the silicone rubber itself, forming a friction fit. The position of the fluorescent marking ring 7 can be adjusted by hand. When the hand is released, the fluorescent marking ring 7 is tightly attached to the observation rod 6 and fixed. The structure is simple. The reason for using strontium aluminate long-afterglow phosphor is that it can "charge" after being exposed to natural light or artificial light for a while, emitting a yellow-green light. This yellow-green light is most easily seen under dark goggles and contrasts sharply with the blue-violet of an oxyhydrogen flame and the orange-red of a molten ball, allowing the operator to distinguish it at a glance through the goggles. The observation rod 6 is equipped with graduations for observing the position of the fluorescent marker ring 7.
[0035] In this invention, the observation rod 6 has two states—positioning state and observation state, see [link / reference] Figure 2 When the positioning pin 5 is inserted into the second positioning hole 35 to fix the connecting rod 4, that is, when the connecting rod 4 is parallel to the clamping arm 1, the observation rod 6 is in a positioning state. The straight-line distance between the 0 mark at the front end of the observation rod 6 and the ceramic clamping block 2 is 15-20mm, which is used to position the ferrule wire, that is, to align the end of the ferrule wire with the 0 mark on the observation rod 6. See also Figure 4 When the positioning pin 5 is inserted into the first positioning hole 34 to fix the connecting rod 4, that is, when the connecting rod 4 is at a 45° angle with the clamping arm 1, the observation rod 6 is in the observation state and is used to observe the size of the welding head of the welding wire when welding the welding wire. When the observation rod 6 is in the observation state, the observation rod 6 is about 1 cm away from the outer flame of the hydrogen-oxygen flame to avoid the hydrogen-oxygen flame directly burning the observation rod and causing damage to the rod.
[0036] The procedure for using this device is as follows:
[0037] 1) Select the ceramic clamping block with the corresponding arc groove according to the diameter of the coupler wire;
[0038] 2) Remove the positioning pin, rotate the connecting rod until the connecting rod is limited by the second limiting shaft, and insert the positioning pin into the second positioning hole and the positioning hole of the connecting rod to fix the connecting rod. At this time, the observation rod is in the positioning state.
[0039] 3) Open the clamp, place the two dipole wires into the arc-shaped grooves respectively, align the ends of the dipole wires with the 0 mark on the observation rod to achieve positioning, and clamp the clamp.
[0040] 4) Based on the diameter of the filament and referring to the theoretical value of the melting length, move the fluorescent marking ring to the target scale L0 (for example, if the diameter of the filament is φ0.5mm, align the rear end of the fluorescent marking ring with the 2.3mm scale).
[0041] 5) Remove the positioning pin, rotate the connecting rod until the connecting rod is limited by the first limiting shaft, and insert the positioning pin into the first positioning hole and the positioning hole of the connecting rod to fix the connecting rod. At this time, the observation rod is in the observation state.
[0042] 6) Hold the clamp in your right hand and support the rear end of the corundum tube with your left hand. Horizontally insert the entire tube into the oxyhydrogen flame to weld the end of the welding wire. Observe the position of the rear edge of the molten ball at the end of the welding wire and the fluorescent marking ring at all times. When the rear edge of the molten ball is aligned with the rear end of the fluorescent marking ring, immediately withdraw the entire tube from the flame.
[0043] The theoretical values in step 4) above are obtained based on theoretical model technology. Specifically, in order to provide the operator with a reasonable initial preset length for melting length, this invention establishes a theoretical relationship model between the wire diameter d, melting length L and welding head diameter D based on the principle of volume conservation.
[0044] Two cylindrical wires, each with a diameter of *d*, have their entire material used to form a spherical welding head within a melting length of *L* at their ends. Ignoring evaporation losses and shape adjustments caused by surface tension during the melting process, based on volume conservation:
[0045]
[0046] Simplifying, we get:
[0047]
[0048] Where: d is the diameter of the ferrule (mm), L is the melting length (mm), and D is the diameter of the welding head (mm).
[0049] Based on the national standards and verification procedures for the diameter of the welding head, the theoretical values of the fusion length corresponding to different wire diameters are calculated as follows:
[0050] Table 1
[0051]
[0052] The above theoretical values serve as a reference for operators to set the position of the fluorescent marker ring. In practical applications, they can be optimized and adjusted through experimental calibration.
[0053] After completing the welding of the thermocouple wire ends, use a caliper to check if the weld head size meets the requirements. Adjust the theoretical melt length value in Table 1 based on the test results. Specifically, refer to the theoretical melt length value in Table 1 and weld a group (at least 5 thermocouples in a group) of thermocouple wires with the same diameter. For example, select 5 thermocouples with a wire diameter of 0.5mm. Weld the wires of all 5 thermocouples according to the theoretical melt length value (2.30mm) in Table 1. After welding, use a caliper to check the diameter of each weld head. Calculate the pass rate and deviation direction. The deviation direction refers to whether the number of unqualified weld heads with diameters greater than the specified weld head diameter or the number of weld heads with diameters smaller than the specified weld head diameter is greater. If the number of unqualified weld heads with diameters greater than the specified weld head diameter is large, decrease the theoretical value of the fusion length L; if the number of weld heads with diameters smaller than the specified weld head diameter is large, increase the theoretical value of the fusion length L. The adjustment step is 0.1~0.2mm each time. Of course, if the number of unqualified weld heads with diameters greater than the specified weld head diameter is the same as the number of weld heads with diameters smaller than the specified weld head diameter, then you can choose to increase or decrease the theoretical value of the fusion length L. Then repeat the above steps until all weld heads meet the requirements after a set of wires are welded according to the theoretical value of the fusion length L. Record the fusion length L* corresponding to the diameter of the wire at this time in Table 1 as the standard process parameter for subsequent welding of the same wire diameter.
[0054] Example 1: Welding clamps suitable for φ0.5mm standard thermocouples
[0055] The main body of the clamp is made of TC4 titanium alloy, shaped like surgical forceps, with a total length of 120mm and a clamping arm length of 30mm. The ceramic clamping block is made of zirconia ceramic, with double circular arc grooves R0.25mm and a center distance of 0.5mm between the two grooves. The observation rod is 1.2mm in diameter and 25mm long, with a scale ranging from 0-10mm; the main scale division is 0.5mm, and the auxiliary scale division is 0.1mm. The fluorescent marking ring is 0.4mm wide and appears yellow-green under the protective eyepiece. The rotating connecting rod is 10mm long and made of titanium alloy.
[0056] Caliper tab openings: φ1.10mm (through), φ1.20mm (reference), φ1.30mm (stop), φ1.50mm (national standard reference).
[0057] Calibration process:
[0058] Initial setting: L = 2.3 mm (theoretical median);
[0059] Ten S-shaped couplers were welded. Caliper gauge inspection: 6 were qualified, 3 were too large, and 1 was too small.
[0060] The proportion is too high; adjust L to 2.1mm.
[0061] Ten more were welded, and all ten passed inspection.
[0062] Modify the theoretical melt length value L*=2.1mm and record it as the standard process parameter for a φ0.5mm standard thermocouple;
[0063] Production application: The operator fixes the fluorescent mark to the 2.1mm scale, clamps and welds it, and removes it when the molten ball reaches the mark line. The pass rate of caliper inspection is consistently above 90%.
[0064] Example 2: Universal Operation of Multi-Specification Couple Wires
[0065] The same clamp can be used to adapt different dipole wires by moving the fluorescent marker:
[0066]
[0067] The operator only needs to slide the fluorescent marker to the corresponding position; the rest of the operation is exactly the same.
[0068] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications made to the present invention by those skilled in the art without departing from the spirit of the present invention shall fall within the protection scope of the present invention.
Claims
1. A clamp for thermocouple welding, comprising an elastic clamping structure consisting of two clamping arms (1), characterized in that: Both clamping arms (1) have detachable ceramic clamping blocks (2) fixedly mounted on their clamping ends. The opposing surfaces of both ceramic clamping blocks (2) are provided with arc-shaped grooves (21). A hinge seat (3) is fixedly mounted on the outer side of one clamping arm (1). The hinge seat (3) is provided with a hinge shaft (31), a first limiting shaft (32), a second limiting shaft (33), a first positioning hole (34), and a second positioning hole (35). One end of a connecting rod (4) is hinged to the hinge seat (3) via the hinge shaft (31). A positioning pin (5) can be selectively inserted into the first positioning hole (34) or... In the second positioning hole (35), the positioning hole on the connecting rod (4) is matched to fix the connecting rod (4). The first limiting shaft (32) and the second limiting shaft (33) are used to limit the rotation angle of the connecting rod (4). An observation rod (6) is fixedly installed at the other end of the connecting rod (4). The observation rod (6) is set perpendicular to the connecting rod (4). A fluorescent marking ring (7) is sleeved on the observation rod (6). The fluorescent marking ring (7) is in frictional contact with the observation rod (6). A scale is set on the observation rod (6) for observing the position of the fluorescent marking ring (7).
2. The fixture for thermocouple welding according to claim 1, characterized in that: The clamping end of the clamping arm (1) is provided with a slot, and the rear end of the ceramic clamping block (2) is provided with a square protrusion (22). After the square protrusion (22) is inserted into the slot, the ceramic clamping block (2) and the clamping arm (1) are locked and fixed by locking screws.
3. The fixture for thermocouple welding according to claim 1, characterized in that: The angle between the line connecting the center of the first positioning hole (34) and the center of the hinge shaft (31) and the line connecting the center of the second positioning hole (35) and the center of the hinge shaft (31) is 45°.
4. The fixture for thermocouple welding according to claim 1, characterized in that: The cross-section of the arc groove (21) is a minor arc or a semi-circular arc.
5. The fixture for thermocouple welding according to claim 1, characterized in that: The fluorescent marking ring (7) is made of strontium aluminate long afterglow phosphor and high temperature resistant silicone rubber, and the inner diameter of the fluorescent marking ring (7) is smaller than the outer diameter of the observation rod (6).
6. The fixture for thermocouple welding according to claim 1, characterized in that: The hinge seat (3) includes a connecting base (36) and two upright plates (37). The two upright plates (37) are arranged parallel to each other on the connecting base (36), and there is a gap between the two upright plates (37) for clamping the connecting rod (4). The connecting base (36) is fixed to the clamping arm (1) by bolts, adhesive, or welding.
7. The fixture for thermocouple welding according to claim 1, characterized in that: The ceramic clamping block (2) is made of zirconia ceramic or silicon nitride ceramic.
8. The fixture for thermocouple welding according to claim 1, characterized in that: The axial length of the fluorescent marking ring (7) is 0.3 to 0.5 mm.