A method for preparing ultra-clean high-purity acetonitrile.

By combining 18-crown-6 grafted polyvinyl alcohol complexing agent with ultrafiltration membrane, the problems of incomplete removal of metal ions and easy pulverization during the regeneration process in the traditional preparation of high-purity acetonitrile were solved, realizing efficient and economical preparation of semiconductor-grade acetonitrile.

CN123106475APending Publication Date: 2026-11-17CHANGYI TIANYU PHARMACEUTRACAL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611091000.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-07-22
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing high-purity acetonitrile preparation technology cannot effectively remove key metal ions in semiconductor processes. Traditional ion exchange resins have poor swelling properties and are prone to pulverization during regeneration, resulting in high material consumption and poor economic efficiency in the purification process. Furthermore, they cannot achieve selective identification and targeted removal.

Method used

The method of combining 18-crown-6 grafted polyvinyl alcohol complexing agent with ultrafiltration membrane is adopted. Through molecular dissolution and reaction with metal ions, a large molecular complex is formed by utilizing the size-selective coordination effect of crown ether cavity. The complex is then retained by ultrafiltration membrane and regenerated by dilute hydrochloric acid back-extraction, forming a closed-loop circulation system.

Benefits of technology

It achieves deep removal of trace metal ions from semiconductor-grade acetonitrile, with a total metal ion content of no more than 10 ppt. This solves the problems of secondary pollution and high material consumption in traditional methods, reduces operating costs, and meets the purity requirements of the semiconductor industry.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123106475A_ABST
    Figure CN123106475A_ABST
Patent Text Reader

Abstract

This invention belongs to the field of acetonitrile preparation technology, specifically a method for preparing ultra-clean, high-purity acetonitrile. The method includes crown ether sulfonation derivatization, crown ether polymer grafting, acetonitrile complexation reaction, ultrafiltration cross-flow retention, complexing agent back-extraction regeneration, and permeate distillation purification. This invention solves the problem of traditional non-selective broad-spectrum adsorption's inability to differentiate and target the removal of key metal ions such as sodium, potassium, iron, and copper ions in semiconductor processes through size-selective coordination of the 18-crown-6 cavity and synergistic chelation with hydroxyl groups on the polyvinyl alcohol backbone. It achieves selective capture based on cavity size matching and multi-functional group synergy, enabling the targeted removal of specific metal ions even against a complex impurity background. Simultaneously, it addresses the problems of poor swelling properties of traditional ion exchange resins in acetonitrile organic phases, easy pulverization during regeneration leading to secondary pollution, and difficulty in removing trace metal ions to semiconductor-grade standards.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of acetonitrile preparation technology, specifically an ultra-clean high-purity acetonitrile and its preparation method. Background Technology

[0002] Acetonitrile is a key solvent for photoresist cleaning and silicon wafer etching in semiconductor manufacturing, and its purity directly determines chip yield. Existing high-purity acetonitrile preparation technologies mainly focus on the removal of organic impurities and energy-saving dehydration. The methods for removing trace metal ions are relatively simple, generally employing ion exchange resins or alumina adsorption columns for passive end-of-pipe adsorption.

[0003] However, the swelling capacity of ion exchange resins decreases in the highly polar organic solvent of acetonitrile, reducing the accessibility of active groups and resulting in insufficient exchange capacity, making it difficult to remove metal ions to semiconductor-grade standards. At the same time, the resin or alumina is prone to pulverization during regeneration, generating micron-sized particles, which become a new source of pollution in acetonitrile products. In addition, existing preparation methods are mostly non-selective broad-spectrum adsorption, which cannot achieve highly selective identification and targeted removal of specific metal ions that are most harmful in semiconductor processes. Furthermore, they lack recyclable liquid-phase complexation and membrane retention coupling processes, resulting in high material consumption and poor economic efficiency in the purification process. Summary of the Invention

[0004] One objective of this invention is to provide an ultra-clean, high-purity acetonitrile and its preparation method, which solves the problems of traditional non-selective broad-spectrum adsorption being unable to differentiate and target the removal of key metal ions such as sodium, potassium, iron, and copper ions in semiconductor processes, as well as the problems of traditional ion exchange resins having poor swelling properties in the acetonitrile organic phase, being prone to pulverization during regeneration leading to secondary pollution, and being unable to remove trace metal ions to semiconductor-grade standards.

[0005] In a first aspect, embodiments of the present invention provide a method for preparing ultra-clean, high-purity acetonitrile, comprising the following steps: S1. Reaction of 18-crown-6 with p-toluenesulfonyl chloride in pyridine yields p-toluenesulfonated 18-crown-6; S2. Dissolve 10g of polyvinyl alcohol in 100ml of anhydrous dimethyl sulfoxide, add sodium hydride and stir at 60℃ for 2h to activate, then add p-toluenesulfonate 18-crown-6, heat to 80℃ for grafting reaction for 12h to obtain reaction solution, add anhydrous acetonitrile with a water content ≤0.01% to reaction solution, and obtain 18-crown-6 grafted polyvinyl alcohol complexing agent after precipitation, filtration and vacuum drying; S3. Mix industrial-grade acetonitrile with 18-crown-6 grafted polyvinyl alcohol complexing agent at a mass ratio of 100:1 to 200:1, and stir at 25°C for 30 min to obtain acetonitrile solution containing macromolecular complexes. S4. Use an ultrafiltration membrane to filter the acetonitrile feed containing macromolecular complexes. Acetonitrile and uncomplexed impurities pass through the ultrafiltration membrane to become permeate, while macromolecular complexes are retained by the ultrafiltration membrane to become concentrate. S5. Add an equal volume of dilute hydrochloric acid aqueous solution to the concentrate, shake at room temperature for 10 min, perform back extraction, separate the liquid and take the organic phase, dry it and dissolve it in anhydrous acetonitrile with a water content ≤0.01% as solvent to obtain the regenerated complexing agent. S6. The permeate is dehydrated by distillation and filtered to obtain ultra-clean, high-purity acetonitrile.

[0006] In one embodiment, in step S1, the molar ratio of 18-crown-6 to p-toluenesulfonyl chloride is 1:(1 to 1.5); the amount of pyridine used is 3 to 5 times the total mass of 18-crown-6 and p-toluenesulfonyl chloride; the reaction temperature is 0°C to 25°C; and the reaction time is 2 to 4 hours.

[0007] In one embodiment, in step S2, the degree of alcoholysis of polyvinyl alcohol is 88%, and the degree of polymerization is 1700; the mass ratio of sodium hydride to polyvinyl alcohol is (0.15~0.25):1, the activation temperature is 55℃~65℃, and the activation time is 1.5h~2.5h; the mass ratio of p-toluenesulfonated 18-crown-6 to polyvinyl alcohol is 1.2:1, the grafting reaction temperature is 75℃~85℃, and the grafting reaction time is 10h~14h.

[0008] In one embodiment, in step S2, the grafting rate of the 18-crown-6 grafted polyvinyl alcohol complexing agent is 30% to 40%, the number average molecular weight is 10 kDa to 15 kDa, and the solubility in acetonitrile is 80 g / L to 90 g / L.

[0009] In one embodiment, in step S3, the metal ions in the industrial-grade acetonitrile include one or more of sodium ions, potassium ions, iron ions, and copper ions, and the total content of metal ions is 0.1 ppm to 10 ppm.

[0010] In one embodiment, in step S3, the stirring reaction temperature is 20°C to 30°C, the reaction time is 20 min to 40 min, and the stirring speed is 150 rpm to 250 rpm.

[0011] In one embodiment, in step S4, the ultrafiltration membrane has a molecular weight cutoff of 2kDa to 3kDa, the membrane material is polyimide, the operating pressure is 0.2MPa to 0.4MPa, the operating temperature is 25℃ to 35℃, and the membrane surface flow rate is 1.5m / s to 2.5m / s.

[0012] In one embodiment, in step S5, the concentration of the dilute hydrochloric acid aqueous solution is 0.05 mol / L to 0.2 mol / L, and the back-extraction time is 5 min to 15 min.

[0013] In one embodiment, in step S6, the distillation and dehydration are carried out by vacuum distillation, with the reboiler temperature controlled at 60°C to 80°C, the vacuum degree at -0.08MPa to -0.095MPa, and the reflux ratio at 2:1 to 4:1; the final filtration uses a polytetrafluoroethylene filter membrane with a pore size of 0.1μm.

[0014] Secondly, embodiments of the present invention provide an ultra-clean high-purity acetonitrile, which is prepared by an ultra-clean high-purity acetonitrile preparation method, wherein the total metal ion content of the ultra-clean high-purity acetonitrile is not greater than 10 ppt.

[0015] The beneficial effects of this invention are: (1) This invention solves the problems of poor swelling of traditional ion exchange resins in acetonitrile organic phase, easy pulverization during regeneration and secondary pollution, and difficulty in removing trace metal ions to semiconductor grade by dissolving 18-crown-6 grafted polyvinyl alcohol complexing agent in molecular state in acetonitrile and reacting it homogeneously with metal ions, and using ultrafiltration membrane to retain macromolecular complexes. This invention realizes the paradigm shift from solid phase adsorption to liquid-liquid complexation and membrane retention. (2) This invention solves the problem that traditional non-selective broad-spectrum adsorption cannot differentiate and target key metal ions such as sodium ions, potassium ions, iron ions, and copper ions in semiconductor processes by using size-selective coordination of the 18-crown-6 cavity and synergistic chelation of hydroxyl groups on the polyvinyl alcohol backbone. It achieves selective capture based on cavity size matching and multi-functional group synergy, so that specific metal ions can still be targetedly removed in the context of complex impurities, avoiding the ineffective occupation of adsorption sites by a large number of non-target impurities. (3) The present invention solves the problems of difficult regeneration of solid adsorbent, high operating cost and large material consumption by using dilute hydrochloric acid back-extraction to regenerate complexing agent and acetonitrile backwashing to restore membrane flux through a closed-loop circulation design. It realizes the cyclic regeneration of complexing agent and membrane module and integration with existing distillation and dehydration processes. Attached Figure Description

[0016] The accompanying drawings are provided to further illustrate the invention and form part of the specification. They are used in conjunction with embodiments of the invention to explain the invention and do not constitute a limitation thereof. In the drawings: Figure 1 This is a process flow diagram of the present invention; Figure 2 The infrared spectra of 18-crown-6, p-toluenesulfonated 18-crown-6, and 18-crown-6 grafted polyvinyl alcohol complexing agent of the present invention are shown in the comparison diagram. Figure 3 This is a schematic diagram of the ultrafiltration cross-flow interception principle of the present invention; Figure 4 This is a diagram showing the recycling performance of the complexing agent of the present invention; Figure 5 This is the ESI-MS spectrum of p-toluenesulfonated 18-crown-6 of the present invention; Figure 6 The infrared spectrum of the ultra-clean, high-purity acetonitrile obtained by the present invention is shown. Detailed Implementation

[0017] The present invention will now be described in further detail with reference to the accompanying drawings. These drawings are simplified schematic diagrams, illustrating only the basic structure of the invention, and therefore only show the components relevant to the invention.

[0018] A method for preparing ultrapure high-purity acetonitrile involves grafting crown ethers onto a polymer backbone to form a macromolecular complexing agent soluble in acetonitrile. The size-selective coordination effect of the crown ether cavity is utilized to capture specific metal ions, forming a macromolecular complex. This complex is then removed by ultrafiltration, achieving deep separation of the metal ions from the liquid phase. The complexing agent can be recycled after back-extraction regeneration, and the ultrafiltration membrane's flux is restored after acetonitrile backwashing. Together, they form a closed-loop circulation system suitable for the industrial continuous production of semiconductor-grade acetonitrile. Ultrapure high-purity acetonitrile, with a total metal ion content not exceeding 10 ppt, is prepared according to this method based on crown ether-polymer complexation and ultrafiltration coupling.

[0019] Includes the following steps: S1. Crown ether sulfonation derivatization. 18-crown-6 is reacted with p-toluenesulfonyl chloride in a molar ratio of 1:(1–1.5) in pyridine to give p-toluenesulfonated 18-crown-6. This step provides active reaction sites for subsequent grafting reactions, allowing the crown ether to undergo etherification with the polymer backbone via the sulfonyl group. The chemical formula of 18-crown-6 is C1. 12 H 24 O6, with a molecular weight of 264.32. The amount of pyridine used is 3 to 5 times the total mass of 18-crown-6 and p-toluenesulfonyl chloride. The reaction temperature is 0°C to 25°C, and the reaction time is 2 to 4 hours. The chemical formula of p-toluenesulfonated 18-crown-6 is C0. 19 H 30 O8S has a molecular weight of 418.

[0020] S2. Crown ether polymer grafting. 10g of polyvinyl alcohol was dissolved in 100mL of anhydrous dimethyl sulfoxide, sodium hydride was added, and the mixture was stirred and activated at 60℃ for 2h. Then, p-toluenesulfonated 18-crown-6 was added, and the temperature was raised to 80℃ for a grafting reaction for 12h, yielding a reaction solution. Anhydrous acetonitrile with a water content ≤0.01% was added to the reaction solution. After precipitation, filtration, and vacuum drying, the 18-crown-6 grafted polyvinyl alcohol complexing agent was obtained. The purpose of this step is to prepare a macromolecular complexing agent with selective metal ion capture capabilities. The addition of anhydrous acetonitrile to the reaction solution serves as a precipitant, utilizing the low solubility of acetonitrile in the polymer to precipitate and separate the grafted product from the reaction system. The anhydrous acetonitrile used here does not participate in the final product preparation and is only used as a precipitant.

[0021] S3. Acetonitrile Complexation Reaction. Industrial-grade acetonitrile is mixed with 18-crown-6 grafted polyvinyl alcohol complexing agent at a mass ratio of 100:1 to 200:1. The metal ions in the industrial-grade acetonitrile are one or more of sodium, potassium, iron, and copper ions. The mixture is stirred at 25°C for 30 minutes to obtain an acetonitrile solution containing a macromolecular complex. The purpose of this step is to ensure sufficient contact between the complexing agent and the metal ions in the acetonitrile, allowing for size-selective coordination within the crown ether cavity to form a stable macromolecular complex.

[0022] S4. Ultrafiltration Cross-flow Retention. An acetonitrile feed solution containing macromolecular complexes is filtered using an ultrafiltration membrane. Acetonitrile and uncomplexed impurities permeate through the ultrafiltration membrane as permeate, while the macromolecular complexes are retained by the membrane as concentrate. The purpose of this step is to utilize the membrane's sieving effect to separate the macromolecular complexes from the acetonitrile solvent, achieving the physical removal of metal ions.

[0023] S5. Back-extraction and regeneration of the complexing agent. An equal volume of dilute hydrochloric acid aqueous solution is added to the concentrate. The mixture is shaken at room temperature for 10 minutes for back-extraction. After separation, the organic phase is collected, dried, and then dissolved in anhydrous acetonitrile with a moisture content ≤0.01% to obtain the regenerated complexing agent. The purpose of this step is to dissociate metal ions from the crown ether cavity through acid washing, restoring the complexing agent's capturing ability and enabling recycling. The use of anhydrous acetonitrile as the solvent provides a pure organic solvent environment, allowing the dried complexing agent to re-dissolve homogeneously, preventing the introduction of moisture and impurities into the recycling system, and ensuring the activity of the regenerated complexing agent. The anhydrous acetonitrile used here for dissolving the regenerated complexing agent differs from the anhydrous acetonitrile used as a precipitant in S2; neither of them participates in the final acetonitrile product.

[0024] S6. Permeate purification by distillation. The permeate is dehydrated by distillation and filtered to obtain ultra-clean, high-purity acetonitrile product. The purpose of this step is to remove residual trace amounts of water and possible colloidal particles from the permeate, ensuring that the acetonitrile purity meets semiconductor-grade standards.

[0025] Detailed parameter descriptions for each step: In S2, the degree of alcoholysis of polyvinyl alcohol is 88%, and the degree of polymerization is 1700. The mass ratio of sodium hydride to polyvinyl alcohol is (0.15–0.25):1, the activation temperature is 55℃–65℃, and the activation time is 1.5h–2.5h. The mass ratio of p-toluenesulfonated 18-crown-6 to polyvinyl alcohol is 1.2:1, the grafting reaction temperature is 75℃–85℃, and the grafting reaction time is 10h–14h. The resulting 18-crown-6 grafted polyvinyl alcohol complexing agent has a grafting rate of 30%–40%, a number average molecular weight of 10kDa–15kDa, and a solubility in acetonitrile of 80g / L–90g / L.

[0026] In S3, the industrial-grade acetonitrile contains one or more of the following metal ions: sodium, potassium, iron, and copper, with a total metal ion content of 0.1 ppm to 10 ppm. The stirring reaction temperature is 20℃ to 30℃, the reaction time is 20 min to 40 min, and the stirring speed is 150 rpm to 250 rpm.

[0027] In S4, the ultrafiltration membrane has a molecular weight cutoff of 2kDa to 3kDa, the membrane material is polyimide, the operating pressure is 0.2MPa to 0.4MPa, the operating temperature is 25℃ to 35℃, and the membrane surface flow rate is 1.5m / s to 2.5m / s.

[0028] In S5, the concentration of the dilute hydrochloric acid aqueous solution is 0.05 mol / L to 0.2 mol / L, and the back-extraction time is 5 min to 15 min. The regenerated complexing agent is recycled at least 5 times, with a single-use loss rate of less than 1%.

[0029] In S6, distillation and dehydration are carried out under reduced pressure, with the reboiler temperature controlled at 60℃~80℃, the vacuum degree at -0.08MPa to -0.095MPa, and the reflux ratio at (2~4):1. The final filtration uses a polytetrafluoroethylene (PTFE) membrane with a pore size of 0.1μm.

[0030] like Figure 2 As shown, infrared spectral analysis revealed that 18-crown-6 at 1100 cm⁻¹ -1 The characteristic absorption peak of COC ether bond appears at 2880 cm⁻¹. -1 A CH stretching vibration peak appears at 1350 cm⁻¹. In addition to retaining the above peak, p-toluenesulfonated 18-crown-6 also exhibits a peak at 1350 cm⁻¹. -1 and 1160cm -1 The newly added sulfonyl S=O asymmetric and symmetric stretching vibration peaks are located at 1600 cm⁻¹. -1 A benzene ring C=C skeletal vibration peak appears at 810 cm⁻¹. -1The appearance of an out-of-plane bending vibration peak of the para-substituted benzene ring at CH3350 cm⁻¹ confirms the successful introduction of the sulfonyl group. The 18-crown-6 grafted polyvinyl alcohol complexing agent exhibits a peak at 3350 cm⁻¹. -1 A broad and strong OH stretching vibration peak appears at this point, originating from the hydroxyl groups on the polyvinyl alcohol backbone, while retaining a peak at 1100 cm⁻¹. -1 The COC ether bond peak at the position proves that the crown ether has been successfully grafted to the polyvinyl alcohol backbone.

[0031] like Figure 1 As shown, the present application discloses a method for preparing ultra-clean high-purity acetonitrile, which includes six steps from S1 to S6, wherein the regenerated complexing agent generated in S5 is recycled back to S3 for reuse, forming a closed-loop circulation system.

[0032] The present application will be described in detail below with reference to specific embodiments. The raw materials in each embodiment all conform to the aforementioned process steps, with only some parameters differing.

[0033] Example 1 A method for preparing ultra-clean, high-purity acetonitrile includes the following steps: S1. 18-crown-6 is reacted with p-toluenesulfonyl chloride in pyridine at a molar ratio of 1:1 to obtain p-toluenesulfonated 18-crown-6; like Figure 5 As shown, the obtained p-toluenesulfonated 18-crown-6 was analyzed by ESI-MS. The test conditions were: ion source temperature 120℃, capillary voltage 3.5kV, cone voltage 40V, scan range m / z 50 to 550, solvent: methanol, flow rate 5μL / min. The spectrum shows a base peak at m / z 419.50, corresponding to the molecular ion peak [M+H]. + [M+Na] appears at m / z 441.50. + The addition peak; the fragment peak m / z 261.16 corresponds to the 18-crown-6 skeletal fragment [C]. 12 H 25 O6] + m / z 155.01 corresponds to the toluenesulfonyl fragment [C7H7SO2] + The m / z value of 91.05 corresponds to the toluene fragment [C7H7]. + Measured molecular ion peak [M+H] + Located at m / z 419.50, the neutral molecular weight, after subtracting the proton mass, is 418.49, consistent with the theoretical calculation of 418.50, proving the successful synthesis of p-toluenesulfonated 18-crown-6.

[0034] S2. Dissolve 10g of polyvinyl alcohol in 100mL of anhydrous dimethyl sulfoxide, add 2g of sodium hydride and stir at 60℃ for 2h to activate. Then add 15g of p-toluenesulfonate-18-crown-6 and heat to 80℃ for grafting reaction for 12h to obtain the reaction solution. Add 500mL of anhydrous acetonitrile with a water content ≤0.01% to the reaction solution. After precipitation, filtration and vacuum drying, the 18-crown-6 grafted polyvinyl alcohol complexing agent is obtained. 1H NMR spectroscopy confirmed successful grafting of the crown ether, with a grafting rate of 35%, a number-average molecular weight of approximately 12kDa, and a solubility of 85g / L in acetonitrile.

[0035] S3. Industrial-grade acetonitrile was mixed with the above complexing agent at a mass ratio of 200:1. Inductively coupled plasma mass spectrometry (ICP-MS) analysis revealed that the total metal ion content in the industrial-grade acetonitrile was approximately 2.47 ppm, including 0.82 ppm sodium ions, 0.35 ppm potassium ions, 0.94 ppm iron ions, and 0.36 ppm copper ions. The mixture was stirred at 200 rpm for 30 min at 25°C to obtain an acetonitrile solution containing a macromolecular complex.

[0036] S4. Pump the above feed solution into a solvent-resistant hollow fiber ultrafiltration membrane module. The membrane material is polyimide, with a molecular weight cutoff of 3 kDa and a membrane area of ​​0.5 m². 2 The operating pressure is controlled at 0.3 MPa, the operating temperature at 30℃, and the membrane surface flow rate at 2 m / s, using cross-flow filtration. Figure 3 As shown, the acetonitrile feed solution containing macromolecular complexes enters through the membrane module inlet. The macromolecular complexes, due to their molecular weight being much larger than the membrane's molecular weight cutoff, are retained by the membrane and discharged from the concentrate outlet. Small acetonitrile molecules and uncomplexed impurities permeate through the membrane pores and are discharged from the permeate outlet, achieving deep separation of metal ions and acetonitrile. The acetonitrile flux on the permeate side reaches 45 L / (m²). 2 (h) The total metal ion content in the permeate was determined to be 7.8 ppt using inductively coupled plasma mass spectrometry (ICP-MS), including 2.1 ppt of sodium ions, 0.8 ppt of potassium ions, 3.2 ppt of iron ions, and 1.7 ppt of copper ions, fully meeting the semiconductor-grade G4 standard. Large molecular complexes were retained on the concentrate side, resulting in a volume concentration ratio of 10:1.

[0037] S5. Place the concentrated solution in a separatory funnel, add an equal volume of 0.1 mol / L dilute hydrochloric acid aqueous solution, shake at room temperature for 10 min, perform back extraction, separate the liquids, take the organic phase, dry it with anhydrous sodium sulfate, and then dissolve it in anhydrous acetonitrile with a water content ≤0.01% to obtain the regenerated complexing agent. Figure 4 As shown, after 5 cycles, the complexing capacity retention rate of the complexing agent for sodium ions is greater than 92%, and the complexing capacity retention rate for iron ions is greater than 91%, proving that the regeneration effect is good and the cycle can be stable.

[0038] S6. The permeate is dehydrated by vacuum distillation at a bottom temperature of 70℃, a vacuum degree of -0.09MPa, and a reflux ratio of 3:1. Then it is filtered through a 0.1μm polytetrafluoroethylene filter membrane to obtain an ultra-clean high-purity acetonitrile product.

[0039] like Figure 6 As shown, infrared spectroscopy was performed on the product, and the results showed that: at 2940 cm⁻¹ -1 A methyl CH stretching vibration peak appears at 2250 cm⁻¹. -1 A cyano C≡N stretching vibration peak appears at 1370 cm⁻¹ (the most characteristic absorption peak of acetonitrile), and at 1370 cm⁻¹... -1 A CH bending vibration peak appears at 920 cm⁻¹. -1 A CC stretching vibration peak appears at 3400 cm⁻¹. -1 The absence of obvious OH stretching vibration peaks nearby indicates extremely low moisture content in the product; 1700 cm⁻¹ -1 The absence of a prominent C=O stretching vibration peak nearby indicates the absence of residual organic carbonyl impurities in the product. The characteristic peaks described above are consistent with the infrared spectrum of standard acetonitrile, proving that the obtained product is pure acetonitrile.

[0040] Example 2 The difference between this embodiment and Example 1 lies in the molar ratio of 18-crown-6 to p-toluenesulfonyl chloride.

[0041] S1. 18-crown-6 was reacted with p-toluenesulfonyl chloride in pyridine at a molar ratio of 1:1.25 to obtain p-toluenesulfonated 18-crown-6; S2. Dissolve 10g of polyvinyl alcohol in 100mL of anhydrous dimethyl sulfoxide, add 2g of sodium hydride and stir at 60℃ for 2h to activate. Then add 12g of p-toluenesulfonated 18-crown-6 and heat to 80℃ for grafting reaction for 12h to obtain a reaction solution. Add 500mL of anhydrous acetonitrile with a water content ≤0.01% to the reaction solution. After precipitation, filtration and vacuum drying, 18-crown-6 grafted polyvinyl alcohol complexing agent is obtained. 1H NMR spectroscopy confirmed successful grafting of the crown ether, with a grafting rate of 38%, a number-average molecular weight of approximately 12.5kDa, and a solubility of 88g / L in acetonitrile.

[0042] S3 to S6 are the same as in Example 1. The total metal ion content in the final product was determined to be 6.5 ppt using inductively coupled plasma mass spectrometry, including 1.7 ppt of sodium ions, 0.6 ppt of potassium ions, 2.7 ppt of iron ions, and 1.5 ppt of copper ions.

[0043] Example 3 The difference between this embodiment and Example 1 lies in the molar ratio of 18-crown-6 to p-toluenesulfonyl chloride.

[0044] S1. 18-crown-6 was reacted with p-toluenesulfonyl chloride in pyridine at a molar ratio of 1:1.5 to obtain p-toluenesulfonated 18-crown-6; S2. Dissolve 10g of polyvinyl alcohol in 100mL of anhydrous dimethyl sulfoxide, add 2g of sodium hydride and stir at 60℃ for 2h to activate. Then add 12g of p-toluenesulfonate-18-crown-6 and heat to 80℃ for grafting reaction for 12h to obtain the reaction solution. Add 500mL of anhydrous acetonitrile with a water content ≤0.01% to the reaction solution. After precipitation, filtration and vacuum drying, 18-crown-6 grafted polyvinyl alcohol complexing agent is obtained. 1H NMR spectroscopy confirmed successful grafting of the crown ether, with a grafting rate of 36%, a number-average molecular weight of approximately 12.2kDa, and a solubility of 86g / L in acetonitrile.

[0045] S3 to S6 are the same as in Example 1. The total metal ion content in the final product was determined to be 7.1 ppt using inductively coupled plasma mass spectrometry, including 1.9 ppt of sodium ions, 0.7 ppt of potassium ions, 3.0 ppt of iron ions, and 1.5 ppt of copper ions.

[0046] Example 4 The difference between this embodiment and Example 1 lies in the ratio of the complexing agent to acetonitrile.

[0047] S1 to S2 are the same as in Example 1; S3. Industrial-grade acetonitrile and the above complexing agent were mixed at a mass ratio of 100:1. Inductively coupled plasma mass spectrometry (ICP-MS) analysis revealed that the total metal ion content in the industrial-grade acetonitrile was approximately 2.47 ppm, including 0.82 ppm sodium ions, 0.35 ppm potassium ions, 0.94 ppm iron ions, and 0.36 ppm copper ions. The mixture was stirred at 200 rpm for 30 min at 25°C to obtain an acetonitrile solution containing a macromolecular complex.

[0048] S4 to S6 are the same as in Example 1. The total metal ion content in the final product was determined to be 6.2 ppt using inductively coupled plasma mass spectrometry, including 1.6 ppt of sodium ions, 0.6 ppt of potassium ions, 2.6 ppt of iron ions, and 1.4 ppt of copper ions. The acetonitrile flux was 38 L / (m³). 2 ·h).

[0049] Comparative Example 1 The same batch of industrial-grade acetonitrile was passed through a 732 cation exchange resin column at a flow rate of 10 BV / h, with a column volume of 100 mL. After treatment, the total metal ion content in the acetonitrile decreased to 0.153 ppm, including 0.051 ppm sodium ions, 0.019 ppm potassium ions, 0.042 ppm iron ions, and 0.041 ppm copper ions, which did not reach the ppt level. Furthermore, after three acid washes and regenerations, the resin exhibited pulverization, with the number of newly added particles of at least 0.5 μm in the acetonitrile increasing from 5 particles / mL to 124 particles / mL, causing secondary pollution.

[0050] Comparative Example 2 Industrial-grade acetonitrile and activated alumina were mixed at a mass ratio of 10:1. The alumina particle size was 2 mm to 4 mm. After stirring at room temperature for 2 hours, the mixture was filtered. The total metal ion content after treatment was reduced to 0.296 ppm, including 0.079 ppm sodium ions, 0.032 ppm potassium ions, 0.081 ppm iron ions, and 0.104 ppm copper ions. The total removal rate was only 88.0%, far lower than that of this application. Furthermore, alumina adsorption is a broad-spectrum, non-selective adsorption process, with little difference in removal rates for various metal ions, making it impossible to target and remove key ions such as iron and copper ions.

[0051] Comparative Example 3 Industrial-grade acetonitrile is directly pumped into a solvent-resistant hollow fiber ultrafiltration membrane module. The membrane material is polyimide, with a molecular weight cutoff of 3 kDa and a membrane area of ​​0.5 m². 2 No complexing agents were added. The operating pressure was controlled at 0.3 MPa, the operating temperature at 30℃, and the membrane surface flow rate at 2 m / s, using cross-flow filtration. Inductively coupled plasma mass spectrometry (ICP-MS) analysis revealed a total metal ion content of 1.85 ppm in the permeate, including 0.61 ppm sodium, 0.28 ppm potassium, 0.52 ppm iron, and 0.44 ppm copper, resulting in a total removal rate of only 25.1%. Because the ultrafiltration membrane's molecular weight cutoff of 3 kDa is much larger than the diameter of dissolved metal ions, the membrane itself has almost no retention capacity for metal ions. This demonstrates that the complexing agent is the core component for achieving deep removal, while the ultrafiltration membrane only acts as a separation carrier; both are indispensable.

[0052] The preparation steps of Examples 1 to 4 and Comparative Examples 1 to 3 were based on Example 1, with the following baseline parameters: a molar ratio of 18-crown-6 to p-toluenesulfonyl chloride of 1:1, a mass ratio of complexing agent to acetonitrile of 200:1, a molecular weight cutoff of 3 kDa for the ultrafiltration membrane, a complexation reaction temperature of 25°C, an ultrafiltration operating pressure of 0.3 MPa, and a back-extraction hydrochloric acid concentration of 0.1 mol / L. Each example changed only one process parameter; all other parameters were identical to those in Example 1. Comparative Example 1 did not use the complexation-ultrafiltration coupling process of this application; instead, cation exchange resin adsorption was used. Comparative Example 2 did not use the complexation-ultrafiltration coupling process of this application; instead, alumina adsorption was used. Comparative Example 3 did not add a complexing agent and directly used ultrafiltration membrane filtration. Specific parameters are shown in Table 1.

[0053] Table 1

[0054] The acetonitrile products prepared in Examples 1 to 4 and Comparative Examples 1 to 3 were subjected to performance testing. The test indicators included total metal ion content, sodium ion content, potassium ion content, iron ion content, copper ion content, total removal rate, and acetonitrile flux. The results are shown in Table 2.

[0055] Table 2

[0056] Note: The removal rates in the table are all removal rates of total metal ion content. They are calculated using the formula: Removal rate = Total content of raw materials minus the total content after treatment, then divided by the total content of raw materials.

[0057] The total metal ion content in Examples 1 to 4 was in the single digits (ppt), while Comparative Example 1 was 153 ppb, Comparative Example 2 was 296 ppb, and Comparative Example 3 was 1850 ppb, a difference of 2 to 3 orders of magnitude, which intuitively demonstrates the advantages of the method of this application in the removal of trace metal ions.

[0058] Combining the data in Tables 1 and 2, the influence of each parameter on performance can be derived, as detailed in the following analysis: 1.18-crown-6 and p-toluenesulfonyl chloride molar ratio effect: Comparison of Examples 1, 2 and 3 In Table 1, the molar ratio was changed to 1:1.25 in Example 2 and 1:1.5 in Example 3, while other parameters remained the same as the 1:1 ratio in Example 1. Corresponding to the performance data in Table 2: In Example 2, the total metal ion content was 6.5 ppt, the lowest among all examples, with sodium ions at 1.7 ppt, iron ions at 2.7 ppt, and copper ions at 1.5 ppt, all lower than in Example 1. This is because a suitable excess of p-toluenesulfonyl chloride made the sulfonation reaction of 18-crown-6 more complete, increasing the density of active sites in the product and raising the subsequent grafting rate to 38%, thus increasing the metal ion capture capacity of the complexing agent. In Example 3, the molar ratio was increased to 1:1.5, and the total metal ion content rose back to 7.1 ppt, with sodium ions at 1.9 ppt and iron ions at 3.0 ppt. This is because excess p-toluenesulfonyl chloride may cause some sulfonated products to undergo self-polymerization or side reactions, or excess reagent residue may affect the subsequent grafting efficiency, resulting in a grafting rate drop to 36% and a decrease in capture capacity compared to the 1:1.25 ratio. Therefore, 1:1.25 is a better molar ratio that balances sulfonation efficiency and product purity.

[0059] 2. Effect of complexing agent dosage ratio: Comparison of Example 1 and Example 4 In Example 4 of Table 1, the mass ratio of complexing agent to acetonitrile was changed from 200:1 to 100:1, i.e., the amount of complexing agent was doubled, while other parameters remained the same as in Example 1. Table 2 shows that the total metal ion content in Example 4 was 6.2 ppt, lower than the 7.8 ppt in Example 1; sodium ions were 1.6 ppt, iron ions 2.6 ppt, and copper ions 1.4 ppt, all lower than in Example 1. This is because the excessive complexing agent increased the number of coordination sites in the feed solution, resulting in more complete metal ion capture. However, the acetonitrile flux decreased from 45 L / (m²). 2 ·h) decreased to 38L / (m 2 (h) Because excessive complexing agent increases the viscosity of the feed solution, it increases the membrane filtration resistance. Therefore, 200:1 is the optimal dosage ratio that balances removal efficiency and flux.

[0060] 3. The necessity of verifying key processes using comparative methods Key processes or components of this application are omitted in Comparative Examples 1, 2, and 3 of Table 1. Their necessity can be verified by referring to the performance data in Table 2. Comparative Example 1 did not use the complexation-ultrafiltration coupling process of this application, but instead used cation exchange resin adsorption. The total metal ion content was 0.153 ppm, which was about 93.8% lower than that of Example 1. However, it could not reach the ppt level. Moreover, the resin was severely pulverized during regeneration, generating a large number of micron-sized particles, causing secondary pollution. This proves that the solid phase adsorption method is not suitable for the purification of semiconductor-grade acetonitrile.

[0061] Comparative Example 2 did not use the complexation-ultrafiltration coupling process of this application, but instead used alumina adsorption. The total metal ion content was 0.296 ppm, and the total removal rate was only 88.0%. Moreover, it was a broad-spectrum non-selective adsorption, with little difference in the removal rate of each metal ion. It could not target the removal of key ions such as iron ions and copper ions, proving that the selectivity and depth of the traditional adsorption method are insufficient.

[0062] Comparative Example 3, without the addition of a complexing agent, directly used ultrafiltration membrane filtration. The total metal ion content was 1.85 ppm, and the total removal rate was only 25.1%. This is because the molecular weight cutoff of the ultrafiltration membrane (3 kDa) is much larger than the diameter of dissolved metal ions, and the membrane itself has almost no retention capacity for metal ions. This proves that the complexing agent is the core to achieve deep removal, while the ultrafiltration membrane only acts as a separation carrier. Both are indispensable.

[0063] Based on the above data and analysis, the advantages of the ultra-clean high-purity acetonitrile preparation method of this application are as follows: Firstly, it achieves a paradigm shift in metal ion adsorption from solid-liquid adsorption to liquid-liquid complexation and membrane retention, avoiding secondary particulate pollution caused by adsorbent pulverization. The complexing agent dissolves in acetonitrile in molecular form and reacts homogeneously with the metal ions, eliminating the risk of solid-phase abrasion and pulverization. The ultrafiltration membrane only retains large molecular complexes and does not directly contact the metal ions, thus controlling membrane fouling.

[0064] Secondly, the removal rate of trace metal ions reaches over 99.7%, which can stably reduce the total metal ion content in acetonitrile from the ppm level to the ppt level. The cavity size of the crown ether matches the diameter of specific metal ions, forming selective inclusion; combined with the absolute retention of the ultrafiltration membrane, deep purification is achieved.

[0065] Third, the complexing agent and ultrafiltration membrane form a closed-loop circulation system, reducing operating costs. The complexing agent is recycled after back-extraction regeneration, with a single-use loss rate of less than 1%; the ultrafiltration membrane has a flux recovery rate of more than 95% after acetonitrile backwashing, and its membrane life is more than three times longer than that of traditional organic phase filtration. The process can be integrated with existing distillation dehydration and filtration processes, and the ultrafiltration coupling section can be embedded at the end of the existing oxidative distillation process without requiring a radical modification to the overall process route, making it suitable for the industrial continuous production of semiconductor-grade acetonitrile.

[0066] In summary, this application, through systematic experimental data from multiple embodiments and comparative examples, fully verifies the synergistic relationship between the complexing agent, ultrafiltration membrane, and back-extraction regeneration process, as well as their significant effect in acetonitrile purification. It not only solves the technical problems of incomplete removal of metal ions, adsorbent pulverization and secondary pollution, and poor selectivity in traditional acetonitrile purification, but also meets the stringent requirements of the semiconductor industry for ppt-level purity, and has broad application value.

[0067] The above embodiments are only used to illustrate the technical solutions of the present invention and are not intended to limit them. Although the present invention has been described in detail with reference to preferred embodiments, those skilled in the art should understand that modifications or equivalent substitutions can still be made to the technical solutions of the present invention, and these modifications or equivalent substitutions cannot cause the modified technical solutions to deviate from the spirit and scope of the technical solutions of the present invention.

Claims

1. A method for preparing ultra-clean, high-purity acetonitrile, characterized in that, Includes the following steps: S1. Reaction of 18-crown-6 with p-toluenesulfonyl chloride in pyridine yields p-toluenesulfonated 18-crown-6; S2. Dissolve 10g of polyvinyl alcohol in 100ml of anhydrous dimethyl sulfoxide, add sodium hydride and stir at 60℃ for 2h to activate, then add p-toluenesulfonate 18-crown-6, heat to 80℃ for grafting reaction for 12h to obtain reaction solution, add anhydrous acetonitrile with a water content ≤0.01% to reaction solution, and obtain 18-crown-6 grafted polyvinyl alcohol complexing agent after precipitation, filtration and vacuum drying; S3. Mix industrial-grade acetonitrile with 18-crown-6 grafted polyvinyl alcohol complexing agent at a mass ratio of 100:1 to 200:1, and stir at 25°C for 30 min to obtain acetonitrile solution containing macromolecular complexes. S4. Use an ultrafiltration membrane to filter the acetonitrile feed containing macromolecular complexes. Acetonitrile and uncomplexed impurities pass through the ultrafiltration membrane to become permeate, while macromolecular complexes are retained by the ultrafiltration membrane to become concentrate. S5. Add an equal volume of dilute hydrochloric acid aqueous solution to the concentrate, shake at room temperature for 10 min, perform back extraction, separate the liquid and take the organic phase, dry it and dissolve it in anhydrous acetonitrile with a water content ≤0.01% as solvent to obtain the regenerated complexing agent. S6. The permeate is dehydrated by distillation and filtered to obtain ultra-clean, high-purity acetonitrile.

2. The method for preparing ultra-clean high-purity acetonitrile according to claim 1, characterized in that, In step S1, the molar ratio of 18-crown-6 to p-toluenesulfonyl chloride is 1:(1 to 1.5); the amount of pyridine used is 3 to 5 times the total mass of 18-crown-6 and p-toluenesulfonyl chloride; the reaction temperature is 0°C to 25°C, and the reaction time is 2 to 4 hours.

3. The method for preparing ultra-clean high-purity acetonitrile according to claim 1, characterized in that, In step S2, the degree of alcoholysis of polyvinyl alcohol is 88%, and the degree of polymerization is 1700; the mass ratio of sodium hydride to polyvinyl alcohol is (0.15~0.25):1, the activation temperature is 55℃~65℃, and the activation time is 1.5h~2.5h; the mass ratio of p-toluenesulfonyl 18-crown-6 to polyvinyl alcohol is 1.2:1, the grafting reaction temperature is 75℃~85℃, and the grafting reaction time is 10h~14h.

4. The method for preparing ultra-clean high-purity acetonitrile according to claim 1, characterized in that, In step S2, the grafting rate of the 18-crown-6 grafted polyvinyl alcohol complexing agent is 30% to 40%, the number average molecular weight is 10 kDa to 15 kDa, and the solubility in acetonitrile is 80 g / L to 90 g / L.

5. The method for preparing ultra-clean high-purity acetonitrile according to claim 1, characterized in that, In step S3, the metal ions in industrial-grade acetonitrile include one or more of sodium ions, potassium ions, iron ions, and copper ions, and the total content of metal ions is 0.1 ppm to 10 ppm.

6. The method for preparing ultra-clean high-purity acetonitrile according to claim 1, characterized in that, In step S3, the stirring reaction temperature is 20℃~30℃, the reaction time is 20min~40min, and the stirring speed is 150rpm~250rpm.

7. The method for preparing ultra-clean high-purity acetonitrile according to claim 1, characterized in that, In step S4, the ultrafiltration membrane has a molecular weight cutoff of 2kDa to 3kDa, the membrane material is polyimide, the operating pressure is 0.2MPa to 0.4MPa, the operating temperature is 25℃ to 35℃, and the membrane surface flow rate is 1.5m / s to 2.5m / s.

8. The method for preparing ultra-clean high-purity acetonitrile according to claim 1, characterized in that, In step S5, the concentration of the dilute hydrochloric acid aqueous solution is 0.05 mol / L to 0.2 mol / L, and the back-extraction time is 5 min to 15 min.

9. The method for preparing ultra-clean high-purity acetonitrile according to claim 1, characterized in that, In step S6, the distillation and dehydration are carried out under reduced pressure, with the reboiler temperature controlled at 60°C to 80°C, the vacuum degree at -0.08MPa to -0.095MPa, and the reflux ratio at 2:1 to 4:1; the final filtration uses a polytetrafluoroethylene filter membrane with a pore size of 0.1μm.

10. An ultra-clean, high-purity acetonitrile, characterized in that, The ultra-clean high-purity acetonitrile is prepared by any one of the methods described in claims 1 to 9, wherein the total metal ion content of the ultra-clean high-purity acetonitrile is not greater than 10 ppt.