Integrated circuit devices
By employing capacitor structures made of different metal oxide materials with rutile phase crystal structures in IC devices, the capacitance and reliability issues of capacitors in a reduced space are solved, achieving the effect of high capacitance and low leakage current.
Patent Information
- Application Number
- CN202610235864.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2025-05-15
- Filing Date
- 2026-02-27
- Publication Date
- 2026-11-17
AI Technical Summary
As IC device sizes shrink, capacitors occupy less space, making it difficult to optimize capacitor structures with existing technologies to provide relatively high capacitance and reliability.
The capacitor structure includes an outer template electrode part, a main electrode part, and a bottom bridging electrode part. The outer template electrode part and the main electrode part are respectively composed of different metal oxide materials with rutile phase crystal structure, and the lower electrode structure is supported by a support film. The dielectric film is composed of TiO2 film to maintain a high dielectric constant and reduce leakage current.
It improves the electrical properties and reliability of the capacitor, increases the capacitance, reduces the resistance and leakage current, and prevents oxidation and deterioration of the conductive areas.
Smart Images

Figure CN123124346A_ABST
Abstract
Description
Cross-references to related applications
[0001] This application claims priority and benefit to Korean Patent Application No. 10-2025-0063521, filed on May 15, 2025, with the Korean Intellectual Property Office, the entire disclosure of which is incorporated herein by reference. Technical Field
[0002] The disclosed concept relates to an integrated circuit (IC) device, and more specifically, to an IC device that includes a capacitor. Background Technology
[0003] As the size of IC devices shrinks, the space occupied by capacitors is also rapidly decreasing. Therefore, it is necessary to develop technologies that can optimize capacitor structure to overcome space and design constraints while providing relatively high capacitance. Summary of the Invention
[0004] The disclosed concept provides an integrated circuit (IC) device that includes a capacitor with improved electrical properties and reliability.
[0005] According to various aspects of the disclosed concept, an IC device is provided, comprising: a conductive region located on a substrate; and a capacitor located on the conductive region, the capacitor including a lower electrode structure, an upper electrode, and a dielectric film located between the lower electrode structure and the upper electrode, wherein the lower electrode structure includes: an outer template electrode portion spaced apart from the conductive region in a substantially vertical direction, the outer template electrode portion contacting the dielectric film and including a first metal oxide having a rutile phase crystal structure; a main electrode portion having a first bottom surface and a first outer sidewall, wherein the first bottom surface and the first outer sidewall contact the outer template electrode portion, the main electrode portion including a second metal oxide and spaced apart from the dielectric film, and the outer template electrode portion located between the main electrode portion and the dielectric film, wherein the second metal oxide includes a material different from the first metal oxide and has a rutile phase crystal structure; and a bottom bridging electrode portion located between the conductive region and the outer template electrode portion, and spaced apart from the main electrode portion in a substantially vertical direction, and the outer template electrode portion located between the bottom bridging electrode portion and the main electrode portion, the bottom bridging electrode portion including a conductive metal nitride.
[0006] According to various aspects of the disclosed concept, an IC device is provided, comprising: a conductive region located on a substrate; a lower electrode structure located on the conductive region; a support film configured to support the lower electrode structure around the lower electrode structure; an upper electrode facing the lower electrode structure on the substrate; and a dielectric film located between the lower electrode structure and the upper electrode, wherein the lower electrode structure includes: an outer template electrode portion spaced apart from the conductive region in a substantially vertical direction, the outer template electrode portion contacting the dielectric film and comprising a first metal oxide having a rutile phase crystal structure; and a main electrode portion having a first bottom surface and a first outer sidewall in contact with the outer template electrode portion. The device includes a second metal oxide spaced apart from a dielectric film, with an outer template electrode portion located between the main electrode portion and the dielectric film. The second metal oxide comprises a material different from that of the first metal oxide and has a rutile phase crystal structure. A bottom bridging electrode portion is located between the conductive region and the outer template electrode portion and spaced apart from the main electrode portion in a substantially vertical direction. The outer template electrode portion is located between the bottom bridging electrode portion and the main electrode portion. A side bridging electrode portion is located between the outer template electrode portion and the support film and spaced apart from the bottom bridging electrode portion. The bottom bridging electrode portion and the side bridging electrode portion comprise the same conductive metal nitride.
[0007] According to various aspects of the disclosed concept, an IC device is provided, comprising: a conductive region located on a substrate; a lower electrode structure located on the conductive region; a support film configured to support the lower electrode structure around the lower electrode structure; an upper electrode facing the lower electrode structure on the substrate; and a dielectric film located between the lower electrode structure and the upper electrode, wherein the lower electrode structure includes: an outer template electrode portion spaced apart from the conductive region in a substantially vertical direction, the outer template electrode portion contacting the dielectric film and comprising tin oxide having a rutile phase crystal structure; a main electrode portion having a first bottom surface and a first outer sidewall, wherein the first bottom surface and the first outer sidewall contact the outer template electrode portion, and the main electrode portion comprising vanadium oxide, molybdenum oxide, and vanadium oxide. The device comprises: niobium, cobalt oxide, or a combination thereof having a rutile phase crystal structure; a main electrode portion spaced apart from a dielectric film and an outer template electrode portion located between the main electrode portion and the dielectric film; a bottom bridging electrode portion located between the conductive region and the outer template electrode portion, and spaced apart from the main electrode portion in a substantially vertical direction, and the outer template electrode portion located between the bottom bridging electrode portion and the main electrode portion; and a side bridging electrode portion located between the outer template electrode portion and the support film and spaced apart from the bottom bridging electrode portion, wherein each of the bottom bridging electrode portion and the side bridging electrode portion comprises titanium nitride (TiN), and the dielectric film comprises a TiO2 film having a rutile phase crystal structure, the TiO2 film being in contact with the outer template electrode portion.
[0008] According to various aspects of the disclosed concept, a method for manufacturing an IC device is provided. The method includes forming a molded structure on a conductive region formed on a substrate. A vertical via is formed in the molded structure to expose the conductive region. An initial bridging electrode layer is formed such that the initial bridging electrode layer covers the conductive region and the molded structure inside the vertical via. An outer template electrode portion and a main electrode portion are formed. The outer template electrode portion is formed on the initial bridging electrode layer inside the vertical via, and the outer template electrode portion comprises a first metal oxide having a rutile phase crystal structure. The main electrode portion covers the outer template electrode portion inside the vertical via and comprises a second metal oxide. The second metal oxide comprises a material different from the first metal oxide and has a rutile phase crystal structure. A portion of the molded structure is removed to expose the sidewalls of the initial bridging electrode layer. A portion of the initial bridging electrode layer is removed from the exposed sidewalls of the initial bridging electrode layer to expose the outer sidewalls of the outer template electrode portion. A dielectric film is formed such that the dielectric film contacts the outer sidewalls of the outer template electrode portion.
[0009] In one embodiment, removing a portion of the initial bridging electrode layer may include forming a bottom bridging electrode portion, which includes the remaining portion of the initial bridging electrode layer. The bottom bridging electrode portion may be formed such that it is located between the conductive region and the outer template electrode portion.
[0010] In one embodiment, removing a portion of the initial bridging electrode layer may include forming a side bridging electrode portion, which includes the remaining portions of the initial bridging electrode layer.
[0011] In an embodiment, a side bridging electrode portion may be formed such that the side bridging electrode portion protrudes from the outer sidewall of the outer template electrode portion in a substantially transverse direction that is substantially parallel to the main surface of the substrate.
[0012] In an embodiment, forming a dielectric film may include forming a TiO2 film having a rutile phase crystal structure so that the TiO2 film contacts the outer wall of the outer template electrode portion.
[0013] In an embodiment, forming the molded structure may include sequentially forming a first molded film, a first support film, a second molded film, and a second support film on a substrate. Each of the first support film and the second support film may include a material having etch selectivity relative to the first molded film and the second molded film, and removing a portion of the molded structure may include selectively removing the first molded film and the second molded film from the first molded film, the first support film, the second molded film, and the second support film.
[0014] In an embodiment, the initial bridging electrode layer may include a conductive metal nitride.
[0015] In an embodiment, after forming the outer template electrode portion and the main electrode portion and before removing a portion of the molded structure, the method may further include forming a capping electrode portion covering the uppermost surface of each of the outer template electrode portion and the main electrode portion. The capping electrode portion may include a conductive metal nitride.
[0016] In an embodiment, the outer template electrode portion may include dopant-free tin oxide or tin oxide containing a dopant of at least one element selected from niobium (Nb), antimony (Sb), and tantalum (Ta).
[0017] In an embodiment, the main electrode portion may include vanadium oxide, molybdenum oxide, niobium oxide, cobalt oxide, or a combination thereof, and the main electrode portion may include Sn dopant in a range of approximately 0 atomic percent (at%) to approximately 10 at%.
[0018] In an embodiment, the main electrode portion may have a column shape with a filled interior or a cup-shaped cross-section structure. Attached Figure Description
[0019] The embodiments will become clearer from the following detailed description taken in conjunction with the accompanying drawings, in which: Figure 1 This is a schematic planar layout showing some components of a memory cell array region of an integrated circuit (IC) device according to an embodiment; Figure 2 This is a cross-sectional view of some components of an IC device according to an embodiment; Figure 3 This is a plan view illustrating an example of the planar shape of a plurality of lower electrode structures and a second support film in an IC device according to an embodiment; Figure 4 This is a cross-sectional view of some components of an IC device according to an embodiment; Figure 5 This is a cross-sectional view of some components of an IC device according to yet another embodiment; Figures 6A to 6K This is a cross-sectional view of the process sequence of a method for manufacturing an IC device according to an embodiment; and Figures 7A to 7E This is a cross-sectional view of the process sequence of a method for manufacturing an IC device according to an embodiment. Detailed Implementation
[0020] In the following description, embodiments will be illustrated in detail with reference to the accompanying drawings. The same reference numerals are used in the drawings to denote the same elements, and repeated descriptions will be omitted.
[0021] Figure 1 This is a schematic planar layout showing some components of the memory cell array region of an integrated circuit (IC) device 10 according to an embodiment. The IC device 10 may be configured as a dynamic random access memory (DRAM) device.
[0022] Reference Figure 1 The IC device 10 may include a plurality of active regions ACT, which, in the view above, are arranged to extend laterally in each of two directions: a first lateral direction (X direction) and a second lateral direction (Y direction) orthogonal to the first lateral direction (X direction). A plurality of word lines WL may intersect the plurality of active regions ACT and extend parallel to each other in the first lateral direction (X direction). On the plurality of word lines WL, a plurality of bit lines BL may extend parallel to each other in the second lateral direction (Y direction). Each of the plurality of bit lines BL may be connected to an active region ACT via a direct contact DC.
[0023] Multiple buried contacts BC can be formed between two adjacent bit lines BL. Multiple conductive landing pads LP can be formed on the multiple buried contacts BC. Each of the multiple conductive landing pads LP can be arranged to overlap at least a portion of the buried contact BC. Multiple lower electrode structures LE can be formed on the multiple conductive landing pads LP. The multiple lower electrode structures LE can be connected to multiple active regions ACT through the multiple buried contacts BC and the multiple conductive landing pads LP.
[0024] Figure 2 This is a cross-sectional view of some components of the IC device 100 according to an embodiment.
[0025] Reference Figure 2 IC device 100 can constitute Figure 1 A portion of the IC device 10 shown. Figure 2 Some components of the IC device 100 are omitted or shown in a simplified manner. However, it should be understood that the construction of the IC device 100 is not limited to... Figure 2 The construction shown in the figure is not the same as the characteristic construction described below.
[0026] IC device 100 may include a substrate 110 containing a plurality of active regions ACT and a lower structure 120 formed on the substrate 110. Conductive regions 124 may pass through the lower structure 120 and be connected to the active regions ACT.
[0027] Substrate 110 may include semiconductor elements (such as silicon (Si) and germanium (Ge)) or compound semiconductors (such as silicon carbide (SiC), gallium arsenide (GaAs), indium arsenide (InAs), and indium phosphide (InP)). Substrate 110 may include a semiconductor substrate and a structure formed on the semiconductor substrate including at least one insulating film or at least one conductive region. The conductive region may include, for example, a doped well or a doped structure. In embodiments, substrate 110 may have various device isolation structures, such as shallow trench isolation (STI) structures. Multiple active regions ACT may be defined in substrate 110 by multiple device isolation regions 112. Device isolation regions 112 may include oxide films, nitride films, or combinations thereof.
[0028] In an embodiment, the lower structure 120 may include an insulating film comprising a silicon oxide film, a silicon nitride film, or a combination thereof. In an embodiment, the lower structure 120 may include various conductive regions, such as wiring layers, contact plugs, transistors, and insulating films configured to insulate the wiring layers, contact plugs, and transistors from each other. Conductive regions 124 may include polysilicon, metal, conductive metal nitrides, metal silicides, or combinations thereof. The lower structure 120 may include reference... Figure 1The description includes multiple bit lines BL. Conductive region 124 may include previously referenced... Figure 1 The embedded contact BC and conductive landing pad LP are described.
[0029] An insulating pattern 126P having an opening 126H may be located on the lower structure 120 and the conductive region 124. The insulating pattern 126P may include silicon nitride, silicon oxynitride, or a combination thereof.
[0030] The lower electrode structure LE1 can be arranged on the conductive region 124. The lower electrode structure LE1 can form a reference. Figure 1 The lower electrode structure LE is described. The lower electrode structure LE1 can extend longitudinally from the top surface of the conductive region 124 through the opening 126H of the insulating pattern 126P in the vertical direction (Z direction). A dielectric film 140 and an upper electrode 150 can be formed on the lower electrode structure LE1. The dielectric film 140 can be located between the lower electrode structure LE1 and the upper electrode 150. The lower electrode structure LE1, the dielectric film 140, and the upper electrode 150 can constitute a capacitor CP1.
[0031] The lower electrode structure LE1 may include a bottom bridging electrode portion 132A, an outer template electrode portion 134, and a main electrode portion 136 sequentially formed on the conductive region 124.
[0032] The bottom bridging electrode portion 132A may be located between the conductive region 124 and the outer template electrode portion 134. The conductive region 124 may be spaced apart from the outer template electrode portion 134 in the vertical direction (Z direction), and the bottom bridging electrode portion 132A is located between the conductive region 124 and the outer template electrode portion 134. The bottom bridging electrode portion 132A may have a bottom surface in contact with the conductive region 124 and a top surface in contact with the outer template electrode portion 134. The bottom bridging electrode portion 132A may be spaced apart from the main electrode portion 136 in the vertical direction (Z direction), and the outer template electrode portion 134 is located between the bottom bridging electrode portion 132A and the main electrode portion 136. The bottom bridging electrode portion 132A may include a portion in contact with the dielectric film 140. The bottom bridging electrode portion 132A may be spaced apart from the upper electrode 150, and the dielectric film 140 is located between the bottom bridging electrode portion 132A and the upper electrode 150.
[0033] In an embodiment, the bottom bridging electrode portion 132A may include a conductive metal nitride. For example, the bottom bridging electrode portion 132A may include titanium nitride (TiN). In an embodiment, the bottom bridging electrode portion 132A may have a thickness selected in the range of about 1 Å to about 50 Å in the vertical direction (Z direction). The vertical direction (Z direction) may be a direction perpendicular to the main surface 110M of the substrate 110.
[0034] The outer template electrode portion 134 may be spaced apart from the conductive region 124 in the vertical direction (Z direction) and may include a first metal oxide having a rutile phase crystal structure. The bottom surface 134B of the outer template electrode portion 134 may face the conductive region 124 and contact the bottom bridging electrode portion 132A. The outer sidewall 134S of the outer template electrode portion 134 may face the upper electrode 150 and the contact dielectric film 140.
[0035] In this embodiment, the outer template electrode portion 134 may include dopant-free tin oxide. Tin oxide may include SnO. x (1.5 ≤ x ≤ 2.0). For example, tin oxide may include SnO2. In an embodiment, the outer template electrode portion 134 may include tin oxide containing a dopant. The dopant included in the outer template electrode portion 134 may be selected from niobium (Nb), antimony (Sb), and tantalum (Ta). For example, the outer template electrode portion 134 may include a SnO2 film containing a dopant selected from Nb, Sb, and Ta. The dopant content in the outer template electrode portion 134 may be selected in the range of about 0 at% to about 10 at%. In the outer template electrode portion 134, the dopant may improve the chemical stability of SnO2 at room temperature (e.g., a temperature of about 20 ºC to about 28 ºC), thereby reducing the likelihood of reduction of the Sn element included in the outer template electrode portion 134 and preventing or minimizing the decrease in the conductivity of the outer template electrode portion 134. In an embodiment, the outer template electrode portion 134 may have a thickness selected in the range of about 1 Å to about 50 Å in the vertical direction (Z direction).
[0036] The main electrode portion 136 may be spaced apart from the conductive region 124 in the vertical direction (Z direction), and the bottom bridging electrode portion 132A and the outer template electrode portion 134 are located between the main electrode portion 136 and the conductive region 124. The main electrode portion 136 may include a second metal oxide, which is a different material from the first metal oxide included in the outer template electrode portion 134 and has a rutile phase crystal structure. The main electrode portion 136 may have a bottom surface 136B and an outer sidewall 136S that contact the outer template electrode portion 134. The bottom surface 136B of the main electrode portion 136 may face the conductive region 124 and contact the outer template electrode portion 134. The outer sidewall 136S of the main electrode portion 136 may face the upper electrode 150 and the dielectric film 140 and contact the outer template electrode portion 134. The outer wall 136S of the main electrode portion 136 may be spaced apart from the dielectric film 140, and the outer template electrode portion 134 is located between the outer wall 136S of the main electrode portion 136 and the dielectric film 140. As used herein, the bottom surface 136B of the main electrode portion 136 may be referred to as the first bottom surface, and the bottom surface 134B of the outer template electrode portion 134 may be referred to as the second bottom surface. As used herein, the outer wall 136S of the main electrode portion 136 may be referred to as the first outer wall, and the outer wall 134S of the outer template electrode portion 134 may be referred to as the second outer wall.
[0037] In an embodiment, the second metal oxide included in the main electrode portion 136 may include vanadium oxide, molybdenum oxide, niobium oxide, cobalt oxide, or a combination thereof. Vanadium oxide may include VO₂. x (1.5 ≤ x ≤ 3.0). For example, vanadium oxide may include VO2, V2O5, or VO3. Molybdenum oxide may include MoO. x (1.5 ≤ x ≤ 3.0). For example, molybdenum oxide may include MoO2 or MoO3. Niobium oxide may include NbO. x (1.5 ≤ x ≤ 3.0). For example, niobium oxide may include NbO, NbO2, or Nb2O5. Cobalt oxide may include CoO. x (1.5≤x≤2.0). For example, cobalt oxide can include CoO, Co2O3, or Co3O4.
[0038] In one embodiment, the second metal oxide included in the main electrode portion 136 may not contain a dopant. Alternatively, the second metal oxide included in the main electrode portion 136 may include a dopant containing Sn. The dopant content in the main electrode portion 136 may be selected in the range of approximately 0 at% to approximately 10 at%. Because the second metal oxide included in the main electrode portion 136 has relatively high conductivity and thermal stability, leakage current generated in the capacitor CP1 can be suppressed, and the capacitor CP1 can provide relatively high capacitance.
[0039] The main electrode portion 136 may have a columnar shape with a filled interior. Therefore, apart from the material included in the main electrode portion 136 (e.g., a second metal oxide) and dopants that may be included as needed, no other constituent materials may exist inside the main electrode portion 136 defined by the outer wall 136S of the main electrode portion 136.
[0040] The lower electrode structure LE1 of capacitor CP1 may further include a capping electrode portion 138, which covers the uppermost surface of each of the outer template electrode portion 134 and the main electrode portion 136. In an embodiment, the capping electrode portion 138 may include a conductive metal nitride. For example, the capping electrode portion 138 may include TiN. In an embodiment, the material of the capping electrode portion 138 may be the same as the material of the bottom bridging electrode portion 132A. In a lateral direction parallel to the main surface 110M of the substrate 110, the width of the capping electrode portion 138 may be greater than the maximum width of each of the outer template electrode portion 134 and the main electrode portion 136.
[0041] The lower electrode structure LE1 of capacitor CP1 may further include at least one side bridging electrode portion 132B protruding from the outer sidewall 134S of the outer template electrode portion 134 at a third vertical level. The third vertical level may be located between the first vertical level of the bottom bridging electrode portion 132A and the second vertical level of the capping electrode portion 138. At least one side bridging electrode portion 132B may protrude outwards from the lower electrode structure LE1 in a lateral direction parallel to the main surface 110M of the substrate 110. As used herein, a vertical level refers to the distance from the main surface 110M of the substrate 110 in the vertical direction (Z direction). In the lower electrode structure LE1, the side bridging electrode portion 132B may be spaced apart from each of the capping electrode portion 138 and the bottom bridging electrode portion 132A.
[0042] In an embodiment, the side bridging electrode portion 132B may include a conductive metal nitride. For example, the side bridging electrode portion 132B may include TiN. In an embodiment, the constituent material of the side bridging electrode portion 132B may be the same as the constituent material of the bottom bridging electrode portion 132A. In an embodiment, the bottom bridging electrode portion 132A, the side bridging electrode portion 132B, and the capping electrode portion 138 may include the same conductive metal nitride. In the lower electrode structure LE1, each of the bottom bridging electrode portion 132A, the side bridging electrode portion 132B, and the capping electrode portion 138 may have a surface in contact with the dielectric film 140.
[0043] At least one support film configured to support the lower electrode structure LE1 may be disposed around the lower electrode structure LE1. The at least one support film may include a first support film SPT1 and a second support film SPT2 spaced apart from each other in the vertical direction (Z direction). The lower electrode structure LE1 may constitute a reference. Figure 1 The described lower electrode structure LE.
[0044] Figure 3 This is a plan view showing an example of the planar shape of a plurality of lower electrode structures LE1 in the IC device 100 and a second support film SPT2 configured to support the plurality of lower electrode structures LE1. Figure 2 The cross-sectional structure shown can be combined with the cross-sectional structure along the cross-section. Figure 3 The portion of the cross section intercepted by line X1-X1' corresponds to this region.
[0045] Reference Figure 2 and Figure 3 Multiple lower electrode structures LE1 can be supported by a first support film SPT1 and a second support film SPT2. The second support film SPT2 can be arranged at a distance from the substrate 110 in the vertical direction (Z direction), and the first support film SPT1 is located between the second support film SPT2 and the substrate 110.
[0046] Multiple lower electrode structures LE1 may be opposite to the upper electrode 150, and a dielectric film 140 is located between the multiple lower electrode structures LE1 and the upper electrode 150. The dielectric film 140 may cover the lower electrode structures LE1, the first support film SPT1, and the second support film SPT2. The dielectric film 140 may include portions that are in contact with the insulating pattern 126P, the first support film SPT1, the second support film SPT2, and the outer template electrode portion 134 of the lower electrode structure LE1, respectively.
[0047] The second support film SPT2 may extend in a lateral direction parallel to the main surface 110M of the substrate 110, surrounding the upper end of each of the plurality of lower electrode structures LE1. The second support film SPT2 may include a plurality of upper holes UH passing through the plurality of lower electrode structures LE1. The inner sidewall of each of the plurality of upper holes UH included in the second support film SPT2 may contact the outer sidewall of the lower electrode structure LE1. For example, the inner sidewall of each of the plurality of upper holes UH included in the second support film SPT2 may contact the outer sidewall of the capping electrode portion 138 included in the lower electrode structure LE1. In the plurality of lower electrode structures LE1, the vertical level of the uppermost surface of the capping electrode portion 138 may be closer to the substrate 110 than the vertical level of the uppermost surface of the second support film SPT2. The vertical distance from the main surface 110M of the substrate 110 to the uppermost surface of the second support film SPT2 may be greater than the vertical distance from the main surface 110M of the substrate 110 to the uppermost surface of the capping electrode portion 138 of each of the plurality of lower electrode structures LE1.
[0048] The first support film SPT1 may extend between the substrate 110 and the second support film SPT2 in a lateral direction parallel to the main surface 110M of the substrate 110, and contact the outer wall of each of the plurality of lower electrode structures LE1. Similar to the plurality of upper holes UH included in the second support film SPT2, the first support film SPT1 may include a plurality of lower holes passing through the plurality of lower electrode structures LE1. The plurality of lower electrode structures LE1 may pass through the plurality of upper holes UH formed in the second support film SPT2 and the plurality of lower holes formed in the first support film SPT1 and extend in the vertical direction (Z direction).
[0049] Figure 3 An example of a planar structure is shown in which four lower electrode structures LE1 are positioned adjacent to each other along the inner sidewall of each of the plurality of upper holes UH included in the second support film SPT2. However, the planar shape of each of the plurality of upper holes UH is not limited to... Figure 3 The invention is shown and can be modified in various ways within the scope of the inventive concept. Each of the plurality of lower holes included in the first support membrane SPT1 may have a planar shape corresponding to the planar shape of each of the plurality of upper holes UH.
[0050] Each of the first support film SPT1 and the second support film SPT2 may comprise a silicon nitride film (SiN), a silicon carbonitride film (SiCN), a boron silicon nitride film (SiBN), or a combination thereof. In one embodiment, the first support film SPT1 and the second support film SPT2 may comprise the same material. In another embodiment, the first support film SPT1 and the second support film SPT2 may comprise different materials. In one example, each of the first support film SPT1 and the second support film SPT2 may comprise SiCN. In another example, the first support film SPT1 may comprise SiCN, and the second support film SPT2 may comprise SiBN. However, the inventive concept is not limited to the materials described above.
[0051] like Figure 2 As shown, the thicknesses of the first support film SPT1 and the second support film SPT2 in the vertical direction (Z direction) can be different from each other. For example, the thickness of the second support film SPT2 in the vertical direction (Z direction) can be greater than the thickness of the first support film SPT1. However, the inventive concept is not limited to this, and the thickness of each of the first support film SPT1 and the second support film SPT2 in the vertical direction (Z direction) can be determined differently as needed. Figure 2 The diagram illustrates a structure in which two support films, including a first support film SPT1 and a second support film SPT2, are arranged around the lower electrode structure LE1, but the inventive concept is not limited thereto. For example, the IC device 100 may include one or at least three support films sequentially formed in the vertical direction (Z direction).
[0052] like Figure 2 As shown, the side bridging electrode portion 132B of the lower electrode structure LE1 can extend in a lateral direction from the outer sidewall 134S of the outer template electrode portion 134 toward the first support film SPT1. The width of the side bridging electrode portion 132B in the lateral direction can be defined by the outer sidewall 134S of the outer template electrode portion 134 and the first support film SPT1.
[0053] In the vertical direction (Z direction), the thickness of the capping electrode portion 138 can be greater than the thickness of the side bridging electrode portion 132B. The sidewall of the capping electrode portion 138 that contacts the second support film SPT2 can protrude outward from the lower electrode structure LE1 in the lateral direction beyond the outer sidewall 134S of the outer template electrode portion 134. Each of the first support film SPT1 and the second support film SPT2 can support the lower electrode structure LE1 at a location other than the outer template electrode portion 134.
[0054] The dielectric film 140 may conformally cover the outer wall of the lower electrode structure LE1, the bottom and top surfaces of each of the first support film SPT1 and the second support film SPT2, and the top surface of the insulating pattern 126P. The dielectric film 140 may include a portion that contacts a portion of the bottom bridging electrode portion 132A of the lower electrode structure LE1 located between the insulating pattern 126P and the outer template electrode portion 134. The dielectric film 140 may include a portion that contacts the uppermost surface of the capping electrode portion 138 of the lower electrode structure LE1. The dielectric film 140 may contact the bottom and top surfaces of the side bridging electrode portion 132B of the lower electrode structure LE1. The bottom surface of the side bridging electrode portion 132B may be the surface facing the substrate 110, and the top surface of the side bridging electrode portion 132B may be the surface opposite to the bottom surface of the side bridging electrode portion 132B. The dielectric film 140 may not include a portion that contacts the main electrode portion 136.
[0055] The dielectric film 140 may include a TiO2 film having a rutile phase crystal structure. At least a portion of the dielectric film 140 in contact with the outer template electrode portion 134 of the lower electrode structure LE1 may include a TiO2 film having a rutile phase crystal structure. In the lower electrode structure LE1, the outer template electrode portion 134 may serve as a crystallization induction layer configured to induce the dielectric film 140 to have a rutile phase crystal structure. For example, when the outer template electrode portion 134 includes a SnO2 film having a rutile phase crystal structure, the metal oxide included in the dielectric film 140 can maintain the rutile phase crystal structure during the formation of the dielectric film 140 from the surface of the outer template electrode portion 134. Therefore, the dielectric film 140 can provide a relatively high dielectric constant and can reduce or eliminate leakage current between the lower electrode structure LE1 and the dielectric film 140.
[0056] In embodiments, the TiO2 film with a rutile phase crystal structure included in the dielectric film 140 may further include a dopant. The dopant that may be included in the TiO2 film may be selected from, but is not limited to, aluminum (Al), germanium (Ge), yttrium (Y), gallium (Ga), lanthanum (La), boron (B), indium (In), and scandium (Sc). The dopant content in the TiO2 film included in the dielectric film 140 may be selected in the range of approximately 0 at% to approximately 10 at%.
[0057] In an embodiment, the dielectric film 140 may have a single-film structure, which includes a TiO2 film having a rutile phase crystal structure. In this case, the dielectric film 140 may include an undoped rutile phase TiO2 film or a doped rutile phase TiO2 film.
[0058] In an embodiment, the dielectric film 140 may have a multilayer film structure, comprising a TiO2 film with a rutile phase crystal structure and at least one high-k dielectric film. In this case, the TiO2 film with the rutile phase crystal structure may be in contact with the outer template electrode portion 134 of the lower electrode structure LE1, and the at least one high-k dielectric film may be spaced apart from the lower electrode structure LE1, with the TiO2 film with the rutile phase crystal structure located between the at least one high-k dielectric film and the lower electrode structure LE1. In an embodiment, the at least one high-k dielectric film may include at least one metal selected from zirconium (Zr), titanium (Ti), strontium (Sr), hafnium (Hf), aluminum (Al), niobium (Nb), cerium (Ce), lanthanum (La), and tantalum (Ta). In an embodiment, the at least one high-k dielectric film may include at least one selected from ZrO2 film, TiO2 film, HfO2 film, Al2O3 film, Nb2O5 film, CeO2 film, La2O3 film, Ta2O3 film, and SrTiO3 film. For example, at least one high-k dielectric film may include, but is not limited to, ZrO2, SrTiO3, or combinations thereof. In embodiments, dielectric film 140 may have a thickness of about 10 Å to about 80 Å, but is not limited to.
[0059] The upper electrode 150 may include a portion facing the lower electrode structure LE1 and therebetween the dielectric film 140, and a portion facing the first support film SPT1 and the second support film SPT2 and therebetween the dielectric film 140.
[0060] The upper electrode 150 may include a metal film, a conductive metal oxide film, a conductive metal nitride film, a conductive metal oxynitride film, or a combination thereof. In embodiments, the upper electrode 150 may include Nb, Nb oxide, Nb nitride, Nb oxynitride, Ti, Ti oxide, Ti nitride, Ti oxynitride, Co, Co oxide, Co nitride, Co oxynitride, Sn, Sn oxide, Sn nitride, Sn oxynitride, or a combination thereof. For example, the upper electrode 150 may include NbN, TiN, CoN, SnO2, or a combination thereof. In embodiments, the upper electrode 150 may include tantalum nitride (TaN), titanium aluminum nitride (TiAlN), tantalum aluminum nitride (TaAlN), vanadium (V), vanadium nitride (VN), molybdenum (Mo), molybdenum nitride (MoN), tungsten (W), tungsten nitride (WN), ruthenium (Ru), ruthenium oxide (RuO2), strontium ruthenium oxide (SrRuO3), iridium (Ir), iridium oxide (IrO2), platinum (Pt), platinum oxide (PtO), SrRuO3 (SRO), (Ba,Sr)RuO3 (BSRO), CaRuO3 (CRO), (La,Sr)CoO3 (LSCo), or combinations thereof. However, the constituent materials of the upper electrode 150 are not limited to the examples described above.
[0061] In reference Figure 2 and Figure 3 In the described IC device 100, the lower electrode structure LE1 of capacitor CP1 may include an outer template electrode portion 134 and a main electrode portion 136. The outer template electrode portion 134 may be in contact with a dielectric film 140, and the main electrode portion 136 may be spaced apart from and surrounded by the outer template electrode portion 134. Each of the outer template electrode portion 134 and the main electrode portion 136 may include a metal oxide having a rutile phase crystal structure. When the dielectric film 140 is formed, the outer template electrode portion 134 may serve as a crystallization induction layer configured to induce the dielectric film 140 to have a rutile phase crystal structure. Due to the outer template electrode portion 134, the material included in the dielectric film 140 can easily maintain a rutile phase crystal structure. Therefore, the dielectric film 140 can provide a relatively high dielectric constant, which can reduce or eliminate leakage current between the lower electrode structure LE1 and the dielectric film 140, and the capacitance of capacitor CP1 can be increased. Therefore, the reliability of IC device 100 can be improved.
[0062] According to reference Figure 2 and Figure 3 In the described IC device 100, in the lower electrode structure LE1 of capacitor CP1, the first metal oxide included in the outer template electrode portion 134 may include a material different from the second metal oxide included in the main electrode portion 136.
[0063] For example, the first metal oxide included in the outer template electrode portion 134 may include a material with excellent corrosion resistance to a predetermined etching atmosphere, and the second metal oxide included in the main electrode portion 136 may include a low-resistance material with relatively high conductivity. More specifically, the first metal oxide included in the outer template electrode portion 134 may include a material with relatively high corrosion resistance to an etching atmosphere (e.g., tin oxide), which is used for the following reference. Figure 6I The process described involves removing the first molding film MD1 and the second molding film MD2 during the manufacturing of the IC device 100. Due to this configuration, even when the outer template electrode portion 134 is exposed after removing the first molding film MD1 and the second molding film MD2, the outer template electrode portion 134 can maintain its rutile phase crystal structure without damage. Consequently, when the dielectric film 140 is formed on the surface of the outer template electrode portion 134, the rutile phase crystal structure of the dielectric film 140 can be strengthened by the outer template electrode portion 134.
[0064] Furthermore, the second metal oxide included in the main electrode portion 136 may comprise a low-resistance material with relatively high conductivity, such as vanadium oxide, molybdenum oxide, niobium oxide, cobalt oxide, or combinations thereof. Due to the above construction, the resistance of the lower electrode structure LE1 can be reduced, and the lower electrode structure LE1 can ensure relatively high conductivity and thermal stability. Moreover, because the second metal oxide included in the main electrode portion 136 has a rutile phase crystal structure, the main electrode portion 136 can also be used together with the outer template electrode portion 134 to induce the dielectric film 140 to have a rutile phase crystal structure. As a result, the dielectric film 140 can more effectively maintain the rutile phase crystal structure.
[0065] Furthermore, the lower electrode structure LE1 of capacitor CP1 may include a bottom bridging electrode portion 132A covering the conductive region 124 between the outer template electrode portion 134 and the conductive region 124. Therefore, during the manufacturing process of the IC device 100, when forming the outer template electrode portion 134 and the main electrode portion 136, each comprising a metal oxide, there is no need to worry about the conductive region 124 being exposed to the oxidizing atmosphere used to form the metal oxide. Thus, deterioration of the conductive region 124 due to oxidation during the formation of the outer template electrode portion 134 and the main electrode portion 136 can be prevented, and therefore, an increase in the interface resistance in the conductive region 124 can be effectively prevented.
[0066] Figure 4 This is a cross-sectional view of some components of the IC device 100A according to an embodiment. Figure 4 The cross-sectional structure of the IC device 100A shown can be compared with that along the Figure 3 The portion of the cross-section intercepted by line X2-X2' corresponds to this. IC device 100A can be configured... Figure 1 A portion of the IC device 10 shown. Figure 4 In the figures, the same reference numerals are used to indicate the same as those in the figures below. Figures 1 to 3 The same elements are used in the same way, and their repeated descriptions are omitted here.
[0067] Reference Figure 4 IC device 100A can basically have the same Figure 2 The IC device 100A shown has the same structure as the IC device 100. However, the IC device 100A may include a capacitor CP1A, which includes a lower electrode structure LE1A, an upper electrode 150, and a dielectric film 140 located between the lower electrode structure LE1A and the upper electrode 150. A first support film SPT1 and a second support film SPT2 configured to support the lower electrode structure LE1A may be formed around the lower electrode structure LE1A. The lower electrode structure LE1A may constitute a reference. Figure 1 The described lower electrode structure LE.
[0068] The lower electrode structure LE1A can essentially have the same characteristics as the reference. Figure 2 The lower electrode structure LE1 described has the same construction. However, in the IC device 100A, the first support film SPT1 and the second support film SPT2 can contact the lower electrode structure LE1A only on one side of the lower electrode structure LE1A in the first lateral direction (X direction).
[0069] The lower electrode structure LE1A may include a capping electrode portion 138A that contacts the second support film SPT2. The capping electrode portion 138A may substantially have the same characteristics as the referenced portion. Figure 2 The described capping electrode portion 138 has the same construction. However, the first sidewall S1, which is one of the two sidewalls in the first lateral direction (X direction) of the capping electrode portion 138A, can contact the second support film SPT2, and the second sidewall S2, which is the other of the two sidewalls, can contact the dielectric film 140. A fillet 138AR can be provided between the uppermost surface 138AT of the capping electrode portion 138A and the second sidewall S2. In the first lateral direction (X direction), the two sides of the capping electrode portion 138A can have an asymmetrical shape about the central axis in the vertical direction (Z direction) of the lower electrode structure LE1A.
[0070] In reference Figure 4 In the described IC device 100A, compared with the reference Figure 2 and Figure 3 Similar to the described IC device 100, the dielectric film 140 can effectively maintain the rutile phase crystal structure. Therefore, the dielectric film 140 can provide a relatively high dielectric constant, reducing or eliminating leakage current between the lower electrode structure LE1A and the dielectric film 140, and increasing the capacitance of the capacitor CP1A. Furthermore, it can prevent the conductive region 124 from deteriorating due to oxidation during the manufacturing of the IC device 100A, and thus effectively prevents an increase in the interface resistance in the conductive region 124, improving the reliability of the IC device 100A.
[0071] Figure 5 This is a cross-sectional view of some components of an IC device 200 according to yet another embodiment. Figure 5 The cross-sectional structure of the IC device 200 shown can be compared with that along the Figure 3 The portion of the cross-section intercepted by line X1-X1' corresponds to this. IC device 200 can be configured... Figure 1 A portion of the IC device 10 shown. Figure 5 In the figures, the same reference numerals are used to indicate the same as those in the figures below. Figures 1 to 3 The same elements are used in the same way, and their repeated descriptions are omitted here.
[0072] Reference Figure 5IC device 200 can basically have the same Figure 2 The IC device 200 shown has the same construction as the IC device 100. However, the IC device 200 may include a capacitor CP2, which includes a lower electrode structure LE2, an upper electrode 250, and a dielectric film 240 located between the lower electrode structure LE2 and the upper electrode 250. The lower electrode structure LE2 may be configured as shown in the reference diagram. Figure 1 The described lower electrode structure LE.
[0073] The lower electrode structure LE2 can extend longitudinally from the top surface of the conductive region 124 through the opening 126H of the insulating pattern 126P in the vertical direction (Z direction). The dielectric film 240 and the upper electrode 250 can be formed on the lower electrode structure LE2.
[0074] The lower electrode structure LE2 may include a bottom bridging electrode portion 232A, an outer template electrode portion 234, a main electrode portion 236, and an inner template electrode portion 238 sequentially formed on the conductive region 124. Furthermore, the lower electrode structure LE2 may also include a first side bridging electrode portion 232B and a second side bridging electrode portion 232C. The first side bridging electrode portion 232B may protrude from the outer template electrode portion 234 toward the first support film SPT1 and contact the first support film SPT1. The second side bridging electrode portion 232C may protrude from the outer template electrode portion 234 toward the second support film SPT2 and contact the second support film SPT2.
[0075] The bottom bridging electrode portion 232A and the outer template electrode portion 234 of the lower electrode structure LE2 can respectively and substantially have the same characteristics as those already referenced. Figure 2 The bottom bridging electrode portion 132A and the outer template electrode portion 134 described have the same structure. The outer template electrode portion 234 may have a bottom surface 234B that contacts the top surface of the bottom bridging electrode portion 232A and an outer sidewall 234S that contacts the dielectric film 240.
[0076] The main electrode portion 236 of the lower electrode structure LE2 may have an outer sidewall 236S1 that contacts the outer template electrode portion 234 and an inner sidewall 236S2 that defines the internal space of the main electrode portion 236. The main electrode portion 236 may have a cylindrical shape with a cup-shaped cross-section. The dielectric film 240 and the upper electrode 250 may respectively and substantially have the same shape as those already referenced. Figure 2 The dielectric film 140 and the upper electrode 150 described have the same construction. However, each of the dielectric film 240 and the upper electrode 250 may include a portion located within an internal space defined by the inner sidewall 236S2 of the main electrode portion 236. The constituent material of the main electrode portion 236 may be the same as that already referred to Figure 2The main electrode portion 136 described is made of the same material. In the lower electrode structure LE2, the outer template electrode portion 234 may include a first metal oxide having a rutile phase crystal structure. The main electrode portion 236 may include a second metal oxide comprising a material different from the first metal oxide and having a rutile phase crystal structure.
[0077] The inner template electrode portion 238 of the lower electrode structure LE2 may have a first surface that contacts the inner sidewall 236S2 of the main electrode portion 236 and a second surface that contacts the dielectric film 240 in the internal space defined by the inner sidewall 236S2 of the main electrode portion 236. The constituent materials of each of the outer template electrode portion 234 and the inner template electrode portion 238 of the lower electrode structure LE2 may be the same as those already referenced. Figure 2 The outer template electrode portion 134 described is made of the same material. The inner template electrode portion 238 of the lower electrode structure LE2 may include a third metal oxide comprising a material different from the second metal oxide included in the main electrode portion 236. In an embodiment, in the lower electrode structure LE2, the first metal oxide included in the outer template electrode portion 234 may include the same material as the third metal oxide included in the inner template electrode portion 238.
[0078] Each of the first side bridging electrode portion 232B and the second side bridging electrode portion 232C of the lower electrode structure LE2 may have a surface that contacts the outer side wall 234S of the outer template electrode portion 234. The first side bridging electrode portion 232B and the second side bridging electrode portion 232C may be spaced apart from each other in the vertical direction (Z direction). In the vertical direction (Z direction), the thickness of the second side bridging electrode portion 232C may be greater than the thickness of the first side bridging electrode portion 232B. The constituent material of each of the first side bridging electrode portion 232B and the second side bridging electrode portion 232C may be the same as that already referenced. Figure 2 The side bridging electrode portion 132B described is made of the same material.
[0079] In reference Figure 5 In the described IC device 200, the outer template electrode portion 234 and the inner template electrode portion 238 can be used as a crystallization induction layer, which is configured to induce a rutile phase crystal structure in the dielectric film 240. Due to the outer template electrode portion 234 and the inner template electrode portion 238, the material included in the dielectric film 240 can easily maintain the rutile phase crystal structure. Therefore, the dielectric film 240 can provide a relatively high dielectric constant, which can reduce or eliminate leakage current between the lower electrode structure LE2 and the dielectric film 240, and the capacitance of the capacitor CP2 can be increased.
[0080] In the lower electrode structure LE2 of capacitor CP2, the first metal oxide and the third metal oxide included in the outer template electrode portion 234 and the inner template electrode portion 238, respectively, can each include materials with excellent corrosion resistance to a predetermined etching atmosphere, and the second metal oxide included in the main electrode portion 236 can include a low-resistance material with relatively high conductivity. As a result, when the dielectric film 240 is formed on the outer template electrode portion 234 and the inner template electrode portion 238, the rutile phase crystal structure of the dielectric film 240 can be strengthened by the outer template electrode portion 234 and the inner template electrode portion 238, the resistance of the lower electrode structure LE2 can be reduced, and the lower electrode structure LE2 can ensure relatively high conductivity and thermal stability. Furthermore, because the second metal oxide included in the main electrode portion 236 has a rutile phase crystal structure, the main electrode portion 236 can also be used together with the outer template electrode portion 234 and the inner template electrode portion 238 to induce the dielectric film 240 to have a rutile phase crystal structure. Therefore, the dielectric film 240 can more effectively preserve the rutile phase crystal structure.
[0081] Furthermore, the lower electrode structure LE2 of capacitor CP2 may include a bottom bridging electrode portion 232A, which covers the conductive region 124 between the outer template electrode portion 234 and the conductive region 124. Therefore, during the manufacturing process of the IC device 200, when forming the outer template electrode portion 234, the main electrode portion 236, and the inner template electrode portion 238, each comprising a metal oxide, there is no need to worry about the conductive region 124 being exposed to the oxidizing atmosphere used to form the metal oxide. Thus, deterioration of the conductive region 124 due to oxidation during the formation of the outer template electrode portion 234, the main electrode portion 236, and the inner template electrode portion 238 can be prevented, and therefore, an increase in the interface resistance in the conductive region 124 can be effectively prevented.
[0082] Next, a method for manufacturing an IC device according to an embodiment will be described in detail with reference to specific examples.
[0083] Figures 6A to 6K This is a cross-sectional view of the process sequence of a method for manufacturing an IC device according to an embodiment. (Refer to...) Figures 6A to 6K Description of manufacturing Figure 2 An example of a method of the IC device 100 shown in the figure. Figures 6A to 6K In the figures, the same reference numerals are used to indicate the same as those in the figures below. Figures 1 to 3 The same elements are used in the same way, and their repeated descriptions are omitted here.
[0084] Reference Figure 6AA lower structure 120 and a conductive region 124 may be formed on a substrate 110 in which the active region is defined by a device isolation region 112. The conductive region 124 may extend through the lower structure 120 and connect to the active region ACT. An insulating layer 126 may then be formed to cover the lower structure 120 and the conductive region 124. The insulating layer 126 may be used as an etch stop layer in subsequent processes. The insulating layer 126 may include an insulating material having etch selectivity relative to the lower structure 120. In embodiments, the insulating layer 126 may include silicon nitride, silicon oxynitride, or a combination thereof.
[0085] A molded structure MDS can be formed on the insulating layer 126. To form the molded structure MDS, a first molded film MD1, a first support film SPT1, a second molded film MD2, and a second support film SPT2 can be sequentially formed on the insulating layer 126. Each of the first molded film MD1 and the second molded film MD2 may include an insulating material having etch selectivity relative to the insulating layer 126. In an embodiment, each of the first molded film MD1 and the second molded film MD2 may include an oxide film. The first support film SPT1 and the second support film SPT2 may each include a material having etch selectivity relative to the first molded film MD1 and the second molded film MD2. The first support film SPT1 and the second support film SPT2 may include a material having a relatively low etch rate relative to the etch atmosphere (e.g., an etchant including ammonium fluoride (NH4F), hydrofluoric acid (HF), and water) used to remove the first molded film MD1 and the second molded film MD2 in subsequent processes.
[0086] Reference Figure 6B ,exist Figure 6A In the resulting structure, a mask pattern MP can be formed on the molded structure MDS. The molded structure MDS can then be anisotropically etched using the mask pattern MP as an etching mask and by using the insulating layer 126 as an etch stop layer, thus forming vertical holes BH in the molded structure MDS. The mask pattern MP can include a nitride film, an oxide film, a polysilicon film, a photoresist film, or a combination thereof. Subsequently, the insulating layer 126 can be anisotropically etched via the vertical holes BH using the mask pattern MP as an etching mask to form an insulating pattern 126P having openings 126H exposing conductive regions 124. During the formation of the openings 126H using the anisotropic etching process, the upper portion of the conductive regions 124 can be etched by over-etching, thus forming a recessed surface in the top surface of the conductive regions 124.
[0087] Reference Figure 6C It can be seen from Figure 6BThe resulting structure removes the mask pattern MP, and then an initial bridging electrode layer 132L can be formed to conformally cover the surface of the conductive region 124, the surface of the insulating pattern 126P, and the surface of the molded structure MDS inside and outside the vertical hole BH. After forming the initial bridging electrode layer 132L, a portion of the vertical hole BH can be left empty on the initial bridging electrode layer 132L. The constituent material of the initial bridging electrode layer 132L can be the same as that already referenced. Figure 2 The bottom bridging electrode portion 132A described herein is made of the same material. The initial bridging electrode layer 132L can be formed using chemical vapor deposition (CVD), metal-organic CVD (MOCVD), or atomic layer deposition (ALD) processes.
[0088] Reference Figure 6D A template electrode layer 134L can be formed inside the vertical hole BH, covering the initial bridging electrode layer 132L. The template electrode layer 134L can conformally cover the initial bridging electrode layer 132L in the remaining space of the vertical hole BH defined by the initial bridging electrode layer 132L. The template electrode layer 134L may include a first metal oxide having a rutile phase crystal structure. The detailed composition of the constituent material of the template electrode layer 134L can be referenced from [reference needed]. Figure 2 The detailed composition of the constituent materials of the outer template electrode portion 134 described is the same.
[0089] In an embodiment, the template electrode layer 134L may comprise tin oxide having a rutile phase crystal structure. The template electrode layer 134L can be formed using an ALD process. In an example of the ALD process for forming the template electrode layer 134L, the ALD cycle described below can be repeated at least once.
[0090] During the ALD cycle, Sn precursors can be supplied to Figure 6COn the substrate of the resulting structure, the process temperature is maintained at a temperature of approximately 100 ºC to approximately 600 ºC (e.g., approximately 300 ºC to approximately 400 ºC). The Sn precursor may include, but is not limited to, R2Sn(NR'R")2 (where R, R', and R" are each hydrogen (H) or C1-C10 alkyl), halogenated Sn, or derivatives thereof. In this case, the process pressure can be maintained at a pressure of approximately 10 Pa to atmospheric pressure. In an embodiment, to form the template electrode layer 134L, a supply gas comprising only the Sn precursor can be supplied to the substrate 110. In an embodiment, to form the template electrode layer 134L, a Sn precursor selectively comprising a dopant element and a supply gas, a compound comprising a dopant element, or a multi-component source comprising a reactant gas can be supplied to the substrate 110. The time period for supplying the supply gas to the substrate 110 once can be maintained at approximately 0.1 seconds to approximately 100 seconds. The Sn precursor and reactant gas can be supplied to the substrate simultaneously or sequentially. By supplying a gas to the substrate 110, a chemisorption layer and a physisorption layer of the Sn precursor can be formed on the surface of the initial bridging electrode layer 132L.
[0091] Subsequently, a first purge gas can be supplied to the substrate 110 to remove unwanted byproducts on the substrate 110. In this case, the remaining physicoadsorption layer of Sn precursor on the substrate 110 can also be removed. For example, an inert gas (e.g., argon (Ar), helium (He), and neon (Ne)) or N2 gas can be used as the first purge gas.
[0092] Subsequently, an oxidizing gas can be supplied to the substrate 110, and thus, a single-atom thin oxide film can be formed from the chemisorption layer of the Sn precursor. The oxidizing gas can be selected from O2, O3, H2O, NO2, NO, N2O, CO, CO2, H2O2, HCOOH, CH3COOH, (CH3CO)2O, alcohols, peroxides, sulfur oxides, plasma O2, remote plasma O2, plasma N2O, plasma H2O, and combinations thereof.
[0093] Subsequently, a second purge gas can be supplied to the substrate 110 to remove unwanted byproducts on the substrate 110. In this case, residual oxidizing gases remaining on the substrate 110 can be removed. For example, an inert gas (e.g., Ar, He, and Ne) or N2 gas can be used as the second purge gas.
[0094] Then, it can be determined whether a template electrode layer 134L with the desired thickness has been obtained on the initial bridging electrode layer 132L, and the above ALD cycle can be repeated at least once until a template electrode layer 134L with the target thickness is obtained.
[0095] Because the conductive region 124 is covered by the initial bridging electrode layer 132L during the formation of the template electrode layer 134L, the conductive region 124 can be protected by the initial bridging electrode layer 132L and is not exposed to the oxidizing gas even when oxidizing gas is supplied to the substrate 110 to form the template electrode layer 134L. Therefore, degradation of the conductive region 124 due to oxidizing gas can be prevented, or an increase in the interface resistance in the conductive region 124 can be prevented.
[0096] Reference Figure 6E ,exist Figure 6D In the resulting structure, a main electrode layer 136L can be formed inside the vertical hole BH, covering the template electrode layer 134L. The main electrode layer 136L can be formed such that it fills the remaining space of the vertical hole BH on the template electrode layer 134L. The main electrode layer 136L may include a second metal oxide, which is a different material from the first metal oxide included in the template electrode layer 134L and has a rutile phase crystal structure.
[0097] The main electrode layer 136L can be formed using an ALD process. The ALD process for forming the main electrode layer 136L is essentially the same as that already referenced. Figure 6D The ALD process for forming the template electrode layer 134L is described similarly. However, to form the main electrode layer 136L, a metal precursor comprising a different metal than the metal used to form the template electrode layer 134L can be used. In embodiments, vanadium (V) precursor, molybdenum (Mo) precursor, niobium (Nb) precursor, or cobalt (Co) precursor can be used as the metal precursor to form the main electrode layer 136L.
[0098] V precursors may include, but are not limited to, vanadium tetrachloride (VCl4), vanadium pentachloride (VCl5), vanadium pentafluoride (VF5), tetradimethylaminovanadium (TDMAV, V(N(CH3)2)4), tetradiethylaminovanadium (TDEAV, V(NEt2)4), tetra(methylethylamino)vanadium (TMEAV, V(NMeEt)4), bis(cyclopentadienyl)vanadium (Cp2V), bis(cyclopentadienyl)dichlorovanadium (Cp2VCl2)), or derivatives thereof.
[0099] Mo precursors may include, but are not limited to, (CpR)2Mo(NR') (where R and R' are each H or C1-C10 alkyl groups) or halogenated Mo.
[0100] Nb precursors may include niobium pentachloride (NbCl5), niobium pentafluoride (NbF5), pentadimethylaminoniobium (PDMAN, Nb(N(CH3)2)5), pentadiethylaminoniobium (PDEAN, Nb(NEt2)5), penta(methylethyl)niobium (PMEAN, Nb(NMeEt)5), tert-butyliminotris(dimethylamino)niobium (TBTDMN, tBuNNb(NMe2)3), and tert-butyliminotris(diethylamino)niobium (TBTDE) N,tBuNNb(NEt2)3), tert-butyliminotris(methylethylamino)niobium (TBTMEN,tBuNNb(NMeEt)3), ethylimino-tris(dimethylamino)niobium ((EtN)Nb(NMe2)3), ethylimino-tris(diethylamino)niobium ((EtN)Nb(NEt2)3), ethylimino-tris(ethylmethylamino)niobium ((EtN)Nb[N(Et)Me]3), or derivatives thereof, but not limited thereto.
[0101] Co precursors may be selected from, but are not limited to, octacarbonyldicobalt, nitrosylcobalt complexes, β-diketones of cobalt(II) and cobalt(III), or their derivatives.
[0102] Reference Figure 6F ,exist Figure 6E In the resulting structure, the main electrode layer 136L, the template electrode layer 134L, and the initial bridging electrode layer 132L can be etched to expose the top surface and sidewalls of the second support film SPT2 included in the molded structure MDS. As a result, an outer template electrode portion 134 and a main electrode portion 136 can be formed on the initial bridging electrode layer 132L inside the vertical hole BH. The outer template electrode portion 134 may include the remainder of the template electrode layer 134L, and the main electrode portion 136 may include the remainder of the main electrode layer 136L. The main electrode portion 136 may cover the outer template electrode portion 134 inside the vertical hole BH. A portion of the vertical hole BH may remain empty on the top surface of each of the initial bridging electrode layer 132L, the outer template electrode portion 134, and the main electrode portion 136.
[0103] Reference Figure 6G ,exist Figure 6F In the resulting structure, a capping electrode layer 138L filling the vertical hole BH can be formed on the top surface of each of the initial bridging electrode layer 132L, the outer template electrode portion 134, and the main electrode portion 136. The capping electrode layer 138L can be formed to fill the vertical hole BH and cover the top surface of the second support film SPT2. The constituent material of the capping electrode layer 138L can be the same as that already referenced. Figure 2The main electrode portion 136 described is made of the same material. The capping electrode layer 138L can be formed using CVD, MOCVD, or ALD processes.
[0104] Reference Figure 6H ,exist Figure 6G In the resulting structure, the capping electrode layer 138L can be etched back to expose the top surface of the second support film SPT2. As a result, a capping electrode portion 138 including the remaining portion of the capping electrode layer 138L can be obtained. The top surface of the capping electrode portion 138 can be coplanar with the top surface of the second support film SPT2.
[0105] Reference Figure 6I ,exist Figure 6H In the resulting structure, the first molded film MD1 and the second molded film MD2 can be selectively removed from the first molded film MD1, the first support film SPT1, the second molded film MD2, and the second support film SPT2 included in the molded structure MDS, and thus, the sidewalls of the initial bridging electrode layer 132L and the top surface of the insulating pattern 126P can be exposed. The first molded film MD1 and the second molded film MD2 can be removed using a wet etching process. For example, the first molded film MD1 and the second molded film MD2 can be removed using an etchant comprising ammonium fluoride (NH4F), hydrofluoric acid (HF), and water. In an example of the process for removing the first molded film MD1 and the second molded film MD2, initially, multiple upper holes can be formed in the second support film SPT2 by patterning the second support film SPT2 (see reference). Figure 3 The first molded film MD2 can be removed through the multiple upper holes (UH) in the first support film SPT1. Then, multiple lower holes can be formed in the first support film SPT1 at positions corresponding to the multiple upper holes (UH), and the first molded film MD1 can be removed through the multiple lower holes in the first support film SPT1. During the removal of the first molded film MD1 and the second molded film MD2, the initial lower electrode structure PL1, including the initial bridging electrode layer 132L, the outer template electrode portion 134, the main electrode portion 136, and the capping electrode portion 138, can be supported by the first support film SPT1 and the second support film SPT2.
[0106] Even when the outer template electrode portion 134 is exposed to the etching atmosphere used for removing the first molding film MD1 and the second molding film MD2 during the removal of the first molding film MD1 and the second molding film MD2, the outer template electrode portion 134 exposed after the removal of the first molding film MD1 and the second molding film MD2 can maintain its rutile phase crystal structure without being damaged because the outer template electrode portion 134 comprises a material with relatively high corrosion resistance to the etching atmosphere (e.g., tin oxide).
[0107] Reference Figure 6J,exist Figure 6I In the resulting structure, a portion of the initial bridging electrode layer 132L can be removed from its exposed sidewalls to expose the outer sidewalls 134S of the outer template electrode portion 134. By removing this portion of the initial bridging electrode layer 132L, a bottom bridging electrode portion 132A and a side bridging electrode portion 132B can be formed. The bottom bridging electrode portion 132A may include the remaining portion of the initial bridging electrode layer 132L, and the side bridging electrode portion 132B may include the remaining portions of the initial bridging electrode layer 132L.
[0108] To remove this portion of the initial bridging electrode layer 132L, a wet etching process can be performed by utilizing the difference in etch selectivity between the material included in the outer template electrode portion 134 and the material included in the initial bridging electrode layer 132L. For example, when the initial bridging electrode layer 132L comprises titanium nitride (TiN), a wet etching process using an etchant comprising sulfuric acid (H2SO4) and hydrogen peroxide (H2O2) can selectively etch a portion of the exposed area of the initial bridging electrode layer 132L. However, the etching process for removing this portion of the initial bridging electrode layer 132L is not limited to this.
[0109] When the initial bridging electrode layer 132L and the capping electrode portion 138 comprise the same material, a portion of the capping electrode portion 138 can be removed from its exposed top surface during the selective removal of a portion of the initial bridging electrode layer 132L, and thus, as Figure 6J As shown, the thickness of the capping electrode portion 138 can be reduced. After reducing the thickness of the capping electrode portion 138, the vertical horizontal plane of the uppermost surface of the capping electrode portion 138 can be closer to the substrate 110 than the vertical horizontal plane of the uppermost surface of the second support film SPT2. In the resulting structure obtained after removing a portion of the initial bridging electrode layer 132L, the bottom bridging electrode portion 132A, the side bridging electrode portion 132B, the outer template electrode portion 134, the main electrode portion 136, and the capping electrode portion 138 can constitute the lower electrode structure LE1.
[0110] Reference Figure 6K , can Figure 6J A dielectric film 140 is formed in the resulting structure, covering the exposed surface of the lower electrode structure LE1. In an embodiment, the dielectric film 140 can be formed using an ALD process.
[0111] In the ALD process for forming dielectric film 140, the ALD cycle described below can be repeated at least once. Initially, a Ti precursor can be supplied onto substrate 110, on which the lower electrode structure LE1 is exposed within the reaction space, and thus, a Ti precursor layer can be formed on the surface of each of the lower electrode structure LE1, the insulating pattern 126P, the first support film SPT1, and the second support film SPT2. The Ti precursor may include titanium tetrachloride (TiCl4), titanium tetrafluoride (TiF4), tetra(isopropanol)titanium (Ti(O-iPr)4), cyclopentadienyl titanium, bis(isopropanol)bis(2,2,6,6-tetramethyl-3,5-heptadecanoic acid)titanium (Ti(O-iPr)2(thd)2), tetradimethylaminotitanium (TDMAT, Ti(NMe2)4), tetra(diethylamino)titanium (TEMAT, (Et2N)4Ti), trimethoxy(pentamethylcyclopentadienyl)titanium ((Cp) * Ti(OMe)3 or its derivatives, but not limited thereto, can be used. The Ti precursor can be supplied to the substrate 110 in a vaporized state. When the Ti precursor is supplied to the substrate 110, the interior of the reaction space in which the substrate 110 is loaded can be maintained at a temperature selected in the range of approximately 100 ºC to approximately 600 ºC. By supplying the Ti precursor to the substrate 110 in a vaporized state, a chemisorbed layer and a physisorbed layer of the Ti precursor can be formed on the surface of each of the lower electrode structure LE1, the insulating pattern 126P, the first support film SPT1, and the second support film SPT2. A purge gas can then be supplied to the substrate 110 in the reaction space to remove unwanted byproducts from the substrate 110. In this case, the remaining physisorbed layer of the Ti precursor on the substrate 110 can also be removed. For example, an inert gas (e.g., Ar, He, and Ne) or N2 gas can be used as the purge gas. Subsequently, an oxidation reaction gas can be supplied to the substrate 110, and thus, a metal oxide film can be formed from the chemisorbed layer of the metal precursor. The oxidation reaction gas may include O2, O3, plasma O2, H2O, NO2, NO, N2O, CO2, H2O2, HCOOH, CH3COOH, (CH3CO)2O, or combinations thereof. Afterwards, a purge gas may be supplied to the substrate 110 to remove unwanted byproducts. The above ALD cycle may be repeated at least once until a TiO2 film of the desired thickness is obtained. At least the portion of the TiO2 film in contact with the outer template electrode portion 134 may have a rutile phase crystal structure. To form the dielectric film 140, at least one high-k dielectric film may also be formed on the TiO2 film as needed.
[0112] Then, you can Figure 6K An upper electrode 150 covering a dielectric film 140 is formed on the resulting structure, and therefore, it is possible to manufacture a structure including... Figure 2 The IC device 100 of capacitor CP1 shown in the figure. The upper electrode 150 can be formed by using CVD process, MOCVD process, physical vapor deposition (PVD) process or ALD process.
[0113] Figures 7A to 7E This is a cross-sectional view of the process sequence of a method for manufacturing an IC device according to an embodiment. (Refer to...) Figures 7A to 7E Description of manufacturing Figure 5 An example of a method of the IC device 200 shown in the figure. Figures 7A to 7E In the figures, the same reference numerals are used to indicate the same as those in the figures below. Figures 1 to 3 The same elements are used in the same way, and their repeated descriptions are omitted here.
[0114] Reference Figure 7A In executing the reference Figure 6A and Figure 6B After describing the process, one can... Figure 6B The resulting structure removes the mask pattern MP, and an initial bridging electrode layer 232L, a first template electrode layer 234L, and a main electrode layer 236L can be sequentially formed inside or outside the vertical hole BH on the surface of the conductive region 124, the surface of the insulating pattern 126P, and the surface of the molded structure MDS. The processes for forming the initial bridging electrode layer 232L, the first template electrode layer 234L, and the main electrode layer 236L can be respectively and substantially the same as those already referenced. Figure 6C , Figure 6D and Figure 6E The processes for forming the initial bridging electrode layer 132L, template electrode layer 134L, and main electrode layer 136L are described similarly. However, the main electrode layer 236L can be formed such that it conformally covers the first template electrode layer 234L to a substantially constant thickness. After forming the main electrode layer 236L, a portion of the vertical hole BH can be left empty on the main electrode layer 236L.
[0115] The constituent material of the initial bridging electrode layer 232L can be the same as that already referenced. Figure 5 The bottom bridging electrode portion 232A, the first side bridging electrode portion 232B, and the second side bridging electrode portion 232C described are made of the same material. For example, the initial bridging electrode layer 232L may include TiN. The material of the first template electrode layer 234L may be the same as that already referenced. Figure 2 The outer template electrode portion 134 described is made of the same material. The main electrode layer 236L can be made of the same material as previously referenced. Figure 2 The main electrode portion 136 described is made of the same material.
[0116] Reference Figure 7B , can Figure 7AIn the resulting structure, a second template electrode layer 238L is formed that conformally covers the exposed surface of the main electrode layer 236L. The process for forming the second template electrode layer 238L can be substantially the same as that already referenced. Figure 6D The process for forming the template electrode layer 134L is similar to that described. In an embodiment, the constituent material of the second template electrode layer 238L may be the same as that of the first template electrode layer 234L.
[0117] Reference Figure 7C It can be seen from Figure 7B The resulting structure involves etching back the second template electrode layer 238L, the main electrode layer 236L, the first template electrode layer 234L, and the initial bridging electrode layer 232L to expose the top surface of the second support film SPT2 included in the molded structure MDS. As a result, an outer template electrode portion 234, a main electrode portion 236, and an inner template electrode portion 238 can be formed on the initial bridging electrode layer 232L. The outer template electrode portion 234 may include the remaining portion of the first template electrode layer 234L. The main electrode portion 236 may include the remaining portion of the main electrode layer 236L. The inner template electrode portion 238 may include the remaining portion of the second template electrode layer 238L. A portion of the vertical hole BH may be left empty on the inner template electrode portion 238.
[0118] Reference Figure 7D , in order to refer to Figure 6I The description is similar, and can be derived from... Figure 7C The resulting structure removes the first molded film MD1 and the second molded film MD2, and exposes the sidewalls of the initial bridging electrode layer 232L.
[0119] Then, with reference Figure 6J In a similar manner, the exposed portion of the initial bridging electrode layer 232L can be removed to expose the outer wall 234S of the outer template electrode portion 234, forming a bottom bridging electrode portion 232A, a first side bridging electrode portion 232B, and a second side bridging electrode portion 232C, including the remaining portion of the initial bridging electrode layer 232L. The bottom bridging electrode portion 232A, the first side bridging electrode portion 232B, the second side bridging electrode portion 232C, the outer template electrode portion 234, the main electrode portion 236, and the inner template electrode portion 238 can constitute the lower electrode structure LE2.
[0120] Reference Figure 7E In order to refer to Figure 6K The process for forming the dielectric film 140 described is similar and can be performed in a manner that allows for... Figure 7D The resulting structure forms a dielectric film 240 covering the exposed surface of the upper electrode structure LE2.
[0121] Then, you can Figure 7E An upper electrode 250 covering a dielectric film 240 is formed on the resulting structure, and therefore, it is possible to manufacture a structure including... Figure 5 IC device 200 for capacitor CP2 shown in the figure.
[0122] Although it has been referenced Figures 6A to 6K and Figures 7A to 7E Describes manufacturing Figure 2 The IC device 100 shown in the figure and Figure 5 The method of the IC device 200 shown is illustrated, but it will be understood that it can be based on the reference within the scope of the inventive concept. Figures 6A to 6K and Figures 7A to 7E The provided description applies various modifications and changes. Figures 2 to 5 IC devices 100, 100A and 200 shown are used to manufacture Figure 4 The IC device 100A shown herein, or an IC device with various modified structures, is also shown.
[0123] Although the inventive concept has been specifically shown and described with reference to embodiments thereof, it will be understood that various changes in form and detail may be made herein without departing from the spirit and scope of the appended claims.
Claims
1. An integrated circuit device, comprising: A conductive region located on the substrate; as well as A capacitor, located on the conductive region, includes a lower electrode structure, an upper electrode, and a dielectric film located between the lower electrode structure and the upper electrode. The lower electrode structure includes: The outer template electrode portion is spaced apart from the conductive region in a substantially vertical direction, the outer template electrode portion is in contact with the dielectric film and includes a first metal oxide having a rutile phase crystal structure; The main electrode portion has a first bottom surface and a first outer sidewall, wherein the first bottom surface and the first outer sidewall are in contact with the outer template electrode portion. The main electrode portion comprises a second metal oxide and is spaced apart from the dielectric film, with the outer template electrode portion located between the main electrode portion and the dielectric film. The second metal oxide comprises a material different from the first metal oxide and has a rutile phase crystal structure. A bottom bridging electrode portion is located between the conductive region and the outer template electrode portion, and is spaced apart from the main electrode portion in the substantially vertical direction, with the outer template electrode portion located between the bottom bridging electrode portion and the main electrode portion. The bottom bridging electrode portion comprises a conductive metal nitride.
2. The integrated circuit device according to claim 1, wherein: The outer template electrode portion has a second bottom surface facing the conductive region and a second outer sidewall facing the upper electrode. The second bottom surface of the outer template electrode portion contacts the bottom bridging electrode portion, and The second outer sidewall of the outer template electrode portion is in contact with the dielectric film.
3. The integrated circuit device according to claim 1, wherein: The lower electrode structure further includes a capping electrode portion, which covers the uppermost surface of each of the outer template electrode portion and the main electrode portion, and The capping electrode portion and the bottom bridging electrode portion are made of the same material.
4. The integrated circuit device of claim 1, further comprising at least one support film configured to support the lower electrode structure around the lower electrode structure. in: The lower electrode structure further includes at least one side bridging electrode portion extending from the outer template electrode portion toward the at least one support film, and The at least one side bridging electrode portion and the bottom bridging electrode portion comprise the same material.
5. The integrated circuit device of claim 1, further comprising a first support film and a second support film, the first support film and the second support film being configured to support the lower electrode structure around the lower electrode structure. in: The second support film is spaced apart from the substrate in the substantially vertical direction, and the first support film is located between the second support film and the substrate. The lower electrode structure also includes: The capping electrode portion covers the uppermost surface of each of the outer template electrode portion and the main electrode portion; and The side bridging electrode portion extends from the outer template electrode portion toward the first support film. The second support membrane is in contact with the outer template electrode portion.
6. The integrated circuit device according to claim 5, wherein, The capping electrode portion, the side bridging electrode portion, and the bottom bridging electrode portion are made of the same material.
7. The integrated circuit device according to claim 5, wherein: In the substantially vertical direction, the thickness of the second support film is greater than the thickness of the first support film, and In the substantially vertical direction, the thickness of the capping electrode portion is greater than the thickness of the side bridging electrode portion.
8. The integrated circuit device according to claim 1, wherein, The main electrode portion has a column shape with a filled interior.
9. The integrated circuit device according to claim 1, wherein: The main electrode portion has a cylindrical shape, and the cylindrical shape has a cup-shaped cross-sectional structure with an inner wall that defines the internal space. The lower electrode structure further includes an inner template electrode portion, which has a first surface that contacts the inner wall of the main electrode portion and a second surface that contacts the dielectric film within the internal space defined by the main electrode portion. The inner template electrode portion includes a third metal oxide having a rutile phase crystal structure, and the third metal oxide includes a material different from the second metal oxide included in the main electrode portion.
10. The integrated circuit device according to claim 9, wherein, The first metal oxide included in the outer template electrode portion is made of the same material as the third metal oxide included in the inner template electrode portion.
11. The integrated circuit device according to claim 9, wherein: Each of the dielectric film and the upper electrode includes a portion located within the internal space defined by the main electrode portion, and The inner template electrode portion is in contact with the dielectric film within the internal space defined by the main electrode portion.
12. The integrated circuit device according to claim 1, wherein, The outer template electrode portion comprises dopant-free tin oxide.
13. The integrated circuit device according to claim 1, wherein, The outer template electrode portion also includes a dopant containing at least one element selected from niobium (Nb), antimony (Sb), and tantalum (Ta).
14. The integrated circuit device according to claim 1, wherein, The main electrode portion includes vanadium oxide, molybdenum oxide, niobium oxide, cobalt oxide, or combinations thereof.
15. The integrated circuit device according to claim 1, wherein: The main electrode portion also includes a dopant containing tin (Sn), and The content of the dopant in the main electrode portion is in the range of 0 at% to 10 at%.
16. The integrated circuit device according to claim 1, wherein, The dielectric film includes a TiO2 film with a rutile phase crystal structure, and the TiO2 film is in contact with the outer template electrode portion.
17. The integrated circuit device according to claim 1, wherein, The bottom bridging electrode portion includes titanium nitride (TiN).
18. An integrated circuit device, comprising: A conductive region located on the substrate; A lower electrode structure is located on the conductive region; A support membrane is configured to support the lower electrode structure around the lower electrode structure. An upper electrode that faces the lower electrode structure on the substrate; as well as A dielectric film is located between the lower electrode structure and the upper electrode. The lower electrode structure includes: The outer template electrode portion is spaced apart from the conductive region in a substantially vertical direction, the outer template electrode portion is in contact with the dielectric film and includes a first metal oxide having a rutile phase crystal structure; The main electrode portion has a first bottom surface and a first outer sidewall that are in contact with the outer template electrode portion. The main electrode portion includes a second metal oxide and is spaced apart from the dielectric film. The outer template electrode portion is located between the main electrode portion and the dielectric film. The second metal oxide includes a material different from the material of the first metal oxide and has a rutile phase crystal structure. A bottom bridging electrode portion, located between the conductive region and the outer template electrode portion, and spaced apart from the main electrode portion in the substantially vertical direction, with the outer template electrode portion located between the bottom bridging electrode portion and the main electrode portion; and The side bridging electrode portion is located between the outer template electrode portion and the support film and is spaced apart from the bottom bridging electrode portion. The bottom bridging electrode portion and the side bridging electrode portion both comprise the same conductive metal nitride.
19. The integrated circuit device according to claim 18, wherein: The lower electrode structure further includes a capping electrode portion covering the uppermost surface of each of the outer template electrode portion and the main electrode portion, the capping electrode portion being spaced apart from each of the bottom bridging electrode portion and the side bridging electrode portion, and The bottom bridging electrode portion, the side bridging electrode portion, and the capping electrode portion all comprise the same conductive metal nitride.
20. An integrated circuit device, comprising: A conductive region located on the substrate; A lower electrode structure is located on the conductive region; A support membrane is configured to support the lower electrode structure around the lower electrode structure. An upper electrode that faces the lower electrode structure on the substrate; as well as A dielectric film is located between the lower electrode structure and the upper electrode. The lower electrode structure includes: The outer template electrode portion is spaced apart from the conductive region in a substantially vertical direction, the outer template electrode portion is in contact with the dielectric film and includes tin oxide having a rutile phase crystal structure; The main electrode portion has a first bottom surface and a first outer sidewall, wherein the first bottom surface and the first outer sidewall are in contact with the outer template electrode portion, the main electrode portion includes vanadium oxide, molybdenum oxide, niobium oxide, cobalt oxide or a combination thereof and has a rutile phase crystal structure, and the main electrode portion is spaced apart from the dielectric film and the outer template electrode portion is located between the main electrode portion and the dielectric film. A bottom bridging electrode portion, located between the conductive region and the outer template electrode portion, and spaced apart from the main electrode portion in the substantially vertical direction, with the outer template electrode portion located between the bottom bridging electrode portion and the main electrode portion; and The side bridging electrode portion is located between the outer template electrode portion and the support film and is spaced apart from the bottom bridging electrode portion. Each of the bottom bridging electrode portion and the side bridging electrode portion comprises titanium nitride (TiN), and The dielectric film includes a TiO2 film with a rutile phase crystal structure, and the TiO2 film is in contact with the outer template electrode portion.
Citation Information
Patent Citations