A method for fabricating a two-stage field plate gate structure and its application
The method of fabricating a two-stage field plate gate structure in one step solves the problem of high photolithography complexity in traditional methods, realizes smaller field plate size and higher precision electric field modulation, and improves the voltage withstand performance of the device.
Patent Information
- Application Number
- CN202611636914.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-10-22
- Publication Date
- 2026-11-17
AI Technical Summary
Traditional gate field plate structure fabrication methods require multiple photolithography steps, which are complex and particularly difficult in RF device applications with small feature sizes. They cannot effectively improve the device's voltage withstand capability and electric field distribution.
A one-step two-stage field plate gate structure fabrication method is adopted. By controlling the exposure depth of the first double-layer resist structure through partitioned exposure dosage settings, the precise formation of the first and second gate field plates is achieved without additional photolithography and overlay, simplifying the process flow.
It achieves smaller field plate size and higher position control accuracy, reduces the difficulty of etching process, improves the breakdown voltage and electric field modulation effect of device, and is suitable for high frequency devices.
Smart Images

Figure CN123124384A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of semiconductor technology, and in particular to a method for fabricating a two-stage field plate gate structure and its application. Background Technology
[0002] Gallium nitride (GaN) and other wide-bandgap semiconductors possess advantages such as high breakdown electric field and high electron mobility. However, a severe field-fed edge effect exists near the drain side of the gate, causing the actual breakdown voltage of the device to be much lower than the theoretical breakdown boundary of the material. To meet the requirements of higher breakdown voltage and greater power density in devices, electric field modulation technology must be introduced, thus field plate structures have attracted widespread attention.
[0003] The gate field plate mainly extends the gate through the dielectric layer to the drift region between the gate and drain. It can introduce new electric field peaks at the gate edge, spreading the originally concentrated single large peak electric field into multiple small peaks. On the one hand, it can improve the device breakdown voltage, and on the other hand, it can reduce the electron trapping effect in the high electric field region and suppress the formation of "virtual gate", thereby improving the dynamic characteristics of the device.
[0004] Employing a multilayer field plate structure can optimize the electric field distribution inside the device, reduce the peak electric field, and thus improve the device's breakdown voltage. However, traditional gate field plate structure fabrication methods require multiple photolithography steps. As the number of field plate structure layers increases, the complexity of processes such as photolithography and etching increases significantly, making it extremely difficult, especially for RF devices with small feature sizes.
[0005] It should be noted that the above content is not necessarily prior art, nor is it intended to limit the scope of patent protection of this application. Summary of the Invention
[0006] This application provides a method for fabricating a two-stage field plate gate structure and its application, in order to solve or alleviate one or more of the technical problems mentioned above.
[0007] To achieve the above objectives, the technical solution of this application is implemented as follows: A method for fabricating a two-stage field plate gate structure includes the following steps: A passivation layer is prepared on the epitaxial structure; the epitaxial structure includes a substrate layer, a buffer layer, a channel layer, and a barrier layer, wherein the barrier layer, the channel layer, and the buffer layer are sequentially disposed on the substrate layer along the vertical direction, and a passivation layer is deposited on the barrier layer; A first double-layer photoresist structure is prepared on the passivation layer, and the first double-layer photoresist structure is subjected to patterned exposure and development processing to obtain a first region and a second region. Using the patterned first double-layer resist structure as a mask, the passivation layer corresponding to the first region is removed, and a second surface of the passivation layer is formed in the second region. The upper surface of the passivation layer, the second surface of the passivation layer, and the exposed surface of the epitaxial structure form a two-stage stepped gate trench opening. Remove the mask, prepare a second double-layer resist structure on the passivation layer surface that completes the two-stage stepped gate trench opening, and perform patterned exposure and development on the second double-layer resist structure to complete gate lithography and expose the two-stage stepped gate trench opening. Metal deposition is performed at the opening of the two-stage stepped gate trench, and the second double-layer resist structure is stripped to form the two-stage field plate gate structure. The two-stage field plate gate structure includes a gate foot and a first gate field plate and a second gate field plate extending from the top of the gate foot toward the drain.
[0008] In some embodiments, the preparation of the first double-layer resist structure specifically involves: coating a first resist on the passivation layer, pre-baking the first resist to form the first resist layer, coating a second resist on the first resist layer, and pre-baking the second resist to form the second resist layer; the first resist layer and the second resist layer constitute the first double-layer resist structure.
[0009] In some embodiments, the first photoresist is an electron beam photoresist, and the first photoresist is baked to form a first photoresist layer; the first photoresist is pre-baked to form the first photoresist layer; the second photoresist is an electron beam photoresist, and the second photoresist is pre-baked to form a second photoresist layer; the baking temperature of the second photoresist layer is not higher than the baking temperature of the first photoresist layer, and the first photoresist layer and the second photoresist layer are dissolved in the same developer.
[0010] In some embodiments, performing patterned exposure and development on the first double-layer resist structure to obtain a first region corresponding to the gate pin and a second region corresponding to the first gate field plate specifically involves: performing electron beam exposure and development on the first double-layer resist structure; the first exposure dose of the first region is determined based on the sum of the thicknesses of the first resist layer and the second resist layer; the second exposure dose of the second region is determined based on the thickness of the second resist layer; the second exposure dose is less than the first exposure dose; the first region is an opening that penetrates the first resist layer and the second resist layer to the surface of the passivation layer near the first resist layer; the second region is an opening that only penetrates the second resist layer.
[0011] In some embodiments, the first resist is a non-photosensitive photoresist, and the first resist is pre-baked to form the first resist layer; the second resist is a photosensitive photoresist, and the second resist is pre-baked to form the second resist layer; the baking temperature of the second resist layer is not higher than the baking temperature of the first resist layer, and the first resist layer and the second resist layer are dissolved in the same developing solution.
[0012] In some embodiments, performing patterned exposure and development on the first double-layer resist structure to obtain a first region corresponding to the gate foot and a second region corresponding to the first gate field plate specifically involves: exposing and developing the first double-layer resist structure, wherein the exposure conditions of the first region are determined based on the thickness of the second resist layer; the boundary of the second region is determined by the thickness of the first resist layer and the development parameters; the first region is an opening that penetrates the first resist layer and the second resist layer to the passivation layer near the surface of the first resist layer, and the second region is an opening that only penetrates the first resist layer.
[0013] In some embodiments, removing the mask and preparing a second double-layer resist structure on the passivation layer surface where the two-stage stepped gate trench opening is completed specifically involves: using the patterned first double-layer resist structure as a mask, performing dry etching to remove the passivation layer corresponding to the first region and expose the upper surface of the barrier layer, while simultaneously forming a second surface of the passivation layer in the second region, wherein the upper surface of the passivation layer, the second surface of the passivation layer, and the upper surface of the barrier layer form a two-stage stepped gate trench opening.
[0014] In some embodiments, removing the mask and preparing a second double-layer resist structure on the passivation layer surface where the two-stage stepped gate trench opening is completed specifically involves: using the patterned first double-layer resist structure as a mask, performing a first dry etching process to remove the passivation layer corresponding to the first region and expose the barrier layer; simultaneously forming a second surface of the passivation layer in the second region; performing a second dry etching process to remove a portion of the barrier layer corresponding to the first region and form a second surface of the barrier layer; and forming a two-stage stepped gate trench opening on the upper surface of the passivation layer, the second surface of the passivation layer, and the second surface of the barrier layer.
[0015] In some embodiments, the length of the first gate field plate is 20 nm to 5000 nm, the length of the second gate field plate is greater than the length of the first gate field plate, and the difference between the two is 20 nm to 5000 nm.
[0016] In some embodiments, the metal covers the two-stage stepped grid groove openings, and the thickness of the metal is greater than the depth of the two-stage stepped grid groove openings.
[0017] Another technical solution of this application is implemented as follows: The aforementioned two-stage field plate gate structure is applied to GaN devices.
[0018] Compared with the prior art, the two-stage field plate gate structure of this application can achieve a smaller field plate size. The first and second gate field plates, which extend from the top of the gate foot towards the drain, realize the one-time molding of the two-stage field plate gate structure without additional photolithography or overlay, and the process is simple and has high precision. Attached Figure Description
[0019] In the accompanying drawings, unless otherwise specified, the same reference numerals throughout the various drawings denote the same or similar parts or elements. These drawings are not necessarily drawn to scale. It should be understood that these drawings depict only some embodiments disclosed in this application and should not be construed as limiting the scope of this application.
[0020] Figure 1 This is a schematic diagram of the extensional structure of Embodiment 1 of this application; Figure 2 This is a schematic diagram of the structure of the epitaxial structure with a passivation layer provided in Embodiment 1 of this application; Figure 3 This is a schematic diagram of the structure of the epitaxial structure of Embodiment 1 of this application, which provides a first resist layer. Figure 4 This is a schematic diagram of the structure of the epitaxial structure of Embodiment 1 of this application, which provides a second resist layer; Figure 5 This is a schematic diagram of the exposure and development process performed on the epitaxial structure of the first double-layer photoresist structure in Embodiment 1 of this application; Figure 6 This is a schematic diagram of the exposure and development process performed on the epitaxial structure of the first double-layer photoresist structure in Embodiment 2 of this application; Figure 7 These are schematic diagrams of the etching of the passivation layer on the epitaxial structure of Embodiments 1 and 3 of this application; Figure 8 These are schematic diagrams of the mask removal structure on the extensional structure of embodiments 1 and 3 of this application; Figure 9 These are schematic diagrams of the structures in embodiments 1 and 3 of this application, showing the provision of a third and a fourth resist layer on the epitaxial structure. Figure 10 This is a schematic diagram of the exposure and development process performed on the epitaxial structure of embodiments 1 and 3 of this application for the second double-layer photoresist structure; Figure 11 These are schematic diagrams of the metal deposited on the epitaxial structure in Embodiments 1 and 3 of this application; Figure 12This is a schematic diagram of the two-stage field plate gate structure in Embodiment 1 of this application; Figure 13 This is a schematic diagram of the structure on which the passivation layer is etched on the epitaxial structure of Embodiment 3 of this application; Figure 14 This is a schematic diagram of the etching of the barrier layer on the epitaxial structure of Embodiment 3 of this application; Figure 15 This is a schematic diagram of the structure of the epitaxial structure of Embodiment 3 of this application, which provides a third resist layer and a fourth resist layer; Figure 16 This is a schematic diagram of the exposure and development process performed on the epitaxial structure of the second double-layer photoresist structure in Embodiment 3 of this application; Figure 17 This is a schematic diagram of the structure of metal deposited on the epitaxial structure in Embodiment 3 of this application; Figure 18 This is another schematic diagram of the two-stage field plate gate structure in Embodiment 1 of this application; Explanation of reference numerals in the attached figures: 1. Two-stage field plate gate structure; 11. Second gate field plate; 12. First gate field plate; 13. Gate foot; 2. Epitaxial structure; 21. Substrate layer; 22. Buffer layer; 23. Channel layer; 24. Barrier layer; 241. Trench; 3. Passivation layer; 31. Two-stage stepped gate trench opening; 4. First double-layer resist structure; 41. First resist layer; 42. Second resist layer; 5. Second double-layer resist structure; 51. Third resist layer; 52. Fourth resist layer; 6. Metal layer. Detailed Implementation
[0021] The embodiments of this application are described in detail below, examples of which are illustrated in the accompanying drawings. In the drawings, for clarity, the dimensions of layers, regions, and elements, as well as their relative dimensions, may be exaggerated. Throughout, the same or similar reference numerals denote the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain this application, and should not be construed as limiting this application. It should be noted that, unless otherwise specified, the embodiments and features in the embodiments of this application can be combined with each other.
[0022] It should be understood that when an element or layer is referred to as "on," "adjacent to," "connected to," or "coupled to" other elements or layers, it may be directly on, adjacent to, connected to, or coupled to other elements or layers, or there may be intervening elements or layers. Conversely, when an element is referred to as "directly on," "directly adjacent to," "directly connected to," or "directly coupled to" other elements or layers, there are no intervening elements or layers. It should be understood that although the terms first, second, third, etc., may be used to describe various elements, components, areas, layers, and / or portions, these elements, components, areas, layers, and / or portions should not be limited by these terms. These terms are only used to distinguish one element, component, area, layer, or portion from another element, component, area, layer, or portion. Therefore, without departing from the teachings of this application, the first element, component, area, layer, or portion discussed below may be referred to as a second element, component, area, layer, or portion. And the discussion of a second element, component, area, layer, or portion does not imply that the first element, component, area, layer, or portion necessarily exists in this application.
[0023] It should be noted that the terms "first," "second," etc., in the specification, claims, and accompanying drawings of this application are used to distinguish similar objects and are not necessarily used to describe a specific order or sequence. It should be understood that such terms can be used interchangeably where appropriate so that the embodiments of this application described herein can be implemented, for example, in orders other than those illustrated or described herein. Furthermore, the terms "comprising" and "having," and any variations thereof, are intended to cover a non-exclusive inclusion; for example, a process, method, system, product, or apparatus that comprises a series of steps or units is not necessarily limited to those steps or units explicitly listed, but may include other steps or units not explicitly listed or inherent to such processes, methods, products, or apparatus.
[0024] In this application, when numerical intervals (i.e., numerical ranges) are involved, unless otherwise specified, the distribution of selectable numerical values within the numerical interval is considered continuous, and includes the two endpoints of the numerical interval (i.e., the minimum and maximum values), as well as every numerical value between these two endpoints. Unless otherwise specified, when a numerical interval refers only to integers within that numerical interval, it includes the two endpoint integers of the numerical range, as well as every integer between the two endpoints, which is equivalent to directly listing every integer. When multiple numerical ranges are provided to describe features or characteristics, these numerical ranges can be merged. In other words, unless otherwise specified, the numerical ranges disclosed in this application should be understood to include any and all subranges included therein. The "numerical value" in the numerical interval can be any quantitative value, such as a number, percentage, ratio, etc. The term "numerical interval" can be broadly included to include percentage intervals, ratio intervals, proportion intervals, etc.
[0025] In the existing technology, the process methods for depositing the field plate dielectric layer and the field plate dielectric materials used in the fabrication of the two-stage field plate gate structure of GaN devices are described as follows: SiO2 or SiN is deposited using plasma-enhanced chemical vapor deposition (PECVD). In this process, PECVD is performed at relatively low temperatures, resulting in a dense and uniform dielectric film. This film can be used for passivation protection of the device surface, suppression of current collapse, or as an isolation dielectric layer between the gate and the semiconductor layer to control the electric field on the device surface.
[0026] The semiconductor layer is patterned using a dry etching process. The dry etching process utilizes plasma to chemically react with the material to be etched in a vacuum chamber, combined with physical ion bombardment to achieve directional removal of the material, thereby forming a gate structure with vertical sidewalls.
[0027] Example 1 Embodiment 1 of this application provides a method for fabricating a two-stage field plate gate structure, including the following steps: S1. A passivation layer 3 is prepared on the epitaxial structure 2; S2. A first double-layer photoresist structure 4 is prepared on the passivation layer 3. The first double-layer photoresist structure 4 is subjected to partitioned patterning exposure and development processing to obtain a first region A corresponding to the gate pin 13 and a second region B corresponding to the first gate field plate 12. S3. Using the patterned first double-layer resist structure 4 as a mask, remove the passivation layer 3 corresponding to the first region A, and at the same time form the second surface of the passivation layer 3 in the second region B. The upper surface of the passivation layer 3, the second surface of the passivation layer 3 and the exposed surface of the epitaxial structure 2 form a two-stage stepped gate groove opening 31. S4. Remove the mask, prepare a second double-layer resist structure 5 on the surface of the passivation layer 3 after the gate trench opening 31 is completed, and perform patterning exposure and development on the second double-layer resist structure 5 to complete gate lithography and expose the two-stage stepped gate trench opening 31. S5. Metal deposition is performed in the two-stage stepped gate trench opening 31 to form the two-stage field plate gate structure 1.
[0028] The method of this application embodiment can obtain a two-stage field plate gate structure 1. The two-stage field plate gate structure prepared by this method is formed in one step. By setting the exposure dose in different areas, the exposure depth of different regions of the first double-layer resist structure 4 can be achieved. There is no need to reserve overlay redundancy between different layers of field plates in advance, which can achieve a smaller field plate size. While realizing electric field modulation, the introduction of parasitic capacitance is reduced, which can support the improvement of the breakdown voltage of high-frequency devices.
[0029] In some embodiments, a method for fabricating a two-stage field plate gate structure includes the following steps: S11. The two-stage field plate gate structure 1 is fabricated on the epitaxial structure 2. The epitaxial structure 2 can be a heterojunction material substrate. The epitaxial structure 2 includes a substrate layer 21, a buffer layer 22, a channel layer 23, and a barrier layer 24. Figure 1 As shown, the barrier layer 24, the channel layer 23, and the buffer layer 22 are sequentially disposed on the substrate layer 21 along the vertical direction. A passivation layer 3 is deposited on the barrier layer 24, as shown. Figure 2 As shown.
[0030] More specifically, a passivation layer 3 is deposited on the epitaxial structure 2. The passivation layer 3 can be made of SiN, SiO2, or other materials. Using PECVD or LPCVD processes, 60nm to 300nm of SiN is deposited on the epitaxial structure 2 as the passivation layer 3. In some embodiments, 120nm of SiN is deposited on the epitaxial structure 2 as the passivation layer 3. In some embodiments, 120nm of SiO2 is deposited on the epitaxial structure 2 as the passivation layer 3.
[0031] More specifically, the substrate layer 21 may be made of SiC, Al2O3, Si, GaN, or other materials that can be used as a substrate, and the thickness of the substrate layer 21 is 200 μm to 600 μm. In some embodiments, the thickness of the substrate layer 21 may be 350 μm. The buffer layer 22 may be made of AlN, GaN, AlGaN, or other materials that can be used as a buffer, and the thickness of the buffer layer 22 is 150 nm to 2500 nm. In some embodiments, the thickness of the buffer layer 22 may be 500 nm. The channel layer 23 may be made of GaN or other materials, and the thickness of the channel layer 23 is 20 nm to 200 nm. In some embodiments, the thickness of the channel layer 23 may be 150 nm. The barrier layer 24 may be made of AlGaN, AlN, InAlN, or other materials, and the thickness of the barrier layer 24 may be 3 nm to 30 nm. In some embodiments, the thickness of the barrier layer 24 may be 25 nm.
[0032] S21. A first resist is coated onto the passivation layer 3, and the first resist is pre-baked to form the first resist layer 41. Figure 3As shown, a second resist is coated on the first resist layer 41, and the second resist is pre-baked to form the second resist layer 42. Figure 4 As shown; the first resist layer 41 and the second resist layer 42 constitute the first double-layer resist structure 4; More specifically, the first photoresist is an electron beam photoresist, preferably polymethyl methacrylate (PMMA). The first photoresist is baked at 200°C for 10 minutes to form a first photoresist layer 41, the thickness of which is 100 nm to 250 nm. The second photoresist is an electron beam photoresist, preferably polymethyl methacrylate-methacrylic acid (PMMA-MAA). The second photoresist is baked at 150°C for 10 minutes to form a second photoresist layer 42, the thickness of which is 150 nm to 2000 nm.
[0033] The baking temperature for the first photoresist can be from 150℃ to 250℃, specifically 150℃, 180℃, 200℃, 220℃, and 250℃, and the baking time can be from 5 minutes to 15 minutes, specifically 5 minutes, 8 minutes, 10 minutes, and 15 minutes. The baking temperature for the second photoresist can be from 100℃ to 200℃, specifically 100℃, 120℃, 130℃, 150℃, 180℃, and 200℃, and the baking time can be from 5 minutes to 15 minutes, specifically 5 minutes, 8 minutes, 10 minutes, and 15 minutes.
[0034] S22. Perform patterned exposure and development on the first double-layer photoresist structure 4 to obtain the first region A corresponding to the gate pin 13 and the second region B corresponding to the first gate field plate 12. More specifically, the first double-layer photoresist structure 4 is subjected to electron beam exposure development. The first region A is an opening penetrating both the first photoresist layer 41 and the second photoresist layer 42 to the surface of the passivation layer 3 near the first photoresist layer 41. The second region B is an opening that only penetrates the second photoresist layer 42. The first exposure dose for the first region A is determined based on the sum of the thicknesses of the first photoresist layer 41 and the second photoresist layer 42. The feature linewidth of the first region A is 20 nm to 500 nm. The second exposure dose for the second region B is determined based on the thickness of the second photoresist layer 42. The feature linewidth of the second region B is 20 nm to 5000 nm. Figure 5As shown, the second exposure dose in the second region B is less than the first exposure dose in the first region A. This allows the first region A to penetrate the first resist layer 41 and the second resist layer 42, while the second region B only penetrates the second resist layer 42. By controlling the thickness of the first resist layer 41, the position of the first gate field plate 12 in the vertical direction can be controlled. Compared with the traditional method of controlling the height of the field plate by adjusting parameters such as dry etching power and time, this method can effectively reduce the difficulty of the etching process and improve the position control accuracy and process repeatability of the first gate field plate 12.
[0035] S3, to Figure 5 The first double-layer resist structure 4, after being patterned, serves as a mask for dry etching, such as... Figure 7 As shown, the passivation layer 3 corresponding to the first region A is removed to expose the upper surface of the barrier layer 24, while a second surface of the passivation layer 3 is formed in the second region B. The upper surface of the passivation layer 3, the second surface of the passivation layer 3, and the upper surface of the barrier layer 24 form a two-stage stepped gate trench opening 31. More specifically, the dry etching process parameters are determined based on the thickness of the passivation layer 3.
[0036] A first step and a second step with progressively increasing depth are formed on the barrier layer 24. The first step penetrates the passivation layer to the surface of the barrier layer near the passivation layer. The passivation layer is etched, with the first step formed by etching the first region A and the second step formed by etching the second region B. The first step and the second step together form a two-stage stepped gate trench opening 31. Wherein, h fp1 This represents the depth of the first step.
[0037] S41. Remove the mask, as follows: Figure 8 As shown, a second double-layer resist structure 5 is prepared on the surface of the passivation layer 3 after completing the two-stage stepped gate slot opening 31. A third resist is coated on the passivation layer 3, and the third resist is pre-baked to form the third resist layer 51. A fourth resist is coated on the third resist layer 51, and the fourth resist is pre-baked to form the fourth resist layer 52. Figure 9 As shown; the third resist layer 51 and the fourth resist layer 52 constitute the second double-layer resist structure 5; More specifically, the third photoresist can be a non-photosensitive photoresist, and can be polydimethylglutarimide (PMGI SF6), or any one of PMGI SF3, PMGI SF4, PMGI SF5, PMGI SF7, PMGI SF8, PMGI SF9, PMGI SF10, PMGI SF11, PMGI SF12, or PMGI SF13. The third photoresist is baked at 200°C for 5 minutes to form a third photoresist layer 51. The thickness of the third photoresist layer 51 is 400 nm to 600 nm; in some embodiments, the thickness of the third photoresist layer 51 can be 500 nm. The fourth photoresist is a photosensitive photoresist, and the fourth photoresist layer 52 can be I... The line (365nm) positive photoresist can be EPI621, AZ701 or EPI620. The fourth resist is baked at 90°C for 1 minute to form a fourth resist layer 52. The thickness of the fourth resist layer 52 is 200nm to 800nm. In some embodiments, the thickness of the fourth resist layer 52 can be 300nm.
[0038] The baking temperature for the third resist can be from 150℃ to 250℃, specifically 150℃, 180℃, 200℃, 220℃, and 250℃, and the baking time can be from 3 minutes to 10 minutes, specifically 3 minutes, 5 minutes, 8 minutes, and 10 minutes. The baking temperature for the fourth resist can be from 70℃ to 110℃, specifically 70℃, 80℃, 90℃, 100℃, and 110℃, and the baking time can be from 1 minute to 3 minutes, specifically 1 minute, 2 minutes, and 3 minutes.
[0039] S42. The second double-layer resist structure 5 is patterned by exposure and development to complete gate lithography, exposing the two-stage stepped gate trench openings 31, such as... Figure 10 As shown; More specifically, the second double-layer resist structure 5 is exposed and developed to form a third region C, which exposes the first step and the second step. The exposure dose of the third region C is determined based on the thickness of the fourth resist layer 52, and the development time is determined based on the thicknesses of the third resist layer 51 and the fourth resist layer 52. The third resist layer 51 and the fourth resist layer 52 are soluble in the same developer. Along the extension direction of the passivation layer 3, i.e., the horizontal direction, the development rate of the fourth resist layer 52 is greater than that of the third resist layer 51, so that the opening length on the fourth resist layer 52 in the horizontal direction is less than the opening length of the third resist layer 51. This facilitates good separation of the metal deposited on the fourth resist layer 52 from the metal deposited in the two-stage stepped gate trench openings 31 during subsequent metal deposition, and also results in a smooth edge for the prepared two-stage field plate gate structure 1.
[0040] S5. Metal deposition is performed in the two-stage stepped gate trench opening 31, and the second double-layer resist structure 5 is stripped to form the two-stage field plate gate structure 1. More specifically, metal is deposited within the two-stage stepped gate opening 31, such as... Figure 11 As shown, metal is deposited on the fourth resist layer 52 and within the two-stage stepped gate trench openings 31 to obtain a metal layer 6. The metal deposited within the two-stage stepped gate trench openings 31 forms a two-stage field plate gate structure 1. The metal on the fourth resist layer 52 is evaporated, and the second double-layer resist structure 5 is stripped away to prepare the two-stage field plate gate structure 1, as shown. Figure 12 As shown.
[0041] Furthermore, the metal can be at least one of Ni, Au, Pt, and Mo, and the thickness of the two-stage field plate gate structure 1 is greater than the thickness of the passivation layer 3. In some embodiments, when the deposited metal is Ni, the thickness of the metal layer 6 is 300 nm.
[0042] Furthermore, such as Figure 12 As shown, the lower surface of the second gate field plate 11 is in contact with the upper surface of the passivation layer 3 (the surface away from the barrier layer 24), the lower surface of the first gate field plate 12 is the second surface of the passivation layer 3, the gate foot 13 is in contact with the upper surface of the barrier layer 24, and the upper surface of the passivation layer 3, the second surface of the passivation layer 3 and the upper surface of the barrier layer 24 form the two-stage stepped gate groove opening 31, which is an opening structure that is wider at the top and narrower at the bottom.
[0043] More specifically, the distance between the second surface of the passivation layer 3 and the bottom of the gate foot 13 (the upper surface of the barrier layer 24) is the depth of the first step, which is also the height h of the first gate field plate 12. fp1 ,like Figure 12 As shown. The height h of the first grid plate 12 fp1 The thickness of the first resist layer 41 is controlled, rather than by multiple photolithography batch etching, which can effectively reduce the difficulty of the etching process and improve the position control accuracy and process repeatability of the first gate field plate 12.
[0044] Furthermore, the length of the first gate field plate 12 is 20 nm to 5000 nm, and the length of the second gate field plate 11 is 20 nm to 5000 nm longer than the length of the first gate field plate 12.
[0045] Example 2 The difference between Example 2 and Example 1 is that in the fabrication method of a two-stage field plate gate structure, S2 and S3 are specifically as follows: S21. A first resist is coated onto the passivation layer 3, and the first resist is pre-baked to form the first resist layer 41. Figure 3 As shown, a second resist is coated on the first resist layer 41, and the second resist is pre-baked to form the second resist layer 42. Figure 4 As shown; the first resist layer 41 and the second resist layer 42 constitute the first double-layer resist structure 4; More specifically, the first photoresist can be a non-photosensitive photoresist, and can be polydimethylglutarimide (PMGI SF6) or any one of PMGI SF3, PMGI SF4, PMGI SF5, PMGI SF7, PMGI SF8, PMGI SF9, PMGI SF10, PMGI SF11, PMGI SF12, or PMGI SF13. The first photoresist is baked at 200°C for 5 minutes to form a first photoresist layer 41, the thickness of which is 50 nm to 3000 nm. The second photoresist is a photosensitive photoresist, and can be I... The line (365 nm) positive photoresist, preferably EPI621 or EPI620, is baked at 90°C for 1 min to form a second photoresist layer 42, the thickness of which is 50 nm to 300 nm.
[0046] The baking temperature for the first photoresist can be from 150℃ to 250℃, specifically 150℃, 180℃, 200℃, 220℃, and 250℃, and the baking time can be from 3 minutes to 10 minutes, specifically 3 minutes, 5 minutes, 8 minutes, and 10 minutes. The baking temperature for the second photoresist can be from 70℃ to 110℃, specifically 70℃, 80℃, 90℃, 100℃, and 110℃, and the baking time can be from 1 minute to 3 minutes, specifically 1 minute, 2 minutes, and 3 minutes.
[0047] S22. Perform patterned exposure and development on the first double-layer photoresist structure 4 to obtain the first region A corresponding to the gate pin 13 and the second region B corresponding to the first gate field plate 12. More specifically, the first double-layer photoresist structure 4 is exposed and developed. The first region A is an opening penetrating both the first photoresist layer 41 and the second photoresist layer 42 to the surface of the passivation layer 3 near the first photoresist layer 41. The second region B is an opening that only penetrates the first photoresist layer. The exposure conditions for the first region A are determined based on the thickness of the second photoresist layer 42, and the feature linewidth of the first region A is 20 nm to 500 nm. The boundary of the second region B is determined by the thickness of the first photoresist layer 41 and the development parameters, and the feature linewidth of the second region B is 20 nm to 5000 nm. Figure 6 As shown. The boundary of the first gate field plate 12 is controlled by the developing process to achieve left-right symmetry of the first gate field plate 12 relative to the gate foot 13. The difference in dissolution rate of the first resist layer 41 and the second resist layer 42 in the developing solution is used to achieve the opening structure jointly formed by the first region A and the second region B. The height of the first gate field plate 12 is controlled by the thickness of the second resist layer 42. Compared with the traditional method of controlling the height of the field plate by batch etching by adjusting parameters such as dry etching power and time, this method can effectively reduce the difficulty of the etching process and improve the position control accuracy and process repeatability of the first gate field plate 12.
[0048] S3, to Figure 6 The first double-layer resist structure 4, after being patterned, serves as a mask for dry etching, such as... Figure 7 As shown, the passivation layer 3 corresponding to the first region A is removed, and a second surface of the passivation layer 3 is formed in the second region B, forming a two-stage stepped gate groove opening 31 to expose the barrier layer 24 below the passivation layer 3.
[0049] Example 3 The difference between Example 3 and Examples 1 and 2 is that in the fabrication method of a two-stage field plate gate structure, S3-S5 specifically involve: S3. Using the patterned first double-layer resist structure 4 as a mask, perform dry etching, such as... Figure 13As shown, the passivation layer 3 and part of the barrier layer 24 corresponding to the first region A are removed, and the passivation layer 3 corresponding to the second region B is removed to form a two-stage stepped gate trench opening 31, exposing the barrier layer 24 below the passivation layer 3. More specifically, the F-based dry etching (i.e., the first dry etching) process parameters are determined based on the thickness of the passivation layer 3, and the passivation layer 3 corresponding to the first region A is completely removed. Then, Cl-based dry etching (i.e., the second dry etching) is performed on the barrier layer 24 to remove part of the barrier layer 24 in the first region A, and a groove 241 is formed in the barrier layer 24, such as... Figure 14 As shown. The Cl-based dry etching process parameters are determined based on the thickness of the etching barrier layer 24. The preferred etching depth should be less than the thickness of the barrier layer 24, and the Cl-based dry etching depth is 3 nm to 25 nm.
[0050] S41. Remove the mask, as follows: Figure 14 As shown, a second double-layer resist structure 5 is prepared on the surface of the passivation layer 3 after completing the two-stage stepped gate slot opening 31. A third resist is coated on the passivation layer 3, and the third resist is pre-baked to form the third resist layer 51. A fourth resist is coated on the third resist layer 51, and the fourth resist is pre-baked to form the fourth resist layer 52. Figure 15 As shown; the third resist layer 51 and the fourth resist layer 52 constitute the second double-layer resist structure 5; More specifically, the third photoresist can be a non-photosensitive photoresist. The third photoresist can be polydimethylglutarimide (PMGI SF6), or any one of PMGI SF3, PMGI SF4, PMGI SF5, PMGI SF7, PMGI SF8, PMGI SF9, PMGI SF10, PMGI SF11, PMGI SF12, or PMGI SF13. The third photoresist is baked at 200°C for 5 minutes to form a third photoresist layer 51. The thickness of the third photoresist layer 51 is 400 nm to 600 nm. In some embodiments, the thickness of the third photoresist layer 51 can be 500 nm. The fourth photoresist is a photosensitive photoresist. The fourth photoresist can be I... The line (365nm) positive photoresist, preferably EPI621 or EPI620, is baked at 90°C for 1 minute to form a fourth photoresist layer 52. The thickness of the fourth photoresist layer 52 is 200nm to 400nm. In some embodiments, the thickness of the fourth photoresist layer 52 may be 300nm.
[0051] The baking temperature for the third resist can be from 150℃ to 250℃, specifically 150℃, 180℃, 200℃, 220℃, and 250℃, and the baking time can be from 3 minutes to 10 minutes, specifically 3 minutes, 5 minutes, 8 minutes, and 10 minutes. The baking temperature for the fourth resist can be from 70℃ to 110℃, specifically 70℃, 80℃, 90℃, 100℃, and 110℃, and the baking time can be from 1 minute to 3 minutes, specifically 1 minute, 2 minutes, and 3 minutes.
[0052] S42. The second double-layer resist structure 5 is patterned by exposure and development to complete gate lithography, forming a two-stage stepped gate trench opening 31, such as... Figure 16 As shown; More specifically, the second double-layer resist structure 5 is exposed and developed to form a third region C, which exposes the first step and the second step. The exposure dose of the third region C is determined based on the thickness of the fourth resist layer 52, and the development time is determined based on the thicknesses of the third resist layer 51 and the fourth resist layer 52. The third resist layer 51 and the fourth resist layer 52 are soluble in the same developer. Along the extension direction of the passivation layer 3, i.e., along the horizontal direction, the development rate of the fourth resist layer 52 is greater than that of the third resist layer 51, so that the opening length on the fourth resist layer 52 along the horizontal direction is less than the opening length of the third resist layer 51. This facilitates good separation of the metal deposited on the fourth resist layer 52 from the metal deposited in the two-stage stepped gate trench openings 31 during subsequent metal deposition, and also results in a smooth edge for the prepared two-stage field plate gate structure 1.
[0053] S5. Metal deposition is performed in the two-stage stepped gate trench opening 31, and the second double-layer resist structure 5 is stripped to form the two-stage field plate gate structure 1. More specifically, metal is deposited within the two-stage stepped gate opening 31, such as... Figure 17 As shown, metal is deposited on the fourth resist layer 52 and within the two-stage stepped gate trench openings 31 to obtain a metal layer 6. The metal deposited within the two-stage stepped gate trench openings 31 forms a two-stage field plate gate structure 1. The metal on the fourth resist layer 52 is evaporated, and the second double-layer resist structure 5 is stripped away to prepare the two-stage field plate gate structure 1, as shown. Figure 18 As shown.
[0054] Furthermore, the metal can be at least one of Ni, Au, Pt, and Mo, and the thickness of the two-stage field plate gate structure 1 is greater than the thickness of the passivation layer 3. In some embodiments, when the deposited metal is a Ni / Au stack, the thickness of the metal layer 6 is 30 nm to 300 nm.
[0055] The fabrication method of the two-stage field plate gate structure of this application produces a two-stage field plate gate structure 1 formed in one step. Different exposure depths in different regions are achieved by setting the exposure dose in zones. No pre-reserved overlay redundancy is needed between different field plate layers, allowing for smaller field plate dimensions. This reduces parasitic capacitance while achieving electric field modulation, supporting increased breakdown voltage for high-frequency devices. Furthermore, the first gate field plate 12 and the second gate field plate 11 are formed in a single photolithography development step, avoiding positional misalignment between the gate field plate and the gate pin 13 caused by overlay errors in traditional methods. This achieves automatic alignment of the first gate field plate 12 and the gate pin 13. The first gate field plate 12 and the second gate field plate 11 are symmetrical, effectively avoiding process errors and simplifying the process.
[0056] Example 4 Embodiment 4 of this application provides a method for fabricating a two-stage field plate gate structure, resulting in a two-stage field plate gate structure 1, as shown in the reference. Figure 12 and Figure 18 The structure is formed on the epitaxial structure 2 and includes: Gate pin 13 and a first gate field plate 12 and a second gate field plate 11 extending from the top of the gate pin 13 toward the drain direction; The epitaxial structure 2 forms a two-stage stepped gate trench opening 31 in the region corresponding to the gate; The lengths of the second gate field plate 11, the first gate field plate 12, and the gate foot 13 decrease sequentially in the horizontal direction, and the two-stage field plate gate structure 1 is connected to the two-stage stepped gate slot opening 31.
[0057] The two-stage field plate gate structure 1 of this application embodiment can achieve a smaller field plate size. The first gate field plate 12 and the second gate field plate 11, which extend from the top of the gate foot 13 towards the drain, realize an integrated multi-stage field plate structure, eliminating the need for additional photolithography and overlay, resulting in a simple process and high precision. While achieving electric field modulation, it reduces the introduction of parasitic capacitance, which can support the improvement of breakdown voltage of high-frequency devices. At the same time, when this two-stage field plate gate structure 1 is applied to GaN devices, it improves the reliability of GaN devices and simultaneously optimizes their power density, taking into account both high-frequency characteristics and process compatibility.
[0058] Furthermore, the lower surface of the second gate field plate 11 abuts against the first surface (i.e., the surface of the passivation layer 3) of the two-stage stepped gate trench opening 31, and the lower surface of the first gate field plate 12 abuts against the second surface (i.e., the second surface of the passivation layer 3) of the two-stage stepped gate trench opening 31. The second gate field plate 11, the first gate field plate 12, and the gate foot 13 together form a two-stage field plate gate structure. By distributing the electric field through the second gate field plate 11 and the first gate field plate 12, the peak electric field is reduced, thereby achieving a significant increase in breakdown voltage, effective suppression of current collapse, and simultaneous optimization of device reliability and power density.
[0059] Furthermore, the gate pin 13, the first gate field plate 12, and the second gate field plate 11 are all on the same metal layer, with no interface contact or interlayer resistance between them. This ensures continuous and smooth electric field transmission, preventing the introduction of additional resistance and losses due to multi-layer metal contact, thus guaranteeing the high-frequency and high-power performance of the device. Furthermore, only one metal deposition is required to simultaneously form the gate pin 13, the first gate field plate 12, and the second gate field plate 11, significantly reducing process steps, improving yield, lowering costs, and shortening the process cycle. The gate pin 13, the first gate field plate 12, and the second gate field plate 11 do not require pre-reserved overlay redundancy, eliminating overlay deviations between multiple metal layers. This also facilitates uniform electric field distribution, avoiding localized electric field concentration, and further improving breakdown voltage and reliability.
[0060] Furthermore, the two-stage field plate gate structure covers the two-stage stepped gate trench opening 31. The length of the second gate field plate 11 is greater than the length of the first gate field plate 12. This arrangement can reduce gate parasitic capacitance, lower gate resistance, and improve the high-frequency characteristics of the device.
[0061] More specifically, the gate foot 13 and the first gate field plate 12 can achieve a symmetrical structure in the vertical direction. The symmetrical structure can make the stress distribution on the surface of the barrier layer 24 more uniform and balanced, while reducing the gate resistance, effectively improving the reliability of operation, improving the consistency of the electrical performance of the device, and effectively avoiding process errors and simplifying the process.
[0062] Furthermore, such as Figure 12 As shown, the epitaxial structure 2 includes at least a barrier layer 24, and the two-stage field plate gate structure 1 is disposed on the upper surface of the barrier layer 24.
[0063] Furthermore, such as Figure 18 As shown, the epitaxial structure 2 includes at least a barrier layer 24, on which a groove 241 is provided. The bottom of the gate foot 13 passes through the lower surface of the barrier layer 24 and contacts the groove 241. This structure can improve the transconductance of the device; achieve a wide range of adjustable threshold voltage; and provide structural support for the two-stage field plate gate structure 1, ultimately achieving high-voltage, high-frequency, and high-reliability device performance.
[0064] Example 5 Embodiment 5 of this application discloses the two-stage field plate gate structure described in Embodiment 4, which is applied to GaN devices.
[0065] It should also be noted that the terms "some embodiments," "other embodiments," and "embodiments" used in this application refer to specific features, structures, or characteristics described in connection with those embodiments, which are included in at least one embodiment described in the general description of this application. The appearance of the same expression in multiple places in the specification does not necessarily refer to the same embodiment. Furthermore, when a specific feature, structure, or characteristic is described in connection with any embodiment, the intention is to suggest that implementing such a feature, structure, or characteristic in conjunction with other embodiments also falls within the scope of this application.
[0066] In the above embodiments, the descriptions of each embodiment have different focuses. For parts not described in detail in a certain embodiment, please refer to the relevant descriptions in other embodiments.
[0067] It should also be noted that the above are merely preferred embodiments of this application and do not limit the scope of patent protection of this application. Any equivalent structural or procedural changes made using the content of this application’s specification and drawings, or direct or indirect applications in other related technical fields, are similarly included within the scope of patent protection of this application.
Claims
1. A method for fabricating a two-stage field plate gate structure, characterized in that, Includes the following steps: A passivation layer is prepared on an epitaxial structure; the epitaxial structure includes a substrate layer, a buffer layer, a channel layer, and a barrier layer, wherein the barrier layer, the channel layer, and the buffer layer are sequentially disposed on the substrate layer along the vertical direction, and a passivation layer is deposited on the barrier layer; A first double-layer photoresist structure is prepared on the passivation layer, and the first double-layer photoresist structure is subjected to patterned exposure and development processing to obtain a first region and a second region. Using the patterned first double-layer resist structure as a mask, the passivation layer corresponding to the first region is removed, and a second surface of the passivation layer is formed in the second region. The upper surface of the passivation layer, the second surface of the passivation layer, and the exposed surface of the epitaxial structure form a two-stage stepped gate trench opening. Remove the mask, prepare a second double-layer resist structure on the passivation layer surface that completes the two-stage stepped gate trench opening, and perform patterned exposure and development on the second double-layer resist structure to complete gate lithography and expose the two-stage stepped gate trench opening. Metal deposition is performed at the opening of the two-stage stepped gate trench, and the second double-layer resist structure is stripped to form the two-stage field plate gate structure. The two-stage field plate gate structure includes a gate foot and a first gate field plate and a second gate field plate extending from the top of the gate foot toward the drain.
2. The method for fabricating a two-stage field plate gate structure according to claim 1, characterized in that, The preparation of the first double-layer resist structure specifically involves: coating a first resist on the passivation layer, pre-baking the first resist to form the first resist layer, coating a second resist on the first resist layer, and pre-baking the second resist to form the second resist layer; the first resist layer and the second resist layer constitute the first double-layer resist structure.
3. The method for fabricating a two-stage field plate gate structure according to claim 2, characterized in that, The first photoresist is an electron beam photoresist, and the first photoresist is pre-baked to form the first photoresist layer; the second photoresist is an electron beam photoresist, and the second photoresist is pre-baked to form the second photoresist layer; the baking temperature of the second photoresist layer is not higher than the baking temperature of the first photoresist layer, and the first photoresist layer and the second photoresist layer are dissolved in the same developing solution.
4. The method for fabricating the two-stage field plate gate structure according to claim 3, characterized in that, The process of patterning and developing the first double-layer resist structure to obtain a first region corresponding to the gate pin and a second region corresponding to the first gate field plate specifically involves: performing electron beam exposure and development on the first double-layer resist structure; determining the first exposure dose of the first region based on the sum of the thicknesses of the first resist layer and the second resist layer; determining the second exposure dose of the second region based on the thickness of the second resist layer; and ensuring that the second exposure dose is less than the first exposure dose. The first region is an opening that penetrates the first resist layer and the second resist layer to the surface of the passivation layer near the first resist layer; and the second region is an opening that only penetrates the second resist layer.
5. The method for fabricating a two-stage field plate gate structure according to claim 2, characterized in that, The first photoresist is a non-photosensitive photoresist, and the first photoresist is pre-baked to form the first photoresist layer; the second photoresist is a photosensitive photoresist, and the second photoresist is pre-baked to form the second photoresist layer; the baking temperature of the second photoresist layer is not higher than the baking temperature of the first photoresist layer, and the first photoresist layer and the second photoresist layer are dissolved in the same developing solution.
6. The method for fabricating a two-stage field plate gate structure according to claim 5, characterized in that, The process of patterning and developing the first double-layer photoresist structure to obtain a first region corresponding to the gate pin and a second region corresponding to the first gate field plate specifically involves: exposing and developing the first double-layer photoresist structure; the exposure conditions of the first region are determined based on the thickness of the second photoresist layer; the boundary of the second region is determined by the thickness of the first photoresist layer and the development parameters; the first region is an opening that penetrates the first photoresist layer and the second photoresist layer to the passivation layer near the surface of the first photoresist layer; and the second region is an opening that only penetrates the first photoresist layer.
7. The method for fabricating a two-stage field plate gate structure according to any one of claims 3 to 6, characterized in that, The process of removing the mask and preparing a second double-layer resist structure on the passivation layer surface where the two-stage stepped gate trench openings are completed specifically involves: using the patterned first double-layer resist structure as a mask, performing dry etching to remove the passivation layer corresponding to the first region and expose the upper surface of the barrier layer; simultaneously forming a second surface of the passivation layer in the second region; and forming a two-stage stepped gate trench opening with the upper surface of the passivation layer, the second surface of the passivation layer, and the upper surface of the barrier layer.
8. The method for fabricating a two-stage field plate gate structure according to any one of claims 3 to 6, characterized in that, The process of removing the mask and preparing a second double-layer resist structure on the passivation layer surface after completing the two-stage stepped gate trench opening specifically involves: using the patterned first double-layer resist structure as a mask, performing a first dry etching process to remove the passivation layer corresponding to the first region and expose the barrier layer; simultaneously forming a second surface of the passivation layer in the second region; performing a second dry etching process to remove part of the barrier layer corresponding to the first region and form a second surface of the barrier layer; and forming a two-stage stepped gate trench opening by the upper surface of the passivation layer, the second surface of the passivation layer, and the second surface of the barrier layer.
9. The method for fabricating a two-stage field plate gate structure according to claim 1, characterized in that, The length of the first gate field plate is 20 nm to 5000 nm, and the length of the second gate field plate is greater than the length of the first gate field plate, with a difference of 20 nm to 5000 nm between them.
10. The method for fabricating a two-stage field plate gate structure according to any one of claims 1 to 6, characterized in that, The metal covers the openings of the two-stage stepped grid grooves, and the thickness of the metal is greater than the depth of the openings of the two-stage stepped grid grooves.
11. A two-stage field-plate gate structure prepared by the method of preparing a two-stage field-plate gate structure according to any one of claims 1 to 10, characterized in that, It is used in GaN devices.