A method for preparing a double perovskite MIS structure electroluminescent device
By using a method for fabricating MIS-structured electroluminescent devices, the challenges of solubility and composition control of Cs2AgInCl6-based double perovskite materials in electroluminescent devices were solved, achieving low-cost, single-component, electrically driven white light emission, improving the uniformity and stability of the material, and verifying its feasibility in the field of electroluminescence.
Patent Information
- Application Number
- CN202611107096.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-07-24
- Publication Date
- 2026-11-17
AI Technical Summary
In the existing technology, Cs2AgInCl6-based double perovskite materials have problems such as low solubility, difficulty in controlling the component ratio, ligand stability issues in the nanocrystalline route, and lack of device structures suitable for poor intrinsic conductivity during thin film preparation, which limits their application in electroluminescent devices.
An MIS-structured electroluminescent device was developed. The substrate was purified by ultrasonic cleaning and oxygen plasma treatment. Microcrystals were grown using an antisolvent-induced crystallization method. An insulating layer was spin-coated and a metal electrode was deposited by high-vacuum thermal evaporation to form a Cs2Na1-xAgxIn1-yBiyCl6 double perovskite microcrystalline layer, enabling carrier injection and recombination luminescence through the insulating layer.
It achieves low-cost and simple single-component electro-driven white light emission, solves the problems of low material solubility and component control, improves the uniformity and stability of the microcrystalline layer, ensures the effectiveness of carrier injection and recombination luminescence, and breaks through the technical limitations of this material in the field of electroluminescence.
Smart Images

Figure CN123124518A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of lighting and display technology, specifically relating to a method for fabricating an electroluminescent device with a MIS structure based on a double perovskite material. Background Technology
[0002] Researchers have synthesized Cs₂AgInCl₆, a material with a potassium cryolite structure, using a simple room-temperature solution method, and utilized Na / Ag alloys and Bi... 3+ Doping achieved highly efficient, stable, and continuous-spectrum broadband white light emission covering almost the entire visible light band (Nature, 2018, 563, 541-545), with a photoluminescence efficiency of 86%, showing great potential for application in white light illumination. However, it was subsequently discovered that the preparation of such all-inorganic chlorine-based double perovskite films is fraught with difficulties, preventing their effective application in electroluminescent devices. Specifically, the following technical bottlenecks exist: First, the low solubility of the material makes thin film preparation difficult. The challenge of solution-based thin film preparation lies in the poor solubility of such materials in various solvents, making it difficult to find suitable solvents to prepare precursor solutions and obtain high-quality thin films using conventional solution methods. Furthermore, the low solubility also makes it difficult to grow large-size single crystals, thus hindering the development of single-crystal devices. Second, multi-element co-evaporation makes precise control of component ratios difficult. For vacuum evaporation deposition of thin films, the alloy-doped double perovskite materials involve many elements (including Cs, Na, Ag, In, Bi, Cl, etc.). The different molecular weights and densities of these elements lead to significant differences in evaporation rates, making it difficult to control the component ratios and quality of the thin film. The final product is prone to deviating from the target stoichiometry, affecting the regulation of luminescence performance. Third, ligand and stability issues in the nanocrystalline route restrict device performance. In the method of preparing thin films using nanocrystals and quantum dots, the presence of electrically insulating organic ligands hinders charge transport performance. Therefore, the colloid needs to be cleaned and purified before film preparation to remove excess ligands. However, the problem of unstable and easily agglomerated colloids after cleaning remains unsolved, resulting in poor film quality, high defect density, and severe nonradiative recombination. Fourth, there is a lack of device structures suitable for the intrinsically poor conductivity of double perovskite systems. The above problems have hindered the development of double perovskite optoelectronic devices. More importantly, Cs2AgInCl6-based double perovskite materials have poor intrinsic conductivity. Traditional LED device structures (such as pn junctions) have high requirements for the doping type and conductivity of such materials, making it difficult to achieve effective carrier injection and recombination luminescence, thus limiting the practical application of this material system in the field of electroluminescence. To date, there is still no suitable device structure for Cs2Na 1-x Ag x In 1-y Bi y Reports indicate that Cl6-based double perovskite materials have been successfully applied to electroluminescent devices.
[0003] This invention focuses on electroluminescent devices. By introducing a material with continuous broadband emission characteristics and creatively applying it to a metal-insulator-semiconductor (MIS) device structure, it enables single-component, electrically driven broadband white light emission. The aim is to provide new materials, methods, and ideas for achieving low-cost, simple-to-fabricate single-material electroluminescent lighting. Summary of the Invention
[0004] To achieve the above objectives, the present invention adopts the following technical solution: This invention provides a method for fabricating a double perovskite MIS structure electroluminescent device, wherein the chemical formula of the double perovskite is Cs₂Na. 1-x Ag x In 1-y Bi y Cl6, where 0 ≤ x ≤ 1, 0 ≤ y ≤ 1. The device, from bottom to top, includes a substrate, a first electrode layer, a double perovskite microcrystalline layer, an insulating layer, and a second electrode layer. The specific fabrication steps are as follows: S1: Cleaning the patterned electrode substrate The substrate with patterned electrodes was ultrasonically cleaned sequentially with cleaning solution, deionized water, acetone, and isopropanol, and then surface treated with a plasma cleaner to remove organic contaminants and improve substrate surface wettability.
[0005] S2: Precipitation of a double perovskite microcrystalline layer Prepare a saturated solution of dimethyl sulfoxide (DMSO) for the double perovskite precursor. Take 30 μL and drop it onto the substrate treated in step S1. Place the substrate in a sealed container containing the antisolvent and let it stand for about 10 h to allow the microcrystals to precipitate, thus obtaining the double perovskite microcrystalline layer.
[0006] S3: Spin-coated insulating layer A chlorobenzene (CB) solution of an insulating polymer is spin-coated onto the double perovskite microcrystalline layer obtained in step S2 to form a dense insulating layer.
[0007] S4: Evaporated metal electrode The MIS structure electroluminescent device is obtained by depositing metal electrodes on an insulating layer under high vacuum conditions using a thermal evaporation method.
[0008] Furthermore, the substrate in step S1 is glass or flexible PET, and the patterned electrode is ITO or FTO.
[0009] Furthermore, in step S2, the concentration of the saturated solution of the double perovskite precursor is approximately 0.1 M, the antisolvent is isopropanol, and the standing time in the sealed container is 10 h.
[0010] Furthermore, in step S3, the insulating polymer is PEO or PMMA, the concentration of the chlorobenzene solution is 10–100 mg / mL, the spin coating speed is 3000 rpm, and the spin coating time is 30 s.
[0011] Furthermore, the vacuum level of the high vacuum condition described in step S4 is not less than 3 × 10⁻⁶. -4 Pa, evaporation rate of 1–3 Å / s, deposition thickness of 50–100 nm, and the deposited metal electrodes include, but are not limited to, Al, Ag, Au, and Cu.
[0012] This invention has the following significant advantages over the prior art: 1. Synergistic improvement of interface purification and wettability ensures uniform nucleation and firm adhesion of microcrystals. Step S1 employs a dual cleaning process combining ultrasonic cleaning and oxygen plasma treatment. Gradient ultrasonic cleaning combined with oxygen plasma treatment can thoroughly remove organic and inorganic contaminants from the substrate surface, enhance the bonding force between the microcrystals and the electrodes, and prevent microcrystal detachment or uneven growth. Oxygen plasma treatment changes the ITO electrode surface from hydrophobic to hydrophilic, significantly reducing the contact angle, ensuring uniform spreading of the DMSO precursor solution, preventing agglomeration, and guaranteeing the uniform growth of large-area microcrystal layers. Moreover, the cleaning process does not require high temperatures and is suitable for flexible PET substrates, laying the foundation for wearable and curved lighting applications.
[0013] 2. Antisolvent-induced crystallization overcomes the dissolution bottleneck, enabling in-situ growth of microcrystals and precise retention of components. Step S2 involves in-situ growth of double perovskite microcrystals on the electrode substrate using an anti-solvent vapor-induced crystallization method, with DMSO selected as the solvent, taking advantage of its effect on Cs₂Na₂ 1-x Ag x In 1-y Bi yThe Cl6 system achieves a solubility of up to 0.1 M, overcoming the bottleneck of its extremely low solubility (<0.01 M) in conventional solvents. The slow diffusion of the antisolvent (isopropanol) vapor induces controlled crystallization, avoiding rapid, intense crystallization and resulting in large-sized crystals with high crystallinity and low defect density. The crystals grow in situ on the electrode surface without transfer, avoiding damage and interface contamination, and ensuring tight electrical contact between the crystals and the electrode. The product composition precisely maintains the precursor stoichiometry, avoiding component deviations caused by element density differences in vapor deposition and the stability reduction and weakened nano-effects caused by colloidal aggregation in nanocrystal methods. The band structure and emission spectrum can be precisely controlled by adjusting the x and y values. A 10-hour settling time ensures sufficient DMSO volatilization and antisolvent diffusion, allowing the crystals to grow to a suitable size (tens to hundreds of micrometers), balancing carrier transport and luminescence performance. Crystallization at room temperature and pressure requires no high temperature, inert atmosphere, or high vacuum, resulting in low energy consumption and simple operation. Both DMSO and isopropanol are low-toxicity reagents, conforming to green chemistry principles.
[0014] 3. Dense insulation layer coverage and interface passivation work together to achieve electrical isolation and injection balance. Step S3 involves spin-coating a PEO or PMMA insulating layer onto the microcrystalline layer to block direct conduction between electrodes, prevent short circuits, and ensure that charge carriers recombine and emit light via the microcrystalline layer; the polar groups of the polymer (ether oxygen bonds in PEO, ester groups in PMMA) passivate the Cl on the microcrystalline surface. - Defect states such as vacancies and dangling metal bonds reduce nonradiative recombination and improve luminescence efficiency; homogenize the electric field distribution on the microcrystalline surface to avoid tip breakdown and improve device withstand voltage stability; the concentration of the spin coating solution is limited to 10–100 mg / mL. Below 10 mg / mL, the insulating layer is too thin and has pinholes, which cannot effectively isolate the microcrystals; above 100 mg / mL, the viscosity is too high, the uniformity decreases, and the driving voltage increases. 50 mg / mL is the preferred concentration, which can achieve the best balance between insulation integrity and tunneling injection; the spin coating parameters of 3000 rpm / 30 s can form a uniform (tens of nanometers) dense and pinhole-free film on irregular microcrystalline surfaces. The rapid evaporation of chlorobenzene solvent avoids excessive swelling and penetration of the polymer, and chlorobenzene and DMSO are immiscible and do not damage the microcrystalline layer.
[0015] 4. High-vacuum thermal evaporation enables non-destructive deposition, ensuring electrode quality and implantation efficiency. Step S4 employs high-vacuum thermal evaporation to deposit metal electrodes. This pure physical vapor deposition method eliminates the need for chemical solvents, avoiding the erosion of the insulating layer and microcrystalline layer caused by solution methods. The substrate temperature is below 50°C to ensure the structural and performance stability of the microcrystalline and insulating layers. The vacuum level is not less than 3 × 10⁻⁶. -4The Pa value reduces the partial pressure of water, oxygen, and organic gases in the chamber, preventing electrode oxidation and contamination, ensuring high electrode purity and low resistivity, and reducing the erosion of microcrystals by water and oxygen. A moderate evaporation rate of 1–3 Å / s provides sufficient time for metal atom surface migration, forming a continuous, dense, and well-adhered thin film, avoiding the porosity caused by excessively fast rates (>5 Å / s) and the inefficiency and impurity adsorption caused by excessively slow rates (<0.5 Å / s). An electrode thickness of 50–100 nm ensures a thin-film resistance of less than 10 Ω / sq for efficient implantation, while avoiding increased internal stress or detachment caused by excessive thickness (>150 nm). This thickness also allows the semi-transparent top electrode to have suitable light transmittance for metals such as Ag and Al. The thermal evaporation method is applicable to various metals such as Al, Ag, Au, and Cu. Different work functions can flexibly adjust the implantation barrier, providing material selection freedom for performance optimization.
[0016] 5. The innovative MIS structural design enables single-component electrically driven white light emission, filling a technological gap. This invention is the first to use Cs2Na 1-x Ag x In 1-y Bi y Cl6 double perovskite microcrystals are applied to MIS electroluminescent devices. Their overall architectural advantages lie in: In the MIS structure, charge carriers emit light through Fowler-Nordheim tunneling or Poole-Frenkel emission, then recombine with the semiconductor layer via the insulating layer, eliminating dependence on pn junctions and reducing requirements on material conductivity. This makes them particularly suitable for intrinsic or weakly conductive double perovskite systems. Furthermore, they utilize the inherent broadband emission characteristics of double perovskites (self-trapped exciton luminescence and Bi...) 3+ Doping bandgap modulation allows for continuous white light emission covering the entire visible light region with a single component, avoiding the drawbacks of poor color stability, color drift, and complex processes associated with multi-component mixing schemes. Adjusting the x-value (Na / Ag ratio) controls the band gap and exciton binding energy, while adjusting the y-value (In / Bi ratio) controls the self-trapped exciton emission and Bi... 3+The relative intensity of the related emissions, working together, achieves continuous spectral tuning from cool white light to warm white light, meeting the needs of different lighting scenarios. The raw materials are common, inexpensive inorganic salts, and the preparation does not require expensive equipment such as MOCVD or molecular beam epitaxy, only conventional glove boxes, spin coaters, and thermal evaporation equipment, resulting in good production line compatibility and potential for large-scale production. This invention is the first to achieve electrically driven white light emission from this material system, breaking the technical limitation that it can only be used for photoluminescence (PL). Compared to the existing technology where this material system can only achieve 86% PL quantum efficiency under ultraviolet light excitation (Nature, 2018, 563, 541-545), the MIS device constructed in this invention can obtain continuous white light emission covering the entire visible light region under DC electric drive, and the peak positions of the electroluminescence (EL) spectrum and the PL spectrum are highly consistent, confirming the effectiveness of carrier injection and recombination luminescence. Although there is still room for improvement in EL efficiency, this invention has verified the feasibility of the material system in electroluminescent devices from scratch, laying a solid foundation for improving the external quantum efficiency of EL through composition optimization, interface engineering and other means, and opening up a new path for the practical application of all-inorganic double perovskite materials in the lighting field. Attached Figure Description
[0017] Figure 1 This is a schematic diagram of the MIS structure electroluminescent device of the present invention.
[0018] Figure 2 The image shows the morphology of the double perovskite microcrystals (left) and the actual electroluminescent device with MIS structure (right) prepared according to the embodiments of the present invention.
[0019] Figure 3 The electroluminescence spectrum of the double perovskite microcrystal photoluminescence and electroluminescence device prepared in the embodiments of the present invention is shown.
[0020] Figure 1 In the diagram, 1. Substrate, 2. Patterned electrode, 3. Double perovskite microcrystals, 4. Insulating layer, 5. Metal electrode. Detailed Implementation
[0021] To further understand the present invention, the technical solution of the present invention will be described in detail below with reference to specific embodiments. It should be noted that these embodiments are only used to illustrate the features and beneficial effects of the present invention and do not constitute any limitation on the scope of protection of the claims of the present invention.
[0022] In the following embodiments, the process methods not described in detail are all conventional methods known in the art. Unless otherwise specified, the materials, reagents, apparatus, and instruments used are all commercially available.
[0023] Example This embodiment provides a Cs2Na-based0.5 Ag 0.5 In 0.5 Bi 0.5 The specific fabrication process of the Cl6 double perovskite microcrystal MIS structure electroluminescent device is as follows: S1: Cleaning the patterned electrode substrate A glass substrate with patterned ITO electrodes is selected (FTO or flexible PET transparent conductive substrates can also be used). The substrate is ultrasonically cleaned sequentially in a special cleaning solution, deionized water, acetone, and isopropanol for 15 minutes each time to remove organic and inorganic contaminants from the surface. After cleaning, the substrate surface is dried with high-purity nitrogen gas, and then placed in a plasma cleaner for oxygen plasma treatment for 5 minutes to further remove residual organic matter and improve the wettability of the substrate surface.
[0024] S2: Precipitation of a double perovskite microcrystalline layer Weigh out stoichiometric amounts of CsCl, NaCl, AgCl, InCl3, and BiCl3 (total molar amount 0.1 mmol), dissolve them in 1.0 mL of dimethyl sulfoxide (DMSO), and stir at 60 °C for 12 h to obtain Cs2Na with a concentration of 0.1 M. 0.5 Ag 0.5 In 0.5 Bi 0.5 A saturated solution of Cl6 double perovskite precursor was prepared. 30 μL of this precursor solution was uniformly dropped onto the center of the ITO substrate treated in step S1. The substrate was then rapidly transferred to a sealed crystallization container containing the antisolvent isopropanol (IPA) (approximately 5 mL of IPA was pre-placed at the bottom of the container). The container was allowed to stand at room temperature for 10 h to allow the DMSO to slowly evaporate and induce the precipitation of microcrystals. After crystallization was complete, the substrate was removed, revealing a uniformly distributed double perovskite microcrystalline layer on the ITO electrode surface.
[0025] S3: Spin-coated insulating layer Polymethyl methacrylate (PMMA) powder was weighed and dissolved in chlorobenzene (CB) to prepare a PMMA-CB solution with a concentration of 50 mg / mL. The solution was then spin-coated onto the surface of the microcrystalline layer obtained in step S2 at a speed of 3000 rpm for 30 s. Subsequently, the layer was annealed on a hot plate at 100 °C for 10 min to remove residual solvent, thereby forming a dense insulating layer on the double perovskite microcrystalline layer.
[0026] S4: Evaporated metal electrode The sample prepared in step S3 is placed in a thermal evaporation device, and the vacuum degree is better than 3×10⁻⁶. -4Under the condition of Pa, silver (Ag) electrodes were deposited by resistance heating. The deposition rate was controlled at 1 Å / s, and the deposition thickness was 100 nm (the electrode material can also be Al, Au, or Cu, with a thickness range of 50-100 nm). After deposition, a complete MIS structure electroluminescent device was obtained.
[0027] Performance testing was conducted on the device fabricated in this embodiment: Under DC voltage drive, the device exhibited typical single-component broadband white light emission, with its electroluminescence spectrum covering the entire visible light region and its peak positions basically matching those of the photoluminescence spectrum of the corresponding microcrystals. This confirms that the MIS structure can effectively realize carrier injection and recombination luminescence of the dual perovskite microcrystals. These results indicate that Cs2Na 0.5 Ag 0.5 In 0.5 Bi 0.5 The Cl6 double perovskite material (x=0.5, y=0.5) has been successfully applied to an electroluminescent device for the first time, breaking the previous technical limitation that this material system could only achieve photoluminescence, and verifying the feasibility and pioneering nature of the technical solution of this invention.
[0028] It should be noted that the general formula of the double perovskite material described in this invention is Cs₂Na. 1-x Ag x In 1-y Bi y Cl6 (where 0≤x≤1, 0≤y≤1). This embodiment only uses x=0.5, y=0.5 as an example for illustration, but those skilled in the art can adjust the component ratios of Na / Ag and In / Bi according to actual needs to control the color temperature and color coordinates of the emission spectrum. At the same time, the type of antisolvent (such as isopropanol, ethanol, etc.), precursor concentration, crystallization time, and insulating layer material (such as PEO, PVP, etc.) can all be adjusted according to the specific implementation situation, and these all fall within the design concept scope of this invention.
Claims
1. A method for fabricating a double perovskite MIS structure electroluminescent device, characterized in that, The device comprises, from bottom to top, a substrate (1), a first electrode layer (2), a double perovskite microcrystalline layer (3), an insulating layer (4), and a second electrode layer (5); the chemical formula of the double perovskite is Cs₂Na. 1-x Ag x In 1-y Bi y Cl6, where 0 ≤ x ≤ 1, 0 ≤ y ≤ 1; The specific preparation steps are as follows: S1: Cleaning the substrate patterned with electrodes; S2: Preparation of a double perovskite microcrystalline layer; S3: Deposit an insulating layer on a double perovskite microcrystalline layer; S4: Deposit a metal electrode on the insulating layer.
2. The method according to claim 1, characterized in that, The substrate in step S1 is glass or flexible PET, and the patterned electrode is ITO or FTO.
3. The method according to claim 1, characterized in that, The cleaning process in step S1 specifically involves ultrasonic cleaning with cleaning solution, deionized water, acetone, and isopropanol in sequence, followed by oxygen plasma surface treatment using a plasma cleaner.
4. The method according to claim 1, characterized in that, The specific method for preparing the double perovskite microcrystalline layer in step S2 is as follows: prepare a saturated solution of dimethyl sulfoxide (DMSO) for the double perovskite precursor, take 30 μL and drop it onto the substrate, place the substrate in a sealed container containing the anti-solvent, and let it stand for 10 h to allow the microcrystals to precipitate.
5. The method according to claim 4, characterized in that, The antisolvent is isopropanol, and the concentration of the precursor saturated solution is 0.1 M.
6. The method according to claim 1, characterized in that, The insulating layer in step S3 is PEO or PMMA, and the deposition method is to spin-coat a chlorobenzene solution of the insulating polymer onto the double perovskite microcrystalline layer.
7. The method according to claim 6, characterized in that, The concentration of the chlorobenzene solution was 10–100 mg / mL, the spin-coating speed was 3000 rpm, and the spin-coating time was 30 s.
8. The method according to claim 1, characterized in that, Step S4 specifically involves: depositing a metal electrode using thermal evaporation, with a vacuum level of not less than 3 × 10⁻⁶. -4 Pa, evaporation rate of 1–3 Å / s, deposition thickness of 50–100 nm.
9. The method according to claim 1, characterized in that, The metal electrode mentioned in step S4 is Al, Ag, Au or Cu.
10. The application of the double perovskite MIS structure electroluminescent device prepared by the method of any one of claims 1 to 9 in single-component electrically driven broadband white light emission.