A hybrid quantum chip fabrication method and a hybrid quantum chip
By employing grayscale lithography and reverse bonding technology in high-order harmonic bulk acoustic resonators, the problem of insufficient control capability of three-dimensional acoustic structures was solved, and the consistency and coherence performance between devices were improved.
Patent Information
- Application Number
- CN202611302581.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-26
- Publication Date
- 2026-11-17
AI Technical Summary
Existing technologies struggle to achieve deterministic control of the three-dimensional acoustic structure of high-harmonic bulk acoustic resonators (HBARs), resulting in poor consistency between devices in large-scale fabrication scenarios.
A dome mechanical oscillator was fabricated on a first substrate using grayscale photolithography, and a superconducting quantum bit was fabricated on a second substrate. The hybrid quantum chip was integrated by inverted pressing. By combining grayscale photolithography and superconducting quantum bits to be fabricated on different substrates, the controllability of the three-dimensional profile and the consistency between devices were improved.
The use of grayscale lithography enables programmable and customized control of three-dimensional acoustic structures, improving the consistency between devices and the coherence performance of HBAR in large-scale fabrication scenarios, while reducing diffraction loss.
Smart Images

Figure CN123124666A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of quantum chip technology, and more particularly to a hybrid quantum chip fabrication method and a hybrid quantum chip. Background Technology
[0002] High-overtone bulk acoustic resonators (HBARs) have become a highly attractive research platform in the field of multimode quantum acoustics due to their extremely high mechanical quality factor, gigahertz-level operating frequency, dense acoustic mode spectrum, and good compatibility with superconducting quantum circuits.
[0003] Among them, high-order harmonic bulk acoustic resonators with three-dimensional acoustic structures, based on their large effective mass and three-dimensional geometric constraints, can confine numerous high-frequency, high-quality mechanical vibration modes within a small space. By coupling the fabricated three-dimensional acoustic structure with nonlinear elements such as superconducting qubits, these dense acoustic modes can be precisely excited, manipulated, and achieve direct interactions between modes. However, current traditional photolithography technology is mainly optimized for planar patterning processes, and its ability to control continuously changing surface contours is very limited. This results in a limitation on the deterministic control of the three-dimensional contours during fabrication, making it difficult to meet the consistency requirements between devices in large-scale fabrication scenarios.
[0004] Therefore, existing technologies still need to be improved and developed. Summary of the Invention
[0005] In view of the shortcomings of the prior art, the purpose of this invention is to provide a hybrid quantum chip fabrication method and a hybrid quantum chip, so as to solve the problems of low deterministic control capability in the fabrication of three-dimensional acoustic structures by existing high-order harmonic bulk acoustic resonators and poor consistency between devices in large-scale fabrication scenarios.
[0006] The technical solution of the present invention is as follows: This invention provides a method for fabricating a hybrid quantum chip, the steps of which include: A dome mechanical oscillator was fabricated on a first substrate using grayscale photolithography. A film is obtained by fabricating peripheral circuitry around the dome-shaped mechanical oscillator on a first substrate. Superconducting qubits are fabricated on a second substrate to obtain a top plate; The top sheet is flipped and pressed onto the bottom sheet to prepare a hybrid quantum chip.
[0007] In a further embodiment of the present invention, a plurality of dome mechanical oscillators are disposed on the first substrate, and a plurality of superconducting qubits are disposed on the second substrate; the dome mechanical oscillators on the first substrate are capacitively coupled to the corresponding superconducting qubits, and the plurality of superconducting qubits are coupled and connected to each other through an adjustable coupler or capacitive coupling.
[0008] A further provision of the present invention includes the step of fabricating the dome mechanical oscillator on the first substrate using grayscale photolithography, comprising: The first substrate is a silicon substrate, and an aluminum nitride layer is prepared by magnetron sputtering on the silicon substrate. Photoresist is applied to the aluminum nitride layer; Design the target dome shape, convert the image grayscale value according to the target dome shape, and obtain the exposure intensity based on the image grayscale value; Exposure is performed on the photoresist according to the exposure intensity to obtain a dome photoresist structure; The aluminum nitride layer is etched using the aforementioned dome photoresist structure to obtain the dome structure; A silicon dioxide mask was prepared by chemical reaction vapor deposition on top of the dome structure; The aluminum nitride layer on the first substrate is etched and cleaned to obtain a dome mechanical oscillator.
[0009] In a further embodiment of the present invention, the steps of designing a target dome shape, converting image grayscale values based on the target dome shape, and obtaining exposure intensity based on the image grayscale values include: Design a target dome shape with a cross-sectional radius of r, and the radius of the target dome shape is R; The target dome shape is read, and the target dome shape is divided into several position coordinates according to the cross section. The photoresist thickness of each position coordinate in the target dome shape is read. The photoresist thickness at the given location coordinates is correlated with the grayscale value to obtain the exposure grayscale value at the given location coordinates. The exposure intensity corresponding to the position coordinate is obtained based on the exposure grayscale value, and the exposure grayscale value and the corresponding exposure intensity of each position coordinate are written into the exposure file.
[0010] A further provision of the present invention, after the steps of converting the exposure intensity of the position coordinates according to the exposure grayscale value and writing the exposure intensity of each position coordinate into an exposure file, wherein the exposure file includes the exposure intensity and exposure grayscale value of each position coordinate, further includes: Write the minimum coordinate unit of each position coordinate and the corresponding exposure size into the exposure file.
[0011] In a further embodiment of the present invention, the step of etching and cleaning the aluminum nitride layer on the first substrate to obtain the dome mechanical oscillator includes: Photoresist is applied to a silicon dioxide mask above the dome structure; The silicon dioxide mask is etched to remove the silicon dioxide mask at the locations where no photoresist is applied; Wet etching is performed on the aluminum nitride layer to remove the aluminum nitride layer at locations where no silicon dioxide mask is applied; The photoresist and silicon dioxide mask above the dome structure are cleaned sequentially to prepare the dome mechanical oscillator.
[0012] A further provision of the present invention includes, prior to the step of pressing the top sheet upside down onto the bottom sheet to prepare the hybrid quantum chip, the following: Photoresist is applied around the dome mechanical oscillator on the film, and the support structure is obtained through photolithography. Apply adhesive to the side of the support structure away from the dome mechanical oscillator.
[0013] In a further embodiment of the present invention, the step of fabricating superconducting qubits on the second substrate to obtain the top plate includes: A tantalum film is deposited on the upper surface of the second substrate, which is a sapphire substrate; The tantalum film is etched until the second substrate underneath is exposed, forming an insulating underlayer structure and an underlayer capacitor; Two layers of electron beam resist are sequentially disposed on the insulating underlayer structure to form a double-layer adhesive structure; Electron beam direct writing exposure was used on the double-layer adhesive structure to obtain the suspended bridge structure; The suspension bridge structure is tilted, and a single layer of aluminum film is deposited by vapor deposition from one side of the suspension bridge structure towards the bottom of the suspension bridge structure. The single-layer aluminum film is oxidized in situ to form an oxide layer on top of the single-layer aluminum film; A top aluminum film is vertically vapor-deposited, and the top aluminum film is disposed on the upper surface of the oxide layer to form a Josephson junction; A conductive connection layer is fabricated around the Josephson junction on the second substrate. The conductive connection layer is electrically connected to the Josephson junction and the underlying capacitor to form a superconducting quantum bit, thus obtaining the top plate.
[0014] In a further embodiment of the present invention, the step of fabricating a conductive connection layer around the Josephson junction on the second substrate, wherein the conductive connection layer is electrically connected to the Josephson junction to obtain the top sheet includes: An aluminum film is deposited around the Josephson junction; Photoresist is applied over the aluminum film to perform photolithography on the interconnect layer lines; The photoresist is etched to obtain a connection layer, which is used to connect the tantalum film and the Josephson junction to form a superconducting quantum bit, thus obtaining the top sheet.
[0015] Based on the same inventive concept, the present invention provides a hybrid quantum chip, wherein the hybrid quantum chip is prepared using the hybrid quantum chip fabrication method described above, comprising: Film, on which a dome mechanical oscillator is provided; A top plate, on which superconducting qubits are disposed, is pressed upside down onto the bottom plate.
[0016] This invention provides a hybrid quantum chip fabrication method and a hybrid quantum chip. The hybrid quantum chip fabrication method includes the following steps: fabricating a dome mechanical oscillator on a first substrate using grayscale photolithography; fabricating peripheral circuitry around the dome mechanical oscillator on the first substrate to obtain a substrate; fabricating superconducting qubits on a second substrate to obtain a top plate; and flip-chip bonding the top plate onto the substrate to fabricate the hybrid quantum chip. This invention discloses a hybrid quantum chip fabrication method based on grayscale photolithography, in which acoustic structures and superconducting qubits 1200 are fabricated on different substrates using grayscale photolithography, and then integrated by flip-chip bonding. This allows for the fabrication of a three-dimensional dome mechanical oscillator using grayscale photolithography, improving the deterministic controllability of the three-dimensional contour and enhancing the consistency between devices in large-scale fabrication scenarios. Attached Figure Description
[0017] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on the structures shown in these drawings without creative effort.
[0018] Figure 1 This is a schematic diagram of the steps in the hybrid quantum chip fabrication method of the present invention.
[0019] Figure 2 This is a schematic diagram of the manufacturing process of the dome mechanical oscillator in this invention.
[0020] Figure 3 This is a schematic diagram of the process for preparing the peripheral circuit of the oscillator in this invention.
[0021] Figure 4 This is a schematic diagram of the fabrication process of superconducting qubits in this invention.
[0022] Figure 5This is a schematic diagram of the process for preparing the conductive connection layer in this invention.
[0023] Figure 6 (a) is a schematic diagram of the structure of the first substrate in this invention. Figure 6 (b) is a schematic diagram of the target dome shape in grayscale lithography of the present invention. Figure 6 (c) is a schematic diagram of the dome mechanical oscillator after grayscale photolithography.
[0024] Figure 7 This is a schematic diagram of the parameters of the target dome shape of the present invention.
[0025] Figure 8 This is a grayscale schematic diagram of the target dome shape of the present invention.
[0026] Figure 9 This is a height curve of the dome mechanical oscillator in this invention.
[0027] Figure 10 This is an atomic force microscope schematic diagram of the wet-etched silicon substrate, the dry-etched silicon substrate, and the dry-etched region at the center of the HBAR in this invention.
[0028] Figure 11 This is a schematic diagram of phonon relaxation time in this invention.
[0029] Figure 12 This is a schematic diagram of the coherence time parameters in this invention; Figure 13 This is a schematic diagram of the structure of the qubits and the peripheral circuitry of the oscillator on the first substrate.
[0030] The labels in the attached figures are as follows: 1. Film; 2. Top film; 100. First substrate; 210. Aluminum film; 220. Tantalum film; 300. Photoresist; 301. Dome photoresist structure; 302. Support structure; 400. Second substrate; 500. Adhesive; 600. Aluminum nitride layer; 601. Dome structure; 602. Dome mechanical oscillator; 700. Silicon dioxide mask; 810. Upper electron beam resist; 820. Lower electron beam resist; 900. Josephson junction; 1000. Connecting layer; 1100. Oscillator peripheral circuit; 1101. Cross-line structure; 1102. Z control line; 1103. XY control line; 1104. Readout line; 1200. Superconducting quantum bit. Detailed Implementation
[0031] This invention provides a method for fabricating a hybrid quantum chip and a hybrid quantum chip. To make the objectives, technical solutions, and effects of this invention clearer and more explicit, the invention will be further described in detail below with reference to the accompanying drawings and examples. It should be understood that the specific embodiments described herein are merely illustrative of the invention and are not intended to limit the invention.
[0032] In the implementation methods and claims, unless otherwise specified in the text, the terms "a," "an," "the," and "the" may also include plural forms. If the embodiments of the present invention involve descriptions of "first," "second," etc., such descriptions are for descriptive purposes only and should not be construed as indicating or implying their relative importance or implicitly specifying the number of indicated technical features. Therefore, a feature defined with "first" or "second" may explicitly or implicitly include at least one of those features.
[0033] It should be further understood that the term "comprising" as used in this specification means the presence of the stated features, integers, steps, operations, elements, and / or components, but does not exclude the presence or addition of one or more other features, integers, steps, operations, elements, components, and / or groups thereof. It should be understood that when we say an element is "connected" or "coupled" to another element, it can be directly connected or coupled to the other element, or there may be intermediate elements. Furthermore, "connected" or "coupled" as used herein can include wireless connections or wireless coupling. The term "and / or" as used herein includes all or any unit and all combinations of one or more associated listed items.
[0034] It will be understood by those skilled in the art that, unless otherwise defined, all terms used herein (including technical and scientific terms) have the same meaning as commonly understood by one of ordinary skill in the art to which this invention pertains. It should also be understood that terms such as those defined in general dictionaries should be understood to have the same meaning as in the context of the prior art, and should not be interpreted in an idealized or overly formal sense unless specifically defined as herein.
[0035] Furthermore, the technical solutions of the various embodiments can be combined with each other, but only if they are feasible for those skilled in the art. If the combination of technical solutions is contradictory or cannot be implemented, it should be considered that such combination of technical solutions does not exist and is not within the scope of protection claimed by this invention.
[0036] Phonons, as crucial mediators of interactions between heat, electricity, and light, have wide applications in thermal management, materials science, and quantum information processing. Optical and electromechanical systems based on multi-mechanical modes not only hold significant promise for quantum storage and quantum conversion but also serve as ideal platforms for studying physical phenomena such as quantum entanglement, multimode phonon lasing, and non-reciprocal photon (phonon) transport. High-harmonic bulk acoustic resonators (HBARs) are multimode, wide-spectrum radio frequency micromechanical resonators developed from traditional bulk acoustic resonators. They possess relatively long coherence times and can function as both superconducting qubits and resonant cavities for different quantum models. With their extremely high mechanical quality factor, gigahertz-level operating frequency, dense acoustic mode spectrum, and good compatibility with superconducting quantum circuits, they have become a highly attractive research platform in the field of multimode quantum acoustics. The presence of numerous manipulable phonon modes in HBARs provides a unique opportunity for the encoding, storage, and processing of quantum information within the acoustic domain. In recent years, experimental demonstrations of coherent interactions between superconducting qubits and phonons, as well as breakthroughs in multimode phonon manipulation techniques, have further solidified HBAR's important position as a core building block for future phonon-based quantum technologies.
[0037] However, the inventors' research revealed that the large-scale development of HBAR-based quantum systems is still limited by the lack of fabrication processes that enable the engineering of three-dimensional acoustic structures. Traditional HBARs are typically fabricated using planar multilayer structures, and their acoustic confinement effect is mainly determined by the thickness and material properties of the piezoelectric layer. Although these devices have supported many groundbreaking experiments, the limited geometric design freedom severely restricts further optimization of acoustic mode confinement, suppression of diffraction losses, and precise control of various stray parasitic modes. Therefore, developing large-scale fabrication techniques that enable the engineering control of three-dimensional acoustic structures is the core key to propelling HBAR platforms towards large-scale quantum information processing.
[0038] However, the three-dimensional microfabrication technology for piezoelectric materials still faces many challenges. Traditional photolithography technology is mainly optimized for planar patterning processes, and its ability to control continuously changing surface contours is very limited. To overcome this technical bottleneck, researchers have explored a variety of solutions, including solvent vapor reflow technology: this technology first completes the initial patterning of the photoresist, and then reshapes the initial photoresist structure into a dome-like shape through thermally induced or solvent-induced polymer reflow. Although solvent vapor reflow technology provides a simple path for fabricating three-dimensional curved structures, its final geometry is determined by a complex reflow dynamic process, involving multiple factors such as solvent diffusion, surface tension, and photoresist material properties. These variables can cause random deviations in the curvature of the final structure, thus limiting the deterministic control of the three-dimensional contour, and making it particularly difficult to meet the consistency requirements between devices in large-scale fabrication scenarios.
[0039] To solve the technical problems existing in the current technology, such as Figure 1 , Figure 4 and Figure 5 As shown, the present invention provides a hybrid quantum chip fabrication method, the steps of which include: S100. A dome mechanical oscillator 602 is fabricated on the first substrate 100 using grayscale photolithography. In this invention, a dome-shaped mechanical oscillator 602 is fabricated using grayscale photolithography. The dome-shaped mechanical oscillator 602 is a high-harmonic volume acoustic resonator (HBAR). Optionally, the dome-shaped mechanical oscillator 602 adopts a spherical structure, which can improve the coherence performance of the HBAR and reduce diffraction loss. It can also adopt a hierarchical structure, a polygonal structure, or other existing resonator structures, which will not be elaborated here. Specifically, this invention uses grayscale photolithography to fabricate a film 1 structure on a first substrate 100. By precisely modulating the exposure dose in the spatial domain, the fabrication of a three-dimensional microstructure can be directly achieved. The grayscale exposure process enables programmable and customized control of the acoustic three-dimensional structure.
[0040] S200: A peripheral circuit 1100 is fabricated around the dome mechanical oscillator 602 on the first substrate 100 to obtain a film 1; A peripheral circuit 1100 is fabricated around the dome mechanical oscillator 602 on a first substrate 100. The peripheral circuit 1100 is used to input control signals that can be used to control quantum computing to the dome mechanical oscillator 602. For example, it includes at least one XY control signal and one Z control signal, which constitute the transmission line of the bottom layer for realizing the electrical excitation and readout of acoustic modes and the suppression of spurious modes, thus obtaining the substrate 1.
[0041] S300, superconducting qubits 1200 are fabricated on the second substrate to obtain top plate 2; Subsequently, a superconducting qubit 1200 with a top sheet 2 structure is fabricated on the second substrate 400. The superconducting qubit 1200 serves as the core unit of the quantum computer, utilizing the quantum effects of superconducting materials to achieve quantum superposition and entanglement, and realizing quantum gate operations through microwave pulses to achieve quantum information processing.
[0042] S400: Press the top sheet 2 upside down onto the bottom sheet 1 to prepare a hybrid quantum chip.
[0043] The top plate 2 is flip-pressed onto the bottom plate 1, so that the superconducting quantum bits 1200 on the top plate 2 and the acoustic resonators, i.e., the dome mechanical oscillators, on the bottom plate 1 are spatially close to each other. An effective quantum state interaction channel is established through capacitive or inductive coupling, thus fabricating a hybrid quantum chip. In this embodiment, the acoustic structure and the superconducting quantum bits 1200 are fabricated on different substrates, and then integrated by flip-chip bonding to obtain a hybrid quantum chip. By introducing flip-chip packaging technology in the fabrication process, the decoherence time of HBAR and superconducting quantum bits 1200 are improved respectively. Optionally, a plurality of dome mechanical oscillators 602 are disposed on the first substrate 100, and a plurality of superconducting quantum bits 1200 are disposed on the second substrate 400; the dome mechanical oscillators 602 on the first substrate 100 are capacitively coupled to the corresponding superconducting quantum bits 1200, and the plurality of superconducting quantum bits 1200 are coupled together through an adjustable coupler, or any existing coupling structure is used for coupling. It should be noted that the number of dome mechanical oscillators 602 and the number of superconducting qubits 1200 can be set according to actual needs. There can be one or several, meaning the structure of the dome mechanical oscillators 602 and superconducting qubits 1200 inside the hybrid quantum chip is scalable. When the number of dome mechanical oscillators 602 and superconducting qubits 1200 is greater than or equal to 2, the number of dome mechanical oscillators 602 and the number of superconducting qubits 1200 are the same, meaning the superconducting qubits 1200 on the top plate 2 of the substrate 1 are correspondingly arranged with the dome mechanical oscillators 602 at the corresponding positions on the substrate 1.
[0044] In some preferred embodiments, the hybrid quantum chip fabrication method of the present invention can be performed after wafer fabrication, whereby one or more hybrid quantum chip architectures can be fabricated on the wafer as a substrate. Specifically, wafers of different materials are first selected as the first substrate 100 and the second substrate 400 of the hybrid quantum chip architecture. The first substrate includes several first substrates 100, and the second substrate includes several second substrates 400. Optionally, the first substrate can be made of silicon, that is, the first substrate 100 can be a silicon substrate, or it can be further made of double-polished silicon substrate. Correspondingly, the second substrate can be made of sapphire, and thus the second substrate 400 can be a sapphire substrate. During fabrication, several dome mechanical oscillators 602 and oscillator peripheral circuits 1100 can be fabricated simultaneously on several first substrates 100 of the first substrate to obtain several fabricated substrates 1. Then, superconducting qubits 1200 are fabricated simultaneously on several second substrates 400 of the second substrate to obtain several fabricated top substrates 2. Therefore, a single step of this fabrication method can be performed once, or it can be repeated multiple times at different locations on the wafer to expand and batch-produce multiple substrates 1 and top wafers 2. Then, the first and second substrates are diced, and the diced substrates 1 and top wafers 2 are assembled together to achieve mass production. That is, after the step of fabricating the superconducting quantum bit 1200 on the second substrate 400 and obtaining the top wafer 2, the method may further include: M100. The first substrate and the second substrate are cut to obtain a plurality of first bottom layers and a plurality of second top layers. The bottom layer is provided with the bottom film 1 and the second top layer is provided with the top film 2.
[0045] In this step, when the plurality of bottom films 1 on the first substrate and the plurality of top films 2 on the second substrate are prepared, the first substrate 100 between each top film 2 is kept in an integrated configuration, and the second substrate 400 between each bottom film 1 is kept in an integrated configuration. Before the top film 2 is flipped over, the first substrate and the second substrate are first wafer cut to cut the bottom film 1 on the first substrate and the top film 2 on the second substrate into small pieces and then cleaning is performed.
[0046] Please refer to the following: Figure 1 and Figure 2 In some preferred embodiments, the step of fabricating the dome mechanical oscillator 602 on the first substrate 100 using grayscale photolithography includes: S110. Set the first substrate 100 as a silicon substrate, and prepare an aluminum nitride layer 600 by magnetron sputtering on the silicon substrate. S120. Apply photoresist 300 onto the aluminum nitride layer 600; S130. Design the target dome shape, convert the image grayscale value according to the target dome shape, and obtain the exposure intensity according to the image grayscale value; S140. Expose the photoresist 300 according to the exposure intensity to obtain the dome photoresist structure 301. S150. The aluminum nitride layer 600 is etched through the dome photoresist structure 301 to obtain the dome structure 601. S160. A silicon dioxide mask 700 is prepared on top of the dome structure 601 by chemical reaction vapor deposition. S170. The aluminum nitride layer 600 on the first substrate 100 is etched and cleaned to obtain the dome mechanical oscillator 602.
[0047] Specifically, the substrate 1 includes a dome mechanical oscillator 602 (i.e., HBAR) and corresponding peripheral circuitry 1100 fabricated on the first substrate 100. The fabrication process of the dome mechanical oscillator 602 may specifically include: magnetron sputtering deposition of an aluminum nitride layer 600 on the first substrate 100. Optionally, the aluminum nitride layer 600 may have a thickness of 950 nm. The SEM morphology characterization of the aluminum nitride layer 600 is as follows: Figure 6 As shown in (a) of the diagram. To etch the dome structure 601, photoresist 300 is first applied to the aluminum nitride layer 600, and grayscale lithography is performed. Grayscale lithography maps the three-dimensional topography to a two-dimensional grayscale distribution, achieving precise spatial modulation of the exposure dose, allowing different exposure doses at different locations on the photoresist 300, thereby lithographically forming the dome photoresist structure 301. The aluminum nitride layer 600 is then etched using the dome photoresist structure 301. Optionally, the etching process of the photoresist 300 can employ dry etching, such as inductively coupled plasma (ICP) etching. After etching, the photoresist 300 has a geometric surface corresponding to the target dome structure 601, resulting in different thicknesses. It is then directly laser-written with grayscale exposure to form the dome shape. The three-dimensional contour of the photoresist 300 is defined by spatially modulating the exposure dose, and then the dome shape is transferred to the aluminum nitride layer 600 by subsequent etching. The resulting dome structure 601 can serve as the core structure of a high-order harmonic bulk acoustic resonator. Figure 6The image shown is a true microscopic representation of the dome structure. After inductively coupled plasma etching, directly using photoresist 300 as a mask for wet etching in phosphoric acid would result in severe lateral etching. Therefore, a chemically reactive silicon dioxide hard mask 700 is used to protect the patterned dome-shaped aluminum nitride region during subsequent wet etching. This silicon dioxide mask 700 exhibits excellent chemical stability in an 85% phosphoric acid environment, precisely protecting the three-dimensional dome structure outline of the pre-designed dome structure 601, while the exposed aluminum nitride around the dome structure 601 can be selectively removed. The aluminum nitride layer 600 at locations other than the dome structure on the first substrate 100 is etched, while the silicon dioxide mask 700 protects the pre-designed dome structure.
[0048] For further details regarding the present invention, please refer to the following: Figure 2 and Figure 7 The steps of designing the target dome shape, converting the image grayscale value according to the target dome shape, and obtaining the exposure intensity based on the image grayscale value include: S131. Design the target dome shape with a cross-sectional radius of r, and the radius of the target dome shape is R; S132. Read the target dome shape, divide the target dome shape into several position coordinates according to the cross section, and read the photoresist thickness of 300 mm in the position coordinates of the target dome shape respectively. S133. Correspond the thickness of the photoresist 300 at the position coordinates with the gray value to obtain the exposure gray value of the position coordinates; S134. Obtain the exposure intensity corresponding to the position coordinates based on the exposure grayscale value, and write the exposure grayscale value and the corresponding exposure intensity of each position coordinate into the exposure file.
[0049] The target dome shape can be considered as a part of a sphere with radius R. First, a dome structure 601 with a cross-sectional radius r is designed. Since the cross-sectional radius r is less than or equal to R, the height h between the sphere and the cross-section at a distance L from the center of the cross-section can be calculated based on r and R. For example, in this invention, the height H of the highest point of the central dome of the target dome shape is less than or equal to the sphere radius R. The height H of the highest point of the central dome can be calculated as follows: ; Therefore, the corresponding height h at a position with a distance L from the center of the cross-section is: ; Assuming the exposure dose is the same at different thicknesses of the photoresist (300mm), the exposure dose at each location can be set according to the thickness value. In practical applications, optionally, the exposure intensity of the laser direct writing can be mapped one-to-one with the grayscale value of the image of the designed target sphere shape, where the grayscale value has a variable range of 0-255. Using the highest point H as the maximum height, the grayscale value (gray) at each location can be calculated. ; The calculated grayscale value (gray) is between 0 and 255, allowing the determination of the corresponding exposure grayscale value based on the designed target dome shape. Subsequently, the exposure intensity corresponding to the position coordinates is obtained based on the exposure grayscale value. Specifically, the laser direct writing device has a pre-determined light intensity output range based on the device signal. It can directly correspond the exposure grayscale value at the corresponding coordinate position to the corresponding value within the laser direct writing device's light intensity output range. This correspondence can be set according to whether the photoresist 300 is selected as a positive or negative resist. The exposure grayscale value and corresponding exposure intensity for each position coordinate are written into the exposure file. The exposure file drives the laser direct writing device to expose the photoresist 300, resulting in a dome photoresist structure 301 with a shape consistent with the dome mechanical oscillator 602. The photolithography uses laser direct writing exposure, and the exposure intensity and designed grayscale value are matched during exposure file conversion. The optimal exposure dose is determined by adjusting the overall exposure power. The exposure file can be used in the hybrid quantum chip processing method. Assuming that the dosage of photoresist 300 is consistent at different thickness locations, in order to achieve as much uniformity as possible, the photoresist 300 is baked with a variable temperature gradient to obtain the dome mechanical oscillator 602.
[0050] Actual exposure images of the dome mechanical oscillator 602 are as follows: Figure 8 As shown, darker colors represent higher grayscale values and correspondingly greater thickness. The red dashed line at the center of the image represents the cross-sectional location. The cross-section from the dashed line is then scanned using a profilometer to obtain the 600mm thickness curves of the aluminum nitride layer at each location, as shown below. Figure 9 As shown, the surface is smooth, which meets the machining accuracy requirements of the 602 dome mechanical oscillator, also known as the HABR.
[0051] In a further embodiment of the preferred embodiment, after the steps of converting the exposure intensity of the position coordinates according to the exposure grayscale value and writing the exposure intensity of each position coordinate into an exposure file, wherein the exposure file includes the exposure intensity and exposure grayscale value of each position coordinate, the method further includes: S135. Write the minimum coordinate unit of each position coordinate and the corresponding exposure size into the exposure file.
[0052] In this step, because the grayscale exposure design is flexible and can be processed into various sizes according to the process, the exposure size and pattern resolution can be further synchronized during fabrication. Specifically, the smallest coordinate unit of the position coordinates defines the physical coordinate scale corresponding to each pixel in the grayscale image on the actual processing scale, to ensure the spatial positioning accuracy of the designed pattern at the micrometer or nanometer scale. The laser direct writing equipment can then perform exposure according to this process document, following the clearly defined spatial coordinate system and the smallest exposure unit, so that the three-dimensional contour information in the grayscale image is accurately reproduced on the surface of 300 layers of photoresist. By adjusting the exposure size parameters, this method can be adapted to the fabrication of devices with different design accuracy requirements, and can simultaneously meet the needs of rapid fabrication of large-size resonant structures and the requirements of high-precision microstructures for lateral resolution, thereby improving the applicability of grayscale photolithography.
[0053] Furthermore, referring to Figure 2 The step of etching and cleaning the aluminum nitride layer 600 on the first substrate 100 to obtain the dome mechanical oscillator 602 includes: S171. Photoresist 300 is applied to the silicon dioxide mask 700 above the dome structure 601. S172. Etch the silicon dioxide mask 700 to remove the silicon dioxide mask 700 at the location outside the dome structure where no photoresist 300 is provided. S173. Perform wet etching on the aluminum nitride layer 600 to remove the aluminum nitride layer 600 at the location outside the dome structure where no photoresist 300 and silicon dioxide mask 700 are provided. S174. The photoresist 300 and the silicon dioxide mask 700 above the dome structure 601 are cleaned sequentially to prepare the dome mechanical oscillator 602.
[0054] In this process, directly using photoresist 300 as a mask for wet etching in phosphoric acid would result in severe lateral etching. Therefore, the silicon dioxide mask 700, due to its excellent chemical stability in an 85% phosphoric acid environment, is used to protect the dome mechanical oscillator 602 in the aluminum nitride layer 600 during wet etching, while removing the aluminum nitride layer 600 at other locations. To this end, photoresist 300 is first applied to the silicon dioxide mask 700 above the dome structure 601, thus preserving the silicon dioxide mask 700 of the dome structure 601 below the photoresist 300 during etching, while removing the silicon dioxide mask 700 at locations where no photoresist 300 is applied. After removing the photoresist 300 at other locations, wet etching is performed on the aluminum nitride layer 600 at each location. Optionally, a hot phosphoric acid wet etching process at 100℃ is used for wet etching, which can achieve large-area removal of aluminum nitride, thereby avoiding the damage caused by dry etching and avoiding the surface performance degradation and roughness increase problems caused by long-term plasma etching. This invention combines dry and wet etching. Dry etching precisely replicates the three-dimensional geometry of the designed target dome shape, while wet etching further reduces surface roughness and eliminates the damaged areas generated during dry etching, resulting in the dome mechanical oscillator 602. By combining local dry etching with selective wet etching, this process can achieve high-fidelity transfer of the grayscale-defined dome contour while maintaining the smoothness of the substrate surface, achieving complementary advantages of dry and wet etching processes. After dry and wet etching, the surface at different locations... Figure 10 As shown, Figure 10 From left to right, the images show surface atomic force microscopy (AFM) images of a wet-etched silicon substrate, a dry-etched silicon substrate, and the center of a dry-etched HBAR. As can be seen, the surface roughness of the wet-etched silicon substrate is only 0.7 nm, while that of the dry-etched substrate reaches 14.6 nm. This invention obtains the HBAR structure of the dome mechanical oscillator 602 through dry etching and processes other locations on the hybrid quantum chip through wet etching, thus ensuring the flatness of other locations on the hybrid quantum chip besides the dome mechanical oscillator 602.
[0055] After completing the fabrication of the dome mechanical oscillator 602 in the previous step, please refer to the following: Figure 3 and Figure 13 The step of fabricating the peripheral circuitry 1100 of the oscillator 602 on the first substrate 100 to obtain the film 1 includes: S210, deposit an aluminum film 210 on the first substrate 100; S220. The filter is photolithographically and etched to obtain the oscillator peripheral circuit 1100; S230. A crossover structure is fabricated above the conventional transmission line using a liftoff process.
[0056] Specifically, the fabrication of the oscillator peripheral circuit 1100 first involves electron beam evaporation of a 100nm aluminum film 210 on the first substrate 100. Subsequently, the underlying circuitry is processed by photolithography etching. Photoresist 300 is applied over the aluminum film 210, and patterns of the circuit insulation lines and the positions of the dome mechanical oscillator 602 are photolithographically etched. The insulating structure of the underlying first substrate 100 is etched onto the aluminum film 210, and the aluminum film 210 covering the dome mechanical oscillator 602 is removed, resulting in the oscillator peripheral circuit 1100. Specifically, the oscillator peripheral circuit 1100 is used to feed in the excitation signal to the dome mechanical oscillator 602 and to read out the state of the superconducting quantum bit 1200. Specifically, the oscillator peripheral circuit 1100 includes a Z control line 1102, an XY control line 1103, and a readout line 1104 for the superconducting quantum bit 1200. The Z control line 1102 is inductively coupled to the superconducting quantum bit 1200 to adjust its frequency. The XY control line 1103 is capacitively coupled to the superconducting quantum bit 1200 to excite it. The readout line 1104 is capacitively coupled to the superconducting quantum bit 1200 to read its state. Subsequently, this embodiment further employs a stripping process to sequentially fabricate a cross-line structure 1101 connecting a 200nm silicon oxide structure and a 300nm aluminum film 210. This cross-line structure 1101 is connected above the X transmission line to connect the aluminum film 210 regions on both sides of the X transmission line, thereby reducing crosstalk and other mode interference, and reducing capacitive crosstalk and stray coupling between transmission lines.
[0057] Furthermore, such as Figure 4 As shown, the step of fabricating superconducting qubits 1200 on the second substrate to obtain top plate 2 includes: S310. A tantalum film 220 is deposited on the upper surface of the second substrate 400, wherein the second substrate 400 is a sapphire substrate. S320: Etch the tantalum film 220 until the second substrate 400 below is exposed to form an insulating underlayer structure and an underlayer capacitor; S330. Two layers of electron beam resist are sequentially disposed on the insulating underlayer structure to form a double-layer adhesive structure. S340. Electron beam direct writing exposure is used on the double-layer adhesive structure to obtain the suspended bridge structure; S350, Incline the suspension bridge structure, and deposit a single layer of aluminum film 210 from one side of the suspension bridge structure downwards. S360. The single-layer aluminum film 210 is oxidized in situ to form an oxide layer on the single-layer aluminum film 210. S370, Vertically evaporated upper aluminum film 210, the upper aluminum film 210 is disposed on the upper surface of the oxide layer to form Josephson junction 900; S380. A conductive connection layer is prepared around the Josephson junction on the second substrate. The conductive connection layer is electrically connected to the Josephson junction and the bottom capacitor to form a superconducting quantum bit 1200, thus obtaining the top plate.
[0058] Specifically, the superconducting quantum bit 1200 of the top chip 2 includes a bottom capacitor formed after tantalum film etching, a Josephson junction, and a conductive interconnect layer disposed above the Josephson junction. The superconducting quantum bit 1200, through the Josephson effect generated when the Josephson junction 900 is operating, enables the superconducting quantum circuit to possess macroscopically observable quantum properties, providing a tunable energy level structure for frequency-matched coupling with different acoustic modes. A conductive interconnect layer 1000 is fabricated around the Josephson junction 900 on the second substrate 400. This conductive interconnect layer 1000 is electrically connected to the Josephson junction 900 to connect the junction to an external electrode or ground plane, ensuring the transmission and bias control of the bit electrical signal, thereby obtaining the top chip 2.
[0059] In this embodiment, firstly, a 100nm tantalum film 220 is deposited on the upper surface of the second substrate 400. The second substrate 400 can be a sapphire substrate, which has the characteristics of low microwave loss and high thermal conductivity, making it suitable as a substrate for the fabrication of superconducting qubits 1200. Photoresist 300 is coated on top of the tantalum film 220, and a bottom layer structure pattern is photolithographically formed. Then, the tantalum film 220 is etched until the underlying sapphire substrate is exposed, forming an insulating bottom layer structure. This etching process removes excess tantalum from the insulating bottom layer structure, leaving an insulating space for the subsequent fabrication of the Josephson junction 900, achieving electrical isolation. Simultaneously, the positions of the tantalum film relative to the insulating space in the horizontal direction can be equivalent to the existence of a bottom layer capacitor, used to determine the energy level structure of the superconducting qubit. It can also be used for coupling, controlling coherence time, and reducing charge noise. Its specific functions can be set according to the relative positions, connection relationships, and equivalent circuit changes between the capacitor and the Josephson junction, which will not be elaborated here. Two layers of electron beam resist are sequentially disposed above the insulating substrate to form a double-layer adhesive structure. This double-layer adhesive structure is composed of two electron beam resists with different dissolution rates stacked together. For example, the upper electron beam resist 810 can be PMMA (Polymethyl Methacrylate) with a dosage of 1500 μC / cm², and the lower electron beam resist 820 can be MMA (Methyl Methacrylate) with a dosage of 250 μC / cm². The specific type and dosage of the electron beam resist selected are related to the specific equipment used, and will not be elaborated here.
[0060] During the development process, the lower etchant has a faster dissolution rate than the upper electron beam resist 810, thus forming a suspended space below the exposure area. This allows for the creation of a suspended bridge structure through direct electron beam writing exposure on the double-layer resist structure. A dual-tilt evaporation system is then used on the suspended bridge structure to deposit a single layer of aluminum film 210 at an angle downwards from either side of the suspended bridge, specifically as follows... Figure 4As indicated by the gray arrows on both sides, tilted evaporation allows aluminum atoms to pass through the suspended bridge region from either side at a certain angle and deposit at specific locations on the substrate surface, forming a submicron-scale junction region. After tilted evaporation, the monolayer aluminum film 210 is oxidized in situ, forming an oxide layer on top of the monolayer aluminum film 210. This oxide layer can be considered equivalent to an extremely thin non-superconducting layer, and its thickness directly determines the intensity of the Josephson effect. After completion, an upper aluminum film 210 is deposited vertically below the suspended bridge structure and placed on the upper surface of the oxide layer, thereby sandwiching the oxide layer between the monolayer aluminum film 210 and the upper aluminum film 210 to form a superconducting-insulating-superconducting hierarchical structure, completing the fabrication of the Josephson junction 900. The fabricated Josephson junction 900 has a thickness of 100 to 200 nanometers and is fabricated using a dual-junction process, enabling wide-range frequency tuning, thus achieving coupling control and characteristic characterization of different HBAR acoustic modes.
[0061] Further reading Figure 4 The step of fabricating a conductive connection layer 1000 around the Josephson junction 900 on the second substrate 400, wherein the conductive connection layer 1000 is electrically connected to the Josephson junction 900 to form a superconducting quantum bit 1200, and obtaining the top plate 2 includes: S381. An aluminum film 210 is deposited around the Josephson junction 900; S382. Photoresist 300 is applied above the aluminum film 210 to perform photolithography on the lines of the interconnect layer 1000. S383. The photoresist 300 is etched to obtain a connecting layer 1000. The connecting layer 1000 is used to connect the tantalum film 220 and the Josephson junction 900 to form a superconducting quantum bit 1200, thus obtaining the top sheet.
[0062] Specifically, an aluminum film 210 is deposited around the fabricated Josephson junction 900. This aluminum film 210 serves as the conductive material for the interconnect layer 1000, providing a conductive path for the electrical interconnection between the Josephson junction 900 and the underlying tantalum film 220 electrode. A photoresist 300 is applied over the aluminum film 210, and the interconnect layer 1000 lines are photolithographically patterned. The pre-defined interconnect layer 1000 pattern is transferred onto the photoresist 300 through exposure and development. In subsequent etching, only the aluminum film 210 at the interconnect layer 1000 locations is retained, while the aluminum film 210 in other areas is removed. After etching the photoresist 300, the interconnect layer 1000 is obtained. The interconnect layer 1000 is electrically contacted with both the tantalum film 220 and the Josephson junction 900, thereby enabling the Josephson junction 900 to form a circuit with the underlying tantalum film 220 electrode through the interconnect layer 1000, realizing the application of external signals and the electrical reading of bit states.
[0063] In some preferred embodiments, such as Figure 5As shown, before the step of pressing the top sheet 2 upside down onto the bottom sheet 1 to prepare the hybrid quantum chip, the method further includes: N100, Photoresist 300 is applied around the dome mechanical oscillator 602 of the film 1, and the support structure 302 is obtained by photolithography; N200, apply adhesive 500 to the side of the support structure 302 away from the dome mechanical oscillator 602.
[0064] In this preferred embodiment, photoresist 300 is first applied around the dome mechanical oscillator 602 of the substrate 1, and a support structure 302 is obtained through photolithography. The support structure 302 can be a support column, support plate, support grid, or any other support structure 302 that can be used to support the flip-chip top plate 2. The height of the support structure 302 is determined by the thickness of the photoresist 300. During lamination, it acts as a rigid spacer between the top plate 2 and the substrate 1, limiting the position of the top plate 2 and thus precisely controlling the relative distance between them, preventing damage to the dome mechanical oscillator 602 or the superconducting quantum bit 1200 structure due to downward pressure. Optionally, the height of the support structure 302 can be 2 micrometers. Adhesive 500 is applied to the side of the support structure 302 away from the dome mechanical oscillator 602. The adhesive 500 can be applied to the aluminum film 210 on the outside of the support structure 302, or to the interface between the top surface of the support structure 302 and the bottom surface of the top plate 2. During the pressing process, it is used to fix the top plate 2 and the bottom plate 1 after they are upside down and aligned, so that the top plate 2 and the bottom plate 1 always remain in contact, avoiding displacement deviation from affecting the performance of the device.
[0065] In summary, this invention discloses a hybrid quantum chip fabrication method. The hybrid quantum chip prepared by this method has a dome mechanical oscillator 602 (HBAR device). The dome mechanical oscillator 602 possesses a well-defined dome structure and excellent mechanical coherence characteristics, with significantly improved three-dimensional profile control. To verify the performance of the prepared hybrid quantum chip, the interaction between the superconducting quantum bit 1200 and the phonon was tested at a temperature of 20 mK using a dilution refrigerator. The phonon relaxation time T1 and coherence time parameter T2 extracted experimentally are as follows: Figure 11 and Figure 12 As shown, both T1 and T2 reach the order of hundreds of microseconds, which fully demonstrates the low-loss characteristics of the prepared acoustic structure and the effectiveness of the preparation process.
[0066] Based on the same inventive concept, this invention provides a hybrid quantum chip, which is fabricated using the hybrid quantum chip fabrication method described above. The chip includes: a substrate 1, on which a dome-shaped mechanical oscillator 602 is disposed; and a top plate 2, on which superconducting qubits 1200 are disposed. The top plate 2 is inverted and pressed onto the substrate 1. The specific details are as described in the embodiments of the hybrid quantum chip fabrication method above, and will not be repeated here.
[0067] This invention provides a method for fabricating a hybrid quantum chip and a hybrid quantum chip, the advantages of which are: Introducing grayscale exposure allows for more flexible changes to the design dimensions of samples, resulting in programmable three-dimensional profiles.
[0068] The combined process of localized dry etching and subsequent wet etching minimizes plasma-induced device damage while preserving a smooth silicon substrate surface, providing suitable conditions for integration with superconducting quantum circuits. Introducing a flip-chip packaging scheme allows for separate optimization of the HBAR structure of the 602 dome mechanical oscillator and the fabrication process of the 1200 superconducting qubits. This paves the way for the large-scale fabrication of customizable three-dimensional quantum acoustic resonators and establishes a universal fabrication framework that can integrate long-lived mechanical modes with superconducting quantum circuits. This scalable acoustic platform will provide core support for subsequent research and development in multimode phonon-based quantum information processing, quantum storage, and hybrid quantum architectures.
[0069] A hybrid quantum chip fabrication method based on grayscale lithography is disclosed. The acoustic structure, namely the dome mechanical oscillator, is fabricated on different substrates by grayscale lithography and superconducting qubits respectively. Then, it is integrated by flip-chip bonding. Thus, the fabrication of a three-dimensional dome mechanical oscillator is realized by grayscale lithography, which improves the deterministic control capability of the three-dimensional contour and enhances the consistency between devices in large-scale fabrication scenarios.
[0070] It should be understood that the application of the present invention is not limited to the examples above. Those skilled in the art can make improvements or modifications based on the above description, and all such improvements and modifications should fall within the protection scope of the appended claims.
Claims
1. A method for fabricating a hybrid quantum chip, characterized in that the steps include... include: A dome mechanical oscillator was fabricated on a first substrate using grayscale photolithography. A film is obtained by fabricating peripheral circuitry around the dome-shaped mechanical oscillator on a first substrate. Superconducting qubits are fabricated on a second substrate to obtain a top plate; The top sheet is flipped and pressed onto the bottom sheet to prepare a hybrid quantum chip.
2. The hybrid quantum chip fabrication method according to claim 1, characterized in that, The first substrate has a plurality of dome mechanical oscillators disposed thereon, and the second substrate has a plurality of superconducting qubits disposed thereon; the dome mechanical oscillators on the first substrate are capacitively coupled to the corresponding superconducting qubits, and the plurality of superconducting qubits are coupled to each other through an adjustable coupler or capacitively coupled.
3. The hybrid quantum chip fabrication method according to claim 1, characterized in that, The step of fabricating the dome mechanical oscillator on the first substrate using grayscale photolithography includes: The first substrate is a silicon substrate, and an aluminum nitride layer is prepared by magnetron sputtering on the silicon substrate. Photoresist is applied to the aluminum nitride layer; Design the target dome shape, convert the image grayscale value according to the target dome shape, and obtain the exposure intensity based on the image grayscale value; Exposure is performed on the photoresist according to the exposure intensity to obtain a dome photoresist structure; The aluminum nitride layer is etched using the aforementioned dome photoresist structure to obtain the dome structure; A silicon dioxide mask was prepared by chemical reaction vapor deposition on top of the dome structure; The aluminum nitride layer on the first substrate is etched and cleaned to obtain a dome mechanical oscillator.
4. The hybrid quantum chip fabrication method according to claim 3, characterized in that, The steps of designing the target dome shape, converting the image grayscale value according to the target dome shape, and obtaining the exposure intensity based on the image grayscale value include: Design a target dome shape with a cross-sectional radius of r, and the radius of the target dome shape is R; The target dome shape is read, and the target dome shape is divided into several position coordinates according to the cross section. The photoresist thickness of each position coordinate in the target dome shape is read. The photoresist thickness at the given location coordinates is correlated with the grayscale value to obtain the exposure grayscale value at the given location coordinates. The exposure intensity corresponding to the position coordinate is obtained based on the exposure grayscale value, and the exposure grayscale value and the corresponding exposure intensity of each position coordinate are written into the exposure file.
5. The hybrid quantum chip fabrication method according to claim 4, characterized in that, After the steps of converting the exposure intensity of the position coordinates based on the exposure grayscale value and writing the exposure intensity of each position coordinate into an exposure file, wherein the exposure file includes the exposure intensity and exposure grayscale value of each position coordinate, the method further includes: Write the minimum coordinate unit of each position coordinate and the corresponding exposure size into the exposure file.
6. The hybrid quantum chip fabrication method according to claim 3, characterized in that, The step of etching and cleaning the aluminum nitride layer on the first substrate to obtain the dome mechanical oscillator includes: Photoresist is applied to a silicon dioxide mask above the dome structure; The silicon dioxide mask is etched to remove the silicon dioxide mask at the locations where no photoresist is applied; Wet etching is performed on the aluminum nitride layer to remove the aluminum nitride layer at locations where no silicon dioxide mask is applied; The photoresist and silicon dioxide mask above the dome structure are cleaned sequentially to prepare the dome mechanical oscillator.
7. The hybrid quantum chip fabrication method according to claim 1, characterized in that, Before the step of pressing the top sheet upside down onto the bottom sheet to prepare the hybrid quantum chip, the method further includes: Photoresist is applied around the dome mechanical oscillator on the film, and the support structure is obtained through photolithography. Apply adhesive to the side of the support structure away from the dome mechanical oscillator.
8. The hybrid quantum chip fabrication method according to claim 1, characterized in that, The step of fabricating superconducting qubits on the second substrate to obtain the top plate includes: A tantalum film is deposited on the upper surface of the second substrate, which is a sapphire substrate; The tantalum film is etched until the second substrate underneath is exposed, forming an insulating underlayer structure and an underlayer capacitor; Two layers of electron beam resist are sequentially disposed on the insulating underlayer structure to form a double-layer adhesive structure; Electron beam direct writing exposure was used on the double-layer adhesive structure to obtain the suspended bridge structure; The suspension bridge structure is tilted, and a single layer of aluminum film is deposited by vapor deposition from one side of the suspension bridge structure towards the bottom of the suspension bridge structure. The single-layer aluminum film is oxidized in situ to form an oxide layer on top of the single-layer aluminum film; A top aluminum film is vertically vapor-deposited, and the top aluminum film is disposed on the upper surface of the oxide layer to form a Josephson junction; A conductive connection layer is fabricated around the Josephson junction on the second substrate. The conductive connection layer is electrically connected to the Josephson junction and the underlying capacitor to form a superconducting quantum bit, thus obtaining the top plate.
9. The hybrid quantum chip fabrication method according to claim 8, characterized in that, The step of fabricating a conductive connection layer around the Josephson junction on the second substrate, wherein the conductive connection layer is electrically connected to the Josephson junction to obtain the top sheet includes: An aluminum film is deposited around the Josephson junction; Photoresist is applied over the aluminum film to perform photolithography on the interconnect layer lines; The photoresist is etched to obtain a connection layer, which is used to connect the tantalum film and the Josephson junction to form a superconducting quantum bit, thus obtaining the top sheet.
10. A hybrid quantum chip, characterized in that, The hybrid quantum chip is prepared using the hybrid quantum chip fabrication method as described in any one of claims 1 to 9, comprising: Film, on which a dome mechanical oscillator is provided; A top plate, on which superconducting qubits are disposed, is pressed upside down onto the bottom plate.