Crucible device for preparing g-C3N4 coated composite material
By designing a crucible device with air holes and a layered structure, the problem of uneven coating of g-C3N4 was solved, efficient preparation of composite materials was achieved, and the uniformity and production efficiency of the coating layer were improved.
Patent Information
- Application Number
- CN202420113027.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-17
- Publication Date
- 2024-10-08
- Estimated Expiration
- 2034-01-17
AI Technical Summary
When the existing technology combines g-C3N4 with other materials, it is difficult to achieve uniform coating and flexibly control the coating thickness, which affects the performance of the product.
A crucible device including a crucible barrel, a barrel lid, a built-in container and a circular crucible plate is designed. By setting up air guide holes and a layered structure, uniform evaporation and deposition of g-C3N4 is achieved, and it is suitable for various coating conditions. Composite material preparation.
The uniform coating of g-C3N4 is achieved, which improves the uniformity and production efficiency of the coating layer, reduces the residue of uncoated materials, and enhances the performance of the composite material.
Smart Images

Figure CN221810404U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of preparing g-C3N4 coated composite materials, in particular to a crucible device for preparing g-C3N4 coated composite materials. Background Art
[0002] g-C3N4 (graphene carbon nitride) is a polymer semiconductor containing C and N atoms. It has the advantages of good optical properties, excellent chemical stability, good biocompatibility, and adjustable electronic structure. It has been widely used in many fields such as photocatalysis, saturated body absorption, bioimaging, environmental monitoring, chemical sensing, and solar cells. In addition, g-C3N4 is often used to compound with other materials to optimize and modify product performance or achieve multifunctional coupling. For example, compounding g-C3N4 with ZnO semiconductor can effectively improve the photoelectric performance and stability of ZnO (CN201610827566.0). For example, since g-C3N4 can produce sufficient reactive oxygen species to destroy tumor cells under ultraviolet and visible light irradiation, the integrated multifunctional coupling of photodynamic therapy, photothermal therapy and fluorescence imaging can be achieved by coating g-C3N4 on the NaGdF4:Yb / Tm@NaGdF4:Yb@NaNdF4:Yb core-shell nanoparticles (Chem. Mater. 2016, 28, 7935).
[0003] So far, the most commonly used method for composite coating of g-C3N4 with other materials (such as fluorescent materials, catalytic materials, etc.) is mainly the solid phase method. This method is to mix the pre-prepared g-C3N4 with the powder material to be coated, grind and stir, and keep it at 400-500℃ for a period of time to obtain the final product. Although the solid phase method has the advantage of simple process, it cannot achieve uniform coating of g-C3N4 on the surface of the powder. More importantly, a large amount of uncoated g-C3N4 is difficult to separate, which significantly affects the performance of the product.
[0004] Recently, g-C3N4 coating by physical vapor deposition has attracted people's attention. This method requires the preparation of a crucible with a built-in cylinder in advance, pouring a certain amount of melamine powder into the bottom of the crucible, and placing the powder to be coated on the top of the built-in cylinder of the crucible; after the crucible is covered and sealed, it is kept at 500-550℃ for a period of time, and the target product is obtained after cooling to room temperature with the furnace. This method effectively reduces the residue of uncoated g-C3N4 in the target product. However, due to the limitations of the crucible structure used, this vapor deposition method can only complete the preparation of powders with one coating condition at a time, and due to the simultaneous evaporation and decomposition of a large amount of melamine, the coating thickness and uniformity of g-C3N4 cannot be flexibly adjusted. Summary of the invention
[0005] In view of the deficiencies in the prior art, the utility model provides a corundum crucible device for preparing a g-C3N4 coated composite material by a physical vapor deposition method, which can realize the preparation of powders with multiple different coating conditions at one time and can control the evaporation amount of g-C3N4 during the deposition process, thereby helping to improve the uniformity and flexibility of the coating.
[0006] In order to achieve the above-mentioned purpose, the utility model adopts the following technical solutions:
[0007] A crucible device for preparing a g-C3N4 coated composite material, the crucible device comprising a crucible barrel, a barrel cover, a built-in container and a plurality of annular crucible plates;
[0008] Positioning blocks evenly distributed on the barrel wall at different heights inside the crucible barrel are circumferentially arranged, and the annular crucible plate is mounted on the positioning blocks;
[0009] The annular crucible plate is annular in shape, and the built-in container passes through the hollow of the annular crucible plate and is tightly attached to the side wall of the annular crucible plate; the built-in container, the crucible barrel and the annular crucible plate form a closed space as a deposition area;
[0010] The built-in container comprises a container wall and a container cover, but has no bottom cover. The built-in container and the solid crucible plate are combined to form a closed evaporation chamber; and air guide holes are arranged on the container wall.
[0011] Preferably, the built-in container is in the shape of an inverted frustum, and its outer diameter gradually decreases from top to bottom.
[0012] Preferably, a plurality of solid crucible plates are arranged in the built-in container, and the solid crucible plates divide the evaporation chamber into a plurality of evaporation chambers by layers. The solid crucible plates correspond to the annular crucible plates one by one and are flush in height.
[0013] Preferably, the ratio of the inner diameter of the crucible barrel to the outer diameter of the top of the built-in container is 2:1-5:3.
[0014] Preferably, the ratio of the inner diameters of the bottom and top of the built-in container is 2:3-3:4.
[0015] Preferably, the air guide hole extends obliquely from the inside of the built-in container to the outside, with an inclination angle of 20-45° and an inner diameter of 0.6-1.2 cm. Preferably, the air guide hole is best inclined downward from the inside of the built-in container to the outside; each air guide hole is at least 1.5-3.0 cm higher than the solid crucible plate of the corresponding evaporation chamber.
[0016] Preferably, each group of 6 to 10 air guide holes is composed of an air guide hole group, and the air guide holes in the air guide hole group are evenly distributed on the same circumference and are not connected; each layer of the evaporation chamber (33) is provided with a plurality of air guide hole groups (5); and the vertical distance between each group of upper and lower adjacent air guide hole groups is 0.5 to 0.8 cm.
[0017] Preferably, the positioning blocks are raised stoppers evenly distributed on the same circumference.
[0018] Preferably, a circular protrusion is provided on the inner side surface of the barrel cover, the diameter of the circular protrusion is matched with the inner diameter of the crucible barrel, and the circular protrusion can be movably embedded in the top of the crucible barrel.
[0019] Preferably, the crucible barrel, barrel cover, built-in container, annular crucible plate and solid crucible plate are made of corundum, and the centers of the crucible barrel, barrel cover and built-in container are on the same axis.
[0020] The beneficial effects of the utility model are:
[0021] 1) A built-in container with air guide holes is provided to allow the g-C3N4 gas to flow evenly from the evaporation chamber to the deposition area; and the flow rate of the g-C3N4 gas to the powder to be coated is slowed down, so that the g-C3N4 gas can be evenly deposited on the surface of the powder to be coated, solving the problem of uneven coating layer thickness;
[0022] 2) By layering the built-in container and the crucible barrel, a variety of composite materials with different coating conditions can be synthesized simultaneously, which significantly improves production efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 It is a structural schematic diagram of the crucible device.
[0024] Figure 2 This is a top view of the inside of the barrel cover.
[0025] Figure 3 Schematic diagram of air guide hole group and air guide hole.
[0026] Explanation of symbols in the figure: 1-crucible barrel; 2-barrel cover; 21-circular protrusion; 3-built-in container; 31-vessel wall; 32-vessel cover; 33-evaporation chamber; 4-circular crucible plate; 5-gas guide hole group; 51-gas guide hole; 6-positioning block; 7-solid crucible plate; 8-deposition area; 9-melamine; 10-powder to be coated. DETAILED DESCRIPTION
[0027] The following is a clear and complete description of the technical solutions in the embodiments of the utility model in conjunction with the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments of the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the protection scope of the utility model.
[0028] In the description of the present application, it should be understood that the terms "upper", "lower", "front", "back", "left", "right", "top", "bottom", "inside", "outside", etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.
[0029] A crucible device for preparing g-C3N4 coated composite materials by vapor deposition method, such as Figure 1 As shown, the original crucible device includes a crucible barrel 1, a barrel cover 2, a built-in container 3 and a plurality of annular crucible plates 4;
[0030] The barrel wall of the crucible barrel 1 at different heights is provided with evenly distributed positioning blocks 6 in the circumferential direction, and the annular crucible plate 4 is mounted on the positioning blocks 6; it is preferable that the positioning blocks 6 at different heights are aligned up and down and evenly distributed in height, so that the annular crucible plate 4 can evenly layer the inside of the crucible barrel 1;
[0031] The annular crucible plate 4 is annular, the built-in container 3 passes through the hollow annular crucible plate 4 and is tightly attached to the side wall of the annular crucible plate 4; the built-in container 3, the crucible barrel 1 and the annular crucible plate 4 form a closed space as a deposition area 8, and the powder 10 to be coated is placed in the deposition area 8;
[0032] The built-in container 3 includes a wall 31 and a cover 32, but no bottom cover. The built-in container 3 is combined with a solid crucible plate 7 to form a closed evaporation chamber 33. Melamine 9 is placed in the evaporation chamber 33. Melamine can be replaced by other raw materials for preparing g-C3N4 by solid phase reaction method, such as cyanuric chloride. An air guide hole 51 is provided on the wall 31.
[0033] In some embodiments, the built-in container 3 is in the shape of an inverted truncated cone, and the outer diameter gradually decreases from top to bottom. In this embodiment, the hollow diameters of the annular crucible plates 4 of different layers match the change of the outer diameter of the built-in container 3.
[0034] The built-in container 3 is provided with a plurality of solid crucible plates 7, which divide the evaporation chamber 33 into a plurality of evaporation chambers 33 by layer. The solid crucible plates 7 correspond to the annular crucible plates 4 one by one and are flush with each other. Preferably, there are two solid crucible plates 7 and two annular crucible plates 4, such as Figure 1 As shown. Since the built-in container 3 is an inverted frustum cone, the solid crucible plate 7 can be fixed by friction and by determining the diameter of the solid crucible plate 7 to achieve the purpose of stratifying the evaporation chamber 33. The stratification of the evaporation chamber 33 can better control the coating thickness of different layers of the powder 10 to be coated.
[0035] The setting of the air guide hole 51 allows the g-C3N4 gas to flow evenly from the evaporation chamber 33 to the deposition area 8; and slows down the flow rate of the g-C3N4 gas to the powder to be coated, so that the g-C3N4 gas can be evenly deposited on the surface of the powder to be coated, solving the problem of uneven thickness of the coating layer; the internal stratification of the crucible barrel 1 and the built-in container 3 can simultaneously synthesize a variety of composite materials with different coating conditions, which significantly improves production efficiency.
[0036] In the above embodiment, the ratio of the inner diameter of the crucible barrel 1 to the outer diameter of the top of the built-in container 3 is 2:1-5:3.
[0037] In the above embodiment, the ratio of the inner diameter of the bottom to the top of the built-in container 3 is 2:3-3:4.
[0038] In the above embodiment, the air guide hole 51 extends obliquely from the inside of the built-in container 3 to the outside, with an inclination angle of 20-45° and an inner diameter of 0.6-1.2 cm. Preferably, the air guide hole 51 is inclined downward from the inside of the built-in container 3 to the outside; each air guide hole 51 is at least 71.5-3.0 cm higher than the solid crucible plate of the corresponding evaporation chamber 33.
[0039] The air guide holes 51 are grouped into an air guide hole group 5 every 6 to 10, and the air guide holes 51 in the air guide hole group 5 are evenly distributed on the same circumference and are not connected. Figure 3 As shown, the distance between the air guide holes 51 is set as needed according to the number of air guide holes 51 and the inner diameter of the built-in container. Each evaporation chamber 33 is provided with multiple groups of air guide holes 5. Two groups of air guide holes 5 can be symmetrically arranged on the wall 31, or three or four groups of air guide holes 5 can be evenly arranged circumferentially on the wall 31. The arrangement is not limited to this. The vertical distance between each group of upper and lower adjacent air guide holes 5 is 0.5-0.8 cm. Figure 3 shown.
[0040] The positioning blocks 6 are raised blocks evenly distributed on the same circumference. Figure 1 Each layer of positioning blocks 6 may be provided with 3 or 4 blocks. Too few positioning blocks 6 are not conducive to stabilizing the annular crucible plate 4, and too many positioning blocks 6 are not conducive to disassembling and assembling the annular crucible plate 4.
[0041] The inner side of the barrel cover 2 is provided with a circular protrusion 21, such as Figure 2 As shown, the diameter of the circular protrusion 21 is adapted to the inner diameter of the crucible barrel 1, and the circular protrusion 21 can be movably embedded in the top of the crucible barrel 1, as shown in FIG. Figure 1 shown.
[0042] The crucible barrel 1, barrel cover 2, built-in container 3, annular crucible plate 4 and solid crucible plate 7 are made of corundum, and the introduction coefficient of corundum is as high as 30W / m*k, which can quickly transfer heat; the centers of the crucible barrel 1, barrel cover 2 and built-in container 3 are on the same axis.
[0043] Method of using the above crucible device:
[0044] First, install the annular crucible plate 4. If there is no stratification in the built-in container 3, the built-in container 3 can be directly in a straight cylindrical shape, and the annular crucible plate 4 can be of the same specification; if there is stratification in the built-in container 3, the annular crucible plate 4 needs to adopt different hollow diameters, and the hollow diameter of the annular crucible plate 4 needs to match the diameter of the corresponding position of the built-in container 3. After the annular crucible plate 4 is installed, the weighed powder 10 to be coated is placed on the annular crucible plate 4, and then the built-in container 3 is installed. Here, it is best to make the air guide holes 51 on the built-in container 3 correspond to the powder 10 to be coated. The cover 32 on the built-in container 3 can be opened. If there is no stratification in the built-in container 3, melamine 9 is directly placed at the bottom of the built-in container 3; if there is stratification in the built-in container 3, melamine 9 and the solid crucible plate 7 are placed in sequence. Then cover the cover 32 and the barrel cover 2 for subsequent preparation and reaction. During the reaction, g-C3N4 prepared from melamine 9 passes through the air guide holes 5, enters the deposition area 8 from the evaporation chamber 3, and uniformly wraps the powder 10 to be coated.
[0045] The above is a description of the embodiments of the utility model. Through the above description of the disclosed embodiments, professionals and technicians in the field can implement or use the utility model. Various modifications to these embodiments will be obvious to professionals and technicians in the field. The general principles defined in this article can be implemented in other embodiments without departing from the spirit or scope of the utility model. Therefore, the utility model will not be limited to these embodiments shown in this article, but will conform to the widest range consistent with the principles and novelties disclosed in this article.
Claims
1. A crucible device for preparing a g-C3N4 coated composite material, characterized in that: The crucible device comprises a crucible barrel (1), a barrel cover (2), a built-in container (3) and a plurality of annular crucible plates (4); Positioning blocks (6) are evenly distributed on the barrel wall at different heights inside the crucible barrel (1) in the circumferential direction, and the annular crucible plate (4) is mounted on the positioning blocks (6); The annular crucible plate (4) is annular in shape, and the built-in container (3) passes through the hollow of the annular crucible plate (4) and is tightly attached to the side wall of the annular crucible plate (4); the built-in container (3), the crucible barrel (1) and the annular crucible plate (4) form a closed space as a deposition area (8); The built-in container (3) comprises a container wall (31) and a container cover (32), but has no bottom cover; the built-in container (3) is combined with a solid crucible plate (7) to form a closed evaporation chamber (33); and an air guide hole (51) is provided on the container wall (31).
2. The crucible device according to claim 1, characterized in that The built-in container (3) is in the shape of an inverted frustum, and its outer diameter gradually decreases from top to bottom.
3. The crucible device according to claim 2, characterized in that: A plurality of solid crucible plates (7) are arranged in the built-in container (3), and the solid crucible plates (7) divide the evaporation chamber (33) into a plurality of evaporation chambers (33) by layer. The solid crucible plates (7) correspond to the annular crucible plates (4) one by one and are flush in height.
4. The crucible device according to claim 1, 2 or 3, characterized in that: The ratio of the inner diameter of the crucible barrel (1) to the outer diameter of the top of the built-in container (3) is 2:1-5:
3.
5. The crucible device according to claim 1, 2 or 3, characterized in that: The ratio of the inner diameter of the bottom to the top of the built-in container (3) is 2:3-3:
4.
6. The crucible device according to claim 1, 2 or 3, characterized in that: The air guide holes (51) extend obliquely from the inside of the built-in container (3) to the outside, with an inclination angle of 20-45 degrees and an inner diameter of 0.6-1.2 cm; each air guide hole (51) is at least 1.5-3.0 cm higher than the solid crucible plate (7) of the corresponding evaporation chamber (33).
7. The crucible device according to claim 6, characterized in that Every 6 to 10 air guide holes (51) form an air guide hole group (5); the air guide holes (51) on the air guide hole group (5) are evenly distributed on the same circumference and are not connected; each layer of the evaporation chamber (33) is provided with a plurality of air guide hole groups (5); and the vertical distance between each group of upper and lower adjacent air guide hole groups (5) is 0.5 to 0.8 cm.
8. The crucible device according to claim 1, 2 or 3, characterized in that: The positioning blocks (6) are raised stoppers that are evenly distributed on the same circumference.
9. The crucible device according to claim 1, 2 or 3, characterized in that: A circular protrusion (21) is provided on the inner side surface of the barrel cover (2); the diameter of the circular protrusion (21) matches the inner diameter of the crucible barrel (1); and the circular protrusion (21) can be movably embedded in the top of the crucible barrel (1).
10. The crucible device according to claim 1, 2 or 3, characterized in that: The crucible barrel (1), the barrel cover (2), the built-in container (3), the annular crucible plate (4) and the solid crucible plate (7) are made of corundum, and the centers of the crucible barrel (1), the barrel cover (2) and the built-in container (3) are on the same axis.