Laser shell and laser local plating structure

By forming a gold or silver layer on the bottom and side walls of the receiving groove of the laser housing, and using matching parts to form a local plating space, the problem of high cost and complex coating of the laser housing is solved, and efficient operation and cost reduction of local plating are achieved. .

CN221828343UActive Publication Date: 2024-10-11GUANGDONG XINGHAN LASER TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420016931.X
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-01-02
Publication Date
2024-10-11
Estimated Expiration
2034-01-02

Smart Images

  • Figure CN221828343U_ABST
    Figure CN221828343U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of lasers, in particular to a laser shell and a laser local plating structure, the laser shell comprises a main body provided with an accommodating groove and a step group arranged at the groove bottom of the accommodating groove, one side of the step group is connected with a first side wall of the accommodating groove, and the other side of the step group is connected with a second side wall of the accommodating groove; a gold layer or a silver layer is formed on the top surface of the step group and the first side wall of the accommodating groove, and no gold layer or silver layer is formed on other surfaces of the laser shell. The thermal conductivity of the gold layer and the silver layer is good, and the heat of the laser chip can be effectively conducted to the step group by arranging the gold layer or the silver layer. And the solderability of the gold layer and the silver layer is good, thereby facilitating the installation of the heat sink and the laser chip. In addition, the oxidation resistance of the gold layer is high, and the situation that the thermal conductivity and weldability are affected due to the fact that an oxidation layer is formed is reduced. And the silver layer is lower in cost than the gold layer, so that the cost of the laser shell is reduced. And no gold layer or silver layer is formed on other surfaces of the laser shell, so that the loss of gold or silver can be reduced, and the cost can be reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of laser technology, and in particular to a laser housing and a local laser plating structure. Background Art

[0002] The laser housing usually needs to be plated with a corresponding coating so that the various performances of the laser housing can meet the requirements. In the related art, the entire laser housing is usually placed in a plating bath for electroplating, so that the entire surface of the laser housing can be plated with a corresponding coating, but the cost of plating the entire surface of the laser housing is too high. Utility Model Content

[0003] In view of the above, it is necessary to provide a laser housing and a laser local plating structure, which can plate a coating on a part of the laser housing.

[0004] In a first aspect, the present application provides a laser housing, comprising a main body provided with a receiving groove and a step group arranged at the bottom of the receiving groove, one side of the step group is connected to the first side wall of the receiving groove, the top surface of the step group and the first side wall of the receiving groove are formed with a gold layer or a silver layer, and the other surfaces of the laser housing are not formed with a gold layer or a silver layer.

[0005] In the above-mentioned laser housing, the gold layer and the silver layer have good thermal conductivity. By setting the gold layer or the silver layer, the heat of the laser chip can be effectively transferred to the step group. The gold layer and the silver layer have good solderability, which is conducive to the installation of the heat sink and the laser chip. In addition, the gold layer has strong oxidation resistance, which reduces the formation of the oxide layer and affects the thermal conductivity and solderability. The silver layer is lower in cost than the gold layer, which is conducive to reducing the cost of the laser housing. No gold layer or silver layer is formed on the other surfaces of the laser housing, which can reduce the loss of gold or silver and help reduce costs.

[0006] In a possible implementation, the laser housing further includes a cover plate, which is connected to the upper side of the main body to close the accommodating groove.

[0007] In a second aspect, a laser local plating structure includes a laser housing and a matching part, wherein the matching part cooperates with the laser housing so that the top surface of the step group, the first side wall of the receiving groove and the matching part form a plating space, and the plating space is used to pass the plating liquid so that the top surface of the step group and the first side wall of the receiving groove are formed with a gold layer or a silver layer.

[0008] In the above-mentioned laser partial plating structure, the laser housing serves as a cathode, and cooperates with a matching piece to form a plating space. Plating liquid is introduced into the plating space, so that the top surface of the step group and the first side wall are in contact with the plating liquid, and a gold layer or a silver layer is electroplated, while other surfaces of the laser housing are not in contact with the plating liquid, so no plating layer is formed. The method of partial plating of the laser housing is simple, which is conducive to improving the efficiency of partial plating.

[0009] In a possible implementation, the matching member includes a baffle and a side plate. The baffle is located in the receiving groove and contacts the first side wall of the receiving groove, and the baffle is directly opposite to the top surface of the step group. The side plate is connected to the baffle and is located in the receiving groove, and the side of the side plate away from the baffle contacts the bottom wall of the receiving groove, and the side plate is located on one side of the electroplating space and contacts the side surface of the step group.

[0010] In a possible implementation manner, the plane where the baffle plate is located is perpendicular to the plane where the side plate is located.

[0011] In a possible implementation, the step group includes a plurality of arranged steps, and the steps gradually rise along the arrangement direction of the steps, and the distance between the baffle and the bottom wall of the accommodating groove gradually increases in the direction in which the steps gradually rise.

[0012] In one possible implementation, the baffle is provided with a liquid inlet hole and a liquid outlet hole connected to the electroplating space, and the matching component also includes a liquid inlet pipe and a liquid outlet pipe, the liquid inlet pipe and the liquid outlet pipe are both connected to the baffle, and the liquid inlet pipe is opposite to the liquid outlet hole, and the liquid outlet pipe is opposite to the liquid outlet hole.

[0013] In a possible implementation, the number of the baffles and the side plates are both two, each of the baffles is connected to one of the side plates, the two baffles are arranged at intervals, and the matching part also includes a connecting plate, one end of the connecting plate is connected to one of the baffles, and the other end is connected to the other baffle.

[0014] In a possible implementation, the laser local plating structure further includes an insulating wetting layer, and the insulating wetting layer is disposed on the baffle and located in the electroplating space.

[0015] In a possible implementation, the insulating wetting layer is dust-free paper.

[0016] In the above-mentioned laser housing and laser partial plating structure, the laser housing is formed with a gold layer or a silver layer on the top surface of the step group and the first side wall of the accommodating groove. The gold layer or the silver layer can be easily installed on the laser chip, and it is also beneficial to conduct the heat of the gold layer or the silver layer to the step group. The other surfaces of the laser housing are not formed with a gold layer or a silver layer, which can reduce the production cost. By providing a matching piece, the matching piece and the laser housing cooperate to form an electroplating space, and the electroplating liquid is passed into the electroplating space, so that the top surface of the step group and the first side wall form a coating, and the partial plating operation of the laser housing is simple. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 It is a three-dimensional structural diagram of a laser housing in one embodiment of the present application.

[0018] Figure 2 It is a three-dimensional structural diagram of a laser housing in another embodiment of the present application.

[0019] Figure 3 yes Figure 1 Top view of the laser housing.

[0020] Figure 4 It is a three-dimensional structural diagram of a matching component in one embodiment of the present application.

[0021] Figure 5 It is a top view of the local laser plating structure in one embodiment of the present application.

[0022] Figure 6 yes Figure 5 Schematic cross-sectional view of the local plating structure of the laser.

[0023] Figure 7 yes Figure 5 A schematic cross-sectional view of the local laser plating structure from another angle.

[0024] Figure 8 It is a cross-sectional schematic diagram of a local laser plating structure in another embodiment of the present application.

[0025] Description of main component symbols:

[0026] 100. Local plating structure of laser;

[0027] 10. Laser housing; 11. Main body; 12. Accommodating groove; 121. Groove bottom; 122. First side wall; 123. Second side wall; 13. Step group; 131. Top surface; 132. Side surface; 133. Step; 14. Cover plate;

[0028] 20. Matching member; 21. Baffle; 211. Outer side; 212. Inner side; 213. First side; 214. Second side; 215. Liquid inlet hole; 216. Liquid outlet hole; 22. Side plate; 221. Outer side; 222. Inner side; 223. First side; 224. Second side; 23. Connecting plate; 24. Liquid inlet pipe; 25. Liquid outlet pipe;

[0029] 30. Insulation wetting layer;

[0030] S. Electroplating space. DETAILED DESCRIPTION

[0031] In order to make the purpose, technical solutions and advantages of the embodiments of the present application clearer, the technical solutions in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of this application.

[0032] It should be understood that, considering the actual tolerance factor, the term "perpendicular" in the technical solution of this application is used to describe the ideal state between two components. In actual production or use, the two components may be in a state that is approximately perpendicular to each other. The two components described as "perpendicular" may not be absolutely straight lines or planes, but may be roughly straight lines or planes. From a macroscopic point of view, the components can be considered "straight lines" or "planes" if the overall extension direction is a straight line or a plane.

[0033] In the description of this application, it should be noted that, unless otherwise clearly specified and limited, the terms "installation", "connection" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a direct connection, or an indirect connection through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.

[0034] In addition, in the drawings used in the following embodiments, hatching is omitted in some cases even in cross-sectional views to make the drawings easier to see. The sizes of the various parts in the cross-sectional views do not correspond to the sizes of the actual devices, and in some cases specific parts are shown in a relatively enlarged manner to make the drawings easier to see.

[0035] See also Figure 1The present embodiment provides a laser housing 10, which includes a main body 11 and a step group 13. The main body 11 is provided with a receiving groove 12, and the receiving groove 12 has a groove bottom 121 and a first side wall 122 and a second side wall 123 adjacent to the groove bottom 121. The first side wall 122 and the second side wall 123 enclose an upper opening. The step group 13 is arranged at the groove bottom 121 of the receiving groove 12, one side of the step group 13 is connected to the first side wall 122, and the step group 13 is not in direct contact with the second side wall 123. The step group 13 has a top surface 131 and a side surface 132, the top surface 131 is adjacent to the first side wall 122, the side surface 132 is adjacent to the groove bottom 121 of the receiving groove 12 and the top surface 131 of the step group 13, and the side surface 132 of the step group 13 is directly opposite to the first side wall 122. The number of step groups 13 of each laser housing 10 is not limited. The present application takes two step groups 13 as an example. When there are two step groups 13, there are also two first side walls 122, and the two first side walls 122 are arranged opposite to each other.

[0036] Optionally, the step group 13 includes a plurality of steps 133, which are arranged in an array and gradually rise along the arrangement direction of the plurality of steps 133. The top surface 131 of the step group 13 is used to install the laser chip, so that the heights of the laser chips are different, so that the laser output by the laser chip will not be blocked. The laser chip generates heat during operation, and the heat is transferred to the step group 13 through the heat sink.

[0037] A gold layer or a silver layer is formed on the top surface 131 of the step group 13 and the first side wall 122 of the accommodating groove 12, and a gold layer or a silver layer is not formed on other surfaces of the laser housing 10, wherein the other surfaces of the laser housing 10 include the outer surface of the main body 11, the groove bottom 121 of the accommodating groove 12, the second groove wall and the side surface 132 of the step group 13.

[0038] The gold layer and the silver layer have good thermal conductivity. By setting the gold layer or the silver layer, the heat of the laser chip can be effectively transferred to the step group 13. The gold layer and the silver layer have good solderability, which is conducive to the installation of the heat sink and the laser chip. In addition, the gold layer has strong oxidation resistance, which reduces the formation of the oxide layer and affects the thermal conductivity and solderability. The silver layer is lower in cost than the gold layer, which is conducive to reducing the cost of the laser housing 10. No gold layer or silver layer is formed on the other surfaces of the laser housing 10, which can reduce the loss of gold or silver and help reduce costs.

[0039] In some embodiments, the laser housing 10 also includes a cover plate 14, which is fixedly connected to the upper side of the main body 11 to close the receiving groove 12, so that the receiving groove 12 is a closed groove body, which is beneficial to protecting various parts in the laser housing 10, such as laser chips, reflectors, focusing lenses, etc.

[0040] The embodiment of the present application also provides a laser local plating structure 100, which includes the above-mentioned laser housing 10 without a cover plate 14, and the laser local plating structure 100 also includes a matching piece 20, the matching piece 20 cooperates with the laser housing 10 so that the top surface 131 of the step group 13, the first side wall 122 of the accommodating groove 12 and the matching piece 20 form a plating space S, and the plating space S is used to pass the plating liquid so that the top surface 131 of the step group 13 and the first side wall 122 of the accommodating groove 12 are formed with a gold layer or a silver layer.

[0041] The laser housing 10 acts as a cathode, and cooperates with the matching piece 20 to form an electroplating space S. The electroplating liquid is passed into the electroplating space S, so that the top surface 131 of the step group 13 and the first side wall 122 can be in contact with the electroplating liquid, and a gold layer or a silver layer is electroplated, while other surfaces of the laser housing 10 are not in contact with the electroplating liquid, so no plating layer is formed. The method of local plating of the laser housing 10 is simple, which is conducive to improving the efficiency of local plating.

[0042] In some embodiments, the matching piece 20 includes a baffle 21 and a side plate 22. Both the baffle 21 and the side plate 22 are located in the receiving groove 12. The baffle 21 contacts the first side wall 122 of the receiving groove 12, and the baffle 21 faces the top surface 131 of the step group 13. The side plate 22 is connected to the baffle 21. The side of the side plate 22 away from the baffle 21 contacts the bottom wall of the receiving groove 12. The side of the side plate 22 located at the electroplating space S contacts the side 132 of the step group 13 and faces the first side wall 122. Thus, by directly placing the matching piece 20 in the receiving groove 12, the baffle 21, the side plate 22, the first side wall 122 of the receiving groove 12, and the top surface 131 of the step group 13 can form the electroplating space S. The method of forming the electroplating space S is simple and quick.

[0043] Optionally, the baffle plate 21 and the side plate 22 are both plate-shaped structures, and the shape of the connection between the baffle plate 21 and the side plate 22 is substantially L-shaped. The baffle plate 21 and the side plate 22 have outer sides 221, 211, inner sides 222, 212, first sides 223, 213 and second sides 224, 214. The outer sides 221, 211 are arranged opposite to the inner sides 222, 212, and the inner sides 222, 212 are both located in the electroplating space S. The inner side 212 of the baffle plate 21 is opposite to the top surface 131 of the step group 13, and the inner side 222 of the side plate 22 is opposite to the first side wall 122 of the receiving groove 12. The first sides 223, 213 are arranged opposite to the second sides 224, 214, and the first side 213 of the baffle plate 21 is in contact with the first side wall 122 of the receiving groove 12. The second side 214 of the baffle 21 is connected to the second side 224 of the side plate 22, and the first side 223 of the side plate 22 is in contact with the groove bottom 121 of the accommodating groove 12. It should be noted that the structure after the baffle 21 and the side plate 22 are connected is not limited to an L-shape, but can also be other shapes, such as a T-shape, a cross shape, etc.

[0044] Optionally, the plane where the side plate 22 is located is perpendicular to the plane where the baffle plate 21 is located, so that the inner side 222 of the side plate 22 can fit with the side surface 132 of the step group 13, which is beneficial to increase the sealing of the electroplating space S.

[0045] In some embodiments, as the step 133 gradually rises, the distance between the baffle plate 21 and the bottom wall of the receiving groove 12 gradually increases, that is, the baffle plate 21 is inclined relative to the groove wall of the receiving groove 12 .

[0046] During electroplating, the fitting 20 can be used as an anode and the laser housing 10 as a cathode. The closer the distance between the anode and the cathode, the faster the coating is formed on the cathode. Therefore, keeping the position of each point on the cathode as close to the distance of the anode as possible can reduce the occurrence of uneven coating thickness on the cathode. Since the steps 133 of the step group 13 gradually rise, the baffle 21 is tilted so that the distance between each step 133 and the baffle 21 is roughly equal, so as to improve the uniformity of the coating thickness on the top surface 131 of the step group 13.

[0047] Optionally, the first side 223 of the side plate 22 is inclined relative to the second side 224 of the side plate 22, so that when the first side 223 of the side plate 22 contacts the bottom wall of the accommodating groove 12, the baffle 21 can be inclined relative to the bottom wall of the accommodating groove 12 and can also maintain the sealing of the electroplating space S.

[0048] Since there are two step groups 13, each matching piece 20 includes two baffles 21 and two side plates 22, each baffle 21 is connected to a side plate 22, and the two baffles 21 are arranged at intervals. One baffle 21, one side plate 22, one step group 13 and a corresponding first side wall 122 form an electroplating space S.

[0049] In some embodiments, the fitting 20 further includes a connecting plate 23, one end of the connecting plate 23 is connected to the second side 214 of one baffle 21, and the other end of the connecting plate 23 is connected to the second side 214 of the other baffle 21. The two baffles 21 are connected through the connecting plate 23, so that the fitting 20 is an integral structure, so that the fitting 20 is matched with the laser housing 10, and when the fitting 20 is installed in the receiving groove 12, the first side 213 of one baffle 21 contacts with one first side wall 122, and the first side 213 of the other baffle 21 contacts with the other first side wall 122, thereby limiting the relative position of the laser housing 10 and the fitting 20, and improving the position accuracy of the fitting 20. Optionally, the number of the connecting plates 23 is two, and the two connecting plates 23 are arranged at intervals along the length direction of the baffle 21, and the connection stability of the two baffles 21 is improved by arranging two connecting plates 23.

[0050] In some embodiments, since both ends of the plating space S have openings, the plating solution can be introduced into one opening and the plating solution in the plating space S can be discharged through the other opening, so that the plating solution in the plating space S can flow continuously, thereby maintaining the concentration of the plating solution.

[0051] In some other embodiments, the baffle 21 is provided with a liquid inlet 215 and a liquid outlet 216, and the electroplating liquid enters the electroplating space S from the liquid inlet 215 and is discharged from the liquid outlet 216. The liquid inlet 215 and the liquid outlet 216 are arranged on the baffle 21, and the positions of the liquid inlet 215 and the liquid outlet 216 are adjacent to the opening of the containing tank 12, so that there is enough space to connect with the pipeline, and the pipeline can be connected to the electroplating tank, so as to facilitate the passage of the electroplating liquid into the electroplating space S, and the shapes of the liquid inlet 215 and the liquid outlet 216 can be set as required, and the shapes of the liquid inlet 215 and the liquid outlet 216 are more standardized, so as to facilitate the passage and outflow of the electroplating liquid. And because the flow rate of the electroplating liquid in the electroplating space S is small and the flow rate is slow, even if there are openings at both ends of the electroplating space S, most of the electroplating liquid will not leak from the openings.

[0052] Furthermore, the laser housing 10 is turned upside down so that the bottom wall of the accommodating groove 12 is located above the fitting 20. Even if a small amount of electroplating liquid leaks from the electroplating space S, it can be separated from the laser housing 10 under the action of gravity, and no plating layer will be formed on other surfaces of the laser housing 10. In addition, since the weight of the laser housing 10 is greater than the weight of the fitting 20, turning the laser housing 10 upside down to press the fitting 20 can improve the stability of the electroplating space S.

[0053] In some embodiments, each baffle 21 is provided with a liquid inlet hole 215 and a liquid outlet hole 216, and the liquid inlet hole 215 and the liquid outlet hole 216 are located at opposite ends of the baffle 21. Each electroplating space S has a separate liquid inlet hole 215 and liquid outlet hole 216, which is beneficial to improving the flow effect of the electroplating liquid in the electroplating space S.

[0054] In some other embodiments, one baffle plate 21 is provided with a liquid inlet hole 215, and the other baffle plate 21 is provided with a liquid outlet hole 216. The connecting plate 23 is hollow and connected to two electroplating spaces S. The electroplating liquid enters one electroplating space S from the liquid inlet hole 215, passes through the connecting plate 23, and then enters the other electroplating space S, and is then discharged from the liquid outlet hole 216 of the electroplating space S.

[0055] In some embodiments, the fitting 20 further includes a liquid inlet pipe 24 and a liquid outlet pipe 25, both of which are connected to the baffle 21, and the liquid inlet pipe 24 is directly opposite to the liquid outlet hole 216, and the liquid outlet pipe 25 is directly opposite to the liquid outlet hole 216. Specifically, the liquid inlet pipe 24 and the liquid outlet pipe 25 are both connected to the outer side 221211 of the baffle 21, and the number of the liquid inlet pipe 24 and the liquid outlet pipe 25 is two, one liquid inlet pipe 24 and the liquid outlet pipe 25 are connected to one baffle 21, and the other liquid inlet pipe 24 and the liquid outlet pipe 25 are connected to the other baffle 21. By providing the liquid inlet pipe 24 and the liquid outlet pipe 25, it is convenient to connect with the pipeline.

[0056] In some embodiments, the laser local plating structure 100 further includes an insulating wetting layer 30, which is disposed on the baffle 21 and is located in the electroplating space S. The electroplating liquid in the electroplating space S will contact the insulating wetting layer 30, and the insulating wetting layer 30 absorbs the electroplating liquid to keep the insulating wetting layer 30 in a wet state. The insulating wetting layer 30 can contact the top surface 131 of the step group 13, thereby ensuring that the top surface 131 of the step group 13 can continue to contact the electroplating liquid. In addition, the provision of the insulating wetting layer 30 can also isolate and insulate the laser housing 10 from the mating part 20. Optionally, the first side 213 of the baffle 21 contacts the first side wall 122 through the insulating wetting layer 30, the first side 223 of the side plate 22 contacts the bottom wall through the insulating wetting layer 30, and the inner side 222 of the side plate 22 contacts the side surface 132 of the step group 13 through the insulating wetting layer 30. In addition, by providing the insulating wetting layer 30 to absorb the plating solution, leakage of the plating solution from the openings at both ends of the plating space S can be reduced.

[0057] In some embodiments, the insulating wetting layer 30 is dust-free paper, which has good water absorption and water retention and can maintain good wettability for a long time. It should be noted that the insulating wetting layer 30 is not limited to dust-free paper, but can also be other materials, such as a non-woven fabric layer, a sponge layer, a polymer absorbent resin layer, etc.

[0058] In summary, the laser housing 10 of the embodiment of the present application is formed with a gold layer or a silver layer on the top surface 131 of the step group 13 and the first side wall 122 of the accommodating groove 12. The gold layer or the silver layer can be provided to facilitate the installation of the laser chip and facilitate the conduction of the heat of the gold layer or the silver layer to the step group 13. The other surfaces of the laser housing 10 are not formed with a gold layer or a silver layer, which can reduce the production cost. By providing a matching piece 20, the matching piece 20 cooperates with the laser housing 10 to form an electroplating space S, and the electroplating liquid is passed into the electroplating space S, so that the top surface 131 of the step group 13 and the first side wall 122 form a coating, and the local plating operation of the laser housing 10 is simple.

[0059] In this article, the directional words such as upper, outer, inner, etc. involved are defined by the positions of the components in the drawings and the positions of the components relative to each other, just for the sake of clarity and convenience in expressing the technical solution. It should be understood that the use of the directional words should not limit the scope of protection requested by this application.

[0060] Obviously, the embodiments described above are only part of the embodiments of the present application, rather than all of the embodiments. The present application is not limited to the details of the above embodiments, and any appropriate changes or modifications made by ordinary technicians in the relevant technical field are deemed to be within the patent scope of the present application.

Claims

1. A laser housing, comprising a main body provided with a receiving groove and a step group arranged at the bottom of the receiving groove, wherein one side of the step group is connected to the first side wall of the receiving groove, characterized in that: A gold layer or a silver layer is formed on the top surface of the step group and the first side wall of the accommodating groove, and no gold layer or a silver layer is formed on other surfaces of the laser housing.

2. The laser housing according to claim 1, characterized in that: It also includes a cover plate, which is connected to the upper side of the main body to close the accommodating groove.

3. A laser local plating structure, characterized in that: Including the laser housing as described in claim 1, the laser local plating structure also includes a matching piece, the matching piece cooperates with the laser housing so that the top surface of the step group, the first side wall of the receiving groove and the matching piece form an electroplating space, and the electroplating space is used to pass the electroplating liquid so that the top surface of the step group and the first side wall of the receiving groove are formed with a gold layer or a silver layer.

4. The laser local plating structure according to claim 3, characterized in that: The matching piece comprises: a baffle, the baffle being located in the accommodating groove and in contact with the first side wall of the accommodating groove, and the baffle being directly opposite to the top surface of the step group; A side plate is connected to the baffle plate and is located in the accommodating groove. The side of the side plate away from the baffle plate contacts the bottom wall of the accommodating groove. The side plate is located on one side of the electroplating space and contacts the side surface of the step group.

5. The laser local plating structure according to claim 4, characterized in that: The plane where the baffle plate is located is perpendicular to the plane where the side plate is located.

6. The laser local plating structure according to claim 4, characterized in that: The step group includes a plurality of steps arranged in an array. The steps gradually rise along the arrangement direction of the steps. In the direction in which the steps gradually rise, the distance between the baffle and the bottom wall of the accommodating groove gradually increases.

7. The laser local plating structure according to claim 4, characterized in that: The baffle is provided with a liquid inlet hole and a liquid outlet hole connected to the electroplating space, and the matching part also includes a liquid inlet pipe and a liquid outlet pipe, the liquid inlet pipe and the liquid outlet pipe are both connected to the baffle, and the liquid inlet pipe is opposite to the liquid outlet hole, and the liquid outlet pipe is opposite to the liquid outlet hole.

8. The laser local plating structure according to claim 4, characterized in that: There are two baffles and two side plates, each of which is connected to one side plate, and the two baffles are spaced apart. The matching component also includes a connecting plate, one end of which is connected to one baffle, and the other end is connected to the other baffle.

9. The laser local plating structure according to claim 4, characterized in that: The laser local plating structure also includes an insulating wetting layer, which is arranged on the baffle and located in the electroplating space.

10. The laser local plating structure according to claim 9, characterized in that: The insulating wetting layer is dust-free paper.