Metal substrate

By arranging a composite layer between the conductive layer of the metal substrate and the metal base plate, including an overlapping transition layer and a diamond film, the problem that it is difficult for the existing metal substrate to achieve thermal conductivity and insulation at the same time is solved, and the excellent performance of the metal substrate is achieved. Thermal conductivity and insulation.

CN221829140UActive Publication Date: 2024-10-11ZHEJIANG WAZAM NEW MATERIAL CO LTD +2
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420067850.2
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-01-10
Publication Date
2024-10-11
Estimated Expiration
2034-01-10

AI Technical Summary

Technical Problem

It is difficult for existing metal substrates to achieve good thermal conductivity and insulation at the same time, and cannot meet the strict requirements for thermal conductivity and insulation performance of electronic products.

Method used

Design a metal substrate that provides a composite layer between the conductive layer and the metal base plate. The composite layer includes an overlapping transition layer and a diamond film to improve the bonding force between the diamond film, the conductive layer and the metal base plate, thereby improving thermal conductivity. sex and insulation.

Benefits of technology

The excellent thermal conductivity and insulation of the metal substrate are achieved, and the balance of thermal conductivity and insulation is ensured by improving the bonding force between the diamond film and the transition layer.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221829140U_ABST
    Figure CN221829140U_ABST
Patent Text Reader

Abstract

The utility model relates to a metal substrate, which comprises a conducting layer, a composite layer and a metal bottom plate which are sequentially stacked, the composite layer comprises at least two transition layers which are stacked, a layer of diamond film is clamped between each two adjacent transition layers, and the peel strength of the transition layers and the conducting layer is gt; 0.5 N / mm, and the peel strength of the transition layer and the metal bottom plate is gt; and the push-pull force of the transition layer and the diamond film is greater than or equal to 100N. According to the metal substrate, the binding force between the diamond film and the conductive layer and the binding force between the diamond film and the metal bottom plate are high, and the metal substrate has excellent heat-conducting property and insulating property.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of electronic industry, in particular to a metal substrate. Background Art

[0002] Metal substrates are basic materials in the electronics industry, primarily used for the processing and manufacturing of printed circuit boards. They are widely used in electronic products such as televisions, radios, computers, servers, mobile communications, and antennas. With the rapid development of electronic products and components, the requirements for the thermal conductivity and insulation properties of metal substrates are becoming increasingly stringent. However, existing metal substrates struggle to achieve both good thermal conductivity and insulation properties. Therefore, the development of new thermally conductive and insulating metal substrates is urgent. Utility Model Content

[0003] Based on this, it is necessary to provide a metal substrate that can simultaneously achieve excellent thermal conductivity and insulation to address the above problems.

[0004] A metal substrate comprising a conductive layer, a composite layer and a metal bottom plate stacked in sequence, wherein the composite layer comprises at least two stacked transition layers, and a diamond film is sandwiched between two adjacent transition layers;

[0005] The peeling strength between the transition layer and the conductive layer is greater than 0.5 N / mm, the peeling strength between the transition layer and the metal base plate is greater than 0.2 N / mm, and the push-pull force between the transition layer and the diamond film is greater than or equal to 100 N.

[0006] In one embodiment, the transition layer has 2 to 4 layers.

[0007] In one embodiment, in the composite layer, the transition layer adjacent to the conductive layer is a first transition layer, and the composite layer satisfies at least one of the following conditions:

[0008] (1) The thickness of the first transition layer is 5 μm to 50 μm, and the thickness of the remaining transition layers except the first transition layer is 5 μm to 10 μm;

[0009] (2) The maximum weight difference of the first transition layer is ≤15g / m 2 Except for the first transition layer, the weight difference of the remaining transition layers is ≤3g / m 2 ;

[0010] (3) The fluidity of the transition layer is 30% to 60%;

[0011] (4) The thickness of the diamond film is 5 μm to 15 μm.

[0012] In one embodiment, the transition layer is selected from a modified diamond powder-thermosetting resin composite film.

[0013] Specifically, the modified diamond powder in the modified diamond powder-thermosetting resin composite film includes: a diamond core and an inorganic coating layer attached to the surface of the diamond core.

[0014] Preferably, the product of the particle size and the specific surface area of ​​the diamond core is 9 to 11;

[0015] And / or, the hydrophilicity and lipophilicity values ​​of the inorganic coating layer are 13-18.

[0016] In one embodiment, the thermal conductivity of the metal base plate is ≥100 W / (m·K).

[0017] In one embodiment, the metal substrate further includes a first thermally conductive resin layer, wherein the first thermally conductive resin layer is disposed between the conductive layer and the composite layer;

[0018] And / or, the metal substrate further includes a second thermally conductive resin layer, and the second thermally conductive resin layer is disposed between the metal bottom plate and the composite layer.

[0019] In one embodiment, the thickness of the first thermally conductive resin layer is 10 μm to 60 μm, and its thermal conductivity is ≥ 4 W / (m·K);

[0020] And / or, the second thermally conductive resin layer has a thickness of 10 μm to 20 μm and a thermal conductivity coefficient of ≥4 W / (m·K).

[0021] In one embodiment, the transition layer adjacent to the conductive layer is a first transition layer, the diamond film adjacent to the first transition layer is a first diamond film, the thickness of the first diamond film is 5 μm to 15 μm, and the ratio of the thickness of the first thermally conductive resin layer to the thickness of the first diamond film is 2:1 to 3:1;

[0022] And / or, the transition layer adjacent to the conductive layer is a first transition layer, the thickness of the first transition layer is 5 μm to 15 μm, and the ratio of the thickness of the first thermally conductive resin layer to the thickness of the first transition layer is 2:1 to 3:1.

[0023] In the metal substrate of the present invention, a composite layer is provided between the conductive layer and the metal base plate. The composite layer includes several overlapping layers of diamond film and transition layer. On the one hand, the diamond film helps to improve the thermal conductivity and insulation of the metal substrate. On the other hand, the transition layer is provided between the diamond film and the conductive layer, and between the diamond film and the metal base plate, effectively improving the bonding strength between the diamond film and the conductive layer and the metal base plate, thereby endowing the metal substrate with excellent thermal conductivity and insulation. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 This is a schematic structural diagram of a metal substrate according to a first embodiment of the present invention;

[0025] Figure 2 This is a schematic structural diagram of the composite layer in the metal substrate according to the first embodiment of the present invention;

[0026] Figure 3 This is a schematic structural diagram of a composite layer in a metal substrate according to a second embodiment of the present invention;

[0027] Figure 4 This is a schematic structural diagram of a composite layer in a metal substrate according to a third embodiment of the present invention;

[0028] Figure 5 This is a schematic structural diagram of a metal substrate according to a fourth embodiment of the present invention.

[0029] In the figure: 10, conductive layer; 20, composite layer; 30, metal base plate; 210, transition layer; 211, first transition layer; 212, second transition layer; 213, third transition layer; 214, fourth transition layer; 220, diamond film; 221, first diamond film; 222, second diamond film; 223, third diamond film; 40, first thermally conductive resin layer; 50, second thermally conductive resin layer. DETAILED DESCRIPTION

[0030] To facilitate understanding of the present invention, the present invention will be described in more detail below. However, it should be understood that the present invention can be implemented in many different forms and is not limited to the embodiments or examples described herein. Rather, these embodiments or examples are provided to provide a more thorough and comprehensive understanding of the disclosure of the present invention.

[0031] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art in the art of the present invention. The terms used herein in the specification of the present invention are only for the purpose of describing specific embodiments or examples and are not intended to limit the present invention.

[0032] Combine Figure 1 FIG. 1 is a schematic structural diagram of a metal substrate according to a first embodiment of the present invention. The metal substrate comprises a conductive layer 10, a composite layer 20 and a metal base plate 30 stacked in sequence; and Figure 2As shown, it is a schematic structural diagram of the composite layer 20 in the metal substrate of the first embodiment provided by the present invention, wherein the composite layer 20 includes at least two stacked transition layers 210, and a layer of diamond film is sandwiched between two adjacent transition layers, wherein the peeling strength between the transition layer and the conductive layer is greater than 0.5N / mm, the peeling strength between the transition layer and the metal base plate is greater than 0.2N / mm, and the push-pull force between the transition layer and the diamond film is greater than 100N.

[0033] It should be noted that Figure 2 The diamond film in the figure is the first diamond film 221; the peel strength range between the transition layer and the conductive layer and the metal base plate is expressed as the peel strength measured at 288°C; the push-pull force between the transition layer and the diamond film is expressed as the maximum pulling force value measured when a 1cm×1cm metal substrate is pulled from the side to separate the diamond film and the transition layer and displace them.

[0034] By providing a diamond film 220 between the conductive layer 10 and the metal base plate 30, both thermal conductivity and insulation are improved, and a transition layer 210 is provided on both sides of the diamond film 220. The peel strength between the transition layer 210 and the conductive layer 10 is greater than 0.5 N / mm, the peel strength between the transition layer 210 and the metal base plate 30 is greater than 0.2 N / mm, and the push-pull force between the transition layer 210 and the diamond film 220 is greater than 100 N. As a result, there is good adhesion between the transition layer 210 and the conductive layer 10, the metal base plate 30, and the diamond film 220, thereby improving the bonding strength between the diamond film 220 and the conductive layer 10 and the metal base plate 30, further ensuring the thermal conductivity and insulation of the metal substrate.

[0035] In one embodiment, the transition layer 210 has 2 to 4 layers, and the diamond film 220 has 1 to 3 layers.

[0036] like Figure 2 As shown, it is a schematic structural diagram of the composite layer 20 in the metal substrate of the first embodiment provided by the utility model. In this embodiment, the composite layer 20 includes a first transition layer 211, a first diamond film 221 and a second transition layer 212 stacked in sequence. The first transition layer 211 is adjacent to the conductive layer 10, and the first diamond film 221 is adjacent to the first transition layer 211.

[0037] like Figure 3As shown, it is a schematic structural diagram of the composite layer 20 in the metal substrate of the second embodiment provided by the present invention. In this embodiment, the composite layer 20 includes a first transition layer 211, a first diamond film 221, a second transition layer 212, a second diamond film 222 and a third transition layer 213 stacked in sequence. The first transition layer 211 is adjacent to the conductive layer 10, and the first diamond film 221 is adjacent to the first transition layer 211.

[0038] like Figure 4 As shown, it is a schematic structural diagram of the composite layer 20 in the metal substrate of the third embodiment provided by the present invention. In this embodiment, the composite layer 20 includes a first transition layer 211, a first diamond film 221, a second transition layer 212, a second diamond film 222, a third transition layer 213, a third diamond film 223 and a fourth transition layer 214 stacked in sequence. The first transition layer 211 is adjacent to the conductive layer 10, and the first diamond film 221 is adjacent to the first transition layer 211.

[0039] In one embodiment, in the composite layer 20 , the transition layer adjacent to the conductive layer is the first transition layer 211 , the thickness of the first transition layer 211 is 5 μm to 50 μm, and the thickness of the remaining transition layers is 5 μm to 10 μm.

[0040] It should be noted that when the number of transition layers 210 is 2, the thickness of the second transition layer 212 is 5 μm to 10 μm; when the number of transition layers 210 is 3 to 4, the thickness of the second transition layer 212, the third transition layer 213 and the fourth transition layer 214 are each independently 5 μm to 10 μm.

[0041] In one embodiment, in the composite layer 20, the transition layer adjacent to the conductive layer is the first transition layer 211, and the weight difference of the first transition layer 211 is ≤15g / m 2 Except for the first transition layer 211, the weight difference of the remaining transition layers is ≤3g / m 2 .

[0042] It should be noted that the extreme difference in grammage represents the difference in grammage between any two areas in the transition layer 210 .

[0043] In one embodiment, the fluidity of the transition layer 210 is 30% to 60%.

[0044] Specifically, a 10 cm×10 cm transition layer sample with a thickness of 180 μm to 220 μm is pressed for 10 minutes at 170° C. and a pressure of 200 psi, and the fluidity is 30% to 60%.

[0045] It should be noted that the fluidity of the first transition layer 211 and the second transition layer 212 is independently 30% to 60%. When the number of transition layers 210 is 3 to 4, the fluidity of the third transition layer 213 and the fourth transition layer 214 is independently 30% to 60%.

[0046] In one embodiment, the thickness of the diamond film 220 is 5 μm to 15 μm.

[0047] It should be noted that the thickness of the first diamond film 221 is 5 μm to 15 μm. When the number of diamond film layers is 2 to 3, the thicknesses of the first diamond film 221 , the second diamond film 222 , and the third diamond film 223 are each independently 5 μm to 15 μm.

[0048] In one embodiment, the transition layer 210 is selected from a modified diamond powder-thermosetting resin composite film.

[0049] Specifically, the modified diamond powder in the modified diamond powder-thermosetting resin composite film includes: a diamond core and an inorganic coating layer attached to the surface of the diamond core.

[0050] In one embodiment, the product of the particle size and the specific surface area of ​​the diamond core is 9-11.

[0051] In one embodiment, the hydrophilicity and lipophilicity values ​​of the inorganic coating layer are 13-18.

[0052] It should be noted that the inorganic coating layer is selected from cubic boron nitride, cubic carbon nitride, silicon carbide, silicon nitride, nitride containing transition metal elements, carbide containing transition metal elements or boride containing transition metal elements, etc. Since the inorganic coating layer has a large surface activity, it has a good bonding force with the diamond film 220, thereby improving the bonding force between the transition layer 210 and the diamond film 220.

[0053] In one embodiment, the absolute value of the zeta potential of the diamond core surface is 10mV to 20mV, and the absolute value of the zeta potential of the inorganic coating surface is 30mV to 50mV. The modified diamond powder surface has an excellent and stable surface zeta potential, which can effectively resist intermolecular forces. This allows for good dispersion of the modified diamond powder in the thermosetting resin, preventing problems such as air gaps or uneven thickness caused by agglomeration of the modified diamond powder, thereby improving the bonding strength between the modified diamond powder-thermosetting resin composite film and the diamond film 220.

[0054] In one embodiment, the thermal conductivity of the modified diamond powder is ≥1250 W / (m·K), which can effectively ensure the thermal conductivity of the modified diamond powder-thermosetting resin composite film.

[0055] In one embodiment, the thermal conductivity of the inorganic coating layer is ≥30 W / (m·K), which can effectively ensure the thermal conductivity of the modified diamond powder.

[0056] In one embodiment, the thermal conductivity of the metal base plate 30 is ≥ 100 W / (m·K). The metal base plate 30 is the supporting structure of the entire metal substrate, isolating and protecting the metal substrate from external interference. The metal base plate 30 also serves as a heat conductor.

[0057] Specifically, the metal bottom plate 30 is selected from a copper plate, an aluminum plate, a copper-aluminum alloy, and the like.

[0058] In one embodiment, the metal substrate further includes a first thermally conductive resin layer 40, which is disposed between the conductive layer 10 and the composite layer 20. The first thermally conductive resin layer 40 can effectively cover the copper teeth on the surface of the conductive layer 10, thereby improving the bonding between the first transition layer 211 and the conductive layer 10. In addition, the thermal conductivity of the first thermally conductive resin layer 40 is stronger than that of the first transition layer 211, which is beneficial to further increase the thermal conductivity of the metal substrate.

[0059] In one embodiment, the metal substrate further includes a second thermally conductive resin layer 50 , and the second thermally conductive resin layer 50 is disposed between the metal bottom plate 30 and the composite layer 20 .

[0060] like Figure 5 1 is a schematic structural diagram of a metal substrate according to a fourth embodiment of the present invention. In this embodiment, the metal substrate includes a conductive layer 10, a first thermally conductive resin layer 40, a composite layer 20, a second thermally conductive resin layer 50 and a metal base plate 30 stacked in sequence.

[0061] Specifically, the first thermally conductive resin layer 40 and / or the second thermally conductive resin layer 50 includes resin and thermally conductive filler.

[0062] It should be noted that the thermally conductive filler is selected from non-modified diamond micropowders such as aluminum oxide, aluminum nitride, boron nitride, and silicon carbide, which is beneficial to further enhance the bonding force between the first thermally conductive resin layer 40 and the conductive layer 10, and the second thermally conductive resin layer 50 and the metal base plate 30, while improving the fluidity of the first thermally conductive resin layer 40 and the second thermally conductive resin layer 50; the resin is selected from resins commonly used in this field, such as epoxy resin, phenolic resin, and silicone resin, and the present invention is not limited to this.

[0063] In one embodiment, the thickness of the first thermally conductive resin layer 40 is 10 μm to 60 μm, and its thermal conductivity is ≥ 4 W / (m·K);

[0064] And / or, the thickness 50 of the second thermally conductive resin layer is 10 μm to 20 μm, and the thermal conductivity thereof is ≥ 4 W / (m·K).

[0065] In one embodiment, the thickness of the first diamond film 221 is 5 μm to 15 μm, and the ratio of the thickness of the first thermally conductive resin layer 40 to the thickness of the first diamond film is 2:1 to 3:1, which can enhance the adhesion between the first diamond film 221 and the conductive layer 10 while ensuring the thermal conductivity of the metal substrate.

[0066] In one embodiment, the thickness of the first transition layer 211 is 5 μm to 15 μm, and the ratio of the thickness of the first thermally conductive resin layer 40 to the thickness of the first transition layer 211 is 2:1 to 3:1, which can better balance the thermal conductivity and insulation of the metal substrate.

[0067] The technical features of the above-mentioned embodiments can be combined arbitrarily. In order to make the description concise, not all possible combinations of the technical features in the above-mentioned embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0068] The above-described embodiments merely represent several implementations of the present invention. While the descriptions are relatively specific and detailed, they should not be construed as limiting the scope of the utility model patent. It should be noted that a person skilled in the art would be able to make various modifications and improvements without departing from the concept of the present invention, and these modifications and improvements fall within the scope of protection of the present invention. Therefore, the scope of protection of the present utility model patent shall be determined by the appended claims.

Claims

1. A metal substrate, characterized in that: The metal substrate comprises a conductive layer, a composite layer and a metal bottom plate which are stacked in sequence, the composite layer comprises at least two stacked transition layers, and a diamond film is sandwiched between two adjacent transition layers; The peeling strength between the transition layer and the conductive layer is greater than 0.5 N / mm, the peeling strength between the transition layer and the metal base plate is greater than 0.2 N / mm, and the push-pull force between the transition layer and the diamond film is greater than or equal to 100 N.

2. The metal substrate according to claim 1, characterized in that: The transition layer has 2 to 4 layers.

3. The metal substrate according to claim 1, characterized in that: In the composite layer, the transition layer adjacent to the conductive layer is a first transition layer, and the composite layer satisfies at least one of the following conditions: (1) The thickness of the first transition layer is 5 μm to 50 μm, and the thickness of the remaining transition layers except the first transition layer is 5 μm to 10 μm; (2) The weight difference of the first transition layer is ≤15g / m 2 Except for the first transition layer, the weight difference of the remaining transition layers is ≤3g / m 2 ; (3) The fluidity of the transition layer is 30% to 60%; (4) The thickness of the diamond film is 5 μm to 15 μm.

4. The metal substrate according to claim 1, characterized in that: The thermal conductivity of the metal bottom plate is ≥100 W / (m·K).

5. The metal substrate according to any one of claims 1 to 4, characterized in that: The metal substrate further comprises a first thermally conductive resin layer, wherein the first thermally conductive resin layer is disposed between the conductive layer and the composite layer; And / or, the metal substrate further includes a second thermally conductive resin layer, and the second thermally conductive resin layer is disposed between the metal base plate and the composite layer.

6. The metal substrate according to claim 5, characterized in that: The thickness of the first thermally conductive resin layer is 10 μm to 60 μm, and its thermal conductivity is ≥ 4 W / (m·K); And / or, the second thermally conductive resin layer has a thickness of 10 μm to 20 μm and a thermal conductivity of ≥4 W / (m·K).

7. The metal substrate according to claim 5, characterized in that: The transition layer adjacent to the conductive layer is a first transition layer, the diamond film adjacent to the first transition layer is a first diamond film, the thickness of the first diamond film is 5 μm to 15 μm, and the ratio of the thickness of the first thermally conductive resin layer to the thickness of the first diamond film is 2:1 to 3:1; And / or, the transition layer adjacent to the conductive layer is a first transition layer, the thickness of the first transition layer is 5 μm to 15 μm, and the ratio of the thickness of the first thermally conductive resin layer to the thickness of the first transition layer is 2:1 to 3:1.