Substrate table bearing device for preparing polycrystalline diamond through MPCVD
By using arc-shaped protruding table components and threaded connections in the substrate table carrying device for preparing polycrystalline diamond by MPCVD, the problems of uniform shape and difficult processing of polycrystalline diamond are solved, and the growth and efficient processing of diversified shapes are achieved to meet the needs market demand and increased growth rates.
Patent Information
- Application Number
- CN202420403142.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-01
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2034-03-01
AI Technical Summary
In the existing technology, the uniform shape of polycrystalline diamond cannot meet market demand, and due to its difficulty in processing, it cannot meet actual demand.
A substrate table carrying device for MPCVD preparation of polycrystalline diamond is designed. The arc-shaped raised table components are arranged in a ladder shape and are connected through threaded columns and threaded grooves, which allows the production of polycrystalline diamonds of different shapes and facilitates the production of polycrystalline diamonds of different shapes. Its processing and removal.
It diversifies the shape of polycrystalline diamond, increases its growth rate, and simplifies the processing and removal process, meets market demand, and increases the practicality of the device.
Smart Images

Figure CN221837144U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of polycrystalline diamond preparation, in particular to a substrate table bearing device used for preparing polycrystalline diamond by MPCVD. Background Art
[0002] Microwave plasma chemical vapor deposition (MPCVD) uses microwaves to form an electric field behind a special resonant cavity, decomposing raw gases such as hydrogen and methane into atomic hydrogen and a series of plasmas, and then depositing and growing diamonds at a certain temperature. Due to its advantages such as pollution-free microwave energy and pure gas raw materials, it has become the preferred solution for preparing large-size, high-quality diamonds.
[0003] In order to increase the diamond deposition rate, the existing technology often makes the substrate table open, and the molybdenum table is very flat. However, when growing polycrystalline diamonds, it will cause the shape of the polycrystalline diamonds to be uniform. Since polycrystalline diamonds are difficult to process, it cannot meet market demand. Utility Model Content
[0004] The utility model provides a substrate stage bearing device for preparing polycrystalline diamond by MPCVD, which has the beneficial effect of being able to produce polycrystalline diamonds of different shapes, and solves the problem mentioned in the above background technology that the uniform shape of polycrystalline diamonds cannot meet market demand.
[0005] To achieve the above-mentioned purpose, the utility model provides the following technical solutions: a substrate stage supporting device for preparing polycrystalline diamond by MPCVD, comprising a substrate stage main body, on which an arc-shaped protrusion stage assembly is arranged, the arc-shaped protrusion stage assembly is arranged in a stepped shape, a threaded column is fixedly connected to the bottom of the arc-shaped protrusion stage assembly, a threaded groove is provided on the substrate stage main body relative to the position of the threaded column, and the threaded column and the threaded groove are threadedly connected.
[0006] Preferably, the arc-shaped protrusion platform assembly consists of a first arc-shaped protrusion platform, a second arc-shaped protrusion platform and a third arc-shaped protrusion platform arranged from the inside to the outside, the number of the second arc-shaped protrusion platforms and the number of the third arc-shaped protrusion platforms are eight, the eight second arc-shaped protrusion platforms and the eight third arc-shaped protrusion platforms are all located on the same circle with the axis of the first arc-shaped protrusion platform as the center, and the distance between the first arc-shaped protrusion platform, the second arc-shaped protrusion platform and the third arc-shaped protrusion platform is fifteen millimeters.
[0007] Preferably, the substrate stage main body, the first arc-shaped raised stage, the second arc-shaped raised stage and the third arc-shaped raised stage are all arranged in a cylindrical structure, and the radius of the substrate stage main body is thirty-five millimeters.
[0008] Preferably, the first arc-shaped raised platform, the second arc-shaped raised platform and the third arc-shaped raised platform each include a first layer component, a second layer component, a third layer component and a fourth layer component arranged in sequence from bottom to top, and the total height of the first layer component, the second layer component, the third layer component and the fourth layer component is 3.08 mm.
[0009] Preferably, the first layer component is composed of protrusions with a radius of 2.45 mm and a protrusion height of 0.48 mm, the second layer component is composed of a cylindrical cone with a radius of 2.75 mm and a height of 0.3 mm, the third layer component is composed of a fillet with a radius of 0.3 mm, and the fourth layer component is a hyperbola, with the upper and lower surfaces of the fourth layer component having a radius of 0.5 mm, a curved surface radius of 3 mm, and an angle of 38.94 degrees.
[0010] Preferably, the surface roughness of the substrate stage body is twenty microns.
[0011] The utility model has the following beneficial effects:
[0012] The substrate stage supporting device for preparing polycrystalline diamond by MPCVD can diversify the shape of the polycrystalline diamond after it grows by arranging an arc-shaped raised stage assembly, thereby meeting market demand, and can prevent the polycrystalline diamond from being too flat after growth, thereby facilitating processing thereof. In addition, the arc-shaped raised stage assembly is arranged in a stepped shape, so that it is convenient to remove the polycrystalline diamond after it grows, and the arc-shaped raised stage assembly is arranged to facilitate disassembly and installation, thereby meeting the growth of polycrystalline diamonds of different shapes, greatly increasing the practicability of the device, and solving the problem in the prior art that the shape of the diamond is uniform and the molybdenum stage is very flat, resulting in difficult processing and failing to meet market demand. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] Figure 1 It is a schematic diagram of the overall structure of the utility model.
[0014] Figure 2 It is a schematic diagram of the exploded structure of the arc-shaped raised platform of the utility model.
[0015] Figure 3 It is a schematic diagram of the exploded structure of the substrate platform main body and the arc-shaped raised platform assembly of the utility model.
[0016] In the figure: 1, substrate stage body; 2, arc-shaped raised stage assembly; 3, threaded column; 4, threaded groove;
[0017] 201, first arc-shaped raised platform; 202, second arc-shaped raised platform; 203, third arc-shaped raised platform;
[0018] 2041, first layer component; 2042, second layer component; 2043, third layer component; 2044, fourth layer component. DETAILED DESCRIPTION
[0019] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0020] Example:
[0021] See also Figure 1-Figure 3 A substrate stage supporting device for preparing polycrystalline diamond by MPCVD, comprising a substrate stage main body 1, an arc-shaped raised stage assembly 2 arranged on the substrate stage main body 1, the arc-shaped raised stage assembly 2 being arranged in a stepped shape, a threaded column 3 being fixedly connected to the bottom of the arc-shaped raised stage assembly 2, a threaded groove 4 being provided on the substrate stage main body 1 at a position corresponding to the threaded column 3, the threaded column 3 and the threaded groove 4 being threadedly connected; the arc-shaped raised stage assembly 2 is composed of a first arc-shaped raised stage 201, a second arc-shaped raised stage 202 and a third arc-shaped raised stage 203 arranged from inside to outside The substrate stage body 1 is composed of an arc-shaped raised platform 203, the number of the second arc-shaped raised platform 202 and the number of the third arc-shaped raised platform 203 are both eight, the eight second arc-shaped raised platforms 202 and the eight third arc-shaped raised platforms 203 are all located on the same circle with the axis of the first arc-shaped raised platform 201 as the center, and the distances between the first arc-shaped raised platform 201, the second arc-shaped raised platform 202 and the third arc-shaped raised platform 203 are all fifteen millimeters; the substrate stage body 1, the first arc-shaped raised platform 201, the second arc-shaped raised platform 202 and the third arc-shaped raised platform 203 are all cylindrically structured, and the radius of the substrate stage body 1 is thirty-five millimeters; the first arc-shaped raised platform 201, the second arc-shaped raised platform 202 and the third arc-shaped raised platform 203 all include a first layer component 2041, a second layer component 2042, a third layer component 2043 and a fourth layer component 2044 arranged in sequence from bottom to top, and the total height of the first layer component 2041, the second layer component 2042, the third layer component 2043 and the fourth layer component 2044 is three point eight millimeters; the first layer component 20 41 is composed of a protrusion with a radius of 2.45 mm and a protrusion height of 0.48 mm, the second layer component 2042 is composed of a cylindrical table with a radius of 2.75 mm and a height of 0.3 mm, the third layer component 2043 is composed of a fillet with a radius of 0.3 mm, the fourth layer component 2044 is a hyperbola, the upper and lower surfaces of the fourth layer component 2044 have a radius of 0.5 mm, a curved surface radius of 3 mm, and an angle of 38.94 degrees; the surface roughness of the substrate stage main body 1 is 20 microns.
[0022] In this embodiment, by providing an arc-shaped protrusion platform assembly 2, the shape of the polycrystalline diamond can be diversified after growth, thereby meeting market demand, and at the same time, the polycrystalline diamond can be prevented from being too flat after growth, thereby facilitating its processing. In addition, the arc-shaped protrusion platform assembly 2 is arranged in a stepped shape, which is convenient for removing the polycrystalline diamond after growth. By providing a threaded column 3 and a threaded groove 4, the arc-shaped protrusion platform assembly 2 is convenient for disassembly and installation, thereby meeting the growth of polycrystalline diamonds of different shapes and greatly increasing the practicability of the device.
[0023] When preparing polycrystalline diamond, the substrate table main body 1 is placed in the deposition table cavity, and six 7mm long molybdenum wires are evenly padded under the substrate table main body 1. The pressure in the deposition table cavity is pumped below 0.5Pa, and then the deposition table cavity side leakage detection is performed. After the cavity side leakage detection is completed, the deposition table cavity is cleaned with hydrogen. After completing the above steps, the microwave is turned on, and then the hydrogen valve is opened. The hydrogen flow value is set to 100l / min, the power is set to 1000W, and the pressure is increased to 3KPa. Then, the automatic temperature rise is turned on, the hydrogen flow value is set to 400l / min, the power increase speed is set to 200W / min, the pressure is set to 0.7KPa / min, the power is increased to 5000W, the pressure is set to 17.5Kpa, the temperature is increased to 700℃, and etching is carried out for 1h.
[0024] After etching is completed, open the nitrogen valve and set the nitrogen flow value to 1.8 l / min, open the oxygen valve and set the oxygen flow value to 0.6 l / min, open the argon valve and set the argon flow value to 8 l / min. Then set the power increase rate to 200 W / min, the pressure to 0.7 KPa / min, increase the power to 5500 W, the pressure to 19.25 KPa, the temperature to 700 ° C, and then etch for another 1 hour.
[0025] After etching is completed, open the methane valve, set the methane flow value to 26l / min, then set the power increase rate to 200W / min, the pressure to 0.7KPa / min, increase the power to 6200W, the pressure to 22Kpa, the temperature to 900℃, and grow for 15h.
[0026] When the growth of polycrystalline diamond is completed, close the valves of methane, nitrogen, oxygen, and argon gases, stop introducing them into the deposition table cavity, and then set the power reduction rate to 50W / min and the pressure to 0.175KPa / min, reduce the power to 1000W, and the pressure to 3KPa, and then cool down in a gradient of 100℃, and then keep warm for 1h every 100℃ until it reaches room temperature, turn off the microwave, stop introducing hydrogen, and open the cavity to obtain polycrystalline diamond.
[0027] According to experiments, when an open substrate table is used for polycrystalline diamond growth experiments, the growth rate is 8.4μm / h, while when this device is used for polycrystalline diamond growth experiments, the growth rate is 10.6μm / h. Therefore, this device can increase the growth rate of polycrystalline diamond. At the same time, it can also produce polycrystalline diamonds of different shapes according to market demand and facilitate the removal of polycrystalline diamonds, which greatly increases the practicality of the device.
[0028] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.
[0029] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the technical principle of the present invention. These improvements and modifications should also be regarded as the protection scope of the present invention.
Claims
1. A substrate stage supporting device for preparing polycrystalline diamond by MPCVD, comprising a substrate stage main body (1), characterized in that: The substrate platform body (1) is provided with an arc-shaped protruding platform component (2), the arc-shaped protruding platform component (2) is arranged in a stepped shape, a threaded column (3) is fixedly connected to the bottom of the arc-shaped protruding platform component (2), a threaded groove (4) is provided on the substrate platform body (1) at a position relative to the threaded column (3), and the threaded column (3) and the threaded groove (4) are threadedly connected.
2. The substrate stage supporting device for preparing polycrystalline diamond by MPCVD according to claim 1, characterized in that: The arc-shaped protrusion platform assembly (2) is composed of a first arc-shaped protrusion platform (201), a second arc-shaped protrusion platform (202) and a third arc-shaped protrusion platform (203) arranged from the inside to the outside, the number of the second arc-shaped protrusion platform (202) and the number of the third arc-shaped protrusion platform (203) are both eight, the eight second arc-shaped protrusion platforms (202) and the eight third arc-shaped protrusion platforms (203) are all located on the same circle with the axis of the first arc-shaped protrusion platform (201) as the center, and the distance between the first arc-shaped protrusion platform (201), the second arc-shaped protrusion platform (202) and the third arc-shaped protrusion platform (203) is fifteen millimeters.
3. The substrate stage supporting device for preparing polycrystalline diamond by MPCVD according to claim 2, characterized in that: The substrate stage body (1), the first arc-shaped raised platform (201), the second arc-shaped raised platform (202) and the third arc-shaped raised platform (203) are all arranged in a cylindrical structure, and the radius of the substrate stage body (1) is thirty-five millimeters.
4. The substrate stage supporting device for preparing polycrystalline diamond by MPCVD according to claim 2, characterized in that: The first arc-shaped protruding platform (201), the second arc-shaped protruding platform (202) and the third arc-shaped protruding platform (203) each include a first layer component (2041), a second layer component (2042), a third layer component (2043) and a fourth layer component (2044) which are arranged in sequence from bottom to top, and the total height of the first layer component (2041), the second layer component (2042), the third layer component (2043) and the fourth layer component (2044) is 3.08 millimeters.
5. The substrate stage supporting device for preparing polycrystalline diamond by MPCVD according to claim 4, characterized in that: The first layer component (2041) is composed of a protrusion with a radius of 2.45 mm and a protrusion height of 0.48 mm, the second layer component (2042) is composed of a cylindrical cone with a radius of 2.75 mm and a height of 0.3 mm, the third layer component (2043) is composed of a fillet with a radius of 0.3 mm, and the fourth layer component (2044) is a hyperbola. The upper and lower surfaces of the fourth layer component (2044) have a radius of 0.5 mm, a curved surface radius of 3 mm, and an angle of 38.94 degrees.
6. The substrate stage supporting device for preparing polycrystalline diamond by MPCVD according to claim 1, characterized in that: The surface roughness of the substrate stage main body (1) is twenty micrometers.