Aluminum profile plastic deformation prevention extrusion die
By designing a temperature-controlled anti-plastic deformation extrusion mold for aluminum profiles, and using heating and cooling technology and a pump conveying system, the problem of deformation of aluminum profiles caused by failure to cool in time is solved, and rapid cooling and solid molding of aluminum profiles are achieved.
Patent Information
- Application Number
- CN202323426465.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-15
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2033-12-15
AI Technical Summary
After aluminum profiles are extruded, failure to cool them in time may cause deformation problems.
An anti-plastic deformation extrusion mold for aluminum profiles is designed. It adopts the temperature control system of mold one and mold two. The heating block and semiconductor refrigerator are used to increase and decrease the mold temperature respectively. The pump body is used to transport hot water and cold water to make the mold The second mold is used for extrusion molding, and the first mold is used for cooling and shaping. It combines the insulation cotton and the rotation system to ensure that the aluminum profile is cooled quickly after extrusion.
It effectively avoids the deformation of aluminum profiles due to insufficient cooling in time, improves the mechanical and physical properties of the material, and ensures the solidity after forming.
Smart Images

Figure CN221848232U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the field of aluminum profiles, in particular to an aluminum profile anti-plastic deformation extrusion die. Background Art
[0002] Industrial aluminum profiles, also known as industrial aluminum extrusions and industrial aluminum alloy profiles, are an alloy material with aluminum as the main component. Aluminum rods are hot-melted and extruded to obtain aluminum materials with different cross-sectional shapes. However, the proportion of the added alloy is different, and the mechanical properties and application fields of the produced industrial aluminum profiles are also different. The extrusion process requires an extrusion die to complete the extrusion operation.
[0003] After being heated, the round cast rod is extruded through an extrusion die and then cooled to improve the mechanical and physical properties of the material. After the aluminum profile is extruded and discharged, it needs to be suspended and moved a short distance to a cooling mechanism for cooling. After the aluminum profile is extruded, it may be deformed due to lack of timely cooling during the process of moving to the cooling mechanism. Therefore, those skilled in the art provide an aluminum profile anti-plastic deformation extrusion die to solve the problems raised in the above background technology. Utility Model Content
[0004] In order to solve the above technical problems, the utility model provides an aluminum profile anti-plastic deformation extrusion die, comprising a die one, a die two, a die three and a box body, wherein the die three is arranged between the die one and the die two, a cavity is arranged inside the die three, and a thermal insulation cotton is installed inside the cavity, an annular cavity is symmetrically arranged inside the die one and the die two, and a plurality of conveying cavities are evenly connected between the two annular cavities, an insulation plate is installed in the middle of the box body, a rotating shaft is symmetrically arranged inside the box body, and the upper end of the rotating shaft passes through the box body and is installed with a bevel gear one, and a plurality of stirring plates are symmetrically installed on the outer surface of the rotating shaft;
[0005] A rotating rod is arranged above the box body, a baffle is symmetrically sleeved on the outer surface of the rotating rod, and the baffle is fixedly connected to the box body, a motor is installed on the right end of the rotating rod, two bevel gears 2 are installed on the outer surface of the rotating rod, and the bevel gears 2 and 1 are meshed, a plurality of heating blocks are installed on the front wall of the box body, a semiconductor refrigerator is symmetrically installed on the right end of the box body, and the semiconductor refrigerator is located behind the insulation board;
[0006] Two extraction pipes are installed at the right end of the box body, and the two extraction pipes are located on both sides of the insulation board. A pump body is installed at the right end of the extraction pipe. A delivery pipe is installed at the right end of the pump body, and the delivery pipe is connected to the delivery cavity of mold one and mold two. A return pipe is installed at the upper end of the box body, and the return pipe is connected to the delivery cavity of mold one and mold two.
[0007] Preferably, connection blocks are installed at both upper and lower ends of the mold 1 and the mold 2.
[0008] Preferably, fixing blocks are installed at both upper and lower ends of the mold 3.
[0009] Preferably, connection grooves are provided at the front and rear ends of the fixing block, and the connection grooves correspond to the positions of the connection blocks.
[0010] Preferably, a cavity is provided inside the fixing block, and the interior of the cavity is slidably connected to the pull plate.
[0011] Preferably, a blocking block is symmetrically mounted on the lower end of the pull plate, and the blocking block passes through the upper end of the connecting groove, and the outer end surfaces of the two blocking blocks are arc surfaces.
[0012] Preferably, a pull rod is installed on the upper end of the pull plate, and the pull rod passes through the fixed block and is installed with a pull ring, and a spring is symmetrically installed on the upper end of the pull plate.
[0013] The utility model is convenient to disassemble and install between the mold one, the mold two and the mold three. The heating block works to increase the water temperature on one side of the insulation board, and the semiconductor refrigerator works to reduce the water temperature on the other side of the insulation board. The pump body transports the hot water and cold water inside the box body to the mold two and the mold one respectively, so that the temperature of the mold two is increased and the temperature of the mold one is reduced. The round cast rod first enters the mold two through extrusion. The high temperature of the mold two effectively helps the aluminum profile to be extruded and formed. The low temperature of the mold one accelerates the cooling and shaping of the aluminum profile, so that the extruded aluminum profile is cooled and firm and not easy to deform, thereby avoiding deformation of the aluminum profile due to failure to cool in time after being heated and extruded. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Figure 1 It is a schematic diagram of the structure of this application;
[0015] Figure 2 It is a schematic diagram of the structure of the connection block of this application;
[0016] Figure 3 It is a structural schematic diagram of the annular cavity of the present application;
[0017] Figure 4 It is a schematic diagram of the structure of the fixed block of this application;
[0018] Figure 5 It is a structural schematic diagram of the box of this application;
[0019] Figure numerals: 1, mold one, 2, mold two, 3, mold three, 4, connecting block, 5, fixing block, 6, connecting groove, 7, cavity, 8, pull plate, 9, blocking block, 10, spring, 11, pull rod, 12, annular cavity, 13, conveying cavity, 14, box body, 15, insulation plate, 16, rotating shaft, 17, stirring plate, 18, bevel gear one, 19, rotating rod, 20, bevel gear two, 21, motor, 22, heating block, 23, semiconductor refrigerator, 24, pump body, 25, extraction pipe, 26, conveying pipe, 27, reflux pipe. DETAILED DESCRIPTION
[0020] The utility model is further described in detail below in conjunction with the accompanying drawings and specific implementation methods.
[0021] The embodiments of the present invention are provided for the purpose of illustration and description, and are not intended to be exhaustive or to limit the present invention to the disclosed forms. Many modifications and variations will be apparent to those of ordinary skill in the art. The embodiments are selected and described to better illustrate the principles and practical applications of the present invention, and to enable those of ordinary skill in the art to understand the present invention and thereby design various embodiments with various modifications suitable for specific uses.
[0022] A plastic deformation-proof extrusion die for aluminum profiles, see Figures 1 to 5 , including mold 1, mold 2, mold 3 and box 14, mold 3 3 is arranged between mold 1 and mold 2, a cavity is arranged inside mold 3, and thermal insulation cotton is installed inside the cavity, connecting blocks 4 are installed at both upper and lower ends of mold 1 and mold 2, and fixed blocks 5 are installed at both upper and lower ends of mold 3, connecting grooves 6 are arranged at the front and rear ends of the fixed block 5, and the connecting grooves 6 correspond to the positions of the connecting blocks 4, a cavity 7 is arranged inside the fixed block 5, a pull plate 8 is slidably connected inside the cavity 7, a blocking block 9 is symmetrically installed at the lower end of the pull plate 8, and the blocking block 9 passes through the upper end of the connecting groove 6, and the outer end faces of the two blocking blocks 9 are arc surfaces, a pull rod 11 is installed at the upper end of the pull plate 8, and the pull rod 11 passes through the fixed block 5 and is installed with a pull ring, and a spring 10 is symmetrically installed at the upper end of the pull plate 8;
[0023] Annular cavities 12 are symmetrically arranged inside mold 1 and mold 2, and a plurality of conveying cavities 13 are evenly connected between the two annular cavities 12. A temperature insulation plate 15 is installed in the middle of the box body 14. A rotating shaft 16 is symmetrically arranged inside the box body 14, and the upper end of the rotating shaft 16 passes through the box body 14 and is installed with a bevel gear 18. A plurality of stirring plates 17 are symmetrically installed on the outer surface of the rotating shaft 16. A rotating rod 19 is arranged above the box body 14, and a baffle is symmetrically sleeved on the outer surface of the rotating rod 19, and the baffle is fixedly connected to the box body 14. A motor 21 is installed at the right end of the rotating rod 19, and two bevel gears 20 are installed on the outer surface of the rotating rod 19, and the bevel gears 20 are installed on the outer surface of the rotating rod 19. Gear 2 20 is meshed with bevel gear 1 18, a plurality of heating blocks 22 are installed on the front wall of the box body 14, a semiconductor refrigerator 23 is symmetrically installed on the right end of the box body 14, and the semiconductor refrigerator 23 is located behind the insulation board 15, two extraction pipes 25 are installed on the right end of the box body 14, and the two extraction pipes 25 are located on both sides of the insulation board 15, a pump body 24 is installed on the right end of the extraction pipe 25, a delivery pipe 26 is installed on the right end of the pump body 24, and the delivery pipe 26 is connected to the delivery chamber 13 of mold 1 1 and mold 2 2, a return pipe 27 is installed on the upper end of the box body 14, and the return pipe 27 is connected to the delivery chamber 13 of mold 1 1 and mold 2 2.
[0024] The working principle of the utility model is: the pull plate 8 is pulled up by the pull ring and the pull rod 11 to compress the spring 10, the pull plate 8 drives the blocking block 9 to rise and retract into the cavity 7, and the connecting blocks 4 of the mold 1 and the mold 2 are respectively inserted into the two connecting grooves 6, and then the pull ring is released, and the pull plate 8 is pushed to reset by the spring 10, and the pull plate 8 is reset to drive the blocking block 9 to insert into the connecting groove 6, so that the blocking block 9 is blocked at one end of the connecting block 4, so that the mold 1, the mold 2 and the mold 3 are installed together;
[0025] The box 14 is filled with water. The heating block 22 works to increase the water temperature on one side of the insulation board 15. The semiconductor refrigerator 23 works to reduce the temperature on the other side of the insulation board 15 of the box 14, so that the water temperature on the other side of the insulation board 15 is reduced. The water temperature on one side of the insulation board 15 in the box 14 is high, and the water temperature on the other side of the insulation board 15 is low. At the same time, the motor 21 drives the rotating shaft 16 to rotate through the rotating rod 19, the bevel gear 20 and the bevel gear 1 18. The rotating shaft 16 drives the stirring plate 17 to rotate to stir the water, thereby improving the heating and cooling efficiency of the water after recycling.
[0026] The pump body 24 transports the hot water and cold water in the box body 14 to the mold 2 2 and the mold 1 1 respectively through the extraction pipe 25 and the delivery pipe 26, so that the temperature of the mold 2 2 increases and the temperature of the mold 1 decreases. The round cast rod first enters the mold 2 2 through extrusion. The high temperature of the mold 2 2 effectively helps the aluminum profile to be extruded and formed. The formed aluminum profile then passes through the mold 3 3 and enters the mold 1 1. The low temperature of the mold 1 accelerates the cooling and shaping of the aluminum profile, so that the extruded aluminum profile is cooled and firm and not easy to deform, thereby avoiding deformation of the aluminum profile due to failure to cool in time after being heated and extruded, and blocking the temperature transfer through the insulation cotton inside the mold 3 3.
Claims
1. An aluminum profile anti-plastic deformation extrusion die, characterized in that: The invention comprises a mold 1 (1), a mold 2 (2), a mold 3 (3) and a box (14), wherein the mold 3 (3) is arranged between the mold 1 (1) and the mold 2 (2), a cavity is arranged inside the mold 3 (3), and a thermal insulation cotton is installed inside the cavity, an annular cavity (12) is symmetrically arranged inside the mold 1 (1) and the mold 2 (2), and a plurality of conveying cavities (13) are evenly connected between the two annular cavities (12), an insulation plate (15) is installed in the middle of the box (14), a rotating shaft (16) is symmetrically arranged inside the box (14), and the upper end of the rotating shaft (16) passes through the box (14) and is installed with a bevel gear 1 (18), and a plurality of stirring plates (17) are symmetrically installed on the outer surface of the rotating shaft (16); A rotating rod (19) is arranged above the box body (14), a baffle is symmetrically sleeved on the outer surface of the rotating rod (19), and the baffle is fixedly connected to the box body (14), a motor (21) is installed at the right end of the rotating rod (19), two bevel gears (20) are installed on the outer surface of the rotating rod (19), and the bevel gears (20) and the bevel gears (18) are meshed, a plurality of heating blocks (22) are installed on the inner front wall of the box body (14), and a semiconductor refrigerator (23) is symmetrically installed at the right end of the box body (14), and the semiconductor refrigerator (23) is located behind the insulation board (15); Two extraction pipes (25) are installed at the right end of the box body (14), and the two extraction pipes (25) are located on both sides of the insulation board (15). A pump body (24) is installed at the right end of the extraction pipe (25). A delivery pipe (26) is installed at the right end of the pump body (24), and the delivery pipe (26) is connected to the delivery chamber (13) of the mold 1 (1) and the mold 2 (2). A return pipe (27) is installed at the upper end of the box body (14), and the return pipe (27) is connected to the delivery chamber (13) of the mold 1 (1) and the mold 2 (2).
2. The anti-plastic deformation extrusion die for aluminum profiles according to claim 1, characterized in that: Connecting blocks (4) are installed at both upper and lower ends of the mold 1 (1) and the mold 2 (2).
3. The anti-plastic deformation extrusion die for aluminum profiles according to claim 1, characterized in that: Fixed blocks (5) are installed at both upper and lower ends of the mold three (3).
4. The anti-plastic deformation extrusion die for aluminum profiles according to claim 3, characterized in that: The fixing block (5) is provided with connection grooves (6) at the front and rear ends, and the connection grooves (6) correspond to the positions of the connection blocks (4).
5. The aluminum profile anti-plastic deformation extrusion die according to claim 3, characterized in that: A cavity (7) is arranged inside the fixed block (5), and a pull plate (8) is slidably connected inside the cavity (7).
6. The aluminum profile anti-plastic deformation extrusion die according to claim 5, characterized in that: The lower end of the pull plate (8) is symmetrically mounted with a blocking block (9), and the blocking block (9) passes through the upper end of the connecting groove (6), and the outer end surfaces of the two blocking blocks (9) are arc surfaces.
7. The anti-plastic deformation extrusion die for aluminum profiles according to claim 5, characterized in that: A pull rod (11) is installed on the upper end of the pull plate (8), and the pull rod (11) passes through the fixed block (5) and is installed with a pull ring. A spring (10) is symmetrically installed on the upper end of the pull plate (8).