Counter-pressure casting pouring system for aluminum alloy box body
By adopting the heat storage steady flow lateral runner and necking riser design in the differential pressure casting gating system of the aluminum alloy box, combined with the riser feeding runner and the casting feeding runner, the problem of box castings is solved It solves the problems of defects such as shrinkage cavities, porosity, pores and slag inclusions, and achieves increased density and stable quality of castings, and is suitable for mass production of large aluminum alloy boxes.
Patent Information
- Application Number
- CN202420389705.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-29
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2034-02-28
AI Technical Summary
During the casting and molding process of box castings, defects such as shrinkage cavities, porosity, pores, and slag inclusions caused by air entrainment are prone to occur. Traditional gravity casting and low-pressure casting processes cannot effectively solve these problems.
A differential pressure casting gating system for aluminum alloy boxes is designed, which adopts a heat-storage steady-flow lateral runner and a necked riser-type first inner gate, combined with a riser feeding runner and a casting feeding runner. The structural parameters of the gating system are optimized to ensure stable temperature of the molten metal and smooth mold filling, minimize secondary oxidation of the molten metal, and solve the feeding problem through the cooperation of the forming cold iron.
It effectively solves defects such as shrinkage cavities, porosity, pores and slag inclusions in castings, achieves increased density and stable quality of castings, and is suitable for mass production of large aluminum alloy boxes.
Smart Images

Figure CN221848617U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the field of casting, in particular to a differential pressure casting pouring system for an aluminum alloy box. Background Art
[0002] Differential pressure casting is a casting method derived from low-pressure casting. This casting method adds a cover to the casting shape, fills it with compressed air, and puts the casting mold under a certain gas pressure. When the alloy liquid fills the casting mold from bottom to top, the casting can crystallize and solidify under higher pressure, obtaining a casting with higher density.
[0003] Box castings are generally large, thin-walled, complex, and high-performance. They need to withstand large loads and have strict airtightness requirements. They are required to have high specific strength (strength / density) and specific stiffness (stiffness / density). At the same time, in order to reduce weight, high-strength aluminum alloys or forged aluminum alloys are generally used as materials.
[0004] In the casting process of box castings, the characteristics are: it is difficult to compensate for shrinkage, and it is easy to produce shrinkage holes, looseness, and defects such as pores and slag inclusions caused by air entrapment. At present, traditional gravity casting and low-pressure casting processes cannot produce such large aluminum alloy castings, which show a series of defects such as shrinkage holes, looseness, pores and slag inclusions. In the field of differential pressure casting, the gating system of most castings is a gap gating system. However, the gap gating system has great limitations. If the inner and outer surfaces of the casting are not processed and there are a large number of reinforcing ribs, it is not suitable for this gating system. Utility Model Content
[0005] The technical problem to be solved by the utility model is that the existing box-type castings are prone to shrinkage holes, looseness, air holes caused by air entrapment, slag inclusions and other defects during casting. The utility model provides a differential pressure casting pouring system for an aluminum alloy box to solve the above problems.
[0006] The technical solution adopted by the utility model to solve its technical problems is: a differential pressure casting pouring system for an aluminum alloy box, comprising a cavity, a straight runner arranged below the cavity and a riser arranged above the cavity, a cross runner is arranged horizontally below the cavity, the cross runner is connected to the straight runner, and a first inner gate is arranged between the cross runner and the cavity; the cross runner is connected to a casting shrinkage feeding runner arranged vertically, and a second inner gate is arranged between the casting shrinkage feeding runner and the cavity; a riser shrinkage feeding runner is arranged between the cross runner and the riser.
[0007] Furthermore: the riser is in an integrally connected form distributed flatly above the cavity.
[0008] Furthermore: the type of the runner is a heat storage steady flow type, and the type of the first inner gate is a necking riser type.
[0009] Further: suppose that the parameter of the structure included in the pouring system is the modulus M, M is the ratio of the volume V of the structure to the effective heat dissipation area S, that is, M=V / S, the straight runner M>the cross runner M>the casting shrinkage feeding runner M, the riser shrinkage feeding runner M>the second inner gate M>the cavity M, the cross runner M>the first inner gate M, the riser M>the riser part M corresponding to the cavity.
[0010] Furthermore, the end length of the cross runner is 0.5-1 times of the width of the cross runner, and the end length of the straight runner is greater than the diameter of the straight runner.
[0011] Further: the average wall thickness of the casting at the position corresponding to the first ingates is denoted as δ, and the length of the first ingates is <5δ; the diameter of the second ingates is denoted as D, and when the length of the second ingates is <1.5D, the type of the second ingates is cylindrical; when the length of the second ingates is ≥1.5D, the type of the second ingates is a necking riser type.
[0012] The beneficial effect of the utility model is that the differential pressure casting pouring system of the aluminum alloy box changes the general cross runner into a heat storage steady flow cross runner, so that the filling is smooth and the temperature of the molten metal is stable, which is beneficial to the filling of the casting and minimizes the secondary oxidation of the molten metal. The first inner gate is designed as a necking riser mode, which is more conducive to the shrinkage compensation of the product in counter-gravity casting. The risers are connected together and a hot riser is directly formed through the riser shrinkage compensation runner, so that the riser is in an effective shrinkage compensation state. The remaining parts that need to be compensated are directly compensated from the diameter channel designed for the heat storage steady flow cross runner, and the use of forming cold iron is combined with the use of forming cold iron to completely solve a series of defects such as shrinkage holes, looseness, pores and slag inclusions in the casting. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] The utility model is further described below in conjunction with the accompanying drawings and embodiments.
[0014] Figure 1 It is a schematic diagram of the structural assembly of the differential pressure casting pouring system of the aluminum alloy box of the utility model;
[0015] Figure 2 yes Figure 1 Schematic diagram of the gating system assembly structure after the cavity is deleted.
[0016] In the figure, 1 is the cavity, 2 is the sprue, 3 is the riser, 4 is the runner, 5 is the casting shrinkage feeder, 6 is the riser shrinkage feeder, 7 is the first ingates, and 8 is the second ingates. DETAILED DESCRIPTION
[0017] Embodiments of the present invention are described in detail below, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and should not be construed as limiting the present invention. On the contrary, the embodiments of the present invention include all changes, modifications and equivalents that fall within the spirit and connotation of the appended claims.
[0018] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "axial", "radial", "circumferential" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present invention.
[0019] In addition, the terms "first", "second", etc. are used for descriptive purposes only and are not to be understood as indicating or implying relative importance. In the description of the present utility model, it should be noted that, unless otherwise clearly specified and limited, the terms "connected" and "connected" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be directly connected or indirectly connected through an intermediate medium. For ordinary technicians in this field, the specific meanings of the above terms in the present utility model can be understood according to specific circumstances. In addition, in the description of the present utility model, unless otherwise specified, "multiple" means two or more.
[0020] Any process or method description in the flowchart or otherwise described herein may be understood to represent a module, fragment or portion of code that includes one or more executable instructions for implementing the steps of a specific logical function or process, and the scope of the preferred embodiments of the present invention includes alternative implementations in which functions may not be performed in the order shown or discussed, including performing functions in a substantially simultaneous manner or in the reverse order depending on the functions involved, which should be understood by technicians in the technical field to which the embodiments of the present invention belong.
[0021] like Figure 1 and Figure 2As shown, the utility model provides a differential pressure casting pouring system for an aluminum alloy box, comprising a cavity 1, a sprue 2 arranged below the cavity 1, and a riser 3 arranged above the cavity 1, a runner 4 is arranged in the horizontal direction below the cavity 1, the runner 4 is connected to the sprue 2, and a first ingates 7 is arranged between the runner 4 and the cavity 1;
[0022] The cross runner 4 is connected with a casting shrinkage-supporting runner 5 arranged vertically, and a second ingates 8 is arranged between the casting shrinkage-supporting runner 5 and the cavity 1; a riser shrinkage-supporting runner 6 is arranged between the cross runner 4 and the riser 3, and the riser 3 is an integrally connected form flatly distributed above the cavity 1, the cross runner 4 is of a heat storage steady flow type, and the first ingates 7 is of a necking riser type.
[0023] The pouring system of the present invention is based on the traditional pouring system, and the design structure is innovative. The general runner 4 is optimized and improved into a heat storage and steady flow runner 4. The mold filling is stable, the temperature of the molten metal is stable, the secondary oxidation of the molten metal is minimized, and defects such as pores and slag inclusions are effectively solved. At the same time, the integrally connected riser 3 is connected with the riser shrinkage-filling runner 6, so that the riser 3 becomes a hot riser 3, and the riser 3 is in an effective shrinkage-filling state. The first inner gate 7 is designed as a shrinking riser type, which is more conducive to the shrinkage compensation of the product in counter-gravity casting. The other parts that need to be compensated for shrinkage are directly compensated from the heat storage and steady flow runner 4. Then, by designing the sprue 2 and the inner gate at other positions and coordinating the use of forming cold iron, a series of defects such as shrinkage holes and looseness of the casting are effectively solved. It is suitable for aluminum alloy castings with a size of less than 2000X2000X800mm (length x width x height) type box.
[0024] Assume that the parameter of the structure included in the pouring system is the modulus M, M is the ratio of the volume V of the structure to the effective heat dissipation area S, that is, M=V / S, the straight runner 2M>the cross runner 4M>the casting shrinkage feeding runner 5M, the riser shrinkage feeding runner 6M>the second inner gate 8M>the cavity 1M, the cross runner 4M>the first inner gate 7M, the riser 3M>the cavity 1 corresponding to the riser 3 part M.
[0025] The end length of the runner 4 is 0.5-1 times the width of the runner 4, and the end length of the sprue 2 is greater than the diameter of the sprue 2. The average wall thickness of the casting at the corresponding first ingates 7 is denoted as δ, and the length of the first ingates 7 is <5δ; the diameter of the second ingates 8 is denoted as D, and when the length of the second ingates 8 is <1.5D, the type of the second ingates 8 is cylindrical; when the length of the second ingates 8 is ≥1.5D, the type of the second ingates 8 is a necking riser type.
[0026] The mold cavity 1 is of an irregular shape, the heat storage and steady flow cross runner 4 is roughly in line with the downward projection surface of the casting and a connecting channel is set, the length of the first inner gate 7 refers to the minimum distance from the smallest end to the smallest end of two adjacent first inner gates 7 of the necking riser type, the end length of the cross runner 4 refers to the shortest distance from the outermost end of the heat storage and steady flow cross runner 4 to the outer circle of the casting shrinkage feed runner 5, and the end length of the straight runner 2 refers to the shortest distance from the upper part of the casting shrinkage feed runner 5 to the outer circle of the second inner gate 8.
[0027] At the same time, the weight of the heat storage steady flow runner 4 should also be 35~50% of the weight of the casting. When the weight of the casting is ≥300Kg, the lower limit is taken. When the weight of the casting is <300Kg, the upper limit is taken, and the height of the riser 3 is 1.5 times the diameter of the riser 3.
[0028] The pouring system with the above parameters can ensure that the cavity 1 is punched smoothly and the temperature of the punching process is stable during pouring, and a good shrinkage compensation effect is taken into account. When used in conjunction with a chiller, a series of defects such as shrinkage cavities, looseness, air holes, slag inclusions, etc. that are prone to occur in large aluminum alloy boxes can be completely solved, and stable mass production can be achieved.
[0029] In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "example", "specific example", or "some examples" means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the utility model. In this specification, the schematic representation of the terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described can be combined in any one or more embodiments or examples in a suitable manner.
[0030] Based on the above ideal embodiments of the utility model, the relevant staff can make various changes and modifications without deviating from the technical concept of the utility model through the above description. The technical scope of the utility model is not limited to the content of the specification, and its technical scope must be determined according to the scope of the claims.
Claims
1. A differential pressure casting pouring system for an aluminum alloy box, comprising a mold cavity (1), a sprue (2) arranged below the mold cavity (1), and a riser (3) arranged above the mold cavity (1). Features: A runner (4) is arranged in a transverse direction below the mold cavity (1), the runner (4) is connected to the sprue (2), and a first ingates (7) is arranged between the runner (4) and the mold cavity (1); The cross runner (4) is connected to a casting shrinkage compensation runner (5) arranged vertically, and a second ingates (8) is arranged between the casting shrinkage compensation runner (5) and the mold cavity (1); and a riser shrinkage compensation runner (6) is arranged between the cross runner (4) and the riser (3).
2. The differential pressure casting pouring system for the aluminum alloy box according to claim 1, Features: The riser (3) is in an integrally connected form and is distributed flatly above the cavity (1).
3. The differential pressure casting pouring system for the aluminum alloy box as claimed in claim 2, Features: The type of the runner (4) is a heat storage steady flow type, and the type of the first ingates (7) is a shrinking riser type.
4. The differential pressure casting pouring system for the aluminum alloy box as claimed in claim 3, Features: Assume that the parameter of the structure included in the pouring system is the modulus M, where M is the ratio of the volume V of the structure to the effective heat dissipation area S, that is, M=V / S, the straight runner (2) M> the cross runner (4) M> the casting shrinkage feeding runner (5) M, the riser shrinkage feeding runner (6) M> the second ingates (8) M> the cavity (1) M, the cross runner (4) M> the first ingates (7) M, and the riser (3) M> the cavity (1) corresponding to the riser (3) portion M.
5. The differential pressure casting pouring system for the aluminum alloy box as claimed in claim 4, Features: The end length of the cross runner (4) is 0.5-1 times the width of the cross runner (4), and the end length of the straight runner (2) is greater than the diameter of the straight runner (2).
6. The differential pressure casting pouring system for the aluminum alloy box as claimed in claim 5, Features: The average wall thickness of the casting at the position corresponding to the first ingating gate (7) is denoted as δ, and the length of the first ingating gate (7) is less than 5δ; the diameter of the second ingating gate (8) is denoted as D, and when the length of the second ingating gate (8) is less than 1.5D, the type of the second ingating gate (8) is cylindrical; when the length of the second ingating gate (8) is ≥1.5D, the type of the second ingating gate (8) is a necking riser type.
Citation Information
Cited By
Pouring system and pouring method for low-pressure casting
CN119703011A