Crucible for single crystal growth
By using structures such as multiple vertically arranged heating coils and choke rings in the crucible, the problem of difficult radial temperature gradient control in existing crucibles is solved, and the stability of single crystal growth and heating efficiency are improved.
Patent Information
- Application Number
- CN202420477831.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-12
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2034-03-12
AI Technical Summary
During single crystal growth in existing crucibles at high temperatures, the radial temperature gradient is difficult to control, affecting the stability of single crystal growth.
A crucible for single crystal growth is designed, which uses multiple vertically arranged heating coils for heating. A choke ring and an electric heater are installed on the inner layer of the crucible, combined with an insulation layer and a tapered groove structure, to achieve convection reduction and Stable control of temperature gradients.
Through the simultaneous energization of multiple heating coils and the use of electric heaters, the temperature gradient is adjusted, which improves the stability of single crystal growth and the heating efficiency of semiconductor materials, reduces the risk of impurity adhesion, and improves the practicality of the crucible.
Smart Images

Figure CN221854854U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of crucibles, in particular to a crucible for single crystal growth. Background Art
[0002] In order to obtain semiconductor materials that meet the requirements of manufacturing devices, it is necessary to grow the purified polycrystalline material into a single crystal. This process is called single crystal growth. The most common method of single crystal growth is to pull a single crystal. The original concept of pulling a single crystal is to use a fixed seed crystal to contact the surface of the molten semiconductor material, and then slowly pull the seed crystal, so that crystals will continue to grow under the seed crystal to form a new single crystal. Single crystal growth is generally carried out in a crucible.
[0003] For example, the authorized patent with announcement number CN205223407U (a crucible for growing aluminum nitride single crystals): includes a crucible cover, a crucible barrel and a guide ring; wherein a lower boss is provided on the lower surface of the crucible cover; the guide ring is a trapezoidal circular ring that is larger at the top and smaller at the bottom; the edge of the lower surface of the lower boss is in gap with the upper edge of the guide ring; a protrusion for supporting the guide ring is provided on the inner surface of the crucible barrel, and the lower edge of the guide ring is in gap with the protrusion; the side surfaces of the lower boss and the guide ring are in gap with the inner surface of the crucible barrel; the crucible cover, the guide ring and the crucible barrel are connected in sequence from top to bottom to form a crucible;
[0004] Although the above-mentioned prior art facilitates the nucleation and crystal growth of aluminum nitride single crystals at high temperatures, most crucibles are currently heated by a single induction coil, and the radial temperature gradient is difficult to control, which affects the stability of single crystal growth; therefore, the market urgently needs to develop a crucible for single crystal growth to help people solve the existing problems. Utility Model Content
[0005] The utility model aims to provide a crucible for single crystal growth, so as to solve the problem in the background art that most crucibles are heated by a single induction coil, the radial temperature gradient is difficult to control, and the stability of single crystal growth is affected.
[0006] To achieve the above-mentioned purpose, the utility model provides the following technical solutions: a crucible for single crystal growth, comprising an outer shell, a crucible body is arranged inside the outer shell, the crucible body comprises a crucible outer layer and a crucible inner layer, the crucible inner layer is fixedly installed inside the crucible outer layer, an outer cylinder body is arranged on the outer side of the crucible outer layer, and the lower end of the outer cylinder body is fixedly connected to the outer shell, a heating coil is arranged between the outer cylinder body and the crucible outer layer, and a plurality of heating coils are arranged, and the plurality of heating coils are arranged in a vertical direction.
[0007] Preferably, a baffle is fixedly installed inside the inner layer of the crucible, and conical grooves are symmetrically arranged above and below the baffle.
[0008] Preferably, a bottom groove is provided at the bottom of the inner part of the outer shell along the lower side of the outer layer of the crucible, an electric heater is provided inside the bottom groove, and the electric heater is fixedly connected to the outer shell.
[0009] Preferably, a heat insulating layer is fixedly installed on the inner side of the outer cylinder, and a top ring plate is arranged on the top of the inner side of the outer cylinder, and the inner side surface of the top ring plate is in contact with the outer side surface of the outer layer of the crucible.
[0010] Preferably, a crucible cover is arranged above the outer layer of the crucible, a convex ring is fixedly installed below the crucible cover, and the convex ring extends into the interior of the inner layer of the crucible, and the outer side surface of the convex ring is in contact with the inner side surface of the inner layer of the crucible.
[0011] Preferably, a cover ring is fixedly mounted on the outer side of the crucible cover, and the inner side surface of the cover ring is in contact with the outer side surface of the outer layer of the crucible.
[0012] Preferably, a seed crystal plate is arranged inside the inner layer of the crucible, a fixing plate is fixedly installed below the seed crystal plate, a lifting rod is fixedly installed above the seed crystal plate, and the upper end of the lifting rod passes through the crucible cover and the convex ring.
[0013] Compared with the prior art, the beneficial effects of the utility model are:
[0014] 1. The utility model provides a heating coil on the outer layer of the crucible, and a plurality of heating coils are provided, and the plurality of heating coils are arranged in a vertical direction. Therefore, when the crucible is heated, the melting work of the material inside the crucible can be carried out by synchronously energizing different heating coils, and when single crystal growth is performed, the heating temperature of the crucible at different heights can be conveniently adjusted by adjusting the current of different heating coils, so that a stable temperature gradient is formed in the crucible, which is conducive to the stable growth of single crystals and increases the practicality of the crucible.
[0015] 2. The utility model arranges a baffle ring in the inner layer of the crucible, so that during the single crystal growth process, the convection caused by the temperature gradient in the crucible can be reduced to a certain extent, preventing impurities from adhering to the single crystal, which is beneficial to the quality of single crystal growth. At the same time, conical grooves are arranged above and below the baffle ring. The arrangement of the conical groove structure can increase the smoothness, making it convenient for the semiconductor material to slide down stably when the semiconductor material is added to the crucible for melting, thereby increasing the practicality of the crucible.
[0016] 3. The utility model arranges a bottom groove at the bottom of the outer shell and an electric heater inside the bottom groove, so that when the semiconductor material in the crucible is heated and melted, the bottom of the crucible can be heated by starting the electric heater, thereby increasing the heating efficiency of the semiconductor material inside the crucible, facilitating the rapid melting of the semiconductor material in the crucible and increasing practicality. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 It is a schematic diagram of a crucible for single crystal growth of the utility model;
[0018] Figure 2 It is a cross-sectional view of a crucible for single crystal growth of the utility model;
[0019] Figure 3 It is an enlarged schematic diagram of the A part of the utility model;
[0020] Figure 4 It is an enlarged schematic diagram of the B part of the utility model;
[0021] Figure 5 It is a schematic structural diagram of the baffle ring of the utility model.
[0022] In the figure: 1. outer shell; 2. outer layer of crucible; 3. inner layer of crucible; 4. baffle; 5. outer cylinder; 6. thermal insulation layer; 7. heating coil; 8. lifting rod; 9. seed crystal plate; 10. fixing plate; 11. crucible cover; 12. convex ring; 13. cover ring; 14. top ring plate; 15. bottom groove; 16. electric heater; 17. conical groove. DETAILED DESCRIPTION
[0023] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all of the embodiments.
[0024] See also Figure 1-5 The utility model provides an embodiment: a crucible for single crystal growth, comprising an outer shell 1, a crucible body is arranged inside the outer shell 1, the crucible body comprises a crucible outer layer 2 and a crucible inner layer 3, the crucible outer layer 2 and the crucible inner layer 3 are both made of graphite material, when a large loss occurs inside the crucible, it is convenient to replace them separately, the crucible inner layer 3 is fixedly installed inside the crucible outer layer 2, an outer cylinder 5 is arranged on the outside of the crucible outer layer 2, and the lower end of the outer cylinder 5 is fixedly connected to the outer shell 1, a heating coil 7 is arranged between the outer cylinder 5 and the crucible outer layer 2, the heating coil 7 is electrically connected to the external control end of the crucible, so as to heat the crucible conveniently, and a plurality of heating coils 7 are arranged, and the plurality of heating coils 7 are arranged in a vertical direction.
[0025] During use, when the crucible is heated, the melting of the material inside the crucible can be carried out by synchronously energizing different heating coils 7, and when single crystal growth is carried out, the heating temperature of the crucible at different heights can be conveniently adjusted by adjusting the current of different heating coils 7, so as to form a stable temperature gradient in the crucible, which is conducive to the stable growth of the single crystal. This solves the problem that most crucibles are heated by a single induction coil, the radial temperature gradient is difficult to control, and the stability of the single crystal growth is affected, thereby increasing the practicality of the crucible.
[0026] Furthermore, a baffle ring 4 is fixedly installed inside the inner layer 3 of the crucible, so that during the growth of the single crystal, the convection caused by the temperature gradient in the crucible can be reduced to a certain extent, and impurities can be prevented from adhering to the single crystal, which is beneficial to the quality of the single crystal growth. Conical grooves 17 are symmetrically arranged above and below the baffle ring 4. The setting of the conical groove structure can increase the smoothness, so that when the semiconductor material is added to the crucible for melting, it is convenient for the semiconductor material to slide downward stably, thereby increasing the practicality of the crucible.
[0027] Furthermore, a bottom groove 15 is provided at the bottom of the inner part of the outer shell 1 along the bottom of the outer layer 2 of the crucible, and an electric heater 16 is provided inside the bottom groove 15, and the electric heater 16 is fixedly connected to the outer shell 1, so that when the semiconductor material in the crucible is heated and melted, the bottom of the crucible can be heated by starting the electric heater 16, thereby increasing the heating efficiency of the semiconductor material inside the crucible, which is beneficial to the rapid melting of the semiconductor material in the crucible.
[0028] Furthermore, an insulating layer 6 is fixedly installed on the inner side of the outer cylinder 5, which can increase the thermal insulation capacity of the outer cylinder 5, reduce the outward dissipation of heat, and increase the stable heating of the crucible. A top ring plate 14 is provided on the top of the inner part of the outer cylinder 5, and the inner side surface of the top ring plate 14 is in contact with the outer side surface of the crucible outer layer 2, which reduces heat loss and increases practicality. It can also support and limit the crucible body, thereby improving the stability of the crucible body.
[0029] Furthermore, a crucible cover 11 is arranged above the crucible outer layer 2, which can cover the top of the crucible body. A convex ring 12 is fixedly installed below the crucible cover 11, and the convex ring 12 extends into the interior of the crucible inner layer 3. The outer side surface of the convex ring 12 is in contact with the inner side surface of the crucible inner layer 3. The provision of the convex ring 12 increases the stability of the contact between the crucible cover 11 and the crucible inner layer 3.
[0030] Furthermore, a cover ring 13 is fixedly mounted on the outer side of the crucible cover 11 , and the inner side of the cover ring 13 fits the outer side of the crucible outer layer 2 . The cover ring 13 increases the contact stability between the crucible cover 11 and the crucible outer layer 2 .
[0031] Furthermore, a seed crystal plate 9 is arranged inside the inner layer 3 of the crucible, and through holes are arranged at the centers of the crucible cover 11 and the convex ring 12 to facilitate the lifting and lowering movement of the seed crystal plate 9. A fixing plate 10 is fixedly installed below the seed crystal plate 9, and a lifting rod 8 is fixedly installed above the seed crystal plate 9. The upper end of the lifting rod 8 passes through the crucible cover 11 and the convex ring 12. The lifting rod 8 is externally connected to a driving device that can drive the lifting rod 8 to lift and lower, which is beneficial to the single crystal growth work and increases practicality.
[0032] Working principle: When in use, add the semiconductor material into the crucible body, then energize different heating coils 7 at the same time, and start the electric heater 16, so that the crucible can be heated from the side and bottom, which is beneficial to the melting efficiency of the semiconductor material in the crucible. After the semiconductor material in the crucible is melted, the heating temperature of the crucible at different heights can be adjusted by adjusting the current of different heating coils 7, so as to form a stable temperature gradient in the crucible, so that the upper part of the melt is in a supercooled state, install the seed crystal on the fixed plate 10 under the seed crystal plate 9, and then use an external drive device to move the seed crystal plate 9 to allow the seed crystal to drop to the surface of the melt. After the surface of the seed crystal is slightly melted, pull and rotate the lifting rod 8 to make the melt in a supercooled state and crystallize on the seed crystal. In the process of continuous pulling and rotation, a large cylindrical single crystal is finally grown.
[0033] It is obvious to those skilled in the art that the present invention is not limited to the details of the exemplary embodiments described above, and that the present invention can be implemented in other specific forms without departing from the spirit or essential features of the present invention. Therefore, the embodiments should be regarded as exemplary and non-restrictive from any point of view, and the scope of the present invention is defined by the appended claims rather than the above description, and it is intended that all changes falling within the meaning and scope of the equivalent elements of the claims be included in the present invention. Any reference numeral in a claim should not be regarded as limiting the claim to which it relates.
Claims
1. A crucible for single crystal growth, comprising an outer shell (1), characterized in that: A crucible body is arranged inside the outer shell (1), and the crucible body comprises a crucible outer layer (2) and a crucible inner layer (3). The crucible inner layer (3) is fixedly installed inside the crucible outer layer (2). An outer cylinder (5) is arranged outside the crucible outer layer (2), and the lower end of the outer cylinder (5) is fixedly connected to the outer shell (1). A heating coil (7) is arranged between the outer cylinder (5) and the crucible outer layer (2), and a plurality of heating coils (7) are arranged, and the plurality of heating coils (7) are arranged in a vertical direction.
2. A crucible for single crystal growth according to claim 1, characterized in that: A baffle ring (4) is fixedly installed inside the crucible inner layer (3), and conical grooves (17) are symmetrically arranged above and below the baffle ring (4).
3. A crucible for single crystal growth according to claim 1, characterized in that: A bottom groove (15) is provided at the bottom of the outer shell (1) below the crucible outer layer (2), an electric heater (16) is provided inside the bottom groove (15), and the electric heater (16) is fixedly connected to the outer shell (1).
4. The crucible for single crystal growth according to claim 1, characterized in that: A heat insulation layer (6) is fixedly installed on the inner side of the outer cylinder (5), and a top ring plate (14) is arranged on the top of the inner side of the outer cylinder (5), and the inner side surface of the top ring plate (14) is in contact with the outer side surface of the crucible outer layer (2).
5. The crucible for single crystal growth according to claim 1, characterized in that: A crucible cover (11) is arranged above the crucible outer layer (2), a convex ring (12) is fixedly installed below the crucible cover (11), and the convex ring (12) extends into the interior of the crucible inner layer (3), and the outer side surface of the convex ring (12) is in contact with the inner side surface of the crucible inner layer (3).
6. A crucible for single crystal growth according to claim 5, characterized in that: A cover ring (13) is fixedly mounted on the outer side of the crucible cover (11), and the inner side surface of the cover ring (13) is in contact with the outer side surface of the crucible outer layer (2).
7. A crucible for single crystal growth according to claim 6, characterized in that: A seed crystal plate (9) is arranged inside the inner layer (3) of the crucible, a fixing plate (10) is fixedly installed below the seed crystal plate (9), and a lifting rod (8) is fixedly installed above the seed crystal plate (9), and the upper end of the lifting rod (8) passes through the crucible cover (11) and the convex ring (12).