Ultra-matte carborundum flash point lettering film

The ultra-matte emery flash-point lettering film with a multi-layer combined structure solves the problems of poor decorativeness and insufficient strength of existing lettering films, achieves higher decorativeness and film integrity, and reduces adhesion and fracture at high temperatures. risk, and improves anti-pollution properties.

CN221873690UActive Publication Date: 2024-10-22GUANGZHOU XIONGXING PLASTIC PRODS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420047909.1
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-01-09
Publication Date
2024-10-22
Estimated Expiration
2034-01-09

AI Technical Summary

Technical Problem

Existing lettering films have poor decorative properties during use, lack film strength, and are prone to adhesion and breakage at high temperatures. They especially perform poorly during laser cutting and thermal transfer processing.

Method used

Ultra-matte emery flash point lettering film adopts a multi-layer combination structure, including base material layer, reinforced structural layer, matte layer, PET glue layer, adhesive layer, emery particle layer, flash layer and protective layer, through transparent glass fiber layer, a matte layer mixed with carbon black powder, a polymer particle film embedded with light-reflective materials, and a light-cured anti-pollution material film to enhance the overall strength and anti-adhesion of the film body.

Benefits of technology

It improves the decoration and film integrity of the lettering film, reduces adhesion and fracture problems at high temperatures, enhances anti-pollution performance, and ensures the stability of laser lettering and thermal transfer processing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221873690U_ABST
    Figure CN221873690U_ABST
Patent Text Reader

Abstract

The ultra-matte carborundum flash point lettering film comprises a base material layer, a pair of reinforcing structure layers, a matte layer, a PET (Polyethylene Terephthalate) adhesive layer, an adhesion layer, a carborundum particle layer, a flash layer and a protective layer, the reinforcing structure layers are arranged on the upper wall surface and the lower wall surface of the base material layer; the matte layer is arranged on the upper wall surface of the reinforcing structure layer; the PET adhesive layer is arranged on the lower wall surface of the reinforcing structure layer; the utility model relates to the technical field of lettering films, and has the beneficial effects that the lettering film solves the problems that the existing lettering film is single in effect, poorer in decoration in use, has no comparative characteristics, is poorer in film body strength, and is easy to adhere and break due to high temperature in laser cutting and thermal transfer printing processing.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of lettering films, in particular to an ultra-matte diamond abrasive flash point lettering film. Background Art

[0002] Engraving film refers to the thermal transfer film that needs to be cut / engraved during the thermal transfer process. It has a certain degree of softness and plasticity, and can form text, patterns or logos on the surface through laser or mechanical engraving. The existing engraving film has a single effect, poor decorative effect when used, relatively no characteristics, and poor film strength. During laser cutting and thermal transfer processing, the film is prone to adhesion and breakage due to high temperature. Summary of the Invention

[0003] In order to achieve the above purpose, the utility model is realized through the following technical solutions: ultra-matte diamond abrasive flash point lettering film,

[0004] It includes: base material layer, a pair of reinforcing structural layers, matte layer, PET adhesive layer, adhesive layer, diamond grain layer, flash layer and protective layer;

[0005] A pair of reinforcing structural layers are arranged on the upper and lower wall surfaces of the base material layer;

[0006] The matte layer is arranged on the upper wall surface of the reinforcement structure layer;

[0007] The PET adhesive layer is arranged on the lower wall surface of the reinforcing structure layer;

[0008] The adhesive layer is disposed above the matte layer;

[0009] The diamond grain layer is arranged on the upper wall surface of the matte layer through the adhesive layer;

[0010] The flash layer is arranged on the upper wall surface of the diamond grain layer;

[0011] The protective layer is arranged on the upper wall surface of the flash layer.

[0012] Preferably, the pair of reinforcing structural layers are transparent glass fiber layers.

[0013] Preferably, the matte layer is an emulsion solvent mixed with carbon black powder.

[0014] Preferably, the flash layer is a film embedded with light-reflecting polymer particles.

[0015] Preferably, a pair of the reinforcing structural layers are adhered to the upper and lower wall surfaces of the substrate layer by a pressure-sensitive adhesive.

[0016] Preferably, the protective layer is a light-cured anti-pollution material film.

[0017] Beneficial effects

[0018] The utility model provides an ultra-matte corundum flash point engraving film, which has the following beneficial effects: this solution adopts a composite structure of multi-layer combination, and sets a matte structure at the bottom. The structure of the corundum particle layer and the flash layer above is highlighted by the black matte below, while increasing the overall strength of the film body, ensuring the integrity of the film body during laser engraving, and setting a protective structure to give it lower surface energy and better anti-adhesion, reducing the adhesion of pollutants on the film surface, solving the problems of the existing engraving film having a single effect, poor decorative effect when used, relatively no characteristics, and poor film strength. During laser cutting and thermal transfer processing, the film body is prone to adhesion and breakage due to high temperature. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 This is a schematic diagram of the three-dimensional cross-sectional structure of the ultra-matte diamond abrasive flash point lettering film described in the present invention.

[0020] Figure 2 This is a schematic diagram of the main cross-sectional structure of the ultra-matte diamond abrasive flash point lettering film described in the present invention.

[0021] In the figure: 1-base material layer; 2-reinforcement structure layer; 3-matt layer; 4-PET adhesive layer; 5-adhesion layer; 6-corundum particle layer; 7-glitter layer; 8-protective layer; 9-pressure-sensitive adhesive. DETAILED DESCRIPTION

[0022] Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making any creative work shall fall within the scope of protection of the present invention.

[0023] Example: See Figure 1-2 , ultra-matte diamond abrasive flash point lettering film,

[0024] It includes: a base material layer 1, a pair of reinforcing structural layers 2, a matte layer 3, a PET adhesive layer 4, an adhesive layer 5, a diamond grain layer 6, a flash layer 7 and a protective layer 8;

[0025] A pair of reinforcing structural layers 2 are provided on the upper and lower wall surfaces of the base material layer 1;

[0026] The matte layer 3 is arranged on the upper wall surface of the reinforcement structure layer 2;

[0027] The PET adhesive layer 4 is arranged on the lower wall surface of the reinforcing structure layer 2;

[0028] The adhesive layer 5 is arranged on the matte layer 3;

[0029] The diamond grain layer 6 is arranged on the upper wall of the matte layer 3 through the adhesive layer 5;

[0030] The flash layer 7 is arranged on the upper wall of the diamond grain layer 6;

[0031] The protective layer 8 is arranged on the upper wall surface of the flash layer 7 .

[0032] In a specific implementation process, further, the pair of reinforcing structure layers 2 are transparent glass fiber layers.

[0033] In a specific implementation process, further, the matte layer 3 is an emulsion solvent mixed with carbon black powder.

[0034] In a specific implementation process, further, the flash layer 7 is a film embedded with polymer particles that can reflect light.

[0035] In a specific implementation process, further, a pair of the reinforcing structure layers 2 are adhered to the upper and lower wall surfaces of the substrate layer 1 through a pressure-sensitive adhesive 9 .

[0036] In a specific implementation process, further, the protective layer 8 is a light-cured anti-pollution material film.

[0037] It should be noted that the pressure-sensitive adhesive 9 is coated on the upper and lower walls of the substrate layer 1, and a pair of reinforcing structural layers 2 made of transparent glass fiber are adhered to the upper and lower walls of the substrate layer 1 through the pressure-sensitive adhesive 9. The strength and toughness of the film are enhanced by the material properties of the glass fiber. The matte layer 3 mixed with carbon black powder on the upper wall of the reinforcing structural layer 2 provides a strong background color for the bottom layer. The corundum particle layer 6 is arranged above the matte layer 3 through the adhesive layer 5. The flash layer 7 embedded with light-reflective polymer particles is arranged above the corundum particle layer 6. Through the background color contrast of the matte layer 3, the flash characteristics of the upper corundum particle layer 6 and the flash layer 7 are highlighted, thereby enhancing the visual perception intensity. The protective layer 8 increases the protection of the film to prevent scratches and damage. The PET adhesive layer 4 is arranged at the bottom of the film to support the engraved film and protect it during thermal transfer processing.

[0038] Although the embodiments of the present invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions and variations may be made to these embodiments without departing from the principles and spirit of the present invention, and the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. Ultra-matte diamond sand flash point lettering film, It is characterized in that include: A base material layer (1), a pair of reinforcing structural layers (2), a matte layer (3), a PET adhesive layer (4), an adhesive layer (5), a corundum particle layer (6), a flash layer (7), and a protective layer (8); A pair of reinforcing structure layers (2) are arranged on the upper and lower wall surfaces of the base material layer (1); The matte layer (3) is arranged on the upper wall surface of the reinforcing structure layer (2); The PET adhesive layer (4) is arranged on the lower wall surface of the reinforcing structure layer (2); The adhesive layer (5) is arranged above the matte layer (3); The diamond grain layer (6) is arranged on the upper wall surface of the matte layer (3) through the adhesive layer (5); The flash layer (7) is arranged on the upper wall surface of the corundum particle layer (6); The protective layer (8) is arranged on the upper wall surface of the flash layer (7).

2. The ultra-matte diamond flash point lettering film according to claim 1, It is characterized in that The pair of reinforcing structural layers (2) are transparent glass fiber layers.

3. The super matte diamond flash point lettering film according to claim 1, It is characterized in that The matte layer (3) is an emulsion solvent mixed with carbon black powder.

4. The ultra-matte diamond flash point lettering film according to claim 1, It is characterized in that The flash layer (7) is a film embedded with light-reflecting polymer particles.

5. The super matte diamond flash point lettering film according to claim 1, It is characterized in that A pair of the reinforcing structure layers (2) are adhered to the upper and lower wall surfaces of the substrate layer (1) via a pressure-sensitive adhesive (9).

6. The super matte diamond flash point lettering film according to claim 1, It is characterized in that The protective layer (8) is a light-cured anti-pollution material film.