Molten salt pipeline with carbon-ceramic lining
By using carbon ceramic material as the lining in the molten salt pipeline, and utilizing the bonding layer and L-shaped groove structure, the problem of traditional molten salt pipelines being easily corroded and brittle at high temperatures is solved, and high-temperature stability and durability are achieved. , extending service life and reducing costs.
Patent Information
- Application Number
- CN202420451506.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-08
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2034-03-08
AI Technical Summary
Traditional metal materials are prone to corrosion, oxidation and wear in high-temperature molten salt environments, and the ceramic inner layer is brittle and not durable at high temperatures, resulting in molten salt pipelines with short service life and high manufacturing costs.
Carbon ceramic material is used as the lining. There is an adhesive layer between the inner tube and the outer tube, which is fixed by an L-shaped groove and adhesive. The inner tube has high strength, high temperature resistance, oxidation resistance and corrosion resistance, and the outer tube It can be welded at will and the inner tube will not fall off due to high temperature expansion, cracking and cold contraction.
It achieves the stability of the inner and outer structures at temperatures above 2000°C, extends the service life of the pipeline, reduces the manufacturing scrap rate and cost, and improves assembly efficiency.
Smart Images

Figure CN221880504U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of molten salt pipelines, and specifically relates to a carbon-ceramic lined molten salt pipeline. Background Art
[0002] In the fields of chemical industry, metallurgy, energy, etc., molten salt is an important industrial medium and is widely used in the production process. However, molten salt is highly corrosive and has high requirements for pipeline materials. Traditional metal materials such as stainless steel and nickel-based alloys are prone to corrosion, oxidation and wear in high-temperature molten salt environments, resulting in a reduced service life of the pipeline and even leakage accidents.
[0003] The existing technology usually adopts a double-layer pipe, and the inner pipe is made of ceramic material. Although this ceramic layer resists the corrosiveness of molten salt, the ceramic layer is fragile and has poor high-temperature stability. It is only suitable for use scenarios with low temperature requirements and cannot withstand high temperatures above 2000°C. When the operating temperature of the formed molten salt pipe exceeds 2000°C, the ceramic inner layer will expand and crack, and the cooling and shrinkage after the temperature drops will easily cause the inner and outer layers to fall off; when the two pipes are welded, the high temperature of the welding is transmitted to the inner layer through the outer steel layer, which will also cause the ceramic inner layer to be unable to withstand the high temperature and crack, resulting in a high manufacturing scrap rate and high manufacturing cost.
[0004] Therefore, a molten salt pipeline that is resistant to high temperatures and has high inner and outer layer structural stability is needed to solve the existing problems. Utility Model Content
[0005] In view of the defects of the prior art, the utility model proposes a carbon-ceramic lined molten salt pipeline, wherein an adhesive layer is provided between the inner pipe and the outer pipe. The inner pipe serves as the carbon-ceramic layer of the carbon-ceramic lined molten salt pipeline, and has the characteristics of high strength, high modulus, high hardness, impact resistance, oxidation resistance, high temperature resistance, acid and alkali resistance and corrosion resistance, so that the inner pipe will not fall off from the outer pipe after cracking due to high temperature expansion and contraction due to cold.
[0006] To achieve the above-mentioned purpose, the utility model provides a carbon-ceramic lined molten salt pipeline, comprising an outer tube, an inner tube sleeved in the outer tube, and a bonding layer located between the outer tube and the inner tube, wherein the inner tube is made of carbon-ceramic material; a protrusion is provided on the outer wall of the inner tube, and a corresponding L-shaped groove is opened on the inner wall of the outer tube, wherein the L-shaped groove has a first end and a second end, and the inner tube protrusion extends into the outer tube along the first end of the L-shaped groove and is rotated to the second end of the L-shaped groove for fixing.
[0007] Furthermore, the first end of the L-shaped groove passes through one end surface of the outer tube, and the second end of the L-shaped groove extends to a certain distance along the circumferential direction of the outer tube.
[0008] Furthermore, the first end of the L-shaped groove is filled with adhesive.
[0009] Furthermore, the first end of the L-shaped groove is a rectangular groove, and the second end is a trapezoidal groove. The outer wall protrusion of the inner tube is a trapezoidal structure, and the two side surfaces of the trapezoidal structure match the trapezoidal groove.
[0010] Furthermore, the outer wall protrusions of the inner tube and the L-shaped grooves are respectively arranged in a circumferential array around the central axes of the outer tube and the inner tube.
[0011] Furthermore, the outer pipe is made of carbon steel or stainless steel.
[0012] Further, the outer tube includes a first process hole, the inner tube includes a second process hole, and the first process hole and the second process hole are in plurality and are respectively arranged at both ends of the outer tube and the inner tube.
[0013] The beneficial effects of the utility model are:
[0014] First, the inner tube of the utility model is sleeved in the outer tube, and there is a bonding layer between the inner tube and the outer tube. The inner tube is made of carbon ceramic material. The inner tube is used as the carbon ceramic layer of the carbon ceramic lined molten salt pipeline. It has the high strength, high modulus, high hardness, impact resistance, oxidation resistance, high temperature resistance, acid and alkali resistance and corrosion resistance of high-performance ceramics. The bending strength can still be maintained at 500-600MPa at 1400 degrees Celsius, and its working temperature can reach 2000 degrees Celsius. The inner tube will not fall off from the outer tube after high-temperature expansion and contraction. When the pipeline is installed and connected, the outer tube steel pipe can be welded arbitrarily, and the inner tube will not break; the protrusion of the inner tube is clamped with the second end of the L-shaped groove, and then the first end of the L-shaped groove is sealed by an adhesive, and the circumferential and axial directions of the inner tube are limited, further improving the structural stability of the inner tube and the outer tube, and effectively preventing the outer tube and the inner tube from loosening;
[0015] Second, in the preferred implementation, the tenon of the utility model enters the tenon groove from the rectangular groove and rotates circumferentially until it fits tightly with the trapezoidal groove to achieve fixation, and the inner tube and the outer tube can be disassembled and replaced by reverse rotation;
[0016] Third, in the preferred implementation, the carbon-ceramic lined molten salt pipeline of the utility model has a process hole for fixing the outer pipe and a process hole for rotating the inner pipe, which is convenient for the installation of the inner pipe and the outer pipe and improves the assembly efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 It is a three-dimensional structural diagram of a carbon-ceramic lined molten salt pipeline of Example 1 of the utility model;
[0018] Figure 2 It is a three-dimensional structural diagram of a carbon-ceramic lined molten salt pipeline of Example 3 of the utility model;
[0019] Figure 3 It is a three-dimensional structural diagram of the outer pipe of the carbon-ceramic lined molten salt pipeline of Example 3 of the utility model;
[0020] Figure 4 yes Figure 2 A partial enlarged view of
[0021] Figure 5 It is a three-dimensional structural diagram of the inner tube of the carbon-ceramic lined molten salt pipeline of Example 3 of the utility model;
[0022] Figure 6 It is a side view of the inner tube of the carbon-ceramic lined molten salt pipeline of Example 3 of the utility model;
[0023] Figure 7 yes Figure 5 AA cross-sectional view.
[0024] Among them, 1-outer tube; 10-mortise; 100-rectangular groove; 101-trapezoidal groove; 11-first process hole; 2-inner tube; 20-tenon; 21-second process hole. DETAILED DESCRIPTION
[0025] In order to enable those skilled in the art to better understand the technical solution of the present application, the present application will be further described in detail below with reference to the accompanying drawings and embodiments.
[0026] The terms such as up, down, left, right, front and back in this application document are based on the positional relationships shown in the drawings. If the drawings are different, the corresponding positional relationships may also change accordingly, so they cannot be understood as limiting the scope of protection.
[0027] In this application, the terms "install", "connected", "connected", "connected", "fixed" and the like should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, an integral connection, a mechanical connection, an electrical connection, or mutual communication, a direct connection, or an indirect connection through an intermediate medium, the internal connection of two components, or the interaction relationship between two components. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.
[0028] Example 1
[0029] Refer to the instruction manual Figure 1 A carbon-ceramic lined molten salt pipeline comprises an outer tube 1, an inner tube 2 sleeved in the outer tube 1, and a bonding layer between the outer tube 1 and the inner tube 2.
[0030] The inner tube 2 is made of carbon ceramic material, formed by pressing a mold and then heat-treated at a high temperature. The outer tube 1 can be made of carbon steel or stainless steel pipe according to the temperature of the molten salt medium.
[0031] With the structure of this embodiment, the outer tube 1 and the inner tube 2 are bonded together by the bonding layer, thereby improving the structural stability of the outer tube 1 and the inner tube 2 after installation; the inner tube 2, as the carbon-ceramic layer of the carbon-ceramic lined molten salt pipeline, has high strength, high modulus, high hardness, impact resistance, oxidation resistance, high temperature resistance, acid and alkali resistance and corrosion resistance. The bending strength can still be maintained at 500-600MPa at 1400 degrees Celsius, and its operating temperature reaches 2000°C. Therefore, the molten salt pipeline will not cause the inner tube and the outer tube to loosen due to expansion and contraction in a high temperature environment, and when the pipeline is installed and connected, the outer tube 1 steel pipe can be welded arbitrarily, and the inner tube 2 will not rupture.
[0032] Example 2
[0033] Based on Example 1, refer to the attached Figure 2-6 The outer wall of the inner tube 2 is provided with a protrusion, and the inner wall of the outer tube 1 is provided with a corresponding L-shaped groove, the first end of the L-shaped groove penetrates one side end surface of the outer tube 1, and the second end of the L-shaped groove extends to a certain distance along the circumference of the outer tube 1. The inner tube 2 extends into the outer tube 1 along the first end of the L-shaped groove and rotates to the second end, and the first end of the L-shaped groove is filled with an adhesive to fix the inner tube 2 in the outer tube 1.
[0034] By adopting the structure of this embodiment, after the installation of the carbon-ceramic lined molten salt pipeline, the protrusion of the inner tube 2 is clamped with the second end of the L-shaped groove, and then the first end of the L-shaped groove is sealed by an adhesive, and the inner tube 2 is limited in both the circumferential and axial directions, effectively preventing the outer tube 1 and the inner tube 2 from loosening.
[0035] Example 3
[0036] Based on Example 2, refer to the attached Figure 7 The outer tube 1 includes a tenon groove 10, and the inner tube 2 includes a tenon 20. The tenon groove 10 is an L-shaped groove, and the first end of the L-shaped groove is Figure 3 The rectangular groove 100 shown; the second end of the L-shaped groove is Figure 3 Trapezoidal groove 101 is shown.
[0037] The tenon 20 is a trapezoidal structure. The two side surfaces of the tenon 20 along the circumferential direction of the inner tube 2 are parallel to each other and match the first surface 10a and the second surface 10b of the tenon groove 10. The two side surfaces 20a and 20b of the tenon 20 along the axial direction of the inner tube 2 have an angle, and the angle opening faces the outside of the inner tube 2. 20a and 20b match the third surface 10c and the fourth surface 10d of the tenon groove 10 respectively.
[0038] With the structure of this embodiment, the tenon 20 enters the tenon groove 10 from the rectangular groove 100 and rotates circumferentially until it fits tightly with the trapezoidal groove 101 to achieve fixation. The inner tube 2 and the outer tube can be disassembled and replaced by rotating in the opposite direction.
[0039] Example 4
[0040] On the basis of Example 3, the outer tube 1 includes a first process hole 11, and the inner tube 2 includes a second process hole 21. There are multiple first process holes 11 and second process holes 21, which are respectively arranged at both ends of the outer tube 1 and the inner tube 2. The outer tube 1 is fixed by clamping the first process hole 11 with a positioning tool, and the inner tube 2 is rotated along its axial direction to the second end of the L-shaped groove by clamping the second process hole 21 with a rotating tool.
[0041] The structure of this embodiment is adopted to facilitate the convenient installation of the inner tube 2 and the outer tube 1, thereby improving the assembly efficiency.
[0042] The above is only an embodiment of the utility model, and the common sense such as the known specific structure and characteristics in the scheme is not described too much here. For those skilled in the art, it is obvious that the utility model is not limited to the details of the above exemplary embodiments, and the utility model can be implemented in other specific forms without departing from the spirit or basic features of the utility model. Therefore, no matter from which point of view, the embodiments should be regarded as exemplary and non-restrictive. The scope of the utility model is limited by the attached claims rather than the above description, and it is intended to include all changes within the meaning and scope of the equivalent elements of the claims in the utility model. Any figure mark in the claims should not be regarded as limiting the claims involved.
Claims
1. A carbon ceramic lined molten salt pipeline, characterized in that: The invention comprises an outer tube (1), an inner tube (2) sleeved in the outer tube (1), and a bonding layer located between the outer tube (1) and the inner tube (2), wherein the inner tube (2) is made of carbon ceramic material; a protrusion is provided on the outer wall of the inner tube (2), a corresponding L-shaped groove is provided on the inner wall of the outer tube (1), the L-shaped groove has a first end and a second end, and the protrusion of the inner tube (2) extends into the outer tube (1) along the first end of the L-shaped groove and is rotated to the second end of the L-shaped groove for fixing.
2. The carbon-ceramic lined molten salt pipeline according to claim 1 is characterized in that: The first end of the L-shaped groove passes through one end surface of the outer tube (1), and the second end of the L-shaped groove extends to a certain distance along the circumference of the outer tube (1).
3. The carbon-ceramic lined molten salt pipeline according to claim 2 is characterized in that: The first end of the L-shaped groove is filled with adhesive.
4. The carbon-ceramic lined molten salt pipeline according to claim 2, characterized in that: The first end of the L-shaped groove is a rectangular groove, and the second end is a trapezoidal groove. The outer wall protrusion of the inner tube (2) is a trapezoidal structure, and the two side surfaces of the trapezoidal structure match the trapezoidal groove.
5. The carbon-ceramic lined molten salt pipeline according to claim 2, characterized in that: The outer wall protrusions of the inner tube (2) and the L-shaped grooves are respectively arranged in a circumferential array around the central axes of the outer tube (1) and the inner tube (2).
6. The carbon-ceramic lined molten salt pipeline according to claim 1, characterized in that: The outer pipe (1) is made of carbon steel or stainless steel.
7. The carbon-ceramic lined molten salt pipeline according to claim 2, characterized in that: The outer tube (1) comprises a first process hole, and the inner tube (2) comprises a second process hole. The first process hole and the second process hole are in plurality and are respectively arranged at both ends of the outer tube (1) and the inner tube (2).