Glass anti-cracking coating

By applying a combination of a polyurethane elastic coating layer and a transparent alkyd enamel layer on the glass to absorb and process the impact force, the problem of the existing glass coating being fragile under impact is solved, achieving higher glass crack resistance and Security.

CN221894887UActive Publication Date: 2024-10-25FUJIAN AOLONG ENVIRONMENTAL PROTECTION NEW MATERIAL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420510900.X
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-16
Publication Date
2024-10-25
Estimated Expiration
2034-03-16

AI Technical Summary

Technical Problem

Existing glass coatings cannot effectively absorb external impact forces, causing the glass to easily shatter when impacted and unable to ensure the safety of the glass.

Method used

A glass anti-cracking coating is used that includes a polyurethane elastic coating layer as the first buffer layer and a transparent alkyd enamel layer as an anti-friction buffer layer. The impact force is absorbed through the anti-friction buffer layer and transmitted to the polyurethane elastic coating layer. , causing it to deform. If the glass breaks, the fragments will be fixed by the buffer layer, and combined with the foaming reaction layer and the water-soluble film block to enhance the impact resistance.

Benefits of technology

Effectively absorbs mild impact, prevents glass from shattering, and gathers fragments in strong impact to improve safety and enhance the anti-cracking ability and impact resistance of glass.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221894887U_ABST
    Figure CN221894887U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of coatings, and provides a glass anti-cracking coating which is strong in impact resistance and safe to use, and comprises a base layer contacted with the surface of glass and an anti-ultraviolet layer arranged on the base layer, a first buffer layer is further arranged on the anti-ultraviolet layer, the first buffer layer is a polyurethane elastic coating layer, and a second buffer layer is arranged on the first buffer layer. An anti-friction buffer layer is further arranged on the first buffer layer, when the glass is impacted, after the anti-friction buffer layer absorbs part of impact force, the impact force is conducted to the first buffer layer made of the polyurethane elastic coating layer, so that the first buffer layer deforms, and if the impact force is too large, the glass is broken; the glass fragments are fixed by tensile deformation of the first buffer layer to adhere the fragmented peel.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of coatings, in particular to a glass anti-cracking coating. Background Art

[0002] Coatings are widely used on the surfaces of various objects. Different effects are achieved by using different ingredients in the coatings and by stacking different coatings in multiple layers. Some coatings can effectively prevent metal corrosion, while others can effectively prevent the surface of workpieces from being scratched and damaged. Water-based coatings use water as a solvent or a dispersion medium. They have excellent non-stickiness and durability, and because they do not use organic solvents, they are non-toxic, have no irritating odor, and do not pollute the environment. They are widely used in various fields. Existing glass coatings are applied to glass to effectively reduce the intensity of ultraviolet rays in the sunlight that passes through the glass, thereby preventing ultraviolet rays in the sunlight from causing damage to people or objects in the room while ensuring indoor lighting.

[0003] Although the above-mentioned existing technology can solve the corresponding technical problems, it still has certain defects: although the existing glass coating can effectively block ultraviolet rays, when the glass is impacted by the outside world, the glass coating cannot effectively absorb the impact force, and then the glass will be directly impacted by the external impact force and shattered. The coating is difficult to ensure the safety of the glass when it is impacted. Utility Model Content

[0004] The utility model aims to provide a glass anti-cracking coating which is highly impact-resistant and safe to use in view of the defects and shortcomings of the prior art.

[0005] To achieve the above-mentioned purpose, the utility model adopts the following technical scheme: a glass anti-crack coating, comprising a base layer in contact with the glass surface and an anti-ultraviolet layer arranged on the base layer, a first buffer layer is also arranged on the anti-ultraviolet layer, the first buffer layer is a polyurethane elastic coating layer, and an anti-friction buffer layer is also arranged on the first buffer layer. When impacted, the anti-friction buffer layer absorbs part of the impact force and transmits the impact to the first buffer layer made of the polyurethane elastic coating layer, so that the first buffer layer is deformed. If the impact is too large and causes the glass to shatter, the first buffer layer is stretched and deformed to adhere the shattered glass fragments so that the glass fragments are fixed.

[0006] A further improvement is that the anti-friction buffer layer is a transparent alkyd enamel layer.

[0007] A further improvement is that transparent glass micro beads are mixed into the anti-friction buffer layer.

[0008] A further improvement is that a foaming reaction layer is provided between the first buffer layer and the anti-friction buffer layer.

[0009] A further improvement is that the foaming reaction layer includes a dry gelatin layer arranged on the top surface of the first buffer layer and an extrusion layer arranged on the top surface of the dry gelatin layer.

[0010] A further improvement is that: a plurality of water-soluble film blocks are arranged in the extrusion layer, and the water-soluble film blocks are filled with aqueous solvent.

[0011] A further improvement is that the thickness of the first buffer layer is 0.3 mm-0.5 mm.

[0012] A further improvement is that the thickness of the anti-friction buffer layer is 0.3mm-0.5mm.

[0013] After adopting the above technical scheme, the beneficial effect of the utility model is as follows: the utility model uses the first buffer layer made of polyurethane elastic coating applied on the outside of the glass to cooperate with the anti-friction buffer layer to elastically absorb the impact received, thereby fully absorbing the low impact force to avoid the glass from breaking. At the same time, when the glass is broken by a strong impact, the ductility of the first buffer layer is used to gather the fragments to prevent the fragments from splashing, and the use safety is stronger. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] In order to more clearly illustrate the embodiments of the utility model or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.

[0015] Figure 1 It is a structural schematic diagram of a front view cross section of the coating of the utility model. DETAILED DESCRIPTION

[0016] The utility model is now further described in conjunction with the accompanying drawings and specific embodiments.

[0017] See also Figure 1As shown, the technical solution adopted in this specific embodiment is: a glass anti-crack coating, comprising a base layer 1 in contact with the glass surface and an anti-ultraviolet layer 2 arranged on the base layer 1, a first buffer layer 3 is further arranged on the anti-ultraviolet layer 2, the first buffer layer 3 is a polyurethane elastic coating layer, an anti-friction buffer layer 4 is further arranged on the first buffer layer 3, the anti-friction buffer layer 4 is a transparent alkyd enamel layer, when impacted, the anti-friction buffer layer 4 absorbs part of the impact force and transmits the impact to the first buffer layer 3 made of the polyurethane elastic coating layer, so that the first buffer layer 3 is deformed, if the impact is too large and causes the glass to break, the first buffer layer 3 is stretched and deformed to adhere the broken pieces so that the glass fragments are fixed, when in use, first apply the anti-friction buffer layer 4 on the glass Apply the base layer 1, then apply the anti-ultraviolet layer 2 on the base layer 1, after the anti-ultraviolet layer 2 is dried, apply the first buffer layer 3 on the anti-ultraviolet layer 2, and then apply the anti-friction buffer layer 4 on the first buffer layer 3 after it is dried. After drying, if the glass is slightly impacted, since the first buffer layer 3 is a polyurethane elastic coating layer with strong ductility and elasticity, the first buffer layer 3 can be used in conjunction with the anti-friction buffer layer 4 to deform and elastically absorb the impact, so that the first buffer layer 3 is concave, and the impact force cannot be transmitted to the glass surface, so that the anti-crack ability of the glass is greatly improved. At the same time, when the glass is broken by a strong impact, the ductility of the first buffer layer 3 can be used to gather the fragments to prevent the fragments from splashing, so that the use safety is stronger;

[0018] The anti-friction buffer layer 4 is mixed with transparent glass beads, which is beneficial to enhancing the wear resistance of the anti-friction buffer layer 4 and making it stronger;

[0019] A foaming reaction layer 5 is provided between the first buffer layer 3 and the anti-friction buffer layer 4. The foaming reaction layer 5 includes a dry gelatin layer provided on the top surface of the first buffer layer 3 and an extrusion layer provided on the top surface of the dry gelatin layer. After being impacted, the dry gelatin layer performs secondary impact absorption, thereby further improving the upper limit of impact absorption.

[0020] The extrusion layer is provided with a plurality of water-soluble film blocks, and sixteen are provided in this embodiment. The water-soluble film blocks are filled with aqueous solvent, which is conducive to squeezing out the solvent after being squeezed, and then combining with the dry gelatin layer, so that the dry gelatin layer has stronger impact resistance;

[0021] The thickness of the first buffer layer 3 is 0.3 mm to 0.5 mm, which is conducive to making the impact resistance stronger and can limit more fragments from splashing;

[0022] The anti-friction buffer layer 4 has a thickness of 0.3 mm to 0.5 mm, which is beneficial for enhancing the impact resistance.

[0023] Working principle of the utility model: when the utility model is used, first apply a base layer 1 on the glass, then apply an anti-ultraviolet layer 2 on the base layer 1, after the anti-ultraviolet layer 2 is dried, apply a first buffer layer 3 on the anti-ultraviolet layer 2, and after the first buffer layer 3 is dried, apply an anti-friction buffer layer 4 thereon. After drying, if the glass is subjected to a slight impact, since the first buffer layer 3 is a polyurethane elastic coating layer with strong ductility and elasticity, the first buffer layer 3 can cooperate with the anti-friction buffer layer 4 to deform and elastically absorb the impact, so that the first buffer layer 3 is concave, and the impact force cannot be transmitted to the glass surface, so that the anti-cracking ability of the glass is greatly improved. At the same time, when the glass is broken by a strong impact, the ductility of the first buffer layer 3 is used to gather the fragments to prevent the fragments from splashing, so that it is safer to use.

[0024] The utility model is intended to protect the structure of the product. The model of each component is not the content of the utility model, and it is also a known technology. Any component on the market that can achieve the above functions of the utility model can be used as a choice. Therefore, the model and other parameters of the component are not described in detail in this utility model. The contribution of this utility model lies in the scientific combination of various components.

[0025] The above shows and describes the basic principle and main features and advantages of the utility model. Those skilled in the art should understand that the utility model is not limited by the above embodiments. The above embodiments and descriptions are only for explaining the principle of the utility model. Without departing from the spirit and scope of the utility model, the utility model may have various changes and improvements, which fall within the scope of the utility model to be protected. The scope of protection of the utility model is defined by the attached claims and their equivalents. Anything not described in detail in the utility model is a well-known technology of those skilled in the art.

Claims

1. A glass anti-crack coating, comprising a base layer (1) in contact with a glass surface and an anti-ultraviolet layer (2) disposed on the base layer (1), characterized in that: A first buffer layer (3) is also provided on the anti-ultraviolet layer (2), the first buffer layer (3) being a polyurethane elastic coating layer, and an anti-friction buffer layer (4) is also provided on the first buffer layer (3). When impacted, the anti-friction buffer layer (4) absorbs part of the impact force and transmits the impact to the first buffer layer (3) made of the polyurethane elastic coating layer, causing the first buffer layer (3) to deform. If the impact is too great and causes the glass to shatter, the first buffer layer (3) is stretched and deformed to adhere the shattered glass fragments so that the glass fragments are fixed.

2. The glass anti-crack coating according to claim 1, characterized in that: The anti-friction buffer layer (4) is a transparent alkyd enamel layer.

3. The glass anti-crack coating according to claim 2, characterized in that: Transparent glass micro beads are mixed into the anti-friction buffer layer (4).

4. The glass anti-crack coating according to claim 1, characterized in that: A foaming reaction layer (5) is provided between the first buffer layer (3) and the anti-friction buffer layer (4).

5. The glass anti-crack coating according to claim 4, characterized in that: The foaming reaction layer (5) comprises a dry gelatin layer arranged on the top surface of the first buffer layer (3) and an extrusion layer arranged on the top surface of the dry gelatin layer.

6. The glass anti-crack coating according to claim 5, characterized in that: A plurality of water-soluble film blocks are arranged in the extrusion layer, and aqueous solvent is contained in the water-soluble film blocks.

7. The glass anti-crack coating according to claim 1, characterized in that: The first buffer layer (3) has a thickness of 0.3 mm to 0.5 mm.

8. The glass anti-crack coating according to claim 1, characterized in that: The anti-friction buffer layer (4) has a thickness of 0.3 mm to 0.5 mm.