High-wear-resistance zirconia all-ceramic veneering device

By designing a highly wear-resistant zirconia all-ceramic veneer device and using engaging teeth and screw fixation structures, the problem of all-ceramic veneers falling off and insufficient tooth tissue area has been solved, achieving long life and high wear resistance, and is suitable for For customers with severe tooth damage.

CN221904107UActive Publication Date: 2024-10-29张增
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420123372.2
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-01-18
Publication Date
2024-10-29
Estimated Expiration
2034-01-18

AI Technical Summary

Technical Problem

All-ceramic veneers are easy to fall off after being used for a period of time, and some customers' teeth are severely damaged, resulting in insufficient dental tissue area available for bonding and poor bonding effects, making it impossible to repair them with all-ceramic veneers.

Method used

A highly wear-resistant zirconia all-ceramic veneer device is designed, including a front veneer tile and a rear veneer tile. The rear veneer tile is placed on the lower side of the inner wall of the front veneer tile. The front veneer tile There are engaging teeth on the inner wall, and engaging grooves and fixing holes on the surface of the back veneer porcelain. They are fixed with screws to ensure that the device is not easy to fall off. Nano carbon crystals are added to the material and surface coating to improve wear resistance.

Benefits of technology

It extends the service life of the all-ceramic veneer device and improves the bonding effect. It is suitable for customers with severe tooth damage, and the nano-carbon crystal coating improves wear resistance and user experience.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221904107U_ABST
    Figure CN221904107U_ABST
Patent Text Reader

Abstract

The utility model discloses a high-wear-resistance zirconium oxide all-ceramic veneering device, and relates to the technical field of all-ceramic veneering. The ceramic tile comprises a front veneering ceramic tile and a rear veneering ceramic tile, the rear veneering ceramic tile is arranged on the lower side of the inner wall of the front veneering ceramic tile, a plurality of clamping teeth are arranged on the lower side of the inner wall of the front veneering ceramic tile, a plurality of clamping grooves are formed in the lower side of the surface of the rear veneering ceramic tile, and fixing holes are formed in the front face and the rear face of the rear veneering ceramic tile. The inner walls of the two fixing holes are jointly provided with rotating shafts, the front ends and the rear ends of the two rotating shafts are fixedly connected with the inner wall of the front veneering ceramic chip, the front side and the rear side of the right face of the rear veneering ceramic chip are each provided with two mounting holes, and the inner walls of the front veneering ceramic chip and the rear veneering ceramic chip are jointly provided with teeth. The utility model has the advantages of long service life and low possibility of falling off, and solves the problem that all-ceramic veneering repair cannot be carried out due to poor sticking effect when the area of tooth tissues for sticking is not enough for customers with relatively large damage to partial teeth.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of all-ceramic veneers, in particular to a highly wear-resistant zirconia all-ceramic veneer device. Background Art

[0002] All-ceramic veneer is a method of cosmetic tooth restoration. It is a method of restoring missing teeth or discolored teeth by fixing a thin layer of porcelain restoration on the patient's teeth through bonding materials without grinding the teeth or grinding them as little as possible.

[0003] The advantages of all-ceramic veneers are that they reduce the amount of teeth grinding, are healthier, and can greatly improve the color of teeth. However, for crooked teeth, the improvement is very slight. If the teeth are obviously crooked, the effect of using ceramic veneers to make the teeth straight is not ideal. The ideal method is to correct the teeth first, wear braces for about one or two years to move the teeth to the correct position, and then do ceramic veneers to further improve the beauty of the teeth.

[0004] All-ceramic veneers are basically bonded to teeth through adhesive materials. After a period of use, they are prone to fall off. In addition, some customers' teeth are severely damaged. When bonding, if the area of ​​tooth tissue available for bonding is insufficient, the bonding effect is poor, and all-ceramic veneer restoration cannot be performed. For this reason, we proposed a highly wear-resistant zirconia all-ceramic veneer device. Utility Model Content

[0005] In order to achieve the above-mentioned purpose, the utility model specifically adopts the following technical solutions:

[0006] A highly wear-resistant zirconia all-ceramic veneer device, comprising a front veneer ceramic sheet and a rear veneer ceramic sheet, the rear veneer ceramic sheet being arranged on the lower side of the inner wall of the front veneer ceramic sheet, a plurality of engaging teeth being arranged on the lower side of the inner wall of the front veneer ceramic sheet, a plurality of engaging grooves being provided on the lower side of the surface of the rear veneer ceramic sheet, fixing holes being provided on the front and rear sides of the rear veneer ceramic sheet, a rotating shaft being provided on the inner walls of the two fixing holes, and both the front and rear ends of the rotating shafts being fixedly connected to the inner wall of the front veneer ceramic sheet, two mounting holes being provided on the front and rear sides of the right side of the rear veneer ceramic sheet, teeth being provided on the inner walls of the front veneer ceramic sheet and the rear veneer ceramic sheet, threaded holes being provided on the right side of the teeth at the two mounting holes, screws being provided on the inner walls of the two threaded holes and the inner walls of the corresponding mounting holes. The all-ceramic veneer device has a long service life and is not easy to fall off, and solves the problem that some customers with severely damaged teeth cannot perform all-ceramic veneer restoration because the bonding effect is poor when the tooth tissue area available for bonding is insufficient.

[0007] Furthermore, the front veneer ceramic sheet and the plurality of engaging teeth are an integrated structure.

[0008] Furthermore, the thickness of the front veneer tile and the back veneer tile are both 1-2 mm.

[0009] Furthermore, an annular groove is provided on the right side of the rear veneer tile around the two mounting holes, and the right end of the screw is arranged inside the annular groove.

[0010] Furthermore, the front veneer ceramics and the back veneer ceramics are both made of zirconium oxide.

[0011] Furthermore, the outer surfaces of the front veneer ceramic tile and the rear veneer ceramic tile are both provided with nano-carbon crystal coatings.

[0012] The beneficial effects of the utility model are as follows:

[0013] 1. During the use of the utility model, after the inner walls of the front veneer tiles and the back veneer tiles are brushed with adhesive material, the front veneer tiles and the back veneer tiles are wrapped around the teeth and attached to the teeth, and the front veneer tiles and the back veneer tiles are fixed to the teeth by the adhesive material. At this time, threaded holes are opened on the teeth, and the back veneer tiles are fixed to the teeth by screws. Under the action of the engaging teeth and the engaging grooves, the front veneer tiles are limited, so that the front veneer tiles are not easy to fall off, and the full-ceramic veneer device can also be used by customers with severe tooth damage, which solves the problem that some customers with severe tooth damage cannot perform full-ceramic veneer restoration because the bonding effect is poor when the tooth tissue area available for bonding is insufficient.

[0014] 2. The utility model ensures the hardness of the front veneer tiles and the back veneer tiles, and the annular groove hides the head of the screw, thereby improving the user experience of the customer.

[0015] 3. The front veneer ceramics and the back veneer ceramics of the utility model are both made of zirconium oxide, and nano-carbon crystal coatings are provided on the outer surfaces of the front veneer ceramics and the back veneer ceramics, thereby ensuring the high wear resistance of the all-ceramic veneer device. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 It is a front cross-sectional structural schematic diagram of the utility model;

[0017] Figure 2 The utility model Figure 1 A schematic diagram of the enlarged structure of part A;

[0018] Figure 3 The utility model Figure 1 A schematic diagram of the enlarged structure of part B;

[0019] Figure 4 It is a three-dimensional structural schematic diagram of the rear veneer tile of the utility model;

[0020] Figure numerals: 1, front veneer tile; 2, back veneer tile; 3, snap-fit ​​teeth; 4, snap-fit ​​groove; 5, fixing hole; 6, rotating shaft; 7, mounting hole; 8, teeth; 9, threaded hole; 10, screw; 11, ring groove. DETAILED DESCRIPTION

[0021] In order to make the purpose, technical solution and advantages of the embodiments of the present utility model clearer, the technical solution in the embodiments of the present utility model will be clearly and completely described below in conjunction with the drawings in the embodiments of the present utility model.

[0022] like Figure 1-4 As shown, a highly wear-resistant zirconia all-ceramic veneer device includes a front veneer ceramic 1 and a rear veneer ceramic 2. The rear veneer ceramic 2 is arranged on the lower side of the inner wall of the front veneer ceramic 1. A plurality of engaging teeth 3 are arranged on the lower side of the inner wall of the front veneer ceramic 1. A plurality of engaging grooves 4 are opened on the lower side of the surface of the rear veneer ceramic 2. Fixing holes 5 are opened on the front and rear sides of the rear veneer ceramic 2. A rotating shaft 6 is jointly arranged on the inner walls of the two fixing holes 5. The front and rear ends of the two rotating shafts 6 are fixedly connected to the inner wall of the front veneer ceramic 1. Two mounting holes 7 are opened on the front and rear sides of the right side of the rear veneer ceramic 2. Teeth 8 are jointly arranged on the inner walls of the front veneer ceramic 1 and the rear veneer ceramic 2. Threaded holes 9 are opened on the right side of the teeth 8 located at the two mounting holes 7. The inner walls of the two threaded holes 9 and the inner walls of the corresponding mounting holes 7 are jointly arranged There are screws 10. During the use of the full-ceramic veneer device, after brushing the inner walls of the front veneer ceramic tile 1 and the back veneer ceramic tile 2 with adhesive material, the front veneer ceramic tile 1 and the back veneer ceramic tile 2 wrap the tooth 8 and fit on the tooth 8, and the front veneer ceramic tile 1 and the back veneer ceramic tile 2 are fixed on the tooth 8 by the adhesive material. At this time, a threaded hole 9 is opened on the tooth 8, and the back veneer ceramic tile 2 is fixed on the tooth 8 by the screw 10. Under the action of the engaging teeth 3 and the engaging groove 4, the front veneer ceramic tile 1 is limited, so that the front veneer ceramic tile 1 is not easy to fall off, and the full-ceramic veneer device can also be used by customers with severe damage to the teeth 8, which solves the problem that some customers with severe damage to the teeth 8 cannot perform full-ceramic veneer restoration because the bonding effect is poor when the tooth tissue area available for bonding is insufficient.

[0023] like Figure 2-4 As shown, in some embodiments, the front veneer tile 1 and the plurality of engaging teeth 3 are an integrated structure, the thickness of the front veneer tile 1 and the rear veneer tile 2 are both 1 to 2 mm, and an annular groove 11 is provided on the right side of the rear veneer tile 2 around the two mounting holes 7, and the right end of the screw 10 is arranged inside the annular groove 11, which ensures the hardness of the front veneer tile 1 and the rear veneer tile 2. The annular groove 11 hides the head of the screw 10, thereby improving the customer's user experience.

[0024] like Figure 1As shown, in some embodiments, the front veneer ceramics 1 and the back veneer ceramics 2 are both made of zirconia, and the outer surfaces of the front veneer ceramics 1 and the back veneer ceramics 2 are both provided with nano-carbon crystal coatings, thereby ensuring the high wear resistance of the all-ceramic veneer device.

[0025] The above description of the disclosed embodiments enables those skilled in the art to implement or use the present invention. Various modifications to these embodiments will be apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but will conform to the widest scope consistent with the principles and novel features disclosed herein.

Claims

1. A highly wear-resistant zirconia all-ceramic veneer device, comprising a front veneer ceramic chip (1) and a back veneer ceramic chip (2), characterized in that: The rear veneer tile (2) is arranged on the lower side of the inner wall of the front veneer tile (1), and a plurality of engaging teeth (3) are arranged on the lower side of the inner wall of the front veneer tile (1). A plurality of engaging grooves (4) are provided on the lower side of the surface of the rear veneer tile (2). The front and rear sides of the rear veneer tile (2) are provided with fixing holes (5), and the inner walls of the two fixing holes (5) are provided with a rotating shaft (6). The front and rear ends of the two rotating shafts (6) are fixedly connected to the inner wall of the front veneer tile (1). Two mounting holes (7) are provided on the front and rear sides of the right side of the rear veneer tile (2). The inner walls of the front veneer tile (1) and the rear veneer tile (2) are provided with teeth (8), and the right side of the teeth (8) is provided with threaded holes (9) in the part located at the two mounting holes (7), and the inner walls of the two threaded holes (9) and the inner walls of the corresponding mounting holes (7) are provided with screws (10).

2. A highly wear-resistant zirconia all-ceramic veneer device according to claim 1, characterized in that: The front veneer tile (1) and the plurality of engaging teeth (3) are an integrated structure.

3. A highly wear-resistant zirconia all-ceramic veneer device according to claim 1, characterized in that: The thickness of the front veneer tile (1) and the back veneer tile (2) are both 1 to 2 mm.

4. A highly wear-resistant zirconia all-ceramic veneer device according to claim 1, characterized in that: An annular groove (11) is provided around the two mounting holes (7) on the right side of the rear veneer tile (2), and the right end of the screw (10) is arranged inside the annular groove (11).

5. A highly wear-resistant zirconia all-ceramic veneer device according to claim 1, characterized in that: The material of the front veneer ceramic tile (1) and the back veneer ceramic tile (2) are both zirconium oxide.

6. A highly wear-resistant zirconia all-ceramic veneer device according to claim 1, characterized in that: The outer surfaces of the front veneer ceramic tile (1) and the rear veneer ceramic tile (2) are both provided with a nano-carbon crystal coating.