Cover plate

By adopting the double-sided mirror imaging principle and multi-layer structural design in the cover plate, combined with preset graphics, the existing cover plate lacks deep bottomless effect and metal texture, and realizes visual three-dimensionality and excellent physical performance.

CN221946201UActive Publication Date: 2024-11-01LENS TECH CHANGSHA
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420459284.X
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-08
Publication Date
2024-11-01
Estimated Expiration
2034-03-08

AI Technical Summary

Technical Problem

The existing covers lack the mirror multi-layer reflection imaging design developed based on optical reflection, which cannot provide a deep bottomless visual effect and metallic texture.

Method used

Using the first coating layer, transparent substrate layer and second coating layer arranged in sequence from the inside to the outside, a double-plane mirror structure is formed in parallel and opposite directions in the space through the double-sided mirror imaging principle, and a multi-layer image reflection is formed in combination with preset graphics. Effect: The visible light reflectivity of the first coating layer and the second coating layer is controlled to achieve a deep bottomless effect.

Benefits of technology

It realizes visual three-dimensionality and metal texture, and has excellent Mohs hardness, friction resistance and alkali sweat resistance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221946201U_ABST
    Figure CN221946201U_ABST
Patent Text Reader

Abstract

The utility model provides a cover plate, which relates to the technical field of consumer electronics and comprises a first coating layer, a transparent substrate layer and a second coating layer which are sequentially arranged from inside to outside, wherein a preset pattern is arranged on the transparent substrate layer and / or the second coating layer; the visible light reflectivity of the first coating layer is not less than 50%; and the visible light reflectivity of the second coating layer is 30%-60%. According to the cover plate provided by the utility model, based on the double-sided mirror imaging principle, the double plane mirrors which are spatially arranged in parallel are formed through the composite multi-layer structures which are sequentially overlapped, and a multi-layer reflection effect is formed on preset patterns in the double plane mirrors, so that the cover plate which has metal texture and deep lighting effect and has excellent Mohs hardness, friction resistance and alkali sweat resistance is formed.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of consumer electronics, and more specifically, to a cover plate. Background Art

[0002] The cover plate can be a back cover, a front cover, a component or an entire shell, etc. It can refer to a detachable or non-detachable shell covering a digital product. For example, it can include but is not limited to: mobile phones, tablets, smart watches, smart translation devices, computers (notebooks, desktops) and related accessories, digital measuring equipment and smart glasses, etc. It can protect the internal components of the product and provide a certain degree of waterproof, dustproof and drop resistance.

[0003] The cover is usually made of plastic, metal, glass, etc. Different materials have different characteristics and advantages and disadvantages. For example, the plastic cover is light, flexible, low-cost, but relatively fragile; the metal back cover is strong and durable, but heavy; the glass cover is high-end and beautiful, but fragile and expensive.

[0004] Now, with the increase in the size of digital products and the diversification of their designs, product covers have also appeared in different forms and designs, such as frosted covers, matte covers, polished covers, etc. For example, high-end smartphones on the market currently mainly choose glass as the back cover material. The processes of brightening coating and hardening coating of glass covers have greatly enriched the design of mobile phone battery covers.

[0005] Currently, there is no cover plate that is specially developed based on optical reflection and uses mirror multi-layer reflective imaging. Utility Model Content

[0006] In order to solve the above defects, the utility model provides a cover plate, which includes:

[0007] A first coating layer, a transparent substrate layer, and a second coating layer are sequentially arranged from the inside to the outside;

[0008] Wherein, a preset pattern is provided on the transparent substrate layer and / or the second coating layer;

[0009] The visible light reflectivity of the first coating layer is not less than 50%;

[0010] The visible light reflectivity of the second coating layer is 30%-60%.

[0011] Preferably, the first coating layer comprises a film structure formed by alternating stacking of high refractive index materials and low refractive index materials; wherein the high refractive index material is a metal oxide.

[0012] Preferably, the metal oxide is any one or more of TiO2, ZrO2, ITO, Nb2O5, Ti3O5 and Ta2O5;

[0013] The low refractive index material is any one or more of SiO2, MgF2, and AlF3.

[0014] Preferably, the thickness of the first coating layer is 400nm-800nm;

[0015] The thickness of the second coating layer is 400nm-700nm.

[0016] Preferably, the visible light reflectivity of the first coating layer is 60%-80%.

[0017] Preferably, the visible light reflectivity of the second coating layer is 35%-45%.

[0018] Preferably, the absorption rate of the second coating layer is 20%-40%.

[0019] Preferably, the second coating layer comprises a film structure composed of a stack of low refractive index material, medium refractive index material and high refractive index material; wherein the first layer of the second coating layer is a low refractive index material layer and is connected to the transparent substrate layer; the ending layer of the second coating layer is a high refractive index material layer.

[0020] Preferably, the low refractive index material is at least one of aluminum and chromium;

[0021] The medium refractive index material is any one of SiO2 and Al2O3 alternately stacked, SiO2 and SiN alternately stacked, SiO2 and CrN alternately stacked, or MgF2 and ZrO2 alternately stacked;

[0022] The high refractive index material is at least one of SiAlO, SiTiN and SiON.

[0023] Preferably, the cover plate further includes a primer layer connected to the outer side of the first coating layer and a protective layer connected to the outer side of the second coating layer.

[0024] The utility model provides a cover plate. The cover plate comprises: a first coating layer, a transparent substrate layer and a second coating layer arranged in sequence from the inside to the outside; wherein a preset pattern is arranged on the transparent substrate layer and / or the second coating layer; the visible light reflectivity of the first coating layer is not less than 50%; and the visible light reflectivity of the second coating layer is 30%-60%.

[0025] The cover plate provided by the utility model is based on the double-sided mirror imaging principle and forms a quasi-double-plane mirror structure design arranged parallel and opposite in space by sequentially stacking a composite multi-layer structure, so as to form a multi-layer image reflection effect for a preset pattern therein. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 It is a schematic diagram of the overall cross section of the cover plate of the utility model;

[0027] Figure 2 This is a schematic diagram of the double-sided mirror imaging principle on which the cover plate of the utility model is based;

[0028] Figure 3 It is a schematic diagram of the optical effect of the finished surface of the cover plate of the utility model.

[0029] Reference numerals:

[0030] 100, cover plate; 1, inner protective layer; 2, first coating layer; 3, transparent substrate layer; 31, preset pattern; 4, second coating layer; 5, outer protective layer; 200, plane mirror; 300, virtual image mirror; 400, real object; 500, virtual image object.

[0031] The realization of the purpose, functional features and advantages of the utility model will be further explained in conjunction with embodiments and with reference to the accompanying drawings. DETAILED DESCRIPTION

[0032] The embodiments of the present application are described in detail below, and examples of the embodiments are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present application, and cannot be understood as limiting the present application.

[0033] In the description of the present application, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.

[0034] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of this application, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.

[0035] In this application, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.

[0036] In the present application, unless otherwise clearly specified and limited, a first feature being “above” or “below” a second feature may mean that the first and second features are in direct contact, or the first and second features are in indirect contact through an intermediate medium. Moreover, a first feature being “above”, “above”, and “above” a second feature may mean that the first feature is directly above or obliquely above the second feature, or simply means that the first feature is higher in level than the second feature. A first feature being “below”, “below”, and “below” a second feature may mean that the first feature is directly below or obliquely below the second feature, or simply means that the first feature is lower in level than the second feature.

[0037] refer to Figure 1 , the utility model provides a cover plate, which includes a first coating layer, a transparent substrate layer, and a second coating layer arranged in sequence from the inside to the outside;

[0038] Wherein, a preset pattern is provided on the transparent substrate layer and / or the second coating layer;

[0039] The visible light reflectivity of the first coating layer is not less than 50%;

[0040] The visible light reflectivity of the second coating layer is 30%-60%.

[0041] refer to Figure 2 In the present invention, the preset graphics superimposed therein are formed into a spatial abyss effect through the principle of double-sided mirror imaging by means of the first coating layer and the second coating layer having a certain visible light reflectivity. That is, based on the principle of double-sided mirror imaging, a quasi-double-plane mirror structure design arranged parallel and opposite in space is formed by sequentially superimposing a composite multi-layer structure, and a multi-layer reflection effect is formed for the preset graphics therein, thereby having a metallic texture and forming an abyss light effect.

[0042] It should be noted that the two-sided mirror imaging principle is one of the basic principles in the field of optics. It refers to the reflection of light when passing through a two-sided mirror (also called a plane mirror), thereby forming a virtual image.

[0043] Specifically, when light is perpendicular to the surface of a two-sided mirror, it will be reflected back along the same path, forming a virtual image that is equal in position, size, and upright to the real object.

[0044] It should be noted that the imaging principle of a two-way mirror is based on certain conditions, including the placement of the object and the mirror, which affects whether the light is reflected at the same angle. In addition, the positional relationship between the object and the two-way mirror affects whether the path of the virtual image remains symmetrical.

[0045] In addition, the effect of reflectivity needs to be considered. Generally speaking, the higher the reflectivity of a two-sided mirror, the brighter the virtual image produced. At the same time, if the virtual image is far away from the two-sided mirror, the reflectivity will also affect the image clarity.

[0046] In the utility model, on the basis of the inner protective layer, a first coating layer is provided as a "first plane mirror", and a second coating layer is provided as a "second plane mirror"; between the two coating layers, a transparent substrate layer with a transparent effect is provided, and a preset pattern is provided on the transparent substrate layer (for example, on its outer surface) and / or on the second coating layer (for example, on its inner surface) as a "real object"; in this case, according to the imaging principle of the double-sided mirror, the "real object" on the transparent substrate layer is reflected by the "first plane mirror" and the "second plane mirror", and in the reflective multi-layer imaging effect, two multi-layer virtual image mirrors other than the plane mirrors as entities are continuously generated within the depth of field, with virtual image objects corresponding to the real objects between the virtual image mirrors or in the virtual image mirrors, thereby forming a reflective multi-layer imaging, and gradually weakening and deep and bottomless effect.

[0047] When light is incident vertically, it is reflected from the surface of the transparent substrate layer of the first plane mirror to the second plane mirror. Then, the light is reflected back to the transparent substrate layer of the first plane mirror and reflected again. This process can be repeated many times, and each reflection will slightly weaken the intensity of the light.

[0048] Since each reflection slightly loses the energy of light, the intensity of light gradually decreases with the increase of the number of reflections, forming a gradually weakening effect of reflected multi-layer imaging. This effect can make the pattern look deep and bottomless, giving people a visual sense of three-dimensionality. For example, the specific optical display form of the cover surface can refer to Figure 3 (Take the preset graphic as "LOGO" as an example).

[0049] It should be noted that the degree of this effect depends on factors such as the refractive index of the transparent substrate layer, the contrast of the pattern, and the incident angle of the light. The specific effect may vary depending on the actual situation.

[0050] In the present invention, by controlling the stacking order of different film layers and setting the visible light reflectivity of different film layers, the desired effect of gradually weakening and deep bottomlessness based on the double-sided mirror imaging principle is achieved. Specifically, the film layers need to be controlled to meet the following two requirements at the same time:

[0051] (1) The visible light reflectivity of the first coating layer is ≥50%;

[0052] (2) The visible light reflectivity of the second coating layer is 30%-60%.

[0053] Among them, by limiting the visible light reflectivity of the first coating layer to be no less than 50%, for example, it can be 60%, 70%, 80%, 90%, etc., it is possible to enhance the brightness of the transparent substrate layer in the middle of the cover and the preset graphic area, as well as the colorful visual effect.

[0054] When the visible light reflectivity of the second coating layer is controlled at 30%-60%, it can produce spatial lamination visible to the naked eye; for example, it can be 30%, 40%, 50%, 60% and so on, wherein the higher the visible light reflectivity, the more effective visible spatial lamination; conversely, the lower the visible light reflectivity, the fewer effective visible spatial laminations.

[0055] As mentioned above, the inner surface of the transparent substrate layer is in contact with the first coating layer, and the preset pattern can be arranged on the outer surface of the transparent substrate layer, on the inner surface of the second coating layer, or in the second coating layer.

[0056] As mentioned above, the transparent substrate layer can be made of transparent materials such as glass, quartz, crystal, gemstone, etc. Its main function is to serve as the middle transparent part of the back cover, shell or back panel of the product, and its thickness can be controlled within the range of 0.5±0.05mm.

[0057] The preset graphics mentioned above may be a logo, a specific pattern, text information, etc., and are disposed on the outer surface of the transparent substrate layer.

[0058] In summary, the cover plate provided by the utility model forms a double plane mirror arranged in parallel in space through a composite multi-layer structure stacked in sequence based on the principle of double-sided mirror imaging. Through the reflection of the transparent substrate layer and the plane mirror, a gradually weakened, deep and bottomless effect of the reflected multi-layer imaging can be formed, creating a visual three-dimensional sense, thereby forming a cover plate with metallic texture and abyss light effect, and having excellent Mohs hardness, friction resistance, and alkali sweat resistance.

[0059] Furthermore, the first coating layer includes a film structure formed by alternating stacking of high refractive index materials and low refractive index materials; wherein the high refractive index material is a metal oxide.

[0060] Further, the metal oxide is any one or more of TiO2, ZrO2, ITO, Nb2O5, Ti3O5 and Ta2O5;

[0061] The low refractive index material is any one or more of SiO2, MgF2, and AlF3.

[0062] As mentioned above, the first coating layer, as the first plane mirror appearing in the inner direction of the back cover, can be made of a film structure composed of two parts of alternately stacked high-refractive-index material and low-refractive-index material.

[0063] The “high refractive index material is a metal oxide”, where the metal oxide refers to a specific type of metal oxide composed of metal elements and oxygen elements with a higher refractive index than the low refractive index material. For example, it may include but is not limited to the following materials:

[0064] (1) Titanium dioxide (TiO2): Due to its high refractive index and good chemical stability, it is often used in anti-reflective coatings and other optical coatings.

[0065] (2) Zirconium oxide (ZrO2): It is also a high refractive index material and is often used to make optical coatings.

[0066] (3) Indium Tin Oxide (ITO): It has transparent conductive properties, but can also be used as a high refractive index material.

[0067] In the cover plate structure, the first coating layer includes alternately stacked high refractive index and low refractive index materials, and this structure is used to achieve the specific optical effect in the utility model, to enhance reflection, transmission or produce specific color effects, etc. Among them, the high refractive index metal oxide here plays the role of enhancing reflectivity and adjusting optical properties.

[0068] In the utility model, the metal oxide used can be any one or more of TiO2, ZrO2, ITO, Nb2O5, Ti3O5 and Ta2O5. The low refractive index material used can be any one or more of SiO2, MgF2 and AlF3. Among them, in the first coating layer, the high refractive index and low refractive index materials can be Nb2O5 and SiO2 respectively, which are selected based on the requirements of economy and durability. The single silicon target and niobium target are conventional coating materials, and the price is moderate to meet the economic efficiency of mass production.

[0069] Furthermore, the thickness of the first coating layer is 400nm-800nm; for example, it can be any value among 400nm, 500nm, 600nm, 700nm, 800nm ​​and 400nm-800nm.

[0070] The thickness of the second coating layer is 400nm-700nm, for example, it can be any value among 400nm, 500nm, 600nm, 700nm and 400nm-700nm.

[0071] Furthermore, the visible light reflectivity of the first coating layer is 60%-80%, for example, it can be any value among 60%, 70%, 80% and 60%-80%.

[0072] Furthermore, the visible light reflectivity of the second coating layer is 35%-45%, for example, it can be any value among 35%, 38%, 39%, 40%, 41%, 42%, 43%, 44%, 45% and 35%-45%.

[0073] Furthermore, the absorption rate of the second coating layer is 20%-40%, for example, it can be any value among 20%, 25%, 30%, 35%, 40% and 20%-40%.

[0074] It should be noted that the reflectivity of the second coating layer can be mainly determined by three aspects, namely, the stacked imaging effect, the physical properties of the film layer and the appearance of the preset graphic (LOGO):

[0075] (1) From the analysis of actual imaging effects, when the reflectivity of the second coating layer decreases, the effective stacking visible in the space will decrease accordingly. Conversely, when it increases, the effective stacking visible in the space will increase. Experimental verification shows that when the visible light reflectivity of the second coating layer is 30%-60%, the effective stacking effect in the space can be displayed.

[0076] In a preferred technical solution, when the visible light reflectivity of the second coating layer reaches 40%±5%, the number of effective clear layers visible in the space is 4-5 layers, and the preset graphic (LOGO) can show an obvious "abyss effect" within the visual area visible to the naked eye.

[0077] (2) Physical properties of the film layer: Since the area of ​​the preset pattern is an exposed area and the actual use environment is complex, the coating layer needs to have good physical properties. After actual testing, ultra-hard physical materials are used to match the film system to achieve the design effect. For example, the exposed film layer of SiO2 / AL2O3 / SiAlO has excellent hardness and corrosion resistance.

[0078] Taking into account the optical properties and actual effects of the selected materials, in the above technical solution, when the visible light reflectivity is 30%-60%, it can produce an effective stacking effect (abyss effect) visible in a certain space.

[0079] However, in actual production, experiments have shown that further increasing the reflectivity on the basis of 60% will greatly increase the difficulty of coating, and when it is lower than 30%, the number of layers is reduced to 2-3 layers due to the attenuation of the reflected light intensity, and the abyss effect is weakened. Therefore, in the above technical parameters, the visible light reflectivity of the second coating layer can produce an effective stacking effect (abyss effect) visible in a certain space within the range of 30%-60%. If it exceeds this range, the effect will be affected to a certain extent; the visible light reflectivity of 40%±5% in the preferred technical solution is the range value that comprehensively considers all options.

[0080] (3) Appearance effect of the preset pattern: When the second coating layer has a reflectivity of about 30%, there will be 70% transmittance at the same time, which will cause the color of the preset pattern area to be affected by the reflected light of the first coating layer, while weakening the metal effect of the preset pattern.

[0081] Therefore, the above problem can be improved by controlling the absorption rate of the second coating layer.

[0082] It should be noted that the absorptivity refers to the degree of light absorption by the coating layer (coating, material). When the coating layer has a higher absorptivity, it can absorb more light and reduce light reflection. The value range of the absorptivity can be determined based on experimental tests to achieve the best effect and appearance.

[0083] In the utility model, the value of the absorptivity of the second coating layer is found through experimental tests. When the absorptivity is lower than 20%, the phenomenon is not significantly improved. When the absorptivity is higher than 40%, the intensity of reflected light is reduced, which affects the lamination effect to a certain extent. Therefore, when the absorptivity of the second coating layer is controlled at 20%-40%, better effects can be achieved. In addition, in a preferred technical solution, when the absorptivity of the second coating layer is 30%±10%, it is a more optimal range value.

[0084] In addition, changes in the light source illumination may also affect the reflection of the above-mentioned visible light, but will not affect the characteristics of the coating layer itself. Specifically, changes in the light source illumination will also change the brightness of the image. The stronger the ambient light, the clearer the layers, and the more visible layers there are. The visible light reflectivity is an optical property of the coating layer and has nothing to do with the light intensity. However, the stronger the light intensity, the stronger the reflection.

[0085] Therefore, the cover plate provided by the present invention can produce more visible layers in an environment with stronger illumination conditions, thereby achieving better optical effects.

[0086] Furthermore, the second coating layer includes a film structure formed by alternately stacking low-refractive index materials, medium-refractive index materials and high-refractive index materials.

[0087] As mentioned above, the second coating layer is formed by alternately stacking materials with different refractive indexes, specifically, low refractive index materials, medium refractive index materials and high refractive index materials.

[0088] In this embodiment, different materials can be classified and limited by the following refractive index ranges:

[0089] (1) Low refractive index material: n≤1.5;

[0090] (2) Medium refractive index material: 1.5<n<2.0

[0091] (3) High refractive index material: n ≥ 2.0.

[0092] Further, the low refractive index material is at least one of aluminum and chromium;

[0093] The medium refractive index material is any one of the following combinations:

[0094] (1) SiO2 and Al2O3 are stacked alternately,

[0095] (2) SiO2 and SiN are stacked alternately,

[0096] (3) SiO2 and CrN are alternately stacked

[0097] (4) MgF2 and ZrO2 are stacked alternately

[0098] The high refractive index material is at least one of SiAlO, SiTiN and SiON.

[0099] Furthermore, the first layer of the second coating layer 4 is a low refractive index material layer and is connected to the transparent substrate layer 3. The low refractive index material is set as the first layer, which can increase the adhesion with the transparent substrate layer 3 and produce the absorption value of the design target, such as aluminum and chromium; the ending layer of the second coating layer 4 is a high refractive index material layer and is connected to the outer protective layer 5. The high refractive index material layer is used as the ending layer, and the SI contained therein can increase the bonding strength with the outer protective layer, and this high refractive index material layer itself can meet the high hardness requirements.

[0100] Furthermore, the cover plate also includes a primer layer connected to the outer side of the first coating layer and a protective layer connected to the outer side of the second coating layer.

[0101] The low refractive index material can be at least one of aluminum and chromium. In a preferred embodiment, aluminum is used as the low refractive index material, and metal Al can have good adhesion on the transparent substrate layer (including glass and other substrates). At the same time, the metal Al has a large visible light absorption property, which reduces the transmittance of the coating area and weakens the influence of the inner surface light to have a metallic texture.

[0102] It should be noted that Al has absorption properties that affect the transmittance of light. The outer surface color of the transparent substrate layer is the result of the comprehensive film system. Highly reflected light can also be silver. When the amount of light absorbed by the film layer is low and the color of the material itself is displayed, the present invention also needs to reduce the transmittance through the absorption of Al so that the second coating layer does not transmit too much reflected light from the first coating layer, thereby affecting the metallic luster.

[0103] As mentioned above, Al2O3 material has high hardness and excellent corrosion resistance, and combined with specific coating process conditions (such as the preparation process described below), the film layer can have excellent physical properties.

[0104] As mentioned above, through experimental determination, among high refractive index materials, selecting SiAlO (or SiTiN, SiON) as the transition layer between the second coating layer and the outer protective layer can effectively improve the bonding ability between the film layer of the second coating layer and the protective layer, and greatly improve the friction resistance and Mohs hardness test level. Under this condition, the dynamic friction coefficient of the protective layer is ≤0.02, which is significantly improved compared with the dynamic friction coefficient of 0.03 of conventional SiO2+AF. At the same time, the hardness of SiAlO is higher than that of SiO2.

[0105] The above-mentioned base layer can be a protective film layer for laminating the adhesive backing. The protective layer is an AF layer (Anti-Fouling layer), which can have the function of waterproof and oil-proof, and is required to have relatively excellent Mohs hardness, friction resistance, and alkali sweat resistance, so as to protect the transparent substrate layer and the two coating layers in the composite multi-layer structure.

[0106] As mentioned above, the primer layer may be an ink layer composed of epoxy resin; the thickness of the primer layer may be 10 μm-15 μm.

[0107] As mentioned above, the protective layer may be a fluorine-containing polymer; and its thickness may be 4nm-8nm.

[0108] For better explanation, the cover plate provided in the present invention provides the following preparation process:

[0109] Step 1, performing a strengthening treatment on glass to obtain a glass substrate (transparent substrate layer);

[0110] Step 2: Use an ultrasonic cleaner to clean and dry the glass substrate;

[0111] Step 3: Use an automated loading machine to move the glass substrate loaded on a special fixture into the preparatory coating chamber of the sputtering coating machine;

[0112] Step 4: Prepare the vacuum pump of the coating chamber and pump the vacuum degree to 5.0*E-1Pa, start the automatic heating tube of the chamber, heat the temperature to 200℃-300℃ and keep it for 30 minutes. Effectively remove the remaining water vapor, CO2 and other impurities on the coating fixture, special adhesive and glass substrate;

[0113] Step 5: The glass substrate is transported to the film-forming chamber under vacuum conditions, and the vacuum degree of the film-forming chamber is maintained at ≤1.0*E-3Pa;

[0114] Step 6: After the vacuum degree reaches the set value, plasma cleaning treatment will be carried out. The specific process parameters are shown in Table 1 below. This step can effectively reduce the surface energy of the glass substrate and enhance the bonding strength between the glass substrate and the coating stack.

[0115] Table 1. Inductively coupled plasma etching (ICP) parameters

[0116] ICP power(kw) Ar(sccm) <![CDATA[O2(sccm)]]> Processing time(s) 2000~3000 200-500 200-500 500-1200

[0117] Step 7, according to the designed coating system, the coating machine completes the coating of the inner surface of the glass substrate; the coating process conditions of the silicon / niobium target are as shown in Table 2, and the coating process conditions of the Al target are as shown in Table 3;

[0118] Table 2. Silicon / niobium target coating process parameters

[0119] ICP power(kw) Ar(sccm) <![CDATA[O2(sccm)]]> Film forming vacuum degree (Pa) Target power(kw) Coating temperature(℃) 2000~2500 100-200 200-300 0.2-0.6 10-12 60-70

[0120] Table 3. Aluminum target coating process parameters

[0121] ICP power(kw) Ar(sccm) <![CDATA[O2(sccm)]]> Film forming vacuum degree (Pa) Target power(kw) Coating temperature(℃) 3000~3500 100-200 200-300 0.2-0.6 8-10 80-90

[0122] Step 8: LOGO (preset graphic) on the outer surface of the glass substrate;

[0123] Step 9, repeat step 2 → step 7 to complete the coating on the outer surface of the glass substrate;

[0124] Step 10, coating AF film (protective layer);

[0125] Step 11: Spray ink (base layer).

[0126] Although the present invention has been disclosed as above with preferred embodiments, it is not intended to limit the present invention. Any person skilled in the art may make some modifications and improvements without departing from the spirit and scope of the present invention. Therefore, the scope of protection of the present invention shall be based on the definition of the claims.

Claims

1. A cover plate, It is characterized in that The cover plate comprises: A first coating layer, a transparent substrate layer, and a second coating layer are sequentially arranged from the inside to the outside; Wherein, a preset pattern is provided on the transparent substrate layer and / or the second coating layer; The visible light reflectivity of the first coating layer is not less than 50%; The visible light reflectivity of the second coating layer is 30%-60%.

2. The cover plate according to claim 1, It is characterized in that The first coating layer includes a film structure formed by alternating stacking of high refractive index materials and low refractive index materials; wherein the high refractive index material is a metal oxide.

3. The cover plate as claimed in claim 2, It is characterized in that The metal oxide is TiO 2 、ZrO 2 、ITO、Nb 2 O 5 、Ti 3 O 5 and Ta 2 O 5 Any one or more of the following; The low refractive index material is SiO 2 MgF 2 , AlF 3 Any one or more of .

4. The cover plate according to claim 1, It is characterized in that The thickness of the first coating layer is 400nm-800nm; The thickness of the second coating layer is 400nm-700nm.

5. The cover plate according to claim 1, It is characterized in that The visible light reflectivity of the first coating layer is 60%-80%.

6. The cover plate according to any one of claims 1 to 5, It is characterized in that The visible light reflectivity of the second coating layer is 35%-45%.

7. The cover plate according to claim 6, It is characterized in that The absorption rate of the second coating layer is 20%-40%.

8. The cover plate according to any one of claims 1 to 5, It is characterized in that The second coating layer includes a film structure composed of a stack of low refractive index material, medium refractive index material and high refractive index material; wherein the first layer of the second coating layer is a low refractive index material layer and is connected to the transparent substrate layer; the ending layer of the second coating layer is a high refractive index material layer.

9. The cover plate according to claim 8, It is characterized in that The low refractive index material is at least one of aluminum and chromium; The medium refractive index material is SiO 2 and Al 2 O 3 Alternating stacking, SiO 2 Alternately stacked with SiN, SiO 2 Alternately stacked with CrN or MgF 2 and ZrO 2 Any set in an alternating stack; The high refractive index material is at least one of SiAlO, SiTiN and SiON.

10. The cover plate according to any one of claims 1 to 5, It is characterized in that The cover plate also includes a primer layer connected to the outer side of the first coating layer and a protective layer connected to the outer side of the second coating layer.