Mining track switch core switch rail manufacturing mold
By using a wedge-shaped structure and a positioning pin connection method, the difficulties in connecting the molds for manufacturing the core tip rails of mining track switches and the problem of glue contamination were solved, thus achieving stable assembly of the molds and high-quality finished products.
Patent Information
- Application Number
- CN202420555701.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-21
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2034-03-21
AI Technical Summary
The existing molds for manufacturing the core switch rails of mining track switches have a complex split structure, making connection difficult and prone to errors. Furthermore, the use of glue or glue rods leads to poor finished product quality and environmental pollution.
The connection method using a wedge structure and positioning pins replaces the traditional glue or glue stick connection. The wedge structure and interference fit ensure the stability and accuracy of the mold.
It simplifies the mold assembly process, reduces connection errors, increases yield, avoids chemical residues and environmental pollution, and improves work efficiency and product quality.
Smart Images

Figure CN221952250U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to a manufacturing mould for a mine track switch core point rail, belonging to the technical field of track switch core point rail manufacturing. Background Art
[0002] Lost foam casting (also known as full mold casting) is a new casting method that combines paraffin or foam models with similar size and shape to the casting into a model cluster, brushes refractory coating and dries it, buries it in dry quartz sand for vibration molding, and pours it under negative pressure to vaporize the model. Liquid metal occupies the position of the model, and forms a casting after solidification and cooling. The prior art often uses this casting technology in casting track switch core point rails. For example, the prior art discloses a mold for a narrow-gauge integral switch core for mining, with announcement number CN203541453U. Although the original split narrow-gauge switch core is designed into an integrally cast switch core with an integral structure through mold processing, the disclosed mold is also a split structure in which mold core rails, mold left wing rails, mold right wing rails and mold bottom plates made of different shapes are bonded together with hot melt glue sticks. In actual application, there are two defects. One is that the complex split structure of the mold will increase In addition to the difficulty of combined connection and the large workload, connection errors are very likely to occur at the joints, reducing the quality rate of the product. Secondly, a large amount of glue or glue sticks are used at the joints in multiple positions. The fixed glue or glue sticks overflowing from the mold surface will directly affect the processing details of the finished track switch core point rail, that is, the actual shape buried in the dry quartz sand, and the uneven surface of the finished product or excess burrs directly affect the difficulty of re-finishing. At the same time, during the casting and melting process of the mold or when vibrating and shaping in the quartz sand, it is very easy to crack or deform, which directly affects the shape of the finished track switch core point rail.
[0003] Therefore, it is urgent to propose a novel manufacturing mold for the switch core point rail of mining rail to solve the above technical problems. Utility Model Content
[0004] The purpose of developing this utility model is to solve the problem that the complex split structure of the mold will increase the difficulty of its combination and connection, and reduce the quality rate of the product. A brief overview of the utility model is given below to provide a basic understanding of certain aspects of the utility model. It should be understood that this overview is not an exhaustive overview of the utility model. It is not intended to determine the key or important parts of the utility model, nor is it intended to limit the scope of the utility model.
[0005] The technical solution of this utility model:
[0006] A mold for manufacturing a mine rail switch core point rail, comprising a first mold block, a second mold block and a third mold block, wherein the right end of the first mold block is fixedly connected to the left end of the second mold block, and the right end of the second mold block is fixedly connected to the left end of the third mold block. The first mold block, the second mold block and the third mold block are connected to form a rail switch core point rail mold, and a Y-shaped switch track is processed on the top of the rail switch core point rail mold.
[0007] Preferably: the second mold block is fixedly connected to the first mold block via a first wedge-shaped structure;
[0008] The wedge-shaped structure includes a first guide shaft, a first locking block and a first wedge-shaped clamping block, one end of the first guide shaft is installed on the right end surface of the first mold block, and the other end of the first guide shaft is fixedly installed with the first locking block, and the left end surface of the second mold block is processed with a connected first guide hole and a first slide groove, the first locking block passes through the first guide hole and is placed in the first slide groove, and the left end surface of the first locking block is clamped against the left side wall of the first slide groove, and the first wedge-shaped clamping block is arranged between the left end surface of the first wedge-shaped clamping block and the left side wall of the first slide groove, and the first wedge-shaped clamping block is fixedly connected to the left end surface of the first locking block or the left side wall of the first slide groove.
[0009] Preferably: the second mold block and the third mold block are fixedly connected via a second wedge-shaped structure;
[0010] The wedge-shaped structure includes a second guide shaft, a second locking block and a second wedge-shaped clamping block, one end of the second guide shaft is installed on the left end surface of the third mold block, and the other end of the second guide shaft is fixedly installed with the second locking block, and the right end surface of the second mold block is processed with a connected second guide hole and a second slide groove, the second locking block passes through the second guide hole and is placed in the second slide groove, and the right side end surface of the second locking block is clamped against the right side wall of the second slide groove, a second wedge-shaped clamping block is arranged between the right side end surface of the second wedge-shaped clamping block and the right side wall of the second slide groove, and the second wedge-shaped clamping block is fixedly connected to the right side end surface of the second locking block or the right side wall of the second slide groove.
[0011] Preferably: the first wedge-shaped structure also includes a positioning rotation pin, which is fixedly arranged on the right side wall of the first slide groove, and a positioning rotation hole is arranged on the right end face of the first locking block, and the central axes of the first guide shaft, the positioning rotation pin and the positioning rotation hole are arranged colinearly.
[0012] Preferably, a wedge-shaped groove is provided at the bottom of the connection between the second mold block and the first mold block and the third mold block, a wedge-shaped positioning block is installed in the wedge-shaped groove, and an interference fit is formed between the two.
[0013] Preferably: the left and right sides of the track switch core point rail mold are respectively provided with a left wing rail and a right wing rail, the middle part of the track switch core point rail mold is provided with a core rail, and the left and right wing rails are surrounded on the left and right sides of the core rail to form a Y-shaped switch.
[0014] The utility model has the following beneficial effects:
[0015] 1. The utility model has a simple structure, ingenious design, convenient disassembly and assembly, and firm assembly, which greatly reduces the manufacturing difficulty of the rail switch core point rail manufacturing mold, improves work efficiency, saves work time, and thus reduces production costs;
[0016] 2. The utility model reduces the connection and installation errors, improves the quality rate of products, avoids deformation or breakage during vibration molding in quartz sand, and reduces the phenomenon of uneven surface or extra burrs on the finished product, which directly greatly reduces the difficulty of re-finishing;
[0017] 3. The utility model abandons the glue or glue stick adhesion of the prior art, making the operation faster and simpler, while avoiding the additional chemical residues caused by the glue or glue stick after the glue or glue stick is poured and melted in the mold, reducing the impurity content of the finished track switch core point rail, making the mold structure more stable and less prone to deformation. Finally, it avoids the smell of glue or glue sticks and chemical volatile substances that may cause harm to the human body, greatly improving the working environment of workers. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 It is a stereoscopic diagram of a manufacturing mold for a mining track switch core point rail according to a specific implementation mode 1;
[0019] Figure 2 It is a front view of a manufacturing mold for a mining track switch core point rail according to the first specific implementation mode;
[0020] Figure 3 It is an exploded view of a manufacturing mold for a mining track switch core point rail according to the second specific implementation mode;
[0021] Figure 4 It is a front view of a mold for manufacturing a mining track switch core point rail according to the second specific implementation mode;
[0022] Figure 5 yes Figure 4 A magnified image of point A;
[0023] Figure 6 yes Figure 4 A magnified view of point B;
[0024] Figure 7 is a schematic diagram of the cooperation between the first wedge-shaped tightening block and the first sliding groove described in the second specific implementation mode;
[0025] Figure 8 is a schematic diagram of the cooperation between the wedge-shaped positioning block and the wedge-shaped groove described in the second specific implementation mode;
[0026] Fig. 9 It is a structural schematic diagram of a mold for manufacturing a switch core point rail for a mining track described in a third specific implementation mode;
[0027] Fig.10 yes Fig. 9 Enlarged view of point C;
[0028] In the figure, 1-the first mold block, 2-the second mold block, 3-the third mold block, 4-Y-shaped fork, 5-the first guide shaft, 6-the first locking block, 7-the first wedge-shaped top tightening block, 8-the first guide hole, 9-the first slide groove, 10-the second guide shaft, 11-the second locking block, 12-the second wedge-shaped top tightening block, 13-the second guide hole, 14-the second slide groove, 15-the wedge-shaped positioning block, 16-the left wing rail, 17-the right wing rail, 18-the core rail, 19-the positioning rotation pin, and 20-the positioning rotation hole. DETAILED DESCRIPTION
[0029] In order to make the purpose, technical solution and advantages of the utility model clearer, the utility model is described below by specific embodiments shown in the accompanying drawings. However, it should be understood that these descriptions are only exemplary and are not intended to limit the scope of the utility model. In addition, in the following description, the description of well-known structures and technologies is omitted to avoid unnecessary confusion of the concept of the utility model.
[0030] Specific implementation method 1: Combination Figure 1-Figure 2 The present embodiment is described. A mining rail switch core point rail manufacturing mold of the present embodiment comprises a first mold block 1, a second mold block 2 and a third mold block 3. The right end of the first mold block 1 is fixedly connected to the left end of the second mold block 2, and the right end of the second mold block 2 is fixedly connected to the left end of the third mold block 3. The first mold block 1, the second mold block 2 and the third mold block 3 are connected to form a rail switch core point rail mold. A Y-shaped switch 4 is processed on the top of the rail switch core point rail mold.
[0031] The first mold block 1, the second mold block 2 and the third mold block 3 are fixedly connected by glue.
[0032] The left and right sides of the track switch core point rail mold are respectively provided with a left wing rail 16 and a right wing rail 17, and the middle part of the track switch core point rail mold is provided with a core rail 18. The left wing rail 16 and the right wing rail 17 are surrounded on the left and right sides of the core rail 18 to form a Y-shaped switch track 4.
[0033] In actual use, before casting, the track switch core point rail mold formed by fixing the first mold block 1, the second mold block 2 and the third mold block 3 together is placed in a pool filled with liquid paint and rolled repeatedly to evenly coat the outer layer of the track switch core point rail mold of the core with the paint, and the track switch core point rail mold coated with the paint is placed in a dry explosion chamber for drying. After the paint is fully dried, the outer layer of the track switch core point rail mold forms a hard shell, and then the track switch core point rail mold is placed in a sand box, and the sand box is filled with sand and compacted and sealed. During casting, the sealed sand box is evacuated, and then molten iron is poured into the track switch core point rail mold through a previously reserved pouring port. At this time, the track switch core point rail mold made of polystyrene material is deeply burned in the high-temperature molten iron, and the molten iron remains in the cavity of the track switch core point rail mold shell. Then, the integrally cast track switch core point rail is made by demoulding and polishing.
[0034] Specific implementation method 2: Combination Figure 3-Figure 8 The present embodiment is described. A mining rail switch core point rail manufacturing mold of the present embodiment comprises a first mold block 1, a second mold block 2 and a third mold block 3. The right end of the first mold block 1 is fixedly connected to the left end of the second mold block 2, and the right end of the second mold block 2 is fixedly connected to the left end of the third mold block 3. The first mold block 1, the second mold block 2 and the third mold block 3 are connected to form a rail switch core point rail mold. A Y-shaped switch 4 is processed on the top of the rail switch core point rail mold.
[0035] Because the existing glue or glue stick will bring additional chemical residues after the mold is poured and melted, affecting the impurity content of the finished rail switch core point rail. At the same time, during the mold pouring and melting process, due to the different melting points of the glue or glue stick and the mold, it will melt in advance or lag, causing the mold to crack or deform, directly affecting the shape of the finished rail switch core point rail. Finally, the smell of the glue or glue stick and the chemical volatile substances will cause harm to the human body and the working environment is bad. Therefore, this embodiment also solves the problem that the existing technology uses glue sticks to connect the mold to affect the impurity content and processing quality of the finished rail switch core point rail, as follows:
[0036] The second mold block 2 is fixedly connected to the first mold block 1 via a first wedge-shaped structure;
[0037] The wedge-shaped structure includes a first guide shaft 5, a first locking block 6 and a first wedge-shaped tightening block 7. One end of the first guide shaft 5 is installed on the right end surface of the first mold block 1, and the other end of the first guide shaft 5 is fixedly installed with the first locking block 6. The left end surface of the second mold block 2 is processed with a first guide hole 8 and a first slide groove 9 that are connected. The first locking block 6 passes through the first guide hole 8 and is placed in the first slide groove 9, and the left end surface of the first locking block 6 is tightened against the left side wall of the first slide groove 9. The first wedge-shaped tightening block 7 is arranged between the left end surface of the first wedge-shaped tightening block 7 and the left side wall of the first slide groove 9. The first wedge-shaped tightening block 7 is fixedly connected to the left end surface of the first locking block 6 or the left side wall of the first slide groove 9.
[0038] The second mold block 2 and the third mold block 3 are fixedly connected via a second wedge-shaped structure;
[0039] The wedge-shaped structure includes a second guide shaft 10, a second locking block 11 and a second wedge-shaped clamping block 12. One end of the second guide shaft 10 is installed on the left end surface of the third mold block 3, and the other end of the second guide shaft 10 is fixedly installed with the second locking block 11. The right end surface of the second mold block 2 is processed with a second guide hole 13 and a second slide groove 14 that are connected. The second locking block 11 passes through the second guide hole 13 and is placed in the second slide groove 14, and the right side end surface of the second locking block 11 is clamped against the right side wall of the second slide groove 14. A second wedge-shaped clamping block 12 is arranged between the right side end surface of the second wedge-shaped clamping block 12 and the right side wall of the second slide groove 14. The second wedge-shaped clamping block 12 is fixedly connected to the right side end surface of the second locking block 11 or the right side wall of the second slide groove 14.
[0040] The second wedge-shaped tightening block 12 has the same structure as the first wedge-shaped tightening block 7, and is both provided for the purpose of providing tightening force, and both have an inclined surface.
[0041] The first guide hole 8 and the second guide hole 13 are both gate-shaped holes with an arc-shaped top. The arc-shaped top surface of the gate-shaped hole is designed to fit with the arc-shaped side walls of the first guide shaft 5 and the second guide shaft 10, and the bottom is designed to accommodate the surface of the first locking block 6 or the second locking block 11 to fit through.
[0042] The bottom of the connection between the second mold block 2 and the first mold block 1 and the third mold block 3 is provided with a wedge groove, and a wedge-shaped positioning block 15 is installed in the wedge groove, and there is an interference fit between the two. The wedge-shaped positioning block 15 is used for positioning to prevent the molds from rotating relative to each other.
[0043] The first wedge-shaped structure and the second wedge-shaped structure are essentially the same in structure, that is, they are the same structure with a mirror image setting. Therefore, in this embodiment, the installation operation method between the second mold block 2 and the first mold block 1 is taken as an example, which is the same as the installation operation method between the second mold block 2 and the third mold block 3.
[0044] The first wedge-shaped structure also includes a positioning rotating pin 19, which is fixedly arranged on the right side wall of the first slide slot 9, and a positioning rotating hole 20 is arranged on the right end face of the first locking block 6. The central axes of the first guide shaft 5, the positioning rotating pin 19 and the positioning rotating hole 20 are arranged in a colinear manner. When the positioning rotating hole 20 on the first slide slot 9 is inserted into the outer side of the positioning rotating pin 19, the positioning rotating pin 19 and the positioning rotating hole 20 rotate and cooperate to provide a limiting effect for the first guide shaft 5 and the positioning rotating pin 19, so as to avoid radial shaking when the first locking block 6 rotates, resulting in failure to fit tightly. Similarly, the second wedge-shaped structure can also be provided with a positioning rotating pin 19 and a positioning rotating hole 20 accordingly.
[0045] The specific operation method is as follows:
[0046] Align the first locking block 6 on the first mold block 1 with the first guide hole 8, and after entering the first guide hole 8, rotate the first mold block 1 to align it with the surface of the second mold block 2. While rotating, the first locking block 6 inserted into the first slide groove 9 is also rotating. Under the action of the inclined surface of the first wedge-shaped tightening block 7, the more it rotates, the tighter the first mold block 1 and the second mold block 2 are clamped, thereby minimizing the joint width to the greatest extent. At the same time, under the action of friction and tightening force, the fitting surface maintains the installation state of the first mold block 1 and the second mold block 2 in alignment. Finally, install the wedge-shaped positioning block 15 with force to make it clamped in the wedge-shaped groove to prevent the first mold block 1 and the second mold block 2 from being easily flipped over, thereby completing the fixed connection between the first mold block 1, the second mold block 2 and the third mold block 3.
[0047] In actual use, before casting, the track switch core point rail mold formed by fixing and connecting the first mold block 1, the second mold block 2 and the third mold block 3 is placed in a pool filled with liquid paint and rolled repeatedly, so that the outer layer of the track switch core point rail mold of the bin core is evenly coated with paint, and the track switch core point rail mold coated with paint is placed in a dry explosion room for drying. After the paint is fully dried, the outer layer of the track switch core point rail mold forms a hard shell, and then the track switch core point rail mold is placed in a sand box, and the sand box is filled with sand, vibrated and sealed. At this time, due to the first mold block 1, the second mold block 2 and the third mold block 3, the track switch core point rail mold is The three mold blocks 3 are not easily deformed due to the connection between the first wedge-shaped structure and the second wedge-shaped structure. During casting, the sealed sand box is evacuated into a vacuum, and then the molten iron is poured into the track switch core point rail mold through a previously reserved gate. At this time, the track switch core point rail mold made of polystyrene material is deepened in the high-temperature molten iron, and the molten iron remains in the cavity of the track switch core point rail mold shell. Since the use of glue or glue sticks in the prior art is abandoned, the track switch core point rail mold of this embodiment avoids the introduction of other additional chemical impurities. Then, the integrally cast track switch core point rail is made through demoulding and polishing.
[0048] Specific implementation method three: Combination Figure 9-10 The present embodiment includes a track switch core point rail mold with a Y-shaped switch track 4 processed on the top, and the track switch core point rail mold is a multi-stage type.
[0049] The track switch core point rail mould is divided into three sections, and every two adjacent sections of the track switch core point rail mould are fixedly connected by a wedge-shaped structure.
[0050] The wedge-shaped structure includes a first guide shaft 5, a first locking block 6 and a first wedge-shaped tightening block 7. One end of the first guide shaft 5 is installed on the right end face of the switch core point rail mold of the previous section of the track, and the other end of the first guide shaft 5 is fixedly installed with the first locking block 6. The left end face of the switch core point rail mold of the latter section of the track is processed with a connected first guide hole 8 and a first slide groove 9. The first locking block 6 passes through the first guide hole 8 and is placed in the first slide groove 9, and the left end face of the first locking block 6 is tightened against the left side wall of the first slide groove 9. The first wedge-shaped tightening block 7 is arranged between the left end face of the first wedge-shaped tightening block 7 and the left side wall of the first slide groove 9. The first wedge-shaped tightening block 7 is fixedly connected to the left end face of the first locking block 6 or the left side wall of the first slide groove 9.
[0051] The first wedge-shaped tightening blocks 7 have the same structure and are all provided for the purpose of providing tightening force, and the surfaces of the first wedge-shaped tightening blocks 7 all have an inclined surface.
[0052] The first guide hole 8 is a gate-shaped hole with an arc-shaped top. The arc-shaped top surface of the gate-shaped hole is for fitting with the arc-shaped side wall of the first guide shaft 5, and the bottom is for accommodating the surface of the first locking block 6 to fit through.
[0053] A wedge-shaped groove is provided at the bottom of the connection between each two adjacent sections of the track turnout core point rail molds, and a wedge-shaped positioning block 15 is installed in the wedge-shaped groove, and there is an interference fit between the two. The wedge-shaped positioning block 15 is used for positioning to prevent the molds from rotating relative to each other.
[0054] The specific operation method is as follows:
[0055] The first locking block 6 on the front section track switch core point rail mold is aligned with the first guide hole 8. After entering the first guide hole 8, the front section track switch core point rail mold is rotated to align it with the surface of the rear section track switch core point rail mold. While rotating, the first locking block 6 inserted into the first slide groove 9 is also rotating. Under the action of the inclined surface of the first wedge-shaped tightening block 7, the more it rotates, the tighter the front section track switch core point rail mold and the rear section track switch core point rail mold are clamped, thereby minimizing the joint width to the greatest extent. At the same time, under the action of friction and tightening force, the fitting surface maintains the installation state of the front section track switch core point rail mold and the rear section track switch core point rail mold in alignment. Finally, the wedge-shaped positioning block 15 is installed with force to make it clamped in the wedge-shaped groove to prevent the front section track switch core point rail mold and the rear section track switch core point rail mold from being easily flipped over, thereby completing the fixed connection between the first mold block 1, the second mold block 2 and the third mold block 3.
[0056] The first wedge-shaped structure also includes a positioning rotating pin 19, which is fixedly arranged on the right side wall of the first slide slot 9, and a positioning rotating hole 20 is arranged on the right end face of the first locking block 6. The central axes of the first guide shaft 5, the positioning rotating pin 19 and the positioning rotating hole 20 are arranged in a colinear manner. When the positioning rotating hole 20 on the first slide slot 9 is inserted into the outer side of the positioning rotating pin 19, the positioning rotating pin 19 and the positioning rotating hole 20 rotate and cooperate to provide a limiting effect for the first guide shaft 5 and the positioning rotating pin 19, so as to avoid radial shaking when the first locking block 6 rotates, resulting in failure to fit tightly. Similarly, the second wedge-shaped structure can also be provided with a positioning rotating pin 19 and a positioning rotating hole 20 accordingly.
[0057] In actual use, before casting, the rail switch core point rail mold formed after the rail switch core point rail mold is fixedly connected is placed in a pool filled with liquid paint and rolled repeatedly to make the outer layer of the rail switch core point rail mold of the core evenly coated with paint, and the rail switch core point rail mold coated with paint is placed in a dry explosion room for drying. After the paint is fully dried, the outer layer of the rail switch core point rail mold forms a hard shell, and then the rail switch core point rail mold is placed in a sand box, and the sand box is filled with sand, vibrated and sealed. At this time, due to the wedge shape of the rail switch core point rail mold Under the connection of the structure, it is not easy to deform. During casting, the sealed sand box is evacuated into a vacuum, and then the molten iron is poured into the track switch core point rail mold through the previously reserved gate. At this time, the track switch core point rail mold made of polystyrene material is deepened in the high-temperature molten iron, and the molten iron remains in the cavity of the track switch core point rail mold shell. Since the use of glue or glue sticks in the prior art is abandoned, the track switch core point rail mold of this embodiment avoids the introduction of other additional chemical impurities. Then, the integrally cast track switch core point rail is made by demoulding and polishing.
[0058] It should be noted that in the above embodiments, as long as the technical solutions are not contradictory, they can be arranged and combined, and those skilled in the art can exhaust all possibilities based on the mathematical knowledge of arrangement and combination. Therefore, the present utility model will no longer describe the technical solutions after arrangement and combination one by one, but it should be understood that the technical solutions after arrangement and combination have been disclosed by the present utility model.
[0059] The above description is only the preferred embodiment of the utility model, and is not intended to limit the utility model. For those skilled in the art, the utility model can have various modifications and changes. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the utility model shall be included in the protection scope of the utility model.
Claims
1. A mining track switch core point rail manufacturing mold, characterized in that: The invention comprises a first mold block (1), a second mold block (2) and a third mold block (3); the right end of the first mold block (1) is fixedly connected to the left end of the second mold block (2); the right end of the second mold block (2) is fixedly connected to the left end of the third mold block (3); the first mold block (1), the second mold block (2) and the third mold block (3) are connected to form a track switch core point rail mold; a Y-shaped switch track (4) is arranged on the top of the track switch core point rail mold.
2. A mining rail switch core point rail manufacturing mold according to claim 1, characterized in that: The second mold block (2) is fixedly connected to the first mold block (1) via a first wedge-shaped structure; The first wedge-shaped structure comprises a first guide shaft (5), a first locking block (6) and a first wedge-shaped pressing block (7); one end of the first guide shaft (5) is mounted on the right end face of the first mold block (1); the other end of the first guide shaft (5) is fixedly mounted with the first locking block (6); the left end face of the second mold block (2) is processed with a first guide hole (8) and a first slide groove (9) which are connected; the first locking block (6) passes through the first guide hole (8) and is placed in the first slide groove (9); the left end face of the first locking block (6) is pressed against the left side wall of the first slide groove (9); the first wedge-shaped pressing block (7) is arranged between the left end face of the first wedge-shaped pressing block (7) and the left side wall of the first slide groove (9); the first wedge-shaped pressing block (7) is fixedly connected to the left end face of the first locking block (6) or the left side wall of the first slide groove (9).
3. A mining rail switch core point rail manufacturing mold according to claim 2, characterized in that: The first wedge-shaped structure also includes a positioning rotating pin (19), which is fixedly arranged on the right side wall of the first sliding groove (9), and a positioning rotating hole (20) is arranged on the right end face of the first locking block (6). The positioning rotating pin (19) and the positioning rotating hole (20) are rotatably matched, and the central axes of the first guide shaft (5), the positioning rotating pin (19) and the positioning rotating hole (20) are arranged colinearly.
4. A mining rail switch core point rail manufacturing mold according to claim 1, characterized in that: The second mold block (2) and the third mold block (3) are fixedly connected via a second wedge-shaped structure; The wedge-shaped structure comprises a second guide shaft (10), a second locking block (11) and a second wedge-shaped pressing block (12); one end of the second guide shaft (10) is mounted on the left end face of the third mold block (3); the other end of the second guide shaft (10) is fixedly mounted with the second locking block (11); the right end face of the second mold block (2) is processed with a second guide hole (13) and a second slide groove (14) which are connected; the second locking block (11) passes through the second guide hole (13) and is placed in the second slide groove (14); the right end face of the second locking block (11) is pressed against the right side wall of the second slide groove (14); a second wedge-shaped pressing block (12) is arranged between the right end face of the second wedge-shaped pressing block (12) and the right side wall of the second slide groove (14); the second wedge-shaped pressing block (12) is fixedly connected to the right end face of the second locking block (11) or the right side wall of the second slide groove (14).
5. The manufacturing mold for a mining rail switch core point rail according to claim 1, characterized in that: The bottom of the connection between the second mold block (2) and the first mold block (1) and the third mold block (3) is provided with a wedge-shaped groove, a wedge-shaped positioning block (15) is installed in the wedge-shaped groove, and the two are interference-fitted.
6. A mining rail switch core point rail manufacturing mold according to claim 1, characterized in that: The left and right sides of the rail switch core point rail mold are respectively provided with a left wing rail (16) and a right wing rail (17), and the middle part of the rail switch core point rail mold is provided with a core rail (18). The left wing rail (16) and the right wing rail (17) are surrounded on the left and right sides of the core rail (18) to form a Y-shaped switch track (4).