Peeling test fixture and peeling test system

By designing the movable cooperation between the clamping frame and the sample block fixing frame, and using the self-weight of the post-cast concrete sample block for fixation, the problems of complex clamp structure and cumbersome disassembly in the existing technology are solved, realizing a simple and efficient peel test between waterproof membrane and post-cast concrete.

CN221959999UActive Publication Date: 2024-11-05ANHUI SKSHU PAINT CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323477523.9
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-19
Publication Date
2024-11-05
Estimated Expiration
2033-12-19

AI Technical Summary

Technical Problem

Existing waterproof membrane peel test fixtures are complex and bulky, and the disassembly of test samples is cumbersome, making the testing work complicated and inconvenient.

Method used

The specially designed clamping frame and the sample fixing frame work together to fix the post-cast concrete sample using the weight of the post-cast concrete sample and the sample fixing frame itself. The clamping device is connected to the tensile testing machine to ensure accurate test angles and no deviation in sample position, making the test simple and easy to operate.

Benefits of technology

It achieves a simple structure, convenient disassembly of the test block, accurate test results, ensures a test angle of 180°, stable block position, and improves test efficiency and accuracy.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221959999U_ABST
    Figure CN221959999U_ABST
Patent Text Reader

Abstract

The utility model relates to a stripping test fixture and a stripping test system, the stripping test fixture is matched with a tensile machine for detecting the stripping condition after a waterproof roll and a post-cast concrete sample block are bonded, and the tensile machine comprises an upper fixture and a lower fixture which can respectively move upwards and downwards relative to each other; the stripping test fixture comprises a clamping frame and a sample block fixing frame which is movably sleeved in the clamping frame and is used for fixing a post-cast concrete sample block. The stripping test device for the waterproof coiled material and the post-cast concrete overcomes the defects that an existing stripping test device for the waterproof coiled material and the post-cast concrete is complex in structure, and the disassembly step of the test sample block is tedious. The post-pouring concrete sample block is fixed by utilizing the self-weight of the post-pouring concrete sample block and the sample block fixing frame, and the device has the advantages of simple structure, convenience in disassembly of the test sample block and easiness in operation.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to a peeling test fixture and a peeling test system, which are particularly applied to the peeling test of waterproof coiled material and post-cast concrete, and are applied to waterproof coiled material detection equipment. Background Art

[0002] The description in this section only provides background information related to the present disclosure and does not constitute prior art. Pre-laid and wet-laid waterproof membranes are now widely used for underground waterproofing of buildings, and their peel strength with concrete is an important indicator for examining their waterproofing effect. The existing peeling test fixture is complex in structure and too bulky, and each time the sample is loaded and unloaded, a lot of disassembly and assembly of the fixture is required, making the test work complicated and bulky (such as CN201920154862.8 discloses a peeling strength test fixture for waterproof membranes and post-cast concrete). Therefore, it has become an urgent task to provide a peeling test fixture and a peeling test system with a simple structure and easy operation. Utility Model Content

[0003] In order to overcome the shortcomings of the existing peeling test device for waterproof membrane and post-cast concrete, such as complex structure and cumbersome disassembly steps of the test sample, the utility model provides a peeling test fixture and a peeling test system, which adopt a specially designed clamping frame and a sample fixing frame to cooperate with each other, and utilize the dead weight of the post-cast concrete sample and the sample fixing frame to fix the post-cast concrete sample. It has the advantages of simple structure, convenient disassembly of the test sample and easy operation.

[0004] The technical solution of the utility model is as follows:

[0005] A peeling test fixture is used in conjunction with a tensile machine to detect the peeling condition of a waterproof membrane and a post-cast concrete sample after bonding. The tensile machine comprises an upper fixture and a lower fixture that can move upward and downward relative to each other respectively; the peeling test fixture comprises a clamping frame and a sample fixing frame that is movably sleeved in the clamping frame and is used to fix the post-cast concrete sample;

[0006] The clamping frame comprises a clamping frame body with a hollow cavity structure having upper and lower openings, and a clamping device connected to the top of the clamping frame body and connected to the upper clamp of the tensile machine;

[0007] The sample block fixing frame includes a fixing frame body and a pair of sliding card joints respectively connected to the opposite side walls of the top of the fixing frame body and corresponding to each other; a pair of corresponding sliding grooves are opened on the opposite side walls of the clamping frame body, and each sliding groove starts from the top of one lateral side of the side wall and extends to the middle of the side wall in a direction close to the other side of the side wall and inclined downward, and the distance between the end faces of the two sliding card joints is greater than the distance between the inner walls of the opposite side walls of the clamping frame body where the sliding grooves are opened; the fixing frame body can be movably inserted in the inner cavity of the clamping frame body The sliding card joint is movably connected in the slide groove, and the fixed frame body moves downward along the slide groove relative to the clamping frame due to its own gravity. When the sliding card joint stops moving in the slide groove, the distance L between the side wall of the fixed frame body away from the starting point of the slide groove and the inner wall of the clamping frame body on the opposite side closest to the side wall is less than the thickness of the post-cast concrete sample; during the test, the upper part of the post-cast concrete sample is clamped between the fixed frame body and the inner wall of the clamping frame body; the bottom end of the waterproof membrane extends out of the bottom end surface of the post-cast concrete sample for a distance and is connected to the lower clamp of the tensile machine.

[0008] The peeling test fixture of the present application adopts a specially designed clamping frame that works in conjunction with a sample fixing frame, and utilizes the deadweight of the post-cast concrete sample and the sample fixing frame to fix the post-cast concrete sample. It has the advantages of simple structure, convenient disassembly of the test sample, and easy operation. Both the clamping frame and the sample fixing frame are frame structures, and the clamping frame is specially designed with a clamping device for connecting to the upper clamp of the tensile testing machine. It adopts a one-end fixed clamping method, which greatly saves the loading and unloading time of the post-cast concrete sample. This solution utilizes the deadweight of the post-cast concrete sample and the sample fixing frame to fix the post-cast concrete sample in a self-locking manner. It is easy to install on the tensile testing equipment and convenient for the disassembly of the test sample. It has a simple structure and is easy to operate.

[0009] The specific process of the peeling test on the post-cast concrete sample is as follows: connect the clamping device to the upper clamp of the tensile machine to fix the clamping frame. Install the upper part of the post-cast concrete sample into the inner cavity of the clamping frame body, and also put the fixed frame body into the inner cavity of the clamping frame body, so that the sliding card joint is inserted into the slide groove. Due to its own weight, the fixed frame body moves downward along the slide groove relative to the clamping frame body, so that the upper part of the post-cast concrete sample is clamped and fixed between the clamping frame body and the fixed frame body. Then, the lower end of the waterproof membrane is fixedly connected to the lower clamp of the tensile machine, and the tensile machine is started. The lower clamp of the tensile machine does not move, and the upper clamp moves upward, and the waterproof membrane peeling test experiment can be carried out. The peeling test fixture can solve the problem of fixing the sample well, and the loading and unloading of the sample is more convenient and quick.

[0010] The clamping device is located directly above the contact surface between the waterproof membrane and the post-cast concrete sample.

[0011] In the peeling test with post-cast concrete (sample block), because the waterproof membrane needs to be folded 180° for testing, it is very easy for the concrete sample block to not be completely fixed using the current relevant technology, resulting in the test result being too large or too small. For example, CN202020710043.X discloses a test device for the peeling strength of waterproof membrane and post-cast concrete. Since the thickness of the sample block cannot be guaranteed to be completely consistent with the thickness of the actual product when the post-cast concrete is prepared, the fixture in comparative document 2 will easily have two unexpected situations: 1. The sample block thickness is too large, and the membrane 5 will scrape against the bottom of the sample block when peeling, resulting in a larger test result value; 2. The sample block thickness is too small, so that the test angle of the membrane 5 is less than 180° (the test angle required by the standard is 180°), resulting in a smaller test result value. For another example, CN201920154862.8 discloses a peeling strength test fixture for waterproofing membrane and post-cast concrete. During the downward stretching process of the sample, the membrane will be subjected to different forces twice. Due to the lack of a lateral fixing structure for the sample, the sample will rotate, which will increase the test width and make the test result value larger. The peeling test fixture of the present application uses the deadweight of the post-cast concrete sample and the sample fixing frame to fix the post-cast concrete sample in a self-locking manner, and sets the clamping device directly above the contact surface between the waterproofing membrane and the post-cast concrete sample (that is, the fixture fixing surface and the test surface of the post-cast concrete sample are on the same plane), ensuring the accuracy of the test angle (180°), so that the test results are accurate, ensuring the correct test direction of the sample (the test angle is 180°), and ensuring the accuracy of the test results.

[0012] The length of the side wall of the fixed frame body away from the starting point of the chute is greater than or equal to the length of the post-cast concrete sample. During the test, the side wall of the post-cast concrete sample is completely attached to the side wall of the fixed frame body.

[0013] The preferred fixed frame body and the design that it is completely fitted with the side wall of the post-cast concrete sample block during the test ensure that the overall position of the post-cast concrete sample block does not shift during the test, further ensuring the accuracy of the test results.

[0014] The clamping device is a clamping plate.

[0015] Preferably, the clamping device has a simple structure and is convenient to connect with the upper clamp of the tensile machine.

[0016] The clamping frame body, the clamping device, the fixed frame body and the sliding card joint are respectively a stainless steel clamping frame body, a stainless steel clamping device, a stainless steel fixed frame body and a stainless steel sliding card joint.

[0017] Stainless steel parts are more durable.

[0018] The clamping frame body is a rectangular parallelepiped structure, with a length and a width of 60 mm and a height of 100 mm; the height of the clamping device is 100 mm.

[0019] The preferred clamping frame body has a moderate shape and size and is convenient to use.

[0020] The fixed frame body is a rectangular parallelepiped structure with a length of 60 mm, a width of 25 mm and a height of 200 mm.

[0021] The preferred fixing frame body has a moderate shape and size and is convenient to use.

[0022] The fixing frame body is a hollow structure made of a stainless steel plate, and the thickness of the stainless steel plate is 5 mm.

[0023] The preferred fixed frame body has high firmness and durability and can save a lot of material costs.

[0024] A peeling test system comprises the peeling test fixture and a tensile machine with an upper fixture and a lower fixture, wherein the tensile machine can drive the upper fixture and the lower fixture to move up and down, the upper fixture of the tensile machine is connected to a clamping device, the waterproof membrane is placed vertically and the top is bent 180 degrees and attached to the side wall of the middle or bottom of a post-cast concrete sample, and the lower fixture of the tensile machine is connected to the bottom end of the waterproof membrane.

[0025] The peeling test system has the advantages of simple structure, easy operation and accurate test results.

[0026] Compared with the prior art, the utility model application has the following advantages:

[0027] 1) The peeling test fixture of the present application adopts a specially designed clamping frame and a sample fixing frame to cooperate flexibly, and uses the deadweight of the post-cast concrete sample and the sample fixing frame to fix the post-cast concrete sample, which has the advantages of simple structure and convenient disassembly of the test sample;

[0028] 2) The clamping device is set just above the contact surface between the waterproof membrane and the post-cast concrete sample (i.e. the fixture fixing surface and the test surface of the post-cast concrete sample are on the same plane), ensuring the accuracy of the test angle (180°), making the test results accurate, ensuring the correct test direction of the sample (the test angle is 180°), and ensuring the accuracy of the test results;

[0029] 3) The preferred fixed frame body and the design that it is completely fitted with the side wall of the post-cast concrete sample during the test ensure that the overall position of the post-cast concrete sample does not shift during the test, further ensuring the accuracy of the test results;

[0030] 4) The peeling test system of the present application has the advantages of simple structure, easy operation and accurate test results. BRIEF DESCRIPTION OF THE DRAWINGS

[0031] Figure 1 It is a side view of the clamping frame of the peeling test fixture and the peeling test system of the utility model;

[0032] Figure 2 It is a front view of the peeling test fixture and the clamping frame of the peeling test system described in the utility model;

[0033] Figure 3 It is a side view of the peeling test fixture and the sample block fixing frame of the peeling test system of the utility model;

[0034] Figure 4 It is a front view of the peeling test fixture and the sample block fixing frame of the peeling test system of the utility model;

[0035] Figure 5 It is a schematic diagram of the assembly and use of the peeling test fixture and the peeling test system described in the utility model;

[0036] Figure 6 The utility model is a peeling test fixture and a peeling test system Figure 5 AA section view.

[0037] Description of labels:

[0038] Waterproof membrane 1, post-cast concrete sample 2, upper clamp 3, lower clamp 4, clamping frame 5, sample fixing frame 6, clamping frame body 5-1, clamping device 5-2, fixing frame body 6-1, sliding card joint 6-2, slide groove 5-1-1. DETAILED DESCRIPTION

[0039] The technical solution of the utility model will be described clearly and completely below in conjunction with the accompanying drawings. Obviously, the described embodiments are part of the embodiments of the utility model, rather than all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in the field without making creative work are within the scope of protection of the utility model. In the description of the utility model, it should be noted that the orientation or position relationship indicated by the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inside", "outside", etc. is based on the orientation or position relationship shown in the accompanying drawings, which is only for the convenience of describing the utility model and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the utility model. In addition, the terms "first", "second", and "third" are only used for descriptive purposes and cannot be understood as indicating or implying relative importance.

[0040] like Figure 1-6 As shown, a peeling test fixture of the utility model is used in conjunction with a tensile machine to detect the peeling condition of a waterproof membrane 1 and a post-cast concrete sample 2 after bonding. The tensile machine includes an upper clamp 3 and a lower clamp 4 that can move upward and downward relative to each other respectively; the peeling test fixture includes a clamping frame 5 and a sample fixing frame 6 movably sleeved in the clamping frame 5 for fixing the post-cast concrete sample 2;

[0041] The clamping frame 5 comprises a clamping frame body 5-1 of a hollow cavity structure with upper and lower openings, and a clamping device 5-2 connected to the top of the clamping frame body 5-1 and connected to the upper clamp 3 of the tensile machine;

[0042] The sample block fixing frame 6 includes a fixing frame body 6-1 and a pair of sliding card joints 6-2 respectively connected to the opposite side walls of the top of the fixing frame body 6-1 and corresponding in position; a pair of corresponding sliding grooves 5-1-1 are opened on the opposite side walls of the clamping frame body 5-1, and each sliding groove 5-1-1 starts from the top of one lateral side of the side wall and extends to the middle of the side wall in a direction close to the other side of the side wall and inclined downward, and the distance between the end faces of the two sliding card joints 6-2 is greater than the distance between the inner walls of the opposite side walls of the clamping frame body 5-1 where the sliding grooves 5-1-1 are opened; the fixing frame body 6-1 can be movably inserted in the inner cavity of the clamping frame body 5-1, and the sliding card joints 6-2 can be moved to the inner cavity of the clamping frame body 5-1. The joint 6-2 is movably connected in the slide groove 5-1-1, and the fixed frame body 6-1 moves downward along the slide groove 5-1-1 relative to the clamping frame 5 due to its own gravity. When the sliding card joint 6-2 stops moving in the slide groove 5-1-1, the distance L between the side wall of the fixed frame body 6-1 away from the starting point of the slide groove 5-1-1 and the inner wall of the clamping frame body 5-1 on the opposite side closest to the side wall is less than the thickness of the post-cast concrete sample 2; during the test, the upper part of the post-cast concrete sample 2 is clamped between the fixed frame body 6-1 and the inner wall of the clamping frame body 5-1; the bottom end of the waterproof membrane 1 extends out of the bottom end surface of the post-cast concrete sample 2 for a distance and is connected to the lower clamp 4 of the tensile machine.

[0043] The clamping device 5 - 2 is located directly above the contact surface between the waterproof membrane 1 and the post-cast concrete sample 2 .

[0044] The length of the side wall of the fixed frame body 6-1 away from the starting point of the chute 5-1-1 is greater than or equal to the length of the post-cast concrete sample 2. During the test, the side wall of the post-cast concrete sample 2 is completely attached to the side wall of the fixed frame body 6-1.

[0045] The clamping device 5 - 2 is a clamping plate.

[0046] The clamping frame body 5-1, the clamping device 5-2, the fixed frame body 6-1 and the sliding card joint 6-2 are respectively a stainless steel clamping frame body, a stainless steel clamping device, a stainless steel fixed frame body and a stainless steel sliding card joint.

[0047] The clamping frame body 5-1 is a rectangular parallelepiped structure, with a length and a width of 60 mm and a height of 100 mm; the height of the clamping device 5-2 is 100 mm.

[0048] The fixed frame body 6 - 1 is a rectangular parallelepiped structure with a length of 60 mm, a width of 25 mm and a height of 200 mm.

[0049] The fixed frame body 6 - 1 is a hollow structure made of a stainless steel plate, and the thickness of the stainless steel plate is 5 mm.

[0050] A peeling test system includes the peeling test fixture described above, and a tensile testing machine with an upper clamp 3 and a lower clamp 4, wherein the tensile testing machine can drive the upper clamp 3 and the lower clamp 4 to move up and down, the upper clamp 3 of the tensile testing machine is connected to the clamping device 5-2, the waterproof membrane 1 is placed vertically and the top is bent 180° and attached to the side wall of the middle or bottom of the post-cast concrete sample 2, and the lower clamp 4 of the tensile testing machine is connected to the bottom end of the waterproof membrane 1.

[0051] In the description of the present utility model, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected" and "connected" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal connection of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present utility model can be understood according to specific circumstances. In addition, the technical features involved in the different embodiments of the present utility model described below can be combined with each other as long as they do not conflict with each other.

Claims

1. A peeling test fixture, used in conjunction with a tensile machine to detect the peeling condition of a waterproof membrane (1) and a post-cast concrete sample (2) after bonding, the tensile machine comprising an upper fixture (3) and a lower fixture (4) that can move upward and downward relative to each other, respectively; characterized in that: The peeling test fixture comprises a clamping frame (5) and a sample block fixing frame (6) movably sleeved in the clamping frame (5) for fixing the post-cast concrete sample block (2); The clamping frame (5) comprises a clamping frame body (5-1) having a hollow cavity structure with upper and lower openings, and a clamping device (5-2) connected to the top of the clamping frame body (5-1) and connected to an upper clamp (3) of a tensile machine; The sample block fixing frame (6) comprises a fixing frame body (6-1) and a pair of sliding card joints (6-2) respectively connected to opposite side walls of the top of the fixing frame body (6-1) and corresponding in position; a pair of sliding grooves (5-1-1) corresponding in position are provided on opposite side walls of the clamping frame body (5-1), each sliding groove (5-1-1) starts from the top of one lateral side of the side wall and extends to the middle of the side wall in a direction close to the other side of the side wall and in a downwardly inclined direction, and the distance between the end faces of the two sliding card joints (6-2) is greater than the distance between the inner walls of the opposite side walls of the clamping frame body (5-1) on which the sliding grooves (5-1-1) are provided; the fixing frame body (6-1) can be movably inserted in the inner cavity of the clamping frame body (5-1), and the sliding card joints (6- 2) the movable card is connected in the slide groove (5-1-1), and the fixed frame body (6-1) moves downward along the slide groove (5-1-1) relative to the clamping frame (5) due to its own gravity. When the sliding card joint (6-2) stops moving in the slide groove (5-1-1), the distance L between the side wall of the fixed frame body (6-1) away from the starting point of the slide groove (5-1-1) and the inner wall of the clamping frame body (5-1) on the opposite side closest to the side wall is less than the thickness of the post-cast concrete sample (2); during testing, the upper part of the post-cast concrete sample (2) is clamped between the fixed frame body (6-1) and the inner wall of the clamping frame body (5-1); the bottom end of the waterproof membrane (1) extends a distance from the bottom end surface of the post-cast concrete sample (2) and is connected to the lower clamp (4) of the tensile machine.

2. The peel test fixture according to claim 1, characterized in that: The clamping device (5-2) is located directly above the contact surface between the waterproof coiled material (1) and the post-cast concrete sample block (2).

3. The peel test fixture according to claim 2, characterized in that: The length of the side wall of the fixed frame body (6-1) away from the starting point of the chute (5-1-1) is greater than or equal to the length of the post-cast concrete sample (2). During testing, the side wall of the post-cast concrete sample (2) is completely attached to the side wall of the fixed frame body (6-1).

4. The peel test fixture according to claim 1, characterized in that: The clamping device (5-2) is a clamping plate.

5. The peel test fixture according to claim 1, characterized in that: The clamping frame body (5-1), the clamping device (5-2), the fixed frame body (6-1) and the sliding card joint (6-2) are respectively a stainless steel clamping frame body, a stainless steel clamping device, a stainless steel fixed frame body and a stainless steel sliding card joint.

6. The peel test fixture according to claim 1, characterized in that: The clamping frame body (5-1) is a rectangular parallelepiped structure, with a length and a width of 60 mm and a height of 100 mm; the height of the clamping device (5-2) is 100 mm.

7. The peel test fixture according to claim 1, characterized in that: The fixed frame body (6-1) is a rectangular parallelepiped structure with a length of 60 mm, a width of 25 mm and a height of 200 mm.

8. The peel test fixture according to claim 7, characterized in that: The fixed frame body (6-1) is a hollow structure made of a stainless steel plate, and the thickness of the stainless steel plate is 5 mm.

9. A peeling test system, characterized in that: It comprises the peeling test fixture as described in any one of claims 1 to 8, and a tensile testing machine with an upper fixture (3) and a lower fixture (4), wherein the tensile testing machine can drive the upper fixture (3) and the lower fixture (4) to move up and down, the upper fixture (3) of the tensile testing machine is connected to the clamping device (5-2), the waterproof membrane (1) is placed vertically and the top is bent 180° and attached to the side wall of the middle or bottom of the post-cast concrete sample (2), and the lower fixture (4) of the tensile testing machine is connected to the bottom end of the waterproof membrane (1).