Double-sided N-Topcon back junction battery
By adopting a double-sided N-Topcon back junction structure in Topcon batteries, using local passivation contact structure and multi-layer film structure, the complexity problem of front emitter passivation and metal composite process in Topcon technology is solved, and the more Efficient passivation effect and simplified production process are suitable for mass production needs.
Patent Information
- Application Number
- CN202323610134.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-28
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2033-12-28
AI Technical Summary
Topcon technology is limited by the front emitter passivation and front metal composite process in improving efficiency. Although existing IBC batteries can improve passivation effect, the process is complex and the mass production yield is low.
Adopting a double-sided N-Topcon back-junction battery structure, the back of the silicon matrix is provided with a first tunnel oxide layer, a boron-doped polysilicon layer and a back passivation layer, and a plurality of second tunnel oxide layers and local phosphorus are provided on the front. The doped polysilicon layer and the front passivation and anti-reverse layer significantly reduce the front metal composite through the local passivation contact structure.
It effectively compensates for the carrier lateral transmission loss on the front surface of the silicon matrix, achieves excellent emitter surface passivation, simplifies the process and is suitable for mass production, and significantly reduces the metal composite on the front.
Smart Images

Figure CN221960982U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to a double-sided N-Topcon back junction battery. Background Art
[0002] In today's world, energy and environmental issues are topics of common global concern. Solar energy, as a clean, safe and convenient renewable energy source, has been widely used. Today, the efficiency of PERC cells has reached a bottleneck. Topcon technology can use some PERC production lines and has low equipment investment, making it the new battery technology with the highest production capacity. Currently, the key factors restricting the further improvement of Topcon technology are front emitter passivation and front metal recombination. IBC cells can effectively improve the passivation effect and reduce recombination, but the process is complicated and the mass production yield is low. Utility Model Content
[0003] The utility model aims to provide a double-sided N-Topcon back junction battery.
[0004] In order to achieve the above purpose, the technical solution adopted by the utility model is:
[0005] A double-sided N-Topcon back junction cell, comprising a silicon substrate, wherein the back side of the silicon substrate is provided with a first tunneling oxide layer, a boron-doped polysilicon layer, a back side passivation layer and a back metal electrode in sequence;
[0006] A plurality of second tunneling oxide layers are arranged on the front side of the silicon substrate, a gap is maintained between two adjacent second tunneling oxide layers, a local phosphorus-doped polysilicon layer is arranged on the side of the second tunneling oxide layer away from the front side of the silicon substrate, a front passivation anti-reflection layer is arranged on the side of the local phosphorus-doped polysilicon layer away from the second tunneling oxide layer and on the front side of the silicon substrate; the battery also includes a positive metal electrode, one end of the positive metal electrode is in contact with the local phosphorus-doped polysilicon layer, and the other end of the positive metal electrode extends outside the front passivation anti-reflection layer.
[0007] In some embodiments, the thickness of the local phosphorus-doped polysilicon layer is in the range of 50-150 nm.
[0008] In some embodiments, the width of the local phosphorus-doped polysilicon layer is in the range of 40-150 μm.
[0009] In some embodiments, the local phosphorus-doped polysilicon layer is made by screen printing phosphorus-containing silicon paste.
[0010] In some embodiments, the first tunnel oxide layer and the second tunnel oxide layer are made of silicon dioxide with a thickness of 1-3 nm.
[0011] In some embodiments, the boron-doped polysilicon layer has a thickness in the range of 50-300 nm.
[0012] In some embodiments, the front passivation anti-reflection layer includes a first silicon oxide layer, a silicon nitride layer, and a second silicon oxide layer that are sequentially arranged.
[0013] In some embodiments, the thickness of the first silicon oxide layer is less than the thickness of the second silicon oxide layer.
[0014] In some embodiments, the thickness of the first silicon oxide layer is in the range of 1-5 nm, the thickness of the silicon nitride layer is in the range of 40-80 nm, and the thickness of the second silicon oxide layer is in the range of 50-100 nm.
[0015] In some embodiments, the back passivation layer is silicon nitride, or the back passivation layer is a combination of a silicon nitride layer and a silicon oxynitride layer; the back passivation layer is a combination of silicon nitride and silicon oxide; or the back passivation layer is a combination of a silicon nitride layer, silicon oxide and a silicon oxynitride layer.
[0016] Due to the application of the above technical solution, the utility model has the following advantages compared with the prior art:
[0017] The double-sided N-Topcon back-junction battery provided by the utility model has a back-junction structure that can compensate for the lateral carrier transmission loss on the front surface of the silicon substrate compared to the traditional front-junction structure, and the front local passivation contact structure can achieve excellent emitter surface passivation and significantly reduce metal recombination on the front side; compared with the IBC battery, this double-sided structure has a simple process and is more suitable for mass production. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 This is a schematic diagram of the structure of a double-sided N-Topcon back-junction battery according to an embodiment of the utility model after preparation step (1);
[0019] Figure 2 This is a schematic diagram of the structure of a double-sided N-Topcon back-junction battery according to an embodiment of the utility model after preparation step (2);
[0020] Figure 3 This is a schematic diagram of the structure of a double-sided N-Topcon back-junction battery according to an embodiment of the utility model after preparation step (3);
[0021] Figure 4 This is a schematic diagram of the structure of a double-sided N-Topcon back-junction battery according to an embodiment of the utility model after preparation step (4);
[0022] Figure 5This is a schematic diagram of the structure of a double-sided N-Topcon back-junction battery according to an embodiment of the utility model after preparation step (5);
[0023] Figure 6 This is a schematic diagram of the structure of a double-sided N-Topcon back-junction battery according to an embodiment of the utility model after preparation step (6);
[0024] Figure 7 This is a schematic diagram of the structure of a double-sided N-Topcon back-junction battery according to an embodiment of the utility model after preparation step (7);
[0025] Figure 8 This is a schematic diagram of the structure of a double-sided N-Topcon back-junction battery according to an embodiment of the utility model after preparation step (8);
[0026] Fig. 9 It is a schematic structural diagram of a double-sided N-Topcon back-junction battery according to an embodiment of the utility model.
[0027] In the above figures: 1-silicon substrate; 2-first tunneling oxide layer; 3-boron-doped polysilicon layer; 4-BSG layer; 5-mask layer; 6-second tunneling oxide layer; 7-intrinsic polysilicon layer; 8-local phosphorus-doped polysilicon layer; 9-PSG layer; 10-front passivation anti-reflection layer, 101-first silicon oxide layer, 102-silicon nitride layer, 103-second silicon oxide layer; 11-back passivation layer; 12-front metal electrode; 13-back metal electrode. DETAILED DESCRIPTION
[0028] The technical solution of the utility model will be described clearly and completely below in conjunction with the accompanying drawings. Obviously, the described embodiments are part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments of the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0029] In the description of the present invention, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first", "second", and "third" are used for descriptive purposes only, and cannot be understood as indicating or implying relative importance.
[0030] Referring to the double-sided N-Topcon back junction cell shown in the figure, the back junction cell includes a silicon substrate 1, the silicon substrate 1 is an N-type silicon wafer, and the back side of the silicon substrate 1 is provided with a first tunneling oxide layer 2, a boron-doped polysilicon layer 3, a back passivation layer 11 and a back metal electrode 13 in sequence, and the first tunneling oxide layer 2 and the boron-doped polysilicon layer 3 passivation contact structure form a back junction with the N-type silicon substrate; a plurality of second tunneling oxide layers 6 are provided on the front side of the silicon substrate 1, and a gap is maintained between two adjacent second tunneling oxide layers 6, that is, the surface area of the second tunneling oxide layer 6 is smaller than the surface area of the front side of the silicon substrate, that is, the second tunneling oxide layer 6 is not completely deposited on the front side of the silicon substrate; a local phosphorus-doped polysilicon layer 13 is provided on the side of the second tunneling oxide layer 6 away from the front side of the silicon substrate A local phosphorus-doped polysilicon layer 8, a local phosphorus-doped polysilicon layer 8 and a second tunneling oxide layer 6 form a local passivation contact structure, a plurality of local phosphorus-doped polysilicon layers 8 are provided, a surface area of the local phosphorus-doped polysilicon layer 8 is smaller than a surface area of the front side of the silicon substrate, a gap is maintained between two adjacent local phosphorus-doped polysilicon layers 8, and the local phosphorus-doped polysilicon layer 8 is not in contact with the front side of the silicon substrate; a front passivation anti-reflection layer 10 is provided on the side of the local phosphorus-doped polysilicon layer 8 away from the second tunneling oxide layer 6 and the front side of the silicon substrate (the side where the second tunneling oxide layer 6 is not deposited); the battery also includes a positive metal electrode 12, one end of the positive metal electrode 12 is in contact with the local phosphorus-doped polysilicon layer 8, and the other end of the positive metal electrode 12 extends to the outside of the front passivation anti-reflection layer 10.
[0031] The local phosphorus-doped polysilicon layer 8 of this example is made by screen printing phosphorus-containing silicon paste. In some embodiments, the width of a single local phosphorus-doped polysilicon layer 8 is in the range of 40-150 μm, and the thickness of the local phosphorus-doped polysilicon layer 8 is in the range of 50-150 nm.
[0032] In this embodiment, the first tunnel oxide layer 2 and the second tunnel oxide layer 6 are made of silicon dioxide, and both have a thickness ranging from 1 to 3 nm. The thickness of the boron-doped polysilicon layer 3 ranges from 50 to 300 nm.
[0033] The front passivation anti-reflection layer 10 comprises a first silicon oxide layer 101, a silicon nitride layer 102 and a second silicon oxide layer 103 which are sequentially arranged. The thickness of the first silicon oxide layer 101 is less than the thickness of the second silicon oxide layer 103. The thickness of the first silicon oxide layer 101 is in the range of 1-5 nm, the thickness of the silicon nitride layer 102 is in the range of 40-80 nm, and the thickness of the second silicon oxide layer 103 is in the range of 50-100 nm.
[0034] The back passivation layer 11 is silicon nitride, or the back passivation layer 11 is a combination of a silicon nitride layer and a silicon oxynitride layer; the back passivation layer 11 is a combination of silicon nitride and silicon oxide; or the back passivation layer 11 is a combination of a silicon nitride layer, silicon oxide and silicon oxynitride layer. The thickness of the back passivation layer 11 is 50-150nm.
[0035] In one embodiment, the thickness of the first tunneling oxide layer 2 is 1.6 nm, and the thickness of the boron-doped polysilicon layer 3 is 110 nm; the local phosphorus-doped polysilicon layer 8 is arranged in parallel in several strips, with a width of 100 μm and a thickness of 90 nm; the front passivation anti-reflection layer includes a first silicon oxide layer, a silicon nitride layer, and a second silicon oxide layer arranged in sequence, the thickness of the first silicon oxide is 3 nm, the thickness of the silicon nitride is 50 nm, and the thickness of the second oxide layer is 70 nm; the back passivation layer 11 adopts a silicon nitride passivation layer with a thickness of 80 nm.
[0036] The preparation method of the double-sided N-Topcon back junction cell in this example is as follows:
[0037] Step 1: Cleaning and double-sided polishing of the N-type silicon wafer 1.
[0038] Step 2: Grow a first tunnel oxide layer 2 on one side of the silicon wafer, and deposit a boron-doped polysilicon layer 3 and a mask layer 5, which is the back side of the silicon wafer.
[0039] The growth method of the first tunnel oxide layer 2 includes but is not limited to high temperature thermal oxidation, atomic layer deposition, ozone oxidation, thermal HNO3 oxidation, etc. The deposition method of the boron-doped polysilicon layer 3 is any one of LPCVD, PECVD or PVD, and the doping methods include diffusion, ion implantation, spin coating, etc. The material of the mask layer 5 can be any one of silicon dioxide, silicon nitride or silicon oxynitride. While depositing the mask layer 5, the boron-doped polysilicon layer 3 is annealed. In this example, PECVD is used to grow the first tunnel oxide layer 2, and the boron-doped polysilicon layer 3 and the mask layer 5 are deposited. The thickness of the first tunnel oxide layer 2 is 1.6nm, the thickness of the boron-doped polysilicon layer 3 is 110nm, and the material of the mask layer 5 is silicon nitride with a thickness of 70nm.
[0040] Step 3: Cleaning: first use chain HF to remove the mask layer 5 and BSG layer 4 plated on the edge and front side, then use alkaline solution to remove the boron-doped polysilicon layer 3 plated on the edge and front side; finally, texturing the front side of the silicon wafer.
[0041] Step 4: grow a second tunnel oxide layer 6 on the front side of the silicon wafer, and deposit an intrinsic polysilicon layer 7. The growth method of the second tunnel oxide layer 6 includes, but is not limited to, high-temperature thermal oxidation, atomic layer deposition, ozone oxidation, thermal HNO3 oxidation, etc. In this example, LPCVD is used to grow the second tunnel oxide layer 6. The intrinsic polysilicon layer 7 is an undoped polysilicon layer, and the deposition method is LPCVD.
[0042] Step 5: Locally doping the intrinsic polysilicon layer 7, the doping method is diffusion after the mask layer or screen printing of phosphorus-containing silicon paste, and then annealing to form a local phosphorus-doped polysilicon layer 8. In this example, screen printing of phosphorus-containing silicon paste is used, and the local phosphorus-doped polysilicon layer 8 is arranged in parallel in a plurality of strips, with a width of 100 μm and a thickness of 90 nm, forming a local passivation contact structure with the second tunneling oxide layer 6.
[0043] Step 6: Cleaning. Alkaline solution is first used to remove the intrinsic amorphous silicon layer 7 plated around the front non-metallic contact area, the edge and the back, and part of the second tunneling oxide layer 6 is cleaned and removed. The front metal contact area (the second tunneling oxide layer 6 and the local phosphorus-doped polysilicon layer 8) is protected by the PSG layer 9 and is not corroded. Then HF solution is used to remove the PSG layer 9, the back mask layer 5 and the back BSG layer 4 of the front metal contact area.
[0044] Step 7: depositing a front passivation anti-reflection layer 10 on the front side of the silicon substrate, the material of which is a first silicon oxide 101, a silicon nitride 102 and a second silicon oxide layer 103. In this example, the thickness of the first silicon oxide 101 is 3 nm, the thickness of the silicon nitride 102 is 50 nm, and the thickness of the second oxide layer 103 is 70 nm.
[0045] Step 8: Deposit a back passivation layer 11. In this example, a silicon nitride passivation layer is used with a thickness of 80 nm.
[0046] Step 9: Prepare the front metal electrode 12 and the back metal electrode 13 on the front and back sides respectively. The metallization method can be screen printing, laser transfer or inkjet method. In this example, screen printing is used.
[0047] The above embodiments are only for illustrating the technical concept and features of the utility model, and their purpose is to enable people familiar with the technology to understand the content of the utility model and implement it accordingly, and they cannot be used to limit the protection scope of the utility model. Any equivalent changes or modifications made according to the spirit of the utility model should be included in the protection scope of the utility model.
Claims
1. A double-sided N-Topcon back junction battery, characterized in that: The invention comprises a silicon substrate, wherein a first tunneling oxide layer, a boron-doped polysilicon layer, a back passivation layer and a back metal electrode are sequentially arranged on the back side of the silicon substrate; a plurality of second tunneling oxide layers are arranged on the front side of the silicon substrate, a local phosphorus-doped polysilicon layer is arranged on the side of the second tunneling oxide layer away from the front side of the silicon substrate, a front passivation anti-reflection layer is arranged on the side of the local phosphorus-doped polysilicon layer away from the second tunneling oxide layer and on the front side of the silicon substrate; the battery further comprises a positive metal electrode, wherein one end of the positive metal electrode is in contact with the local phosphorus-doped polysilicon layer, and the other end of the positive metal electrode extends outside the front passivation anti-reflection layer.
2. The double-sided N-Topcon back-junction battery according to claim 1, characterized in that: The thickness of the local phosphorus-doped polysilicon layer is in the range of 50-150 nm.
3. The double-sided N-Topcon back-junction battery according to claim 1, characterized in that: The width of the local phosphorus-doped polysilicon layer is in the range of 40-150 μm.
4. The double-sided N-Topcon back-junction cell according to claim 1, characterized in that: The local phosphorus-doped polysilicon layer is made by screen printing phosphorus-containing silicon paste.
5. The double-sided N-Topcon back-junction cell according to claim 1, characterized in that: The first tunneling oxide layer and the second tunneling oxide layer are made of silicon dioxide and have a thickness of 1-3 nm.
6. The double-sided N-Topcon back-junction cell according to claim 1, characterized in that: The thickness of the boron-doped polysilicon layer is in the range of 50-300 nm.
7. The double-sided N-Topcon back-junction battery according to claim 1, characterized in that: The front passivation anti-reflection layer comprises a first silicon oxide layer, a silicon nitride layer and a second silicon oxide layer which are arranged in sequence.
8. The double-sided N-Topcon back-junction cell according to claim 7, characterized in that: The thickness of the first silicon oxide layer is smaller than the thickness of the second silicon oxide layer.
9. The double-sided N-Topcon back-junction cell according to claim 8, characterized in that: The thickness of the first silicon oxide layer is in the range of 1-5 nm; the thickness of the silicon nitride layer is in the range of 40-80 nm; and the thickness of the second silicon oxide layer is in the range of 50-100 nm.
10. The double-sided N-Topcon back-junction battery according to claim 9, characterized in that: The back passivation layer is silicon nitride, or the back passivation layer is a combination of a silicon nitride layer and a silicon oxynitride layer; the back passivation layer is a combination of silicon nitride and silicon oxide; or the back passivation layer is a combination of a silicon nitride layer, silicon oxide and a silicon oxynitride layer.
Citation Information
Cited By
Preparation method of double-sided Topcon back junction battery and battery
CN117855330A
Solar cell and preparation method thereof
CN119342934A