Pot cover assembly and cooking utensil
By setting thickened sections and thinned sections in the injection molding area of the pot cover assembly, the plastic flow direction is controlled and the support ribs are added, the problem of flow marks during the injection molding of the cooking utensils is solved, and the production quality and appearance quality are improved.
Patent Information
- Application Number
- CN202323336033.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-06
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2033-12-06
AI Technical Summary
During the injection molding process, the side of the cooking utensil is prone to traces due to uneven plastic flow during the injection molding process, which affects the appearance of the product and production quality.
A pot lid assembly is designed. By setting thickened sections and thinned sections in the injection molding area, the plastic flow direction is controlled, so that the plastic flows along the thickened section to the side wall, and the structural strength is increased through the support ribs and the flow marks are reduced. Hidden danger.
It effectively reduces flow marks caused by different plastic flow rates, improves the production quality and appearance quality of the cover, and reduces production costs.
Smart Images

Figure CN221963422U_ABST
Abstract
Description
Technical Field
[0001] The present application belongs to the technical field of kitchen appliances, and specifically relates to a pot cover assembly and a cooking utensil. Background Art
[0002] The appearance parts of cooking utensils are usually treated by spraying the injection molded parts to improve the appearance quality of the appearance parts and meet the diverse needs of users. However, the spraying process is relatively complicated and has strict requirements on the construction environment, which leads to high costs and environmental pollution. Therefore, more and more appearance parts are made of spray-free materials.
[0003] Taking the cover of a cooking utensil as an example, the cover has a glue injection plane with a glue inlet. When the cover is produced, molten plastic is injected from the glue inlet, and then the plastic is divided into multiple strands along the glue injection plane and moves toward the four sides of the cover, and converges at the side of the cover to form.
[0004] Since the flow rate and direction of the plastic flowing from different positions to the side of the face cover are different, and they will intersect at multiple locations on the side of the face cover, it is easy for multiple marks to be formed on the side of the face cover, making it extremely easy for injection molding marks to appear on the appearance of the face cover, thereby affecting the production quality of the product. Utility Model Content
[0005] The present application provides a pot cover assembly and a cooking utensil to control the flow direction of molten plastic and improve the production quality of the cover.
[0006] The technical solution adopted in this application is:
[0007] A pot cover assembly comprises a cover, wherein the cover comprises a top wall and a side wall surrounding the outer periphery of the top wall and extending downward, the top wall having an injection molding area, a convex rib surrounding the injection molding area between the injection molding area and the side wall, an injection molding port being arranged in the injection molding area, the convex rib having a thinning section and a thickening section with a cross-sectional area larger than the thinning section along its circumference, so that plastic in the injection molding area flows to the side wall via the thickening section.
[0008] The pot cover assembly described in this application also includes the following additional technical features:
[0009] The face cover has a front end and a rear end which are arranged opposite to each other, and a central axis which passes through the front end, the rear end and the center of the face cover, and the injection port is located on the central axis and is arranged close to the front end.
[0010] The thickened section is arranged corresponding to the front end and is located outside the injection port.
[0011] The thinning section comprises a thin-walled area arranged corresponding to the rear end and thick-walled areas located on both sides of the thin-walled area, and the cross-sectional area of the thin-walled area is smaller than the cross-sectional area of the thick-walled area;
[0012] And / or, the thinning section is provided with a blocking groove corresponding to the rear end.
[0013] The width of the thinned section is smaller than the width of the thickened section;
[0014] And / or, the height of the thinned section is smaller than the height of the thickened section, so that the cross-sectional area of the thinned section is smaller than the cross-sectional area of the thickened section.
[0015] A supporting rib is arranged on the inner side of the side wall. The supporting rib has an outer end connected to the side wall and an inner end opposite to the outer end. There is a gap between the inner end and the convex rib.
[0016] The width of the outer end is smaller than the width of the inner end.
[0017] A plurality of blocking ribs are arranged at intervals between the injection port and the thinning section.
[0018] A connecting rib is arranged between the side wall and the top wall, and the connecting rib has a thickening section arranged corresponding to the thickening section and a thinning section arranged corresponding to the thinning section, and the thickness of the thickening section is greater than the thickness of the thinning section.
[0019] The present application also discloses a cooking utensil, comprising a pot body and the pot cover assembly, wherein one end of the pot cover assembly is hinged to the pot body so that the pot cover assembly can rotate to open and close the pot body;
[0020] Alternatively, the pot cover assembly is removably placed on the pot body.
[0021] Due to the adoption of the above technical solution, the beneficial effects achieved by this application are as follows:
[0022] 1. The pot cover assembly in the present application includes a face cover, which includes a top wall and a side wall surrounding the outer periphery of the top wall and extending downward, the top wall having an injection molding area, a convex rib surrounding the injection molding area between the injection molding area and the side wall, an injection molding port being arranged in the injection molding area, the convex rib having a thinning section and a thickening section whose cross-sectional area is larger than that of the thinning section along its circumference, so that the plastic in the injection molding area flows to the side wall via the thickening section. It can be understood that when the face cover is produced, the molten plastic is injected from the injection molding port, and then the plastic flows along the top wall. Since the cross-sectional area of the thinning section is smaller than that of the thickening section, the cross-sectional area of the flow channel at the location of the thickening section is larger than that of the flow channel at the location of the thinning section, thereby making The resistance of the plastic flowing toward the thickened section is smaller than the resistance of the plastic flowing toward the thinned section, so that the flow speed of the plastic toward the thickened section is greater than the flow speed of the plastic toward the thinned section, thereby making the plastic in the injection molding area flow to the side wall via the thickened section, and the plastic flowing to the side wall is divided into two streams that flow circumferentially along the top wall and finally meet at the end of the side wall away from the thickened section, so that the plastic flowing through the thickened section reaches the side wall first, that is, the plastic flowing to the side wall all flows out from the thickened section, and since the initial speed and flow stroke of the two streams of plastic are the same, the flow speed of the two streams of plastic at the intersection is the same, thereby reducing the risk of flow marks caused by different flow speeds of plastic, thereby improving the production quality of the cover.
[0023] 2. As a preferred embodiment of the present application, the face cover has a front end and a rear end that are relatively arranged, and a central axis passing through the front end, the rear end and the center of the face cover. The injection port is located on the central axis and is arranged close to the front end, thereby making the distance between the injection port and the front end closer, so that the plastic first flows to the front end through the thickened section, thereby making the plastic avoid the front end at the intersection of the side wall. When the user uses the cooking utensil equipped with the face cover, the front end of the face cover is generally facing one end of the user, so that the user can most easily see the front end of the face cover, so that the intersection of the plastic is in the user's blind spot, thereby improving the user experience; at the same time, the injection port is located on the central axis to further ensure that the flow rate of the plastic at the intersection of the side walls is consistent, thereby further reducing the risk of flow marks on the side walls.
[0024] 3. As a preferred embodiment of the present application, the thickened section is arranged at the front end corresponding to the front end and is located outside the injection port, so that the distance between the injection port and the thickened section is closer, further accelerating the flow rate of the plastic toward the thickened section, thereby accelerating the flow rate of the plastic flowing toward the side wall through the thickened section, and then making the plastic flowing through the thickened section first reach the side wall located at the rear end of the face cover, so as to further ensure that the plastic on the side wall flows out through the thickened section, further reducing the hidden danger of flow marks on the side wall; at the same time, the injection port is located on the central axis, so as to further ensure that the flow stroke of the plastic divided into two streams through the thickened section is the same, thereby further reducing the hidden danger of flow marks on the face cover, so as to further improve the appearance quality of the face cover. In addition, for the user, when the user uses the cooking utensil equipped with the face cover, the rear end of the face cover is generally the end away from the user, so that the intersection of the plastic is in the user's blind spot, thereby improving the user's experience.
[0025] 4. As a preferred embodiment of the present application, a support rib is provided on the inner side of the side wall, and the support rib has an outer end connected to the side wall and an inner end opposite to the outer end, and there is a gap between the inner end and the convex rib, so that the support member supports the side wall to increase the structural strength of the side wall, and the support rib can also strengthen the top wall to increase the structural strength of the top wall, thereby increasing the service life of the cover; in addition, there is a gap between the inner end of the support rib and the convex rib, thereby increasing the resistance of the plastic flowing toward the outer side of the top wall through the thinning section, further reducing the flow rate of the plastic flowing toward the outer side of the top wall through the thinning section, further ensuring that the plastic flowing through the thickening section reaches the side wall earlier, further ensuring that when the cover is produced, the plastic first fills the side wall and then fills other positions, further reducing the hidden dangers of flow marks such as air marks and bonding lines on the side wall, and further improving the appearance quality of the cover. In addition, there is a gap between the inner end of the support rib and the convex rib, which can also reduce the amount of plastic required for the production of the cover, thereby reducing the production cost of the cover.
[0026] 5. As a preferred embodiment of the present application, the width of the outer end is smaller than the width of the inner end, so as to further increase the resistance of the plastic flowing toward the outside of the top wall through the thinning section, and then further reduce the flow rate of the plastic flowing toward the outside of the top wall through the thinning section, and further ensure that the plastic through the thickening section reaches the side wall earlier, so that the plastic reaching the side wall through the thickening section first fills the side wall, further reducing the hidden danger of flow marks such as air marks and bonding lines on the side wall, thereby further improving the appearance quality of the cover. At the same time, the resistance of the plastic flowing to the side wall through the thickening section to flow toward the inside of the top wall is increased, so as to further ensure that the plastic flowing to the side wall through the thickening section first flows along the circumference of the top wall, and then ensure the flow rate of the plastic flowing to the side wall through the thickening section and flowing along the circumference of the top wall, further reducing the hidden danger of flow marks on the side wall. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] The drawings described herein are used to provide a further understanding of the present application and constitute a part of the present application. The illustrative embodiments of the present application and their descriptions are used to explain the present application and do not constitute an improper limitation on the present application. In the drawings:
[0028] Figure 1 This is a schematic diagram of the structure of the face cover in one embodiment of the present application, in which the double-headed arrow indicates the central axis;
[0029] Figure 2 for Figure 1 A magnified view of the middle A area;
[0030] Figure 3 This is a schematic diagram of the structure of the cover in one embodiment of the present application, in which the arrow indicates the flow direction of the plastic through the thickened section;
[0031] Figure 4 A partial structural schematic diagram of the cover described in one embodiment of the application;
[0032] Figure 5 A cross-sectional view of the face cover in one embodiment of the present application;
[0033] Figure 6 for Figure 5 Magnified view of area B.
[0034] Reference numerals:
[0035] 1. Surface cover; 11. Top wall; 111. Injection molding area; 112. Injection molding port; 113. Convex rib; 114. Thinning section; 115. Thickening section; 116. Extension section; 12. Side wall; 121. Support rib; 122. First section; 123. Second section;
[0036] 2. Block the convex ribs;
[0037] 3. Leave blank area;
[0038] 4. Connect the ribs;
[0039] 5. Exhaust pipe. DETAILED DESCRIPTION
[0040] In order to more clearly illustrate the overall concept of the present application, a detailed description is given below in an illustrative manner in conjunction with the accompanying drawings.
[0041] In the following description, many specific details are set forth to facilitate a full understanding of the present application. However, the present application may also be implemented in other ways different from those described herein. Therefore, the scope of protection of the present application is not limited to the specific embodiments disclosed below.
[0042] In addition, in the description of the present application, it should be understood that the orientations or positional relationships indicated by the terms "top", "bottom", "inside", "outside", "axial", "radial", "circumferential", etc. are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.
[0043] In this application, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection, an electrical connection, or a communication; it can be a direct connection, or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.
[0044] In the present application, unless otherwise clearly specified and limited, the first feature "above" or "below" the second feature may be that the first and second features are in direct contact, or the first and second features are in indirect contact through an intermediate medium. In the description of this specification, the description with reference to the terms "implementation method", "example", "one embodiment", "example" or "specific example" means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present application. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in an appropriate manner in any one or more embodiments or examples.
[0045] Reference Figures 1 to 6 A pot cover assembly includes a cover 1, the cover 1 includes a top wall 11 and a side wall 12 surrounding the outer periphery of the top wall 11 and extending downward, the top wall 11 has an injection molding area 111, a convex rib 113 surrounding the injection molding area 111 is provided between the injection molding area 111 and the side wall 12, an injection molding port 112 is provided in the injection molding area 111, and the convex rib 113 has a thinning section 114 and a thickening section 115 with a cross-sectional area larger than the thinning section 114 along its circumference, so that the plastic in the injection molding area 111 flows to the side wall 12 via the thickening section 115.
[0046] When the face cover 1 is produced, the molten plastic is injected from the injection port 112, and then the plastic flows along the top wall 11. Since the cross-sectional area of the thinning section 114 is smaller than the cross-sectional area of the thickening section 115, the cross-sectional area of the flow channel at the location of the thickening section 115 is larger than the cross-sectional area of the flow channel at the location of the thinning section 114, so that the resistance of the plastic flowing toward the thickening section 115 is smaller than the resistance of the plastic flowing toward the thinning section 114, so that the flow speed of the plastic toward the thickening section 115 is greater than the flow speed of the plastic toward the thinning section 114, thereby making the injection area 111 The plastic flows to the side wall 12 through the thickened section 115, so that the plastic flowing through the thickened section 115 reaches the side wall 12 first, that is, the plastic flowing to the side wall 12 all flows out from the thickened section 115, and the plastic flowing to the side wall 12 is divided into two streams that flow along the circumferential direction of the top wall 11 and finally meet at one end of the side wall 12 away from the thickened section 115. Since the initial speed and flow stroke of the two streams of plastic are the same, the flow speed of the two streams of plastic at the intersection is the same, thereby reducing the hidden danger of flow marks caused by different flow speeds of the plastic, thereby improving the production quality of the cover 1.
[0047] In a preferred embodiment, referring to Figure 1 and Figure 3 The cover 1 has a front end and a rear end that are relatively arranged, and a central axis that passes through the front end, the rear end and the center of the cover 1. The injection port 112 is located on the central axis and is arranged close to the front end, so that the plastic first flows to the front end through the thickened section 115, so that the plastic avoids the front end at the intersection of the side wall 12. When the user uses the cooking utensil installed with the cover 1, the front end of the cover 1 is generally facing the end of the user, so that the user can see the front end of the cover 1 most easily, so that the intersection of the plastic is in the user's blind spot, thereby improving the user's experience. At the same time, the injection port 112 is located on the central axis to further ensure that the flow rate of the plastic at the intersection of the side wall 12 is consistent, thereby further reducing the hidden danger of flow marks on the side wall 12.
[0048] The present application does not specifically limit the position of the thickened section 115. Preferably, refer to Figure 1 and Figure 3 The thickened section 115 is arranged corresponding to the front end and is located outside the injection port 112 .
[0049] Specifically, the thickened section 115 is symmetrically arranged about the central axis so that the plastic flowing to the side wall 12 through the thickened section 115 is more evenly divided into two streams and moves along the circumference of the top wall 11 to ensure that the flow rate of the plastic divided into two streams through the thickened section 115 remains consistent. The thickened section 115 is arranged at the front end and is located outside the injection port 112, so that the distance between the injection port 112 and the thickened section 115 is closer, further accelerating the flow rate of the plastic toward the thickened section 115, thereby accelerating the flow rate of the plastic flowing toward the side wall 12 through the thickened section 115, and then making the plastic flowing through the thickened section 115 reach the side wall 12 located at the rear end of the face cover 1 first, so as to further ensure that the plastic of the side wall 12 flows out through the thickened section 115, and further reduce the hidden danger of flow marks on the side wall 12; at the same time, the injection port 112 is located at the central axis, so as to further ensure that the flow stroke of the plastic divided into two strands through the thickened section 115 is the same, and further reduce the hidden danger of flow marks on the face cover 1, so as to further improve the production quality of the face cover 1. In addition, for the user, when the user uses the cooking utensil equipped with the face cover 1, the rear end of the face cover 1 is generally the end away from the user, so that the intersection of the plastic is in the user's blind spot, thereby improving the user's use experience.
[0050] In other embodiments, the thickened section 115 may also be located at one side of the front end.
[0051] The present application does not specifically limit the structure of the thinning section 114, and it may adopt any one of the following embodiments:
[0052] Embodiment 1. In this embodiment, the thinning section 114 has a thin-walled area corresponding to the rear end and thick-walled areas on both sides of the thin-walled area. The cross-sectional area of the thin-walled area is smaller than the cross-sectional area of the thick-walled area, thereby making the resistance of the plastic flowing toward the thin-walled area greater than the resistance of the plastic flowing toward the thick-walled area, so as to reduce the flow velocity of the plastic flowing toward the thin-walled area, thereby reducing the flow velocity of the plastic toward the rear end of the face cover 1, further ensuring that the plastic flowing toward the side wall 12 through the thickening section 115 first reaches the side wall 12 at the rear end, further reducing the hidden danger of flow marks on the side wall 12; at the same time, the amount of plastic used in the production of the face cover 1 is reduced, thereby reducing the production cost of the face cover 1.
[0053] The present application does not specifically limit the formation method of the cross-sectional area of the thin-walled area being smaller than the cross-sectional area of the thick-walled area. Preferably, the height of the thin-walled area is the same as that of the thick-walled area, and the thickness of the thin-walled area is smaller than that of the thick-walled area, so that the cross-sectional area of the thin-walled area is smaller than that of the thick-walled area, so as to reduce the flow rate of the plastic toward the thin-walled area, and further reduce the hidden danger of flow marks on the side wall 12. In other implementation examples, the thickness of the thin-walled area can be consistent with the thickness of the thick-walled area, and the height of the thin-walled area can be smaller than that of the thick-walled area; or the thickness of the thin-walled area can be smaller than that of the thick-walled area, and the height of the thin-walled area can be smaller than that of the thick-walled area.
[0054] Embodiment 2. In this embodiment, a blocking groove is provided at the rear end corresponding to the thinning section 114. Since the face cover 1 is provided with a blocking groove, it is necessary to provide a corresponding molding rib inside the mold. Then, when the plastic flows toward the rear end, the molding rib on the mold will block the plastic. At the same time, the existence of the molding rib reduces the flow area of the plastic when it flows toward the rear end, so as to further increase the resistance of the plastic to flow toward the rear end, thereby reducing the flow rate of the plastic toward the rear end, further ensuring that the plastic flowing toward the side wall 12 through the thickened section 115 first reaches the side wall 12 at the rear end, further reducing the hidden danger of flow marks on the side wall 12 due to different flow rates of the plastic.
[0055] The present application does not make any specific limitation on the structure of the blocking groove, which may be a multi-segment strip structure arranged at intervals in a direction perpendicular to the central axis, or a strip structure arranged continuously in a direction perpendicular to the central axis, as long as it can increase the resistance of the plastic flowing toward the rear end.
[0056] Embodiment 3, this embodiment is preferred, the thinning section 114 has a thin-walled area set at the corresponding rear end and thick-walled areas on both sides of the thin-walled area, the cross-sectional area of the thin-walled area is smaller than the cross-sectional area of the thick-walled area, and the thinning section 114 is provided with a blocking groove at the corresponding rear end to further increase the flow resistance of the plastic toward the rear end, and then further reduce the flow velocity of the plastic toward the thin-walled area, thereby reducing the flow velocity of the plastic toward the face cover 1 via the thinning section 114 toward the rear end of the face cover 1, further ensuring that the plastic flowing toward the side wall 12 via the thickening section 115 first reaches the side wall 12 at the rear end, thereby further reducing the hidden danger of flow marks on the side wall 12 due to different flow velocities of the plastic.
[0057] The present application does not specifically limit the formation method of the cross-sectional area of the thickened section 115 being larger than the cross-sectional area of the thinned section 114, and any one of the following embodiments may be adopted:
[0058] Embodiment 1. In this embodiment, referring to Figure 1 , Figure 3 and Figure 4 The width of the thinning section 114 is smaller than the width of the thickening section 115, and the height of the thinning section 114 is the same as the height of the thickening section 115, so that the cross-sectional area of the thinning section 114 is smaller than the cross-sectional area of the thickening section 115, and then the flow resistance of the plastic toward the thinning section 114 is greater than the flow resistance of the plastic toward the thickening section 115, so that the flow rate of the plastic toward the thickening section 115 is greater than the flow rate toward the thinning section 114, so as to ensure that the plastic flowing to the side wall 12 passes through the thickening section 115, so as to reduce the hidden danger of flow marks on the side wall 12 and improve the appearance quality of the cover 1.
[0059] Embodiment 2. In this embodiment, the height of the thinning section 114 is less than the height of the thickening section 115, and the width of the thinning section 114 is the same as the width of the thickening section 115, so that the cross-sectional area of the thinning section 114 is smaller than the cross-sectional area of the thickening section 115, thereby making the flow resistance of the plastic toward the thinning section 114 greater than the flow resistance of the plastic toward the thickening section 115, so that the flow rate of the plastic toward the thickening section 115 is greater than the flow rate toward the thinning section 114, so as to ensure that the plastic flowing to the side wall 12 passes through the thickening section 115, so as to reduce the hidden danger of flow marks on the side wall 12 and improve the appearance quality of the cover 1.
[0060] Embodiment three. In this embodiment, the width of the thinning section 114 is smaller than the width of the thickening section 115, and the height of the thinning section 114 is smaller than the height of the thickening section 115, so that the cross-sectional area of the thinning section 114 is smaller than the cross-sectional area of the thickening section 115, so as to further increase the resistance difference between the plastic flowing toward the thinning section 114 and the thickening section 115, thereby further increasing the flow velocity difference between the plastic flowing toward the thinning section 114 and the thickening section 115, further ensuring that the plastic passing through the thickening section 115 first fills the side wall 12, thereby further reducing the risk of flow marks on the side wall 12 due to different flow velocities.
[0061] In a preferred embodiment, referring to Figure 1 , Figure 2 , Figure 3 , Figure 4 and Figure 6 A supporting rib 121 is provided on the inner side of the side wall 12 . The supporting rib 121 has an outer end connected to the side wall 12 and an inner end opposite to the outer end. There is a gap between the inner end and the convex rib 113 .
[0062] Specifically, the support rib 121 is connected to the top wall 11 so that the support member supports the side wall 12 to increase the structural strength of the side wall 12. At the same time, the support rib 121 can also strengthen the top wall 11 to increase the structural strength of the top wall 11, thereby increasing the service life of the cover 1. In addition, there is a gap between the inner end of the support rib 121 and the convex rib 113, thereby increasing the resistance of the plastic to flow toward the outside of the top wall 11 through the thinning section 114, further reducing the flow rate of the plastic flowing toward the outside of the top wall 11 through the thinning section 114, further ensuring that the plastic flowing through the thickening section 115 reaches the side wall 12 first, further ensuring that when the cover 1 is produced, the plastic first fills the side wall 12 and then fills other positions, further reducing the hidden dangers of flow marks such as air marks and bonding lines on the side wall 12, thereby further improving the appearance quality of the cover 1. Furthermore, there is a gap between the inner end of the supporting rib 121 and the convex rib 113 , which can also reduce the amount of plastic required for producing the face cover 1 , thereby reducing the production cost of the face cover 1 .
[0063] The present application does not specifically limit the structure of the support rib 121. Preferably, refer to Figure 2 and Figure 6 , the width of the outer end is smaller than the width of the inner end, so as to further increase the resistance of the plastic flowing toward the outside of the top wall 11 through the thinning section 114, and then further reduce the flow rate of the plastic flowing toward the outside of the top wall 11 through the thinning section 114, and further ensure that the plastic passing through the thickening section 115 reaches the side wall 12 earlier, so that the plastic reaching the side wall 12 through the thickening section 115 first fills the side wall 12, further reducing the hidden danger of flow marks such as air marks and bonding lines on the side wall 12, thereby further improving the appearance quality of the cover 1. At the same time, the resistance of the plastic flowing to the side wall 12 through the thickening section 115 to flow toward the inside of the top wall 11 is increased, so as to further ensure that the plastic flowing to the side wall 12 through the thickening section 115 first flows along the circumference of the top wall 11, and then ensure the flow rate of the plastic flowing to the side wall 12 through the thickening section 115 and flowing along the circumference of the top wall 11, and further reduce the hidden danger of flow marks on the side wall 12. In other embodiments, the high end of the outer end may be smaller than the height of the inner end.
[0064] The present application does not specifically limit the formation method of the width of the outer end being smaller than the width of the inner end. Preferably, refer to Figure 2 and Figure 6 The support rib 121 is divided into a first section 122 and a second section 123 connected to the first section 122 along the direction close to the convex rib 113, the inner end is located at the end of the second section 123 away from the first section 122, the outer end is located at the end of the first section 122 away from the second section 123, and the width of the first section 122 is smaller than the width of the second section 123, so that the width of the outer end is smaller than the width of the inner end. In other embodiments, the width of the support rib 121 gradually increases along the direction close to the convex rib 113.
[0065] In a preferred embodiment, referring to Figure 1 and Figure 3 A plurality of barrier ribs 2 are arranged between the injection port 112 and the thinning section 114 so that the amount of plastic required between the injection port 112 and the thinning section 114 is larger, and then the plastic flowing toward the thinning section 114 fills the barrier ribs 2 and then continues to flow toward the periphery of the top wall 11, thereby reducing the flow rate of the plastic flowing toward the periphery of the top wall 11 through the thinning section 114, and further reducing the hidden danger of marks being formed on the side wall 12.
[0066] Preferably, a gap area 3 is provided between the injection port 112 and the thickened section 115. It is understandable that the gap area 3 is a blank area, i.e., no other structure is provided in this area, so as to greatly reduce the amount of plastic required between the injection port 112 and the thickened section 115, thereby increasing the speed at which the plastic flows toward the side wall 12 through the thickened section 115, thereby ensuring that the plastic passing through the thickened section 115 reaches the side wall 12 first, so as to further reduce the hidden danger of marks being formed on the side wall 12.
[0067] In a preferred embodiment, referring to Figure 1 , Figure 3 and Figure 5 An exhaust pipe 5 is provided between the injection port 112 and the thinning section 114 to further increase the amount of plastic required between the injection port 112 and the thinning section 114, so that the plastic flowing toward the thinning section 114 fills the exhaust pipe 5 and then continues to flow toward the peripheral side of the top wall 11, thereby reducing the flow rate of the plastic flowing toward the peripheral side of the top wall 11 through the thin-wall section 114, thereby further reducing the hidden danger of marks being formed on the side wall 12.
[0068] In a preferred embodiment, referring to Figure 5 and Figure 6 A connecting rib 4 is provided between the side wall 12 and the top wall 11. The connecting rib 4 has a thickening section provided corresponding to the thickening section 115 and a thinning section provided corresponding to the thinning section 114. The thickness of the thickening section is greater than the thickness of the thinning section, so as to further increase the resistance difference between the plastic flowing toward the thickening section 115 and the plastic flowing toward the thinning section 114, thereby further increasing the flow velocity difference between the plastic flowing toward the thickening section 115 and the plastic flowing toward the thinning section 114, further ensuring that the plastic passing through the thickening section 115 reaches the side wall 12 first, thereby further reducing the hidden danger of flow marks on the side wall 12.
[0069] Preferably, the thickness of the reduced thickness section is smaller than the thickness of the side wall 12 to increase the resistance of the plastic flowing to the side wall 12 to flow toward the top wall 11, to ensure that the plastic flowing to the side wall 12 continues to flow along the circumference of the top wall 11, to further ensure that the plastic passing through the thickened section 115 reaches the intersection of the plastics first, thereby further reducing the risk of flow marks on the side wall 12.
[0070] In a preferred embodiment, referring to Figure 5 and Figure 6An extension portion 116 extending downward is provided on the circumferential side of the top wall 11, the extension portion 116 is spaced apart from the side wall 12 and is located on the inner side of the side wall 12, the connecting rib position 4 is located at the bottom of the side wall 12 and the extension portion 116, and the inner side of the connecting rib position 4 is connected to the extension portion 116, and the outer side of the connecting rib position 4 is connected to the extension portion 116, and at the same time, the supporting rib 121 extends downward to between the extension portion 116 and the side wall 12 to increase the structural strength of the side wall 12, thereby increasing the structural strength of the cover body, so as to increase the service life of the cover body.
[0071] The present application also discloses a cooking utensil, comprising a pot body and the pot cover assembly, wherein the pot cover assembly is arranged on the top of the pot body so that the pot cover assembly and the pot body together form a sealed cooking cavity.
[0072] The present application does not specifically limit the connection method between the pot cover assembly and the pot body, and it can adopt any one of the following embodiments:
[0073] Embodiment 1: In this embodiment, one end of the pot cover assembly is hinged to the pot body so that the pot cover assembly can rotate to open and close the pot body, thereby improving the user experience.
[0074] Embodiment 2. In this embodiment, the pot cover assembly is removably placed on the pot body, that is, when the cooking cavity is opened, the pot cover assembly is separated from the pot body, and when the cooking cavity is closed, the pot cover assembly is connected to the top of the pot body, so as to achieve the effect of making it easy for the user to clean the pot cover assembly.
[0075] Anything not described in this application can be achieved by adopting or drawing on existing technologies.
[0076] The various embodiments in this specification are described in a progressive manner, and the same or similar parts between the various embodiments can be referenced to each other, and each embodiment focuses on the differences from other embodiments.
[0077] The above is only an embodiment of the present application and is not intended to limit the present application. For those skilled in the art, the present application may have various changes and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present application should be included in the scope of the claims of the present application.
Claims
1. A pot cover assembly, comprising a cover, wherein the cover comprises a top wall and a side wall surrounding the periphery of the top wall and extending downward, wherein: The top wall has an injection molding area, a convex rib surrounding the injection molding area is provided between the injection molding area and the side wall, an injection molding port is provided in the injection molding area, and the convex rib has a thinning section and a thickening section whose cross-sectional area is larger than the thinning section along its circumference, so that the plastic in the injection molding area flows to the side wall via the thickening section.
2. A pot cover assembly according to claim 1, characterized in that: The face cover has a front end and a rear end which are arranged opposite to each other, and a central axis which passes through the front end, the rear end and the center of the face cover, and the injection port is located on the central axis and is arranged close to the front end.
3. A pot cover assembly according to claim 2, characterized in that: The thickened section is arranged corresponding to the front end and is located outside the injection port.
4. A pot cover assembly according to claim 2, characterized in that: The thinning section comprises a thin-walled area arranged corresponding to the rear end and thick-walled areas located on both sides of the thin-walled area, and the cross-sectional area of the thin-walled area is smaller than the cross-sectional area of the thick-walled area; And / or, the thinning section is provided with a blocking groove corresponding to the rear end.
5. A pot cover assembly according to claim 1, characterized in that: The width of the thinned section is smaller than the width of the thickened section; And / or, the height of the thinned section is smaller than the height of the thickened section, so that the cross-sectional area of the thinned section is smaller than the cross-sectional area of the thickened section.
6. A pot cover assembly according to claim 1, characterized in that: A supporting rib is arranged on the inner side of the side wall. The supporting rib has an outer end connected to the side wall and an inner end opposite to the outer end. There is a gap between the inner end and the convex rib.
7. A pot cover assembly according to claim 6, characterized in that: The width of the outer end is smaller than the width of the inner end.
8. A pot cover assembly according to claim 1, characterized in that: A plurality of blocking ribs are arranged at intervals between the injection port and the thinning section.
9. A pot cover assembly according to claim 1, characterized in that: A connecting rib is arranged between the side wall and the top wall, and the connecting rib has a thickening section arranged corresponding to the thickening section and a thinning section arranged corresponding to the thinning section, and the thickness of the thickening section is greater than the thickness of the thinning section.
10. A cooking utensil, comprising a pot, characterized in that: It also includes a pot cover assembly as claimed in any one of claims 1 to 9, wherein one end of the pot cover assembly is hinged to the pot body so that the pot cover assembly can rotate to open and close the pot body; Alternatively, the pot cover assembly is removably placed on the pot body.