Energy-saving monocrystalline silicon furnace

By applying a thermal insulation silver layer with a thickness of 0.1-1um on the inner side wall of the furnace body of a single crystal silicon furnace, the problem of poor insulation effect is solved, the power consumption reduction and temperature stability are improved, and the single Preparation efficiency and economicality of crystalline silicon furnace.

CN221971730UActive Publication Date: 2024-11-08广东银度光能科技有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420494802.1
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-13
Publication Date
2024-11-08
Estimated Expiration
2034-03-13

AI Technical Summary

Technical Problem

The existing single crystal silicon furnaces have poor thermal insulation effect, resulting in high power consumption, affecting the stability of single crystal silicon growth and preparation cost.

Method used

The inner wall of the single crystal silicon furnace is equipped with a heat-insulating silver layer of 0.1-1um thickness, made of dielectric layer nickel-chromium alloy or nickel-chromium-molybdenum alloy, reflecting infrared radiation to reduce heat loss and improving heat insulation effect .

Benefits of technology

It effectively reduces the power consumption of the single crystal silicon furnace, improves the insulation effect of the furnace temperature, and makes the preparation process more energy-saving.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221971730U_ABST
    Figure CN221971730U_ABST
Patent Text Reader

Abstract

The utility model relates to the field of monocrystalline silicon preparation equipment, in particular to an energy-saving monocrystalline silicon furnace. The utility model provides an energy-saving monocrystalline silicon furnace which comprises a furnace body and a crucible arranged in the furnace body and used for containing raw materials, a furnace opening of the furnace body faces upwards and is aligned with the furnace opening of the furnace body, a heater is arranged beside the crucible and used for heating the crucible, and a bottom thermal field device used for regulating and controlling the temperature in the furnace body is arranged below the crucible. The inner side wall of the furnace body is totally or partially provided with a heat insulation silver layer. The monocrystalline silicon furnace is good in heat insulation effect, low in power consumption and energy-saving.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the field of single crystal silicon preparation equipment, in particular to an energy-saving single crystal silicon furnace. Background Art

[0002] Single crystal silicon is the base material of most semiconductor components. Currently, most single crystal silicon is prepared by the Czochralski method (i.e., J. Czochralski method) with the help of a single crystal silicon furnace (also known as a reduction furnace). The existing single crystal silicon furnace includes a furnace body with a furnace mouth facing upward, a crucible for holding raw materials is arranged inside the furnace body, and the crucible mouth faces upward and is aligned with the furnace mouth of the furnace body; a heater is arranged around the crucible to heat it, and a bottom heat field device is arranged under the crucible. When single crystal silicon needs to be prepared, high-purity polycrystalline silicon raw materials are first placed in a crucible. The heater heats the crucible to melt the raw materials in it into silicon liquid. Then, the heating temperature of the heater is slightly lowered, so that the temperature of the molten silicon liquid drops appropriately to produce a certain degree of supercooling. A silicon single crystal (called a seed crystal) fixed on the seed crystal axis is then extended into the furnace body from the furnace mouth and inserted into the surface of the silicon liquid melt in the crucible. The silicon liquid melt at the solid-liquid interface at the lower end of the seed crystal is cooled and crystallized along the lower end of the seed crystal. Thereafter, the seed crystal is slowly pulled upward, and the silicon crystal continues to grow at the lower end of the seed crystal. In the process of silicon crystal growth, it is necessary to first control the parameters such as the seed crystal rising speed so that a thin crystal neck of about 100 mm in length and 3 to 5 mm in diameter grows below it, which is used to eliminate the dislocation of atomic arrangement caused by the strong thermal shock of the high-temperature solution on the seed crystal. This process is called seeding; then, the seed crystal is controlled to rise at an appropriate speed and the temperature of the silicon liquid melt is controlled so that a silicon crystal with a diameter that meets the process requirements (generally 75 to 300 mm) grows below the seed crystal. This process is called shoulder release (the aforementioned silicon crystal with a diameter of 75 to 300 mm formed during the shoulder release process is called a crystal shoulder in the industry); then, the seed crystal rising speed is suddenly increased to perform a shoulder rotation operation, so that the crystal shoulder turns to an approximate right angle; then enter the equal diameter process, and by controlling the bottom thermal field temperature and the seed crystal rising speed, a silicon single crystal column of a certain diameter specification is grown; finally, when most of the silicon liquid has completed crystallization, the crystal is gradually reduced to form a tail-shaped cone, which is called the finishing process. At this point, a single crystal silicon body is pulled and can be taken out and stored after a period of insulation and cooling. This type of single crystal silicon furnace requires long-term continuous heating during the pulling process, but its own thermal insulation effect is poor, resulting in high power consumption. High power consumption will not only cause the pulling cost to increase, but also affect the stability of single crystal silicon growth. Utility Model Content

[0003] The technical problem to be solved by the utility model is to provide a single crystal silicon furnace, which has good heat insulation effect, low power consumption and is more energy-saving.

[0004] In order to solve the above problems, the utility model provides an energy-saving single crystal silicon furnace, including a furnace body, a furnace mouth of the furnace body facing upward, and a crucible for containing raw materials arranged in the furnace body, the crucible mouth facing upward and aligned with the furnace mouth of the furnace body, a heater is provided on the side of the crucible to heat it, and a bottom thermal field device for regulating the temperature in the furnace body is provided below the crucible, and a heat insulating silver layer is provided on the inner side wall of the furnace body in whole or in part.

[0005] Furthermore, the thickness of the heat-insulating silver layer is 0.1-1 um.

[0006] Furthermore, a dielectric layer is provided between the heat-insulating silver layer and the inner side wall of the furnace body, and the heat-insulating silver layer is attached to the inner side wall of the furnace body through the dielectric layer.

[0007] Furthermore, the dielectric layer is made of nickel-chromium alloy or nickel-chromium-molybdenum alloy.

[0008] Furthermore, the thickness of the dielectric layer is 50-200 nm.

[0009] Beneficial effect: Since a heat-insulating silver layer is provided on the inner wall of the single crystal silicon furnace body, and the silver layer itself can reflect a large amount of infrared rays (infrared radiation), when the heat source (heater) in the furnace emits heat source radiation outward, the infrared radiation in the heat source radiation hits the heat-insulating silver layer on the inner wall of the furnace body and is reflected inward, thereby reducing the amount of infrared radiation emitted to the outside of the furnace body and thus reducing heat loss. Therefore, the heat insulation effect of the single crystal silicon furnace of the utility model is better, the inside of the single crystal silicon furnace can be easily maintained at a certain temperature, the power consumption is low and it is more energy-saving. BRIEF DESCRIPTION OF THE DRAWINGS

[0010] Figure 1 This is a schematic diagram of the structure of a single crystal silicon furnace.

[0011] Figure 2 yes Figure 1 A magnified schematic diagram of part A.

[0012] Explanation of symbols:

[0013] 1-single crystal silicon furnace; 11-furnace body; 12-furnace mouth; 2-crucible; 21-crucible mouth; 3-seed crystal; 4-crucible supporting rod; 5-heater; 6-bottom thermal field device; 7-medium layer; 8-thermal insulation silver layer. DETAILED DESCRIPTION

[0014] The present invention is further described in detail below in conjunction with specific implementation methods.

[0015] See Figure 1The single crystal silicon furnace 1 includes a furnace body 11, and its furnace mouth 12 faces upward. The crucible 2 is accommodated in the furnace body 11, and the crucible mouth 21 of the crucible 2 faces upward and is aligned with the furnace mouth 12 of the furnace body 11. When preparing a single crystal silicon body, the seed crystal 3 can extend from the furnace mouth 12 of the furnace body 11 into the furnace body 11, and then extend from the crucible mouth 21 into the crucible 2. The crucible 2 includes a quartz crucible part (not shown in the figure) for holding silicon raw materials and a graphite crucible part (not shown in the figure) sleeved on the outside of the quartz crucible part, the graphite crucible part is at the bottom and the quartz crucible part is at the top. The crucible support rod 4 is installed and supported at the bottom end of the crucible 2; the cylindrical heater 5 is sleeved on the outside of the crucible 2 to heat the crucible 2 uniformly around the circumference; the bottom thermal field device 6 is installed below the crucible 2, responsible for regulating the temperature in the furnace body 11. The crucible 2, seed crystal 3, quartz crucible part, graphite crucible part, crucible supporting rod 4, heater 5 and bottom thermal field device 6 are all prior art, and their specific structures and working principles are not described in detail here.

[0016] See Figure 2 , a dielectric layer 7 with a thickness of 50-200nm is provided on all the inner side walls of the furnace body 11, and a heat-insulating silver layer 8 with a thickness of 0.1-1um is provided on the inner side wall of the dielectric layer 7; the dielectric layer 7 is made of nickel-chromium alloy or nickel-chromium-molybdenum alloy, and has good adhesion to the inner side wall of the furnace body 11, and also has good adhesion to the heat-insulating silver layer 8, so the heat-insulating silver layer 8 can be well adhered to the inner side wall of the furnace body 11 through the dielectric layer 7. Not preferably, the dielectric layer 7 may not be provided, and the heat-insulating silver layer 8 may be directly provided on the inner side wall of the furnace body 11. Both the heat-insulating silver layer 8 and the dielectric layer 7 may be electroplated or coated to the corresponding positions by magnetron sputtering, multi-arc ion plating, evaporation plating or cold spraying. Since the silver layer of the heat-insulating silver layer 8 can reflect a large amount of infrared rays (infrared radiation), the heater 5 (and the heat source such as the bottom thermal field device 6) in the furnace will emit heat source radiation outward when generating heat. The infrared radiation in the heat source radiation will be reflected inward after hitting the heat-insulating silver layer 8 on the inner wall of the furnace body 11, thereby reducing the amount of infrared radiation emitted to the outside of the furnace body 11 and reducing heat loss. The single crystal silicon furnace 1 thus achieves a better heat insulation effect, and the heat preservation effect of the temperature in the furnace is also better. The power consumption required by the heat source such as the heater 5 to maintain the temperature in the furnace at a certain value is also lower, that is, it is more energy-saving. In this embodiment, the heat-insulating silver layer 8 is provided on all the inner walls of the furnace body 11 (adhered to the inner wall of the furnace body 11 through the dielectric layer 7). In other embodiments, the heat-insulating silver layer 8 can be provided only on a part of the inner wall of the furnace body 11.

[0017] The above is only an implementation method of the invention, and does not limit the scope of patent protection. Those skilled in the art can make non-substantial changes or substitutions based on the invention, which still fall within the scope of patent protection.

Claims

1. An energy-saving single crystal silicon furnace, comprising a furnace body, the furnace mouth of the furnace body facing upward, and a crucible for holding raw materials arranged in the furnace body, the crucible mouth facing upward and aligned with the furnace mouth of the furnace body, a heater is arranged beside the crucible to heat it, and a bottom thermal field device for regulating the temperature in the furnace body is arranged below the crucible, characterized in that: The inner side wall of the furnace body is entirely or partially provided with a heat-insulating silver layer.

2. The single crystal silicon furnace according to claim 1, characterized in that: The thickness of the heat-insulating silver layer is 0.1-1 um.

3. The single crystal silicon furnace according to claim 1 or 2, characterized in that: A dielectric layer is provided between the heat-insulating silver layer and the inner side wall of the furnace body, and the heat-insulating silver layer is attached to the inner side wall of the furnace body through the dielectric layer.

4. The single crystal silicon furnace according to claim 3, characterized in that: The dielectric layer is specifically made of nickel-chromium alloy or nickel-chromium-molybdenum alloy.

5. The single crystal silicon furnace according to claim 3, characterized in that: The thickness of the dielectric layer is 50-200 nm.