Titanium alloy blade laser cladding atmosphere protection device
By designing a laser cladding atmosphere protection device for titanium alloy blades, the atmosphere protection sleeve provides a continuous protection atmosphere, which solves the problems of difficult transformation of existing equipment and easy oxidation of welds, and achieves efficient titanium alloy blade repair effect.
Patent Information
- Application Number
- CN202420420667.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-05
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2034-03-05
AI Technical Summary
During the repair process of titanium alloy blades, existing laser cladding equipment has problems such as difficult transformation of the molding chamber, poor accuracy after transformation, and easy oxidation of welds and heat-affected zones, resulting in insufficient protective atmosphere and affecting the repair effect.
A titanium alloy blade laser cladding atmosphere protection device was designed, including an atmosphere protection chamber, a blade clamping tool, a cladding head and an atmosphere protection sleeve. The flexible sealing cover and an atmosphere protection sleeve provide a continuous protective atmosphere, avoiding the Gas turbulence meets the weld control requirements.
It effectively avoids oxidation of welds and heat-affected zones, improves the repair effect, reduces the difficulty of transformation and material consumption, and is suitable for small-scale production and testing stages, improving work efficiency and quality stability.
Smart Images

Figure CN221983904U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of laser cladding, and in particular relates to an atmosphere protection device for laser cladding of a titanium alloy blade. Background Art
[0002] The compressor blades are made of titanium alloy. After long-term wear and tear, the blade tips will be worn out due to defects in the design and manufacturing process, making the blades shorter than the normal range of use and no longer suitable for continued use. In addition, the scrap rate of blade wear is high and the demand for spare parts is large. After process analysis and testing of compressor titanium alloy blades, the existing maintenance method uses laser cladding technology to perform additive repair on the surface to be clad at the blade tip to complete size restoration.
[0003] Laser cladding technology is an additive repair technology that uses high-energy laser beam radiation to melt the thin layer of substrate and the alloy powder fed into the workpiece surface simultaneously, thereby achieving metallurgical bonding between the material and the substrate. The main measures for laser cladding and extension protection of titanium alloy blades in the existing technology are: (1) filling and cleaning the equipment molding chamber with argon; (2) modifying the cladding head and making a drag cover; (3) filling the back of the fixture with argon for protection.
[0004] Existing laser cladding equipment has the following defects:
[0005] (1) Existing laser cladding equipment needs to be equipped with a molding cabin that can be filled with argon for cleaning. The cabin of the molding cabin is larger than the size of the compressor blade, and it is difficult to ensure that the oxygen concentration is quickly reduced to meet the welding protection requirements of titanium alloy. Therefore, the cleaning process generally takes 3 to 5 hours, which is too long and consumes a lot of protective gas. It is not suitable for small batches of multi-material product repair work;
[0006] (2) During the welding process, titanium alloy materials are prone to oxidation problems in the weld and heat-affected zone, and high protection requirements are placed on the weld and heat-affected zone. The national standard stipulates the surface color of the weld, where silver or yellow is acceptable, and narrow dark strips are allowed near the boundary of the protective gas. Dark brown, purple, blue, gray or off-white are not allowed:
[0007] When laser cladding is used to repair a thick plate with an interface, the gas protection effect during the cladding process is good. The lens protection gas, powder feeding gas, and restraint gas can effectively form an atmosphere protection for the weld area. After welding, the weld area and the heat-affected area are silver or yellow, meeting the welding requirements.
[0008] However, since the wear part of the titanium alloy blade of this type of compressor is the blade tip, and the thickness of the titanium alloy blade tip is as thin as 0.6-1.0mm, it is necessary to modify the cladding head, which is difficult and easily affects the cladding accuracy of the equipment;
[0009] (3) After the modification of the cladding head, the lens gas, powder feeding gas, and restraint gas are prone to turbulence at the blade tip during the laser cladding repair process, and cannot form a complete protective function for the atmosphere in the weld area. The blade tip extension weld is blue, and the heat-affected zone is blue and purple, which does not meet the weld control requirements. It is very easy to cause oxidation problems in the weld and heat-affected zone, and the product qualification rate is low.
[0010] Therefore, it is very necessary to design an atmosphere protection device for laser cladding of titanium alloy blades. Utility Model Content
[0011] In order to solve the problems of difficulty in modifying the drag cover of the forming cabin of the existing laser cladding equipment, poor accuracy after modification, and easy oxidation of the weld and heat affected zone during welding, the utility model provides a titanium alloy blade laser cladding atmosphere protection device, which provides good protection conditions for the additive manufacturing and repair of titanium alloy blades.
[0012] To achieve the above purpose, the technical solution provided by the utility model is:
[0013] A titanium alloy blade laser cladding atmosphere protection device, which is special in that:
[0014] It includes atmosphere protection cabin, blade clamping tooling, cladding head and atmosphere protection sleeve;
[0015] The atmosphere protection cabin comprises a cabin body and a cabin door; the cabin body is a transparent cabin body, and the top of the cabin body is a flexible sealing cover; the cladding head is arranged on the top of the cabin body, and the flexible sealing cover is sealed with the cladding head, so that the flexible sealing cover is deformed with the movement of the cladding head and remains sealed, and the flexible sealing cover does not undergo plastic deformation;
[0016] A sleeve installation hole is provided on one side wall of the cabin body, and a hatch door opening adapted to the cabin door is provided on the other side wall;
[0017] The blade clamping tool is arranged in the cabin, and clamps the blade to be clad so that the blade tip faces upward and remains horizontal;
[0018] The atmosphere protection sleeve comprises an air inlet conduit, a sleeve body and a straight pipe joint; the straight pipe joint is adapted to be installed in the sleeve installation hole and maintains sealing;
[0019] The air inlet duct is arranged on the outer side of the cabin, one end of which is an air inlet and the other end is connected to a straight pipe joint; the air inlet is connected to an external air source;
[0020] The sleeve body is arranged on the inner side of the cabin, one end of which is an air supply port, and the other end is connected to the straight pipe joint; the air supply port is a "U"-shaped jet part, that is, a plurality of inward jet holes are opened on the two side arms of the "U"-shaped jet part; the length of the "U"-shaped jet part is greater than the length of the blade tip, and when the blade is clamped in place, the horizontal projection of the blade tip on the sleeve body falls on the "U"-shaped jet part, and the blade tip is in the gap between the two side arms of the "U"-shaped jet part; the two side arms of the "U"-shaped jet part are provided with relatively dense holes with a diameter of 0.1 mm, and the protective gas blows a protective atmosphere to the blade tip through the dense holes; the air inlet duct and the sleeve body are installed at both ends of the straight pipe joint, and the straight pipe joint is sealed and installed on the sleeve mounting hole of the protective cabin.
[0021] Furthermore, the horizontal distances between the air injection holes of the two side arms of the "U"-shaped air injection portion and the two side edges of the blade to be clad are 1 to 2 mm.
[0022] Further, the hatch includes a sealing plate, a hatch tightening valve and a hatch cross arm;
[0023] The sealing plate is a circular plate, and is adapted to be installed on the hatch door opening; the diameter of the sealing plate is greater than the length of the blade to be clad, and the height of the lowest point of the sealing plate is less than or equal to the height of the blade clamping tooling;
[0024] The sealing plate and the hatch cross arm are both provided with valve mounting holes at their centers, and the hatch tightening valve is adapted to be mounted on the two valve mounting holes at the same time;
[0025] The hatch cross arm is fixed to the side wall of the cabin body by fasteners, and the sealing plate is compressed by tightening the hatch valve so that the sealing plate seals the cabin body.
[0026] Furthermore, the air intake duct, the straight pipe joint, and the sleeve body are connected in sequence and kept horizontal.
[0027] Furthermore, the blade clamping tooling is an inverse tenon-groove of the blade, so that the blade tip to be clad faces upward and remains horizontal.
[0028] The concept of the utility model:
[0029] For titanium alloy blade tips as thin as 0.6 to 1.0 mm, the original cladding head needs to blow out shielding gas, powder feeding gas and restraining gas at the same time during laser cladding, which easily generates turbulence at the blade tip. The shielding gas cannot directly protect the blade cladding area and heat-affected zone. The blade tip extension weld is blue, and the heat-affected zone is blue and purple, which does not meet the weld control requirements.
[0030] To avoid turbulence, the existing technology chooses to modify the cladding head of the original equipment. However, since the thickness of the titanium alloy blade tip is as thin as 0.6 to 1.0 mm, the modification of the cladding head is difficult and requires high modification accuracy. The modification is also likely to affect the accuracy of the original equipment, and thus the protective effect of laser cladding on the blade cannot be guaranteed after the cladding head is modified.
[0031] Therefore, the utility model improves the design of blowing out protective gas. It is no longer blown out from the cladding head, but the protective atmosphere is continuously provided from the atmosphere protection sleeve on the side of the molding chamber, thereby avoiding the generation of turbulence, reducing the difficulty of modifying the cladding head, and providing good protection conditions for additive manufacturing and repair of titanium alloy blades.
[0032] The advantages of the utility model are:
[0033] 1. During the blade tip extension process, the utility model uses laser cladding to form an atmosphere protection sleeve in the atmosphere protection device, so that the gas jet portion of the atmosphere protection sleeve fits the two sides and heat-affected zone of the blade for protection; at the same time, dense small holes are provided on the two inner sides of the gas jet portion to continuously provide a protective atmosphere to the weld area, meet the weld control requirements, avoid turbulence and reduce oxidation problems, and provide good protection conditions for additive manufacturing and repair of titanium alloy blades.
[0034] 2. The cladding head is sealed and connected to the flexible sealing cover. After the hatch is closed, a sealed cabin for laser cladding is formed. The overall protective gas-filled environment is constructed to meet the sealing requirements, reduce the probability of oxidation during the material cladding process, and improve the additive repair effect.
[0035] 3. The cladding head of the utility model is adapted to the size of the blade tip, and is suitable for small-batch production and repair in the test phase. It saves inert gas while meeting the requirements of cladding, and has great economic value while improving quality stability.
[0036] 4. The utility model adopts the reverse tenon-groove structure to clamp the blades. The tenon-groove structure makes it easy to clamp the blades, shortening the original clamping time from 5 to 10 minutes to 10 to 20 seconds, greatly improving the work efficiency;
[0037] 5. The cabin material of the utility model is made of PVC transparent plastic, which is convenient for operators to observe the cladding process and reduces the difficulty of operation. BRIEF DESCRIPTION OF THE DRAWINGS
[0038] Figure 1 : Structural perspective view of atmosphere protection device;
[0039] Figure 2 : Perspective view of the protective sleeve structure;
[0040] Figure 3 : Schematic diagram of the protective casing structure;
[0041] Figure 4 : Schematic diagram of the atmosphere protection cabin structure;
[0042] Figure 5 : Perspective view of blade clamping fixture structure;
[0043] Figure 6 : Perspective view of atmosphere protection hatch structure;
[0044] In the figure: 1- cladding head; 2- atmosphere protection sleeve; 3- atmosphere protection cabin; 4- blade clamping tool; 5- atmosphere protection cabin door;
[0045] 201-flat nozzle; 202-intake duct; 203-straight pipe joint; 204-flared outer sleeve nut; 205-sleeve body;
[0046] 301-flexible sealing cover; 302-sleeve mounting hole; 303-cross arm mounting hole; 304-cabin door opening;
[0047] 501-sealing plate; 502-fixing pin; 503-door cross arm; 504-door tightening valve. DETAILED DESCRIPTION
[0048] Embodiments of the present utility model are described in detail below, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are intended to be used to explain the present invention, and should not be construed as limiting the present invention.
[0049] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present invention.
[0050] like Figure 1 A titanium alloy blade laser cladding atmosphere protection device is shown.
[0051] It includes an atmosphere protection cabin 3, a blade clamping tool 4, a cladding head 1 and an atmosphere protection sleeve 2;
[0052] like Figure 4The atmosphere protection cabin 3 shown is a transparent cabin, which is convenient for operators to observe the internal cladding process; the bottom, front, rear, left and right plates of the cabin of this embodiment are all made of PVC transparent plastic, which is convenient for operators to observe the cladding process and reduces the difficulty of operation.
[0053] The atmosphere protection cabin 3 includes a cabin body and a cabin door;
[0054] The cabin is transparent, which is convenient for operators to observe; the top of the cabin is a flexible sealing cover 301; the flexible sealing cover 301 is sealed with the cladding head 1, so that the flexible sealing cover 301 can be deformed and kept sealed with the movement of the cladding head 1, and the flexible sealing cover 301 will not be plastically deformed; after the gas enters the cabin, the flexible sealing cover bulges, which is convenient for operators to judge the inflation state;
[0055] The flexible sealing cover 301 in this embodiment is made of polyethylene film; the cladding head 1 in this embodiment is suitable for cladding blades as thin as 0.6-1.0 mm in thickness. The distance between the cladding head 1 and the blade tip is 4-6 mm, so that the blade tip to be clad is at the laser focus position of the cladding head 1.
[0056] A sleeve installation hole 302 matching with the straight pipe joint 203 is provided on one side wall of the cabin body, and a cross arm installation hole 303 and a hatch door opening 304 are provided on the other side wall of the cabin body, which are matched with the hatch door cross arm 503 and the sealing plate 501 respectively;
[0057] The hatch door includes a sealing plate 501, a hatch door tightening valve 504, a hatch door cross arm 503 and two fixing pins 502;
[0058] The sealing plate 501 is a circular plate, and the sealing plate 501 is adapted to be installed on the hatch door opening 304; the diameter of the sealing plate 501 is greater than the length of the blade to be clad, and the height of the lowest point of the sealing plate 501 is less than or equal to the height of the blade clamping fixture 4, so as to ensure that the blade to be clad can pass through the hatch door opening 304 and be clamped on the blade clamping fixture 4;
[0059] The sealing plate 501 and the hatch cross arm 503 are both provided with valve mounting holes at their centers, and the hatch tightening valve 504 is simultaneously adapted to be installed on the two valve mounting holes; two pin holes are provided on the side wall of the cabin body where the hatch door opening 304 is located, and two fixing pins are adapted to the pin holes;
[0060] The hatch cross arm 503 is fixed to the side wall of the cabin body by two fixing pins 302, and the sealing plate 501 is pressed by the hatch tightening valve 504, so that the sealing plate 501 seals the cabin body after closing the door, constructing an overall protective gas-filled environment and reducing the probability of oxidation during the material cladding process.
[0061] The blade clamping tool 4 is arranged in the cabin, which clamps the blade to be clad and makes the blade tip face up and keep it horizontal; during the clamping process, the blade is pushed in from the corresponding position of the tenon groove and clamped and fixed; preferably, the blade clamping tool is a blade reverse tenon groove, which is convenient for clamping and can shorten the original clamping time of 5 to 10 minutes to 10 to 20 seconds, greatly improving work efficiency.
[0062] The utility model comprehensively considers the improvement cost and the improvement success rate, and selects to use the method of adding a group of protective gas circuits to provide a soft gas protection measure without turbulence for cladding.
[0063] The protective gas circuit is an atmosphere protective sleeve 2, which includes an air inlet duct 202, a sleeve body 205, a straight pipe joint 203 and two flared outer sleeve nuts 204; the straight pipe joint 203 is adapted to be installed with the sleeve mounting hole 302 and maintained sealed;
[0064] The air inlet duct 202 is arranged on the outer side of the cabin, with one end being an air inlet and the other end being a flat nozzle; the air inlet is connected to an external air source;
[0065] The sleeve body 205 is arranged on the inner side of the cabin, with one end being an air supply port and the other end being a flat nozzle; the air supply port is a "U"-shaped jet part, that is, a plurality of inward jet holes are opened on the two side arms of the "U"-shaped jet part; the length of the "U"-shaped jet part is greater than the length of the blade tip, and when the blade is clamped in place, the horizontal projection of the blade tip on the sleeve body falls on the "U"-shaped jet part, and the blade tip is in the gap between the two side arms of the "U"-shaped jet part, thereby ensuring the protective effect of the protective atmosphere on the blade tip laser cladding;
[0066] Preferably, the horizontal distance between the jet holes of the two side arms of the "U"-shaped jet part and the two side edges of the blade to be clad is 1 to 2 mm, which continuously provides a protective atmosphere for both sides of the blade and the heat-affected zone. It is suitable for small-batch production and repair in the test stage. It saves inert gas while meeting the requirements of cladding, and has great economic value while improving quality stability.
[0067] In this embodiment, by providing relatively positioned dense holes with a diameter of 0.1 mm on the two side arms of the "U"-shaped jet portion, the shielding gas can continuously provide a protective atmosphere to the blade tip through the dense holes, preventing turbulence at the blade tip, meeting the weld control requirements, avoiding turbulence and reducing oxidation problems.
[0068] Two flared outer sleeve nuts 204 are respectively arranged on the two flat nozzles; the air intake duct 202 and the sleeve body 205 are installed at both ends of the straight pipe joint 203 through two flared outer sleeve nuts; preferably, the air intake duct 202, the straight pipe joint 203, and the sleeve body 205 are sequentially connected and kept horizontal. The straight pipe joint 203 is sealed and installed on the sleeve installation hole of the protective cabin.
[0069] Installation process of this utility model:
[0070] Step 1: Install the straight pipe joint 203 on the sleeve installation hole of the protective cabin and ensure the seal, then install two flared outer sleeve nuts 204 at both ends of the straight pipe joint 203, and horizontally connect the air intake duct 202 and the sleeve body 205 to the straight pipe joint 203;
[0071] Step 2: vertically place the blade clamping tool 4 below the sleeve body 205;
[0072] Step 3: Fit the sealing plate 501 on the hatch door opening 304, then insert the two fixing pins 502 through the hatch cross arm 503 and into the pin hole, and finally tighten the hatch tightening valve 504 to press the sealing plate 501, so that the sealing plate 501 seals the cabin; after the hatch is closed, a sealed cabin is formed, and the overall protective gas filling environment is constructed to reduce the probability of oxidation during the material cladding process;
[0073] Step 4: Move the atmosphere protection device as a whole to the work surface, move the cladding head 1, adjust the height of the cladding head 1 to 4-6 mm from the blade tip height, make the blade tip to be clad at the laser focus position of the cladding head 1, and then fit the polyethylene film 301 to the cladding head 1 and clamp it.
[0074] The process of laser cladding the blade to be clad using the utility model:
[0075] Step 1: Open the hatch door by tightening the hatch valve 504, and then install the blade to be clad on the blade clamping fixture, ensuring that the horizontal projection of the blade tip on the casing body 205 falls on the "U"-shaped jet part, and the blade tip is in the gap between the two side arms of the "U"-shaped jet part;
[0076] Step 2: Move the cladding head 1, adjust the height of the cladding head 1 to 4-6 mm from the blade tip, so that the blade tip to be clad is at the laser focus position of the cladding head 1, and then fit and clamp the flexible sealing cover 301 to the cladding head 1;
[0077] Step 3: Close the hatch and tighten the hatch tightening valve 504;
[0078] Step 4: connect the external protective gas source to the air inlet conduit 202, introduce inert gas, and turn on the lens protective gas and the restraining gas to replace the air in the atmosphere protection chamber 3 for 5 to 10 minutes;
[0079] Step 5: Adjust the flow rates of the inert gas, lens protection gas and restraint gas to a size suitable for laser cladding, so that the blade tip and the heat-affected zone are in a local atmosphere protection environment;
[0080] Step 6: Adjust the laser cladding parameters and clad the blade to be clad.
[0081] The above description is only a specific implementation mode of the present utility model, but the protection scope of the present utility model is not limited thereto. Any technician familiar with the technical field can easily think of various equivalent modifications or substitutions within the technical scope disclosed in the present utility model, and these modifications or substitutions should be included in the protection scope of the present utility model.
Claims
1. A titanium alloy blade laser cladding atmosphere protection device, characterized in that: It includes atmosphere protection cabin, blade clamping tooling, cladding head and atmosphere protection sleeve; The atmosphere protection cabin comprises a cabin body and a cabin door; the cabin body is a transparent cabin body, and the top of the cabin body is a flexible sealing cover; the cladding head is arranged on the top of the cabin body, and the flexible sealing cover is sealed with the cladding head, so that the flexible sealing cover is deformed with the movement of the cladding head and remains sealed, and the flexible sealing cover does not undergo plastic deformation; A sleeve installation hole is provided on one side wall of the cabin body, and a hatch door opening adapted to the cabin door is provided on the other side wall; The blade clamping tool is arranged in the cabin, and clamps the blade to be clad so that the blade tip faces upward and remains horizontal; The atmosphere protection sleeve comprises an air inlet conduit, a sleeve body and a straight pipe joint; the straight pipe joint is adapted to be installed in the sleeve installation hole and maintains sealing; The air inlet duct is arranged on the outer side of the cabin, one end of which is an air inlet and the other end is connected to a straight pipe joint; the air inlet is connected to an external air source; The sleeve body is arranged on the inner side of the cabin, one end of which is an air supply port, and the other end is connected to the straight pipe joint; the air supply port is a "U"-shaped jet part, that is, a plurality of inward jet holes are opened on the two side arms of the "U"-shaped jet part; the length of the "U"-shaped jet part is greater than the length of the blade tip, and when the blade is clamped in place, the horizontal projection of the blade tip on the sleeve body falls on the "U"-shaped jet part, and the blade tip is in the gap between the two side arms of the "U"-shaped jet part; the two side arms of the "U"-shaped jet part are provided with relatively dense holes with a diameter of 0.1 mm, and the protective gas blows a protective atmosphere to the blade tip through the dense holes; the air inlet duct and the sleeve body are installed at both ends of the straight pipe joint, and the straight pipe joint is sealed and installed on the sleeve mounting hole of the protective cabin.
2. The titanium alloy blade laser cladding atmosphere protection device according to claim 1, characterized in that: The horizontal distances from the air jet holes of the two side arms of the "U"-shaped air jet part to the two side edges of the blade to be clad are 1 to 2 mm.
3. The titanium alloy blade laser cladding atmosphere protection device according to claim 1, characterized in that: The hatch door comprises a sealing plate, a hatch door tightening valve and a hatch door cross arm; The sealing plate is a circular plate, and is adapted to be installed on the hatch door opening; the diameter of the sealing plate is greater than the length of the blade to be clad, and the height of the lowest point of the sealing plate is less than or equal to the height of the blade clamping tooling; The sealing plate and the hatch cross arm are both provided with valve mounting holes at their centers, and the hatch tightening valve is adapted to be mounted on the two valve mounting holes at the same time; The hatch cross arm is fixed to the side wall of the cabin body by fasteners, and the sealing plate is compressed by tightening the hatch valve so that the sealing plate seals the cabin body.
4. The titanium alloy blade laser cladding atmosphere protection device according to claim 1, characterized in that: The air intake duct, the straight pipe joint and the sleeve body are connected in sequence and kept horizontal.
5. The titanium alloy blade laser cladding atmosphere protection device according to claim 1, characterized in that: The blade clamping tool is an inverse tenon groove of the blade, so that the blade tip to be clad faces upward and remains horizontal.