Cavity extending tool for cold press forming die
By designing the cavity extension tooling for cold press forming molds, the layered line problem caused by multiple charges in ceramic cold press forming is solved, and the uniformity and production efficiency of ceramic blanks are improved.
Patent Information
- Application Number
- CN202420494770.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-14
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2034-03-14
AI Technical Summary
During the cold pressing process of ceramics, multiple charges lead to the formation of layered lines, affecting the performance and production efficiency of the ceramic blank.
A cavity extension tool for cold press forming molds is designed, including a cylinder, a top ring plate, a bottom ring plate and a reinforcement plate, which is used to expand the height of the mold cavity so that one load can achieve the pressing of multiple loads. Effect, avoid stratification defects.
It effectively avoids the layering defects inside the ceramic blank, improves production efficiency, and ensures the uniformity and performance of the ceramic blank.
Smart Images

Figure CN221985378U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of ceramic preparation, in particular to a cavity extension tooling for a cold pressing molding die. Background Art
[0002] Ceramics include industrial ceramics and special ceramics, among which special ceramics refer to ceramics with special mechanical, physical or chemical properties. Special ceramics are made of inorganic non-metallic materials as the basic raw materials, mixed with other compounds in a specific proportion, and prepared by molding, sintering and other processes. According to different uses, special ceramics can be divided into structural ceramics and functional ceramics. Structural ceramics have the characteristics of high strength, high hardness, high temperature resistance, corrosion resistance, and oxidation resistance. They are suitable for harsh environments or engineering application conditions. The application fields include pan-semiconductor equipment, wear-resistant machinery, national defense and military industry, aerospace, etc.
[0003] Common structural ceramic materials include silicon carbide, aluminum oxide, silicon nitride, etc. Silicon carbide materials are widely used in nuclear power, wind power, lithium batteries, semiconductors, photovoltaics and other fields due to their extremely high elastic modulus, thermal conductivity and low thermal expansion coefficient. Silicon nitride ceramics have high thermal conductivity, high mechanical properties, excellent insulation and corrosion resistance, and are widely used in electrode devices, aerospace, automobile manufacturing and other fields.
[0004] In the ceramic preparation process, ceramic molding is a crucial link. Molding technology largely determines the uniformity of the green body and the ability to prepare complex-shaped parts, and directly affects the reliability of the material and the cost of the final ceramic parts. At present, the molding method of ceramics mainly includes cold pressing. Cold pressing technology usually places the powder in a fixed-shaped mold for pressing. Cold pressing is commonly used for the molding of materials such as silicon nitride, silicon carbide, boron nitride, boron carbide, titanium boride and spinel.
[0005] Common molds for cold pressing include graphite molds, which are mainly used to pour ceramic granules into the mold cavity of the graphite mold. When the ceramic granules fill the mold cavity, a hydraulic press is used to press them. Under the action of high pressure, the ceramic granules are compressed to a certain height and then stop; then fill the compressed space with granules again, and repeat the previous process, and then fill the granules again for pressing; then continue to repeat the previous step until no more ceramic granules can be filled into the effective mold cavity of the graphite mold. However, after multiple times of filling in ceramic granules for pressing, a delamination line will be formed during the sintering process of the ceramic powder, resulting in a sudden change point in the performance difference of the ceramic blank near the delamination line, which greatly affects the performance of the ceramic blank.
[0006] Therefore, how to avoid multiple loading during the ceramic blank forming process is a technical problem that urgently needs to be solved in this field. Utility Model Content
[0007] In view of the shortcomings of the prior art, the purpose of the utility model is to provide a cavity extension tooling for a cold pressing mold, which can avoid multiple feedings during the ceramic cold pressing forming process, ensure that there are no stratification defects inside the ceramic blank, and improve production efficiency.
[0008] To achieve this purpose, the utility model adopts the following technical solutions:
[0009] The utility model provides a cavity extension tool for a cold pressing forming mold, the cavity extension tool comprising a cylinder;
[0010] The top of the cylinder is provided with a top ring plate, the inner circle of which is connected to the edge of the inner wall of the cylinder; the bottom of the cylinder is provided with a bottom ring plate, the inner circle of which is connected to the edge of the inner wall of the cylinder; and the outer wall of the cylinder is provided with a reinforcing rib plate;
[0011] The cold pressing forming mold comprises a graphite mold, the graphite mold comprises a cylindrical shell and a graphite tray arranged at the bottom of the shell, and the shell comprises a graphite guard plate layer and a shell layer arranged concentrically in sequence from the inside to the outside;
[0012] The cylinder of the cavity extension tooling is concentrically arranged with the shell of the cold pressing forming mold, and the bottom edge of the inner side wall of the cylinder coincides with the top edge of the inner side wall of the graphite guard plate layer.
[0013] In the utility model, the cavity extension tooling refers to a tooling used to lengthen the height of the graphite mold powder loading cavity, the purpose of which is to enable the cavity to load more ceramic granules, calculate the total mass of the granules required to be added in combination with the volume and density of the blank, and add the required mass of granules at one time by using the cavity extension tooling, so that the pressing effect of one loading can achieve the pressing effect after multiple loadings in the existing process, thereby avoiding the generation of stratification defects inside the product and improving production efficiency. In the utility model, the cavity extension tooling is placed above the graphite mold when in use, so that the cylinder of the cavity extension tooling is concentric with the shell of the cold pressing mold, and the bottom edge of the inner side wall of the cylinder coincides with the top edge of the inner side wall of the graphite guard plate layer, so that the cold pressing head can move upward or downward in the axial direction, and the cavity extension tooling includes a top ring plate, a bottom ring plate, a cylinder and a reinforcing rib plate, wherein the top ring plate is convenient for hoisting the cavity extension tooling; the bottom ring plate is used to fit the upper surface of the graphite mold, and the reinforcing rib plate is used to avoid deformation of the cylinder.
[0014] In the utility model, the material of the cavity extension tooling is generally selected from 304 stainless steel to prevent the surface of the cavity extension tooling from rusting during use and thus contaminating the ceramic granulation material.
[0015] In the utility model, the graphite mold includes a graphite guard layer, a shell layer and a graphite support plate. The graphite guard layer generally includes two semi-cylindrical graphite guard layers spliced in half. The graphite guard layer surrounds a mold cavity, and the ceramic granules are generally placed in the mold cavity. The shell layer is generally a carbon-carbon shell. When the ceramic granules are pressed, the axially applied pressure will eventually be transmitted to the carbon-carbon shell.
[0016] Preferably, the top ring plate includes a first top semi-ring plate and a second top semi-ring plate forming a closed ring shape.
[0017] Preferably, the bottom ring plate includes a first bottom semi-ring plate and a second bottom semi-ring plate forming a closed ring shape.
[0018] Preferably, the reinforcing rib plate extends to the surface of the bottom ring plate in a direction away from the cylinder.
[0019] Preferably, the reinforcing rib plate is in a triangular shape.
[0020] Preferably, the number of the reinforcing ribs is at least 2, for example, 2, 3, 4, 5, 6, 7 or 8, but is not limited to the listed values, and other unlisted values within the numerical range are also applicable.
[0021] Preferably, the inner diameter of the cylinder is 350-550mm, for example, it can be 350mm, 360mm, 370mm, 380mm, 390mm, 400mm, 410mm, 420mm, 430mm, 440mm, 450mm, 460mm, 470mm, 480mm, 490mm, 500mm, 510mm, 520mm, 530mm, 540mm or 550mm, but is not limited to the listed values, and other unlisted values within the numerical range are also applicable.
[0022] Preferably, the outer diameter of the top ring plate is 650-750 mm, for example, it can be 650 mm, 660 mm, 670 mm, 680 mm, 690 mm, 700 mm, 710 mm, 720 mm, 730 mm, 740 mm or 750 mm, but is not limited to the listed values, and other unlisted values within the numerical range are also applicable.
[0023] Preferably, the height of the cylinder is 100-250 mm, for example, it can be 100 mm, 110 mm, 120 mm, 130 mm, 140 mm, 150 mm, 160 mm, 170 mm, 180 mm, 190 mm, 200 mm, 210 mm, 220 mm, 230 mm, 240 mm or 250 mm, but is not limited to the listed values, and other unlisted values within the numerical range are also applicable.
[0024] Preferably, the outer diameter of the bottom ring plate is 850-950 mm, for example, it can be 850 mm, 860 mm, 870 mm, 880 mm, 890 mm, 900 mm, 910 mm, 920 mm, 930 mm, 940 mm or 950 mm, but is not limited to the listed values, and other unlisted values within the numerical range are also applicable.
[0025] The operation process of the cavity extension tooling provided by the utility model for cold pressing of ceramic granules is as follows:
[0026] Place the cavity extension tooling above the graphite mold, so that the cylinder of the cavity extension tooling is concentric with the shell of the cold pressing mold, and the bottom edge of the inner side wall of the cylinder coincides with the top edge of the inner side wall of the graphite guard plate layer, so that the cold pressing head can move upward or downward in the axial direction. According to the volume and measured density of the blank specified by the processing requirements, calculate the mass of ceramic granules to be added, and load the required mass of ceramic granules into the mold cavity of the graphite mold at one time. The part exceeding the mold cavity is borne by the cavity extension tooling, that is, loaded into the cylinder of the cavity extension tooling, and then pressed by the cold pressing head.
[0027] Compared with the prior art, the beneficial effects of the utility model are:
[0028] The cavity extension tooling provided by the utility model can avoid multiple feedings during the cold pressing process of ceramics, ensure that there is no delamination defect inside the ceramic blank, and improve production efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] Figure 1 This is a schematic diagram of the structure of the combination of the cavity extension tooling and the graphite mold described in Example 1 of the utility model;
[0030] Figure 2 This is a schematic diagram of the longitudinal section structure of the combination of the cavity extension tooling and the graphite mold described in Example 1 of the utility model;
[0031] Figure 3 This is a schematic diagram of the structure of the graphite mold described in Example 1 of the utility model;
[0032] In the figure: 1-first top semi-ring plate; 2-second top semi-ring plate; 3-first bottom semi-ring plate; 4-second bottom semi-ring plate; 5-reinforcement rib plate; 6-shell layer; 7-graphite guard plate layer; 8-graphite tray. DETAILED DESCRIPTION
[0033] The technical solution of the utility model is further explained below with reference to the accompanying drawings and through specific implementation methods.
[0034] The utility model is further described in detail below. However, the following examples are only simple examples of the utility model and do not represent or limit the scope of protection of the utility model. The scope of protection of the utility model shall be subject to the claims.
[0035] It should be understood that, in the description of the present utility model, the terms "center", "longitudinal", "lateral", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside" and the like indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings, which is only for the convenience of describing the present utility model and simplifying the description, and does not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present utility model. In addition, the terms "first", "second", etc. are only used for descriptive purposes, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first", "second", etc. may explicitly or implicitly include one or more of the features. In the description of the present utility model, unless otherwise specified, "multiple" means two or more.
[0036] It should be noted that in the description of the present invention, unless otherwise clearly specified and limited, the terms "disposed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood by specific circumstances.
[0037] Those skilled in the art should understand that the present invention necessarily includes necessary pipelines, conventional valves and general pump equipment for realizing a complete process, but the above content does not belong to the main invention point of the present invention. Those skilled in the art can add layouts on their own based on the process flow and equipment structure selection, and the present invention does not make special requirements and specific limitations on this.
[0038] Example 1
[0039] This embodiment provides a cavity extension tool for a cold press forming mold. The schematic diagram of the structure after the cavity extension tool and the graphite mold are combined is as follows: Figure 1 As shown, the longitudinal section structure diagram is as follows Figure 2 As shown, the structural diagram of the graphite mold is as follows Figure 3 As shown,
[0040] The cavity extension tooling includes a cylinder, a top ring plate is arranged on the top of the cylinder, the top ring plate includes a first top semi-ring plate 1 and a second top semi-ring plate 2 which are enclosed in a closed ring shape, the inner circle of the top ring plate is connected to the inner side wall edge of the cylinder, a bottom ring plate is arranged on the bottom of the cylinder, the bottom ring plate includes a first bottom semi-ring plate 3 and a second bottom semi-ring plate 4 which are enclosed in a closed ring shape, the inner circle of the bottom ring plate is connected to the inner side wall edge of the cylinder, a reinforcing rib plate 5 is arranged on the outer side wall of the cylinder, the reinforcing rib plate 5 extends to the surface of the bottom ring plate in a direction away from the cylinder, the reinforcing rib plate 5 is in a triangular shape, the number is 4, the inner diameter of the cylinder is 400 mm, the outer diameter of the top ring plate is 700 mm, the outer diameter of the bottom ring plate is 900 mm, and the height of the cylinder is 200 mm;
[0041] The cold pressing forming mold comprises a graphite mold, the graphite mold comprises a cylindrical shell and a graphite tray 8 arranged at the bottom of the shell, the shell comprises a graphite guard plate layer 7 and a shell layer 6 which are arranged concentrically from the inside to the outside, the shell layer 6 is a carbon-carbon shell, the graphite guard plate layer 7 surrounds a mold cavity, and the ceramic granulated material is placed in the mold cavity;
[0042] The cylinder of the cavity extension tooling is concentrically arranged with the shell of the cold pressing mold, and the bottom edge of the inner side wall of the cylinder coincides with the top edge of the inner side wall of the graphite guard plate layer 7 .
[0043] The operation process of the cavity extension tooling provided in this embodiment for cold pressing of ceramic granules is as follows:
[0044] Place the cavity extension tooling above the graphite mold, so that the cylinder of the cavity extension tooling is concentric with the shell of the cold-pressing mold, and the bottom edge of the inner side wall of the cylinder coincides with the top edge of the inner side wall of the graphite guard plate layer 7, so that the cold-pressing head can move upward or downward in the axial direction. According to the volume and measured density of the blank specified by the processing requirements, calculate the mass of the ceramic granules to be added, and load the required mass of ceramic granules into the mold cavity of the graphite mold at one time. The part exceeding the mold cavity is borne by the cavity extension tooling, that is, loaded into the cylinder of the cavity extension tooling, and then pressed by the cold-pressing head.
[0045] In summary, the cavity extension tooling provided by the utility model can avoid multiple feedings during the ceramic cold pressing forming process, ensure that there are no stratification defects inside the ceramic blank, and improve production efficiency.
[0046] The applicant declares that the above is only a specific implementation method of the present utility model, but the protection scope of the present utility model is not limited thereto. The technicians in the relevant technical field should understand that any changes or substitutions that can be easily thought of by the technicians in the relevant technical field within the technical scope disclosed in the present utility model fall within the protection scope and disclosure scope of the present utility model.
Claims
1. A cavity extension tool for a cold press forming mold, characterized in that: The cavity extension tooling includes a cylinder; The top of the cylinder is provided with a top ring plate, the inner circle of which is connected to the edge of the inner wall of the cylinder; the bottom of the cylinder is provided with a bottom ring plate, the inner circle of which is connected to the edge of the inner wall of the cylinder; and the outer wall of the cylinder is provided with a reinforcing rib plate; The cold pressing forming mold comprises a graphite mold, the graphite mold comprises a cylindrical shell and a graphite tray arranged at the bottom of the shell, and the shell comprises a graphite guard plate layer and a shell layer arranged concentrically in sequence from the inside to the outside; The cylinder of the cavity extension tooling is concentrically arranged with the shell of the cold pressing mold, and the bottom edge of the inner side wall of the cylinder coincides with the top edge of the inner side wall of the graphite guard plate layer.
2. The cavity extension tooling for cold press forming mold according to claim 1, characterized in that: The top ring plate includes a first top semi-ring plate and a second top semi-ring plate which form a closed ring shape.
3. The cavity extension tool for cold press forming mold according to claim 1, characterized in that: The bottom ring plate comprises a first bottom semi-ring plate and a second bottom semi-ring plate which form a closed ring shape.
4. The cavity extension tool for cold press forming mold according to claim 1, characterized in that: The reinforcing rib plate extends to the surface of the bottom ring plate in a direction away from the cylinder.
5. The cavity extension tool for cold press forming mold according to claim 4, characterized in that: The reinforcing rib plate is in a triangular shape.
6. The cavity extension tool for cold press forming mold according to claim 1, characterized in that: The number of the reinforcing rib plates is at least 2.
7. The cavity extension tool for cold press forming mold according to claim 1, characterized in that: The inner diameter of the cylinder is 350-550 mm.
8. The cavity extension tool for cold press forming mold according to claim 1, characterized in that: The outer diameter of the top ring plate is 650-750 mm.
9. The cavity extension tool for cold press forming mold according to claim 1, characterized in that: The height of the cylinder is 100-250 mm.