Thermal shock resistant hook brick

By using a multi-layer ceramic fiberboard insulation layer on the hook bricks, the problem of insufficient thermal impact resistance of existing hook bricks is solved, which significantly improves the thermal impact resistance, extends the service life and ensures the safety of the glass kiln .

CN221988398UActive Publication Date: 2024-11-12ZIBO AIJIEXU CORUNDUM MATERIAL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323251126.X
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-11-29
Publication Date
2024-11-12
Estimated Expiration
2033-11-29

Smart Images

  • Figure CN221988398U_ABST
    Figure CN221988398U_ABST
Patent Text Reader

Abstract

The utility model belongs to the technical field of manufacturing of electric smelting refractory materials, and particularly discloses a heat shock resistant hook brick which comprises a brick body, and one end of the brick body is bent downwards to form a hook body. A first heat insulation layer is fixedly connected to the lower side of the brick body, a second heat insulation layer is fixedly connected to the lower side of the hook body, the first heat insulation layer is arranged on one side of the hook body, a third heat insulation layer is fixedly connected to the other side of the hook body, a mounting groove is formed in the side portion of the hook body, and the third heat insulation layer is fixedly connected into the mounting groove; the device is simple in structure and flexible to operate; the first heat insulation layer, the second heat insulation layer and the third heat insulation layer are made of high-temperature-resistant ceramic fiber plates, so that the heat impact resistance is greatly improved; the generation frequency of cracks is effectively reduced, the cracking phenomenon is avoided, and the improvement effect is remarkable.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the technical field of fused refractory material manufacturing, in particular to a heat-shock resistant hook brick. Background Art

[0002] In the height direction of the melting pool of the glass kiln, from bottom to top, there are the pool bottom pavement, pool wall, hook bricks, breast wall and arch. Among them, the hook brick is the key part, which is usually located at the bottom of the breast wall to block the flame in the kiln and prevent the flame from penetrating and burning the breast wall support plate and palm iron.

[0003] The existing Chinese utility model patent with announcement number CN202757425U provides a precast brick for a receiving chute tongue, including a precast brick body, a refractory material is arranged in the precast brick body, an anchor is arranged in the refractory material, the precast brick body is connected to the embedded steel plate through the anchor, the embedded steel plate is connected to the connecting piece, and the precast brick is resistant to erosion, has good wear resistance and high strength after high-temperature treatment; the embedded steel plate protrudes from the body and is welded to the arc-shaped heat-resistant steel casting of the receiving chute, which is firmly fixed and not easy to be eroded and fall off; the heat-resistant steel casting is protected from being exposed to the outside, the oxidation rate of the heat-resistant steel casting is slowed down, and the service life of the refractory lining of the rotary kiln receiving chute tongue is extended, thereby improving the service life of the receiving chute and the equipment operation rate. However, during the use of glass kilns, hook bricks are prone to turning around: for example, when the flame hits the hook brick during the heating process of the kiln; when the hook bricks are repeatedly subjected to temperature changes caused by the reversal of the flame in the glass kiln during the use of float and bottle kilns; when the material pile is too high, it causes erosion on the head of the hook brick, and the hook brick and the pool wall brick are not tightly sealed, allowing external cooling air to enter. If the hook brick turns around, the flame will directly hit the breast wall support plate and the palm iron, causing deformation of the upper structure such as the breast wall and the large arch, and collapse in severe cases. In addition, it was observed that the head of the hook brick in the melting pool of the glass kiln that had been in use for more than ten years was crushed. In order to ensure the safe use of glass kilns, the heat shock resistance of the hook bricks must be improved. Utility Model Content

[0004] Aiming at the problem that the heat shock resistance of hook bricks in the prior art needs to be improved, a heat shock resistant hook brick is proposed.

[0005] The utility model provides the following technical solutions:

[0006] A heat shock resistant hook brick comprises a brick body, one end of which is bent downward to form a hook body; a first insulation layer is fixedly connected to the lower side of the brick body, a second insulation layer is fixedly connected to the lower side of the hook body, the first insulation layer is arranged on one side of the hook body, and a third insulation layer is fixedly connected to the other side of the hook body.

[0007] Preferably, a mounting groove is provided on the side of the hook body, and the third heat insulation layer is fixedly connected in the mounting groove.

[0008] Preferably, the depth of the installation groove is set at 5-15 mm, and the thickness of the third insulation layer is 10-80 mm.

[0009] Preferably, the end surface of the third heat insulation layer is arranged flush with the hook body.

[0010] Preferably, the upper side of the hook body is provided with a chamfer.

[0011] Preferably, the bottom ends of the first thermal insulation layer and the third thermal insulation layer abut against the second thermal insulation layer.

[0012] Preferably, the end surfaces at both ends of the second thermal insulation layer are arranged flush with the outer side surfaces of the first thermal insulation layer and the third thermal insulation layer.

[0013] Preferably, the third thermal insulation layer is a ceramic fiberboard with a temperature above 1600°C.

[0014] Preferably, the second heat insulation layer is a ceramic fiber board or ceramic fiber paper with a temperature above 1500° C. and a thickness of 2-20 mm.

[0015] Preferably, the first heat insulating layer is a ceramic fiber board or ceramic fiber paper with a temperature above 1000° C. and a thickness of 3-30 mm.

[0016] Compared with the prior art, the utility model has the following beneficial effects:

[0017] 1. The utility model has a simple structure and flexible operation;

[0018] 2. The first heat insulation layer, the second heat insulation layer and the third heat insulation layer of the utility model adopt high temperature resistant ceramic fiberboard, and the heat shock resistance is greatly improved;

[0019] 3. The hook brick of the utility model effectively reduces the number of cracks, and no cracking occurs, and the improvement effect is significant. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Figure 1 It is a main structural schematic diagram of the utility model;

[0021] Figure 2 It is a three-dimensional structural schematic diagram of the utility model;

[0022] In the accompanying drawings, 1, brick body; 2, hook body; 3, chamfer; 4, first thermal insulation layer; 5, second thermal insulation layer; 6, third thermal insulation layer. DETAILED DESCRIPTION

[0023] The directional words mentioned in the following embodiments, such as "up", "down", "left", "right", etc., are only referenced to the directions of the drawings. Therefore, the directional words used are used to illustrate rather than limit the invention of the utility model.

[0024] like Figure 1-2 As shown, a heat shock resistant hook brick comprises a brick body 1, one end of the brick body 1 is bent downward to form a hook body 2; a first thermal insulation layer 4 is fixedly connected to the lower side of the brick body 1, a second thermal insulation layer 5 is fixedly connected to the lower side of the hook body 2, the first thermal insulation layer 4 is arranged on one side of the hook body 2, and a third thermal insulation layer 6 is fixedly connected to the other side of the hook body 2, a mounting groove is arranged on the side of the hook body 2, and the third thermal insulation layer 6 is fixedly connected in the mounting groove.

[0025] Specifically, the utility model has an overall length of 365mm, an overall width of 330mm and a thickness of 300mm, a hook body 2 of 330mm in height and 180mm in width; the installation groove is 50mm away from the top of the hook body 2, the depth is set at 10mm, and the cross-section is 130mm*300mm; the thickness of the third insulation layer 6 is 10mm, and the end face of the third insulation layer 6 is set flush with the hook body 2, preferably an alumina, mullite or alumina-mullite ceramic fiberboard. The upper end of the ceramic fiberboard is an inclined structure, and the height difference between the inside and outside is the same as the height difference of the slot of the hook brick body head. The ceramic fiberboard is adhered to the slot position of the hook brick by an adhesive, and the two are tightly matched.

[0026] Specifically, a chamfer 3 is provided on the upper side of the hook body 2 .

[0027] Specifically, the bottom ends of the first thermal insulation layer 4 and the third thermal insulation layer 6 abut against the second thermal insulation layer 5 ; the end surfaces of both ends of the second thermal insulation layer 5 are arranged flush with the outer side surfaces of the first thermal insulation layer 4 and the third thermal insulation layer 6 .

[0028] Specifically, the third heat insulation layer 6 is a ceramic fiberboard with a temperature above 1600°C.

[0029] Specifically, the second heat insulation layer 5 is a ceramic fiber board or ceramic fiber paper with a temperature above 1500° C. and a thickness of 5 mm.

[0030] Specifically, the first heat insulation layer 4 is a ceramic fiber board or ceramic fiber paper with a temperature above 1000° C. and a thickness of 3 mm.

[0031] Specifically, the utility model can be used for masonry after drying. The second insulation layer 5 is horizontally arranged at the lower side, and the third insulation layer 6 faces the inside of the kiln. Multiple heat-shock-resistant hook bricks are arranged in the same layer and connected to each other. A thermal shock test was conducted on the hook bricks with the insulation structure of the utility model and the hook bricks with the usual structure. After the test started, the hook bricks of the two structures were placed in an insulation electric furnace at a temperature of 1100°C, taken out after insulation for 30 minutes, cooled in the air for 10 minutes, and then placed in the insulation electric furnace again. The cycle was repeated 10 times to confirm the number of cracks and collapses of the two samples. The statistical results are as follows:

[0032]

[0033] Compared with the conventional method, the method of the utility model effectively reduces the number of times cracks are generated, and no collapse occurs, and the improvement effect is significant.

Claims

1. A heat shock resistant hook brick, characterized in that: The invention comprises a brick body (1), one end of the brick body (1) being bent downward to form a hook body (2); a first heat insulation layer (4) is fixedly connected to the lower side of the brick body (1), a second heat insulation layer (5) is fixedly connected to the lower side of the hook body (2), the first heat insulation layer (4) is arranged on one side of the hook body (2), and a third heat insulation layer (6) is fixedly connected to the other side of the hook body (2).

2. The heat shock resistant hook brick according to claim 1, characterized in that: The side of the hook body (2) is provided with a mounting groove, and the third heat insulation layer (6) is fixedly connected in the mounting groove.

3. The heat shock resistant hook brick according to claim 2, characterized in that: The depth of the installation groove is set at 5-15 mm, and the thickness of the third heat insulation layer (6) is 10-80 mm.

4. The heat shock resistant hook brick according to claim 2, characterized in that: The end surface of the third heat insulation layer (6) is arranged flush with the hook body (2).

5. The heat shock resistant hook brick according to claim 1, characterized in that: The upper side of the hook body (2) is provided with a chamfer (3).

6. The heat shock resistant hook brick according to claim 1, characterized in that: The bottom ends of the first heat insulation layer (4) and the third heat insulation layer (6) abut against the second heat insulation layer (5).

7. The heat shock resistant hook brick according to claim 1 or 6, characterized in that: The end surfaces at both ends of the second heat insulation layer (5) are arranged flush with the outer side surfaces of the first heat insulation layer (4) and the third heat insulation layer (6).

8. The heat shock resistant hook brick according to claim 1, characterized in that: The third heat insulating layer (6) is a ceramic fiberboard with a temperature of more than 1600°C.

9. The heat shock resistant hook brick according to claim 1, characterized in that: The second heat insulating layer (5) is a ceramic fiber board or ceramic fiber paper with a temperature above 1500°C and a thickness of 2-20 mm.

10. The heat shock resistant hook brick according to claim 1, characterized in that: The first heat insulating layer (4) is a ceramic fiber board or ceramic fiber paper with a temperature above 1000° C. and a thickness of 3-30 mm.