Asphalt pavement pitted surface repairing structure
By setting a combined structure of waterproof layer, interface layer and anti-skid layer on asphalt pavement, and using specific materials to form an effective bond, the structural damage caused by peeling and pitting is solved, and the service life of asphalt pavement is extended.
Patent Information
- Application Number
- CN202420069268.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-11
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2034-01-11
AI Technical Summary
Existing asphalt pavements are prone to developing into potholes due to peeling and pitting damage, leading to structural damage and affecting service quality and lifespan.
It adopts a combination structure of waterproof layer, interface layer, anti-slip layer and rough surface repair layer, using waterproof emulsion acrylic high elastic emulsion, low viscosity polyurethane resin material and anti-slip sand to form an effective bond, prevent water vapor penetration and enhance the bond strength.
It effectively prevents moisture from entering the gaps, enhances bonding strength, extends the service life of asphalt pavement, and solves the structural damage problem caused by peeling and pitting.
Smart Images

Figure CN221989004U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of pavement structures, in particular to a pitted surface repair structure for an asphalt pavement. Background Art
[0002] The main reason for the roughness (peeling) of asphalt pavement is water accumulation. Under the repeated effects of traffic load and temperature expansion and contraction, the moisture on the surface of the asphalt pavement invades the interface between asphalt and aggregate. The asphalt film gradually peels off from the aggregate surface, resulting in insufficient bonding between the aggregates and causing pavement peeling and roughness damage.
[0003] Peeling and roughening of the road surface is a common disease of asphalt pavements. If not treated in time, it will gradually develop into potholes, causing structural damage and seriously affecting the quality and service life of the asphalt pavement. Utility Model Content
[0004] The purpose of the utility model is to provide an asphalt pavement pockmarking repair structure, aiming to solve the technical problem in the prior art that pavement peeling and pockmarking damage is a common disease of asphalt pavements at present. If not handled in time, it will gradually develop into potholes, causing structural damage and seriously affecting the use quality and service life of the asphalt pavement.
[0005] To achieve the above-mentioned purpose, the utility model adopts an asphalt pavement surface repair structure, including an asphalt main layer, a waterproof layer, an interface layer, an anti-skid layer and a pockmarked surface repair layer, the asphalt main layer is the asphalt pavement to be repaired, the waterproof layer is coated on the top of the asphalt main layer to be repaired, the interface layer is arranged on the waterproof layer, and the interface layer penetrates the waterproof layer and penetrates into the gaps in the asphalt main layer, the anti-skid layer is arranged above the interface layer and is located on a side of the interface layer away from the waterproof layer, and the pockmarked surface repair layer is arranged on the anti-skid layer and is located on a side of the anti-skid layer away from the interface layer.
[0006] Wherein, the asphalt pavement pitting repair structure further includes a coating layer, and the coating layer is arranged on a side of the pitting repair layer away from the anti-slip layer.
[0007] Wherein, the asphalt pavement pitted surface repair structure further includes a smoothing layer, and the smoothing layer is arranged on the coating layer and is located on a side of the coating layer away from the pitted surface repair layer.
[0008] Wherein, the waterproof layer is a waterproof emulsion acrylic high elastic emulsion.
[0009] Wherein, the interface layer is an elastic interface layer, and the interface layer is made of a low-viscosity polyurethane resin material.
[0010] Wherein, the anti-skid layer is anti-skid sand.
[0011] Wherein, the mesh size of the anti-slip sand of the anti-slip layer is 15-20 meshes.
[0012] Wherein, the thickness of the pitted surface repair layer is 1mm-1.5mm.
[0013] The utility model discloses an asphalt pavement pitting repair structure. When repairing the asphalt pavement, firstly clean the asphalt main layer, use a fan to blow away the dust in the cracks of the asphalt main layer, and then pour the waterproof layer. The specific steps are: sprinkle the waterproof emulsion acrylic high elastic emulsion on the original asphalt pavement, and the spreading amount is 1.5-2.1kg / m 2 , 20 minutes after pouring the waterproof layer, spread the interface layer, preferably made of low-viscosity polyurethane resin material, with a spreading amount of 1.5-2.1 kg / m 2 , evenly spread 15-20 mesh sand on the interface layer to form the anti-skid layer. After about 2 hours, apply the rough surface repair layer for sealing with a thickness of 1mm-1.5mm to complete the repair of the asphalt main layer. The waterproof layer can effectively prevent water vapor from entering. The interface layer penetrates into the gap of the asphalt main layer and is in complete contact with it. The interface layer has certain flexibility and elasticity in hot and cold environments and has large stretching. The interface layer can increase the bonding strength between the crack wall and the anti-skid layer. In this way, the technical problem that the damage of peeling and rough surface of the road surface in the prior art is a common disease of asphalt pavements, which will gradually develop into potholes if not handled in time, causing structural damage and seriously affecting the use quality and service life of asphalt pavements is solved. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] In order to more clearly illustrate the embodiments of the utility model or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0015] Figure 1 The utility model is a structural schematic diagram of a pitted surface repair structure of an asphalt pavement.
[0016] 1- Asphalt main layer, 2- Waterproof layer, 3- Interface layer, 4- Anti-skid layer, 5- Hemp surface repair layer, 6- Film layer, 7- Smoothing layer. DETAILED DESCRIPTION
[0017] The embodiments of the present invention are described in detail below, and examples of the embodiments are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are intended to be used to explain the present invention, and should not be construed as limiting the present invention.
[0018] See also Figure 1 , Figure 1 It is a structural schematic diagram of an asphalt pavement pitting repair structure of the utility model, and the utility model provides an asphalt pavement pitting repair structure: comprising an asphalt main layer 1, a waterproof layer 2, an interface layer 3, an anti-skid layer 4 and a pitting repair layer 5, wherein the asphalt main layer 1 is an asphalt pavement to be repaired, the waterproof layer 2 is coated on the upper part of the asphalt main layer 1 to be repaired, the interface layer 3 is arranged on the waterproof layer 2, and the interface layer 3 penetrates the waterproof layer 2 and penetrates into the gap of the asphalt main layer 1, the anti-skid layer 4 is arranged on the upper part of the interface layer 3 and is located on the side of the interface layer 3 away from the waterproof layer 2, and the pitting repair layer 5 is arranged on the anti-skid layer 4 and is located on the side of the anti-skid layer 4 away from the interface layer 3;
[0019] The waterproof layer 2 is a waterproof emulsion acrylic high elastic emulsion;
[0020] The interface layer 3 is an elastic interface layer 3, and the interface layer 3 is made of a low-viscosity polyurethane resin material;
[0021] The anti-skid layer 4 is anti-skid sand;
[0022] The mesh size of the anti-slip sand of the anti-slip layer 4 is 15-20 meshes;
[0023] The thickness of the pitted surface repair layer 5 is 1 mm-1.5 mm.
[0024] In this embodiment, when the asphalt pavement is repaired, the asphalt main layer 1 is first cleaned, the dust in the cracks of the asphalt main layer 1 is blown away by a fan, and then the waterproof layer 2 is poured. The specific steps are: the waterproof emulsion acrylic high elastic emulsion is spread on the original asphalt pavement, and the spreading amount is 1.5-2.1 kg / m 2 After pouring the waterproof layer for 220 minutes, spread the interface layer 3, which is preferably made of low-viscosity polyurethane resin material, with a spreading amount of 1.5-2.1 kg / m 2, evenly spread 15-20 mesh sand on the interface layer 3 to form the anti-skid layer 4. After about 2 hours, apply the rough surface repair layer 5 for sealing with a thickness of 1mm-1.5mm to complete the repair of the asphalt main layer 1. The waterproof layer 2 can effectively prevent water vapor from entering. The interface layer 3 penetrates into the gap of the asphalt main layer 1 and is in complete contact with it. The interface layer 3 has certain flexibility and elasticity in both hot and cold environments and has large stretching. The interface layer 3 can increase the bonding strength between the crack wall and the anti-skid layer 4. In this way, the technical problem that the damage of peeling and rough surface of the road surface in the prior art is a common disease of asphalt pavements, which will gradually develop into potholes if not handled in time, causing structural damage and seriously affecting the use quality and service life of asphalt pavements is solved.
[0025] Furthermore, the asphalt pavement roughening repair structure further includes a coating layer 6 , and the coating layer 6 is arranged on a side of the roughening repair layer 5 away from the anti-slip layer 4 .
[0026] In this embodiment, by providing the coating layer 6, after the rough surface repair layer 5 is scraped onto the anti-slip layer 4, the coating layer 6 can protect the rough surface repair layer 5 between the completion of the repair and the putting into use.
[0027] Furthermore, the asphalt pavement roughening repair structure further includes a smoothing layer 7 , and the smoothing layer 7 is disposed on the film layer 6 and is located on a side of the film layer 6 away from the roughening repair layer 5 .
[0028] In this embodiment, by providing the smoothing layer 7 , the coating layer 6 can be evenly covered on the rough surface repairing layer 5 .
[0029] The beneficial effects of the utility model are as follows: the asphalt pavement pitting repair structure of the utility model has a simple and reasonable structure, can effectively overcome the stress in the gap, prevent moisture from penetrating, improve the bonding firmness of the asphalt pavement repair, solve the problems of high cost and short service life of asphalt pavement pitting repair, and has strong practicality.
[0030] The above disclosure is only a preferred embodiment of the present invention, and certainly cannot be used to limit the scope of rights of the present invention. Ordinary technicians in this field can understand that all or part of the processes of the above embodiment and equivalent changes made according to the claims of the present invention still fall within the scope covered by the utility model.
Claims
1. A structure for repairing rough asphalt pavement, characterized in that: It includes an asphalt main layer, a waterproof layer, an interface layer, an anti-skid layer and a pitted surface repair layer, wherein the asphalt main layer is an asphalt pavement to be repaired, the waterproof layer is coated on the top of the asphalt main layer to be repaired, the interface layer is arranged on the waterproof layer, and the interface layer penetrates the waterproof layer and penetrates into the gaps in the asphalt main layer, the anti-skid layer is arranged above the interface layer and is located on a side of the interface layer away from the waterproof layer, and the pitted surface repair layer is arranged on the anti-skid layer and is located on a side of the anti-skid layer away from the interface layer.
2. The asphalt pavement surface repair structure according to claim 1, characterized in that: The asphalt pavement pitting repair structure further comprises a coating layer, and the coating layer is arranged on a side of the pitting repair layer away from the anti-skid layer.
3. The asphalt pavement surface repair structure according to claim 2, characterized in that: The asphalt pavement pitted surface repairing structure also includes a smoothing layer, which is arranged on the film layer and located on a side of the film layer away from the pitted surface repairing layer.
4. The asphalt pavement surface repair structure according to claim 3, characterized in that: The waterproof layer is a waterproof emulsion acrylic high elastic emulsion.
5. The asphalt pavement surface repair structure according to claim 4, characterized in that: The interface layer is an elastic interface layer, and the interface layer is made of a low-viscosity polyurethane resin material.
6. The asphalt pavement surface repair structure according to claim 5, characterized in that: The anti-skid layer is anti-skid sand.
7. The asphalt pavement surface repair structure according to claim 6, characterized in that: The mesh number of the anti-skid sand in the anti-skid layer is 15-20 meshes.