Edge beam structure of energy storage pack water cooling plate
Through laser welding technology, vertical welding joints are used in the side beam of the battery-pack water-cooled plate, which solves the problem of moving the welding direction in the prior art, simplifies the process steps and improves production efficiency and structural strength.
Patent Information
- Application Number
- CN202323566364.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-26
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2033-12-26
AI Technical Summary
The welding direction of the welding point of the existing battery pack water-cooled plate edge beam requires moving the edge beam or welding gun position, which increases the process difficulty and processing steps complexity.
The welding process is simplified by laser welding technology, and the welding direction of the edge beam is connected through the first welding point and the second welding point in the vertical direction. The welding direction of the edge beam is in the vertical direction, without moving the edge beam plate or welding gun position .
The processing steps of edge beams are simplified, welding efficiency and production efficiency are improved, heat-affected zones are reduced, and efficient production and structural strength enhancement are achieved.
Smart Images

Figure CN221994553U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of battery packaging, in particular to a side beam structure of a water cooling plate of an energy storage package. Background Art
[0002] The battery and energy storage pack shell is a device that covers the outside of multiple batteries connected in parallel or in series to protect the batteries. The shell consists of two parts, namely the thicker upper cover and the thinner water-cooling plate. The edge of the water-cooling plate needs to be reinforced with side beams to increase the moment of inertia of the cross section, improve the bending and torsion resistance of the water-cooling plate, and withstand the impact of the external environment on the water-cooling plate.
[0003] There are usually two types of combined structures of side beams and water-cooled plates, namely, the side beams are wrapped around the inside of the edge of the water-cooled plate to form a closed structure, or the water-cooled plate is half-wrapped around the outside of the side beams to form a non-closed structure. The side beams are usually formed by pressing a sheet in one step, and the connected parts of some sheets are fixed by welding. The welding directions of existing side beam welding points include horizontal and vertical directions, which requires moving the side beam position or the welding gun position to adapt to the welding point position, increasing the process difficulty. Utility Model Content
[0004] The purpose of the utility model is to provide a side beam structure of a water cooling plate of an energy storage package to solve the problems raised in the above-mentioned prior art.
[0005] Provided is a side beam structure of a water cooling plate of an energy storage pack, comprising:
[0006] The water-cooling plate comprises a water-cooling plate upper plate, a waterway plate and a water inlet extension plate;
[0007] A side beam, comprising a first connecting section, a first supporting section, a second connecting section, a second supporting section, a third connecting section, an outer frame section, a fourth connecting section, a third supporting section and a fifth connecting section arranged in sequence along a length direction, wherein the first connecting section and the third connecting section are welded to form a first welding point, and the second connecting section and the fifth connecting section are welded to form a second welding point;
[0008] The water inlet extension plate is fitted and fixed to the third connecting section, the water channel plate is fitted and fixed to the fifth connecting section, and the upper plate of the water cooling plate is fitted and fixed to the fourth connecting section.
[0009] Furthermore, a cavity is formed among the first connecting segment, the first supporting segment, the third connecting segment, the outer frame segment and the fourth connecting segment.
[0010] Furthermore, the first welding spot and the second welding spot are formed by laser welding.
[0011] Compared with the prior art, the beneficial effects of the utility model are:
[0012] The first connecting section and the third connecting section are connected by a first welding point in the vertical direction, and the second connecting section and the fifth connecting section are connected by a second welding point in the vertical direction. During the side beam forming process, the welding directions of the welding points are all in the vertical direction. There is no need to move the side beam plate or welding gun to find the welding points, which simplifies the processing steps. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] In order to facilitate understanding by those skilled in the art, the present invention is further described below in conjunction with the accompanying drawings.
[0014] Figure 1 The figure is a schematic diagram of the overall structure of a side beam structure of a water-cooled plate of an energy storage package.
[0015] In the figure: 1. water-cooling plate; 11. upper plate of water-cooling plate; 12. waterway plate; 13. water inlet extension plate; 2. side beam; 21. first connecting section; 22. first supporting section; 23. second connecting section; 24. second supporting section; 25. third connecting section; 26. outer frame section; 27. fourth connecting section; 28. third supporting section; 29. fifth connecting section; 31. first welding point; 32. second welding point; 4. cavity. DETAILED DESCRIPTION
[0016] In order to make the purpose, technical solution and advantages of the utility model more clear, the utility model is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the utility model and are not used to limit the utility model, that is, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. The components of the embodiments of the utility model described and shown in the drawings here can be arranged and designed in various different configurations.
[0017] Therefore, the following detailed description of the embodiments of the utility model provided in the accompanying drawings is not intended to limit the scope of the utility model claimed for protection, but merely represents selected embodiments of the utility model. Based on the embodiments of the utility model, all other embodiments obtained by those skilled in the art without creative work are within the scope of protection of the utility model.
[0018] See also Figure 1As shown, in an embodiment of the utility model, a side beam structure of a water-cooled plate of an energy storage pack includes a water-cooled plate 1 and a side beam 2. The water-cooled plate 1 includes a water-cooled plate upper plate 11, a waterway plate 12 and a water inlet extension plate 13. The side beam 2 includes a first connecting segment 21, a first supporting segment 22, a second connecting segment 23, a second supporting segment 24, a third connecting segment 25, an outer frame segment 26, a fourth connecting segment 27, a third supporting segment 28 and a fifth connecting segment 29 which are sequentially arranged along the length direction. A first welding point 31 is formed by welding between the first connecting segment 21 and the third connecting segment 25, a second welding point 32 is formed between the second connecting segment 23 and the fifth connecting segment 29, the water inlet extension plate 13 is fitted and fixed to the third connecting segment 25, the waterway plate 12 is fitted and fixed to the fifth connecting segment 29, and the water-cooled plate upper plate 11 is fitted and fixed to the fourth connecting segment 27.
[0019] The upper plate 11 of the water-cooled plate is used to install the battery pack, and the waterway plate 12 covers the side of the upper plate 11 of the water-cooled plate away from the battery pack. A bulge is formed on the surface of the waterway plate 12, and a connecting cavity is formed between the upper plate 11 of the water-cooled plate for circulating coolant. The water inlet extension plate 13 is in the shape of a long strip, and a plurality of water inlet extension plates 13 cover the side of the waterway plate 12 away from the upper plate 11 of the water-cooled plate, which is used to strengthen the connection stability of the waterway plate 12 and enhance the overall strength of the water-cooled plate 1.
[0020] The side beam 2 is divided into two parts by the first connecting section 21 and the first supporting section 22. The part away from the water-cooling plate 1 provides a mounting platform for the water-cooling plate upper plate 11, and the part close to the water-cooling plate 1 provides a mounting platform for the waterway plate 12 and the water inlet extension plate 13. The first welding point 31 and the second welding point 32 connect the two parts by welding to increase the structural strength and stability. The first supporting section 22 acts as a reinforcing rib to improve the deformation resistance of the side beam 2.
[0021] The first welding spot 31 and the second welding spot 32 are formed by laser welding. Laser welding has excellent positioning and welding accuracy, produces a very small heat-affected zone, has almost no thermal deformation, and generally has a high welding speed, which can achieve efficient production. In addition, laser welding also has deep welding capabilities and can be used to weld thicker materials without multiple operations.
[0022] When manufacturing the side beam 2, starting from the third connecting section 25, the third connecting section 25 and the second supporting section 24 are pressed to form an inflection point, the second supporting section 24 and the second connecting section 23 are pressed to form an inflection point, the second connecting section 23 and the first supporting section 22 are pressed to form an inflection point, and the first supporting section 22 and the first connecting section 21 are pressed to form an inflection point. When the first connecting section 21 overlaps with the third connecting section 25, a laser welding gun is used to align the welding point for welding to form a first welding point 31. Then the outer frame section 26 and the third connecting section 25 form an inflection point, the outer frame section 26 and the fourth connecting section 27 form an inflection point, the fourth connecting section 27 and the third supporting section 28 form an inflection point, and the third supporting section 28 and the fifth connecting section 29 form an inflection point. When the fifth connecting section 29 overlaps with the second connecting section 23, a laser welding gun is used to align the welding point for welding to form a second welding point 32.
[0023] When welding the first welding point 31 and the second welding point 32, since the welding directions of the two welding points are both in the vertical direction, there is no need to move the position of the plate or the position of the welding gun to find the welding point after pressing the plate. A single laser welding gun can complete the processing by continuous welding in one direction, which simplifies the process steps and improves the processing efficiency.
[0024] A cavity 4 is formed between the first connecting segment 21 , the first supporting segment 22 , the third connecting segment 25 , the outer frame segment 26 and the fourth connecting segment 27 , which can provide a buffer when the side beam 2 is impacted and reduce the deformation degree of the side beam 2 .
[0025] The above contents are merely examples and explanations of the structure of the utility model. The technicians in this technical field may make various modifications or additions to the specific embodiments described or replace them in a similar manner. As long as they do not deviate from the structure of the utility model or exceed the scope defined in the claims, they should all fall within the protection scope of the utility model.
Claims
1. A side beam structure of a water-cooled plate of an energy storage package, characterized in that: include: A water-cooling plate (1), comprising a water-cooling plate upper plate (11), a waterway plate (12) and a water inlet extension plate (13); A side beam (2), comprising a first connecting section (21), a first supporting section (22), a second connecting section (23), a second supporting section (24), a third connecting section (25), an outer frame section (26), a fourth connecting section (27), a third supporting section (28) and a fifth connecting section (29) which are sequentially arranged along a length direction, wherein the first connecting section (21) and the third connecting section (25) are welded to form a first welding point (31), and the second connecting section (23) and the fifth connecting section (29) are welded to form a second welding point (32); The water inlet extension plate (13) is fitted and fixed to the third connecting section (25), the water channel plate (12) is fitted and fixed to the fifth connecting section (29), and the water cooling plate upper plate (11) is fitted and fixed to the fourth connecting section (27).
2. The side beam structure of the water cooling plate of the energy storage pack according to claim 1 is characterized in that: A cavity (4) is formed between the first connecting section (21), the first supporting section (22), the third connecting section (25), the outer frame section (26) and the fourth connecting section (27).