Civil air defense engineering protective door with anti-corrosion structure

By using reinforcement layers, buffer layers, fire-proof layers and corrosion-proof layers in civil defense engineering protective doors, combined with epoxy resin and ceramic anti-corrosion coatings, the corrosion problem of protective doors is solved, extending service life and improving aesthetics.

CN222010020UActive Publication Date: 2024-11-15SUQIAN HONGTAI INTELLIGENT MFG TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420486496.7
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-13
Publication Date
2024-11-15
Estimated Expiration
2034-03-13

AI Technical Summary

Technical Problem

Since the existing civil defense engineering protective doors are mainly metal, they are prone to corrosion after long-term use, which affects normal use and aesthetics.

Method used

Anti-corrosion components including reinforcement layer, buffer layer, fire layer and corrosion protection layer are adopted, combined with epoxy resin coating and ceramic anti-corrosion coating to enhance the corrosion resistance of the protective door.

Benefits of technology

Effectively prevent corrosion of protective doors, extend service life and improve aesthetics, and solves the corrosion problem of metal protective doors after long-term use.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222010020U_ABST
    Figure CN222010020U_ABST
Patent Text Reader

Abstract

The utility model relates to a civil air defense construction protective door with an anti-corrosion structure, which comprises a door frame and a protective door body arranged on the door frame, a door lock for controlling the protective door body to open and close is arranged on the front side of the protective door body, and the protective door body comprises a door body base layer, an anti-corrosion assembly and a heat preservation assembly. According to the civil air defense engineering protective door with the anti-corrosion structure, the first anti-corrosion layer and the second anti-corrosion layer are arranged in the civil air defense engineering protective door with the anti-corrosion structure, epoxy resin coating is selected as the material of the first anti-corrosion layer, and meanwhile ceramic anti-corrosion coating is selected as the material of the second anti-corrosion layer; by utilizing the excellent anti-corrosion performance of the epoxy resin coating and the ceramic anti-corrosion coating, the anti-corrosion performance of the protective door for the civil air defense engineering is improved, the protective door for the civil air defense engineering is prevented from being corroded in the using process, the service life of the protective door for the civil air defense engineering is prolonged, and the attractiveness of the protective door for the civil air defense engineering is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of civil air defense engineering, in particular to a civil air defense engineering protective door with an anti-corrosion structure. Background Art

[0002] Civil air defense projects, also known as civil air defense fortifications, refer to underground protective buildings built separately to ensure the shelter of personnel and materials, civil air defense command, and medical rescue in wartime, as well as basements that can be used for air defense in wartime built in combination with ground buildings. Protective doors are indispensable facilities in civil air defense projects. Protective doors are doors that can withstand various shock waves or collisions of heavy objects. They are generally made of steel materials. Protective doors can be opened on one side or on both sides. In order to firmly fix the protective doors to the building, most protective doors are opened on one side.

[0003] Chinese patent CN217925585U discloses a civil air defense project protective door with an impact-resistant composite structure, including a door frame and a protective frame, wherein the protective frame is arranged in the door frame, a protective door is arranged in the protective frame, an impact-resistant pressure relief buffer mechanism is arranged between the protective door and the protective frame, and the impact-resistant pressure relief buffer mechanism includes an air cylinder, a piston plate, a buffer airbag and a dispersed buffer component, which belongs to the technical field of civil air defense project protective doors, and specifically refers to a civil air defense project protective door with an impact-resistant composite structure, which can effectively buffer and relieve the impact force on the outer panel of the protective door, and avoid the strong impact of the shock wave and damage the protective door.

[0004] The above patent prevents the shock wave from generating a strong impact and damaging the protective door. However, during the use of the protective door of the civil air defense project, since the material of the protective door is mostly metal, the problem of corrosion of the protective door is not taken into consideration. After long-term use, the protective door will be corroded, affecting the normal use and aesthetics of the protective door. Therefore, a civil air defense project protective door with a corrosion-resistant structure is proposed to solve the above problem. Utility Model Content

[0005] In view of the shortcomings of the prior art, the utility model provides a civil air defense project protective door with an anti-corrosion structure, which has the advantage of good anti-corrosion performance and solves the problem that during the use of the civil air defense project protective door, the material of the protective door is mostly metal, and the corrosion of the protective door is not taken into consideration. After long-term use, the protective door will be corroded, affecting the normal use and aesthetics of the protective door.

[0006] To achieve the above object, the utility model provides the following technical solution: a civil air defense engineering protective door with an anti-corrosion structure, comprising a door frame and a protective door body arranged on the door frame, characterized in that: a door lock for controlling the opening and closing of the protective door body is arranged on the front of the protective door body;

[0007] The protective door body comprises a door body base, an anti-corrosion component and a heat preservation component, wherein the anti-corrosion component is arranged on the back of the door body base, and the heat preservation component is arranged on the front of the door body base;

[0008] The anti-corrosion component includes a reinforcing layer, a buffer layer, a fireproof layer and a first anti-corrosion layer. The reinforcing layer is fixed on the back of the door body base layer, the buffer layer is fixed on the back of the reinforcing layer, the fireproof layer is fixed on the back of the buffer layer, and the first anti-corrosion layer is fixed on the back of the fireproof layer.

[0009] Furthermore, the reinforcement layer is composed of concrete and steel mesh, and the buffer layer is a polyurethane foam plastic layer.

[0010] Furthermore, the fireproof layer is a fireproof gypsum board layer, and the first anti-corrosion layer is an epoxy resin coating layer.

[0011] Furthermore, the thickness of the door body base layer is greater than the thickness of the reinforcement layer, and the thickness of the door body base layer is greater than the thickness of the first anti-corrosion layer.

[0012] Furthermore, the thermal insulation component includes a thermal insulation layer, a sound insulation layer and a second anti-corrosion layer, the thermal insulation layer is fixed on the front side of the door body base layer, the sound insulation layer is fixed on the front side of the thermal insulation layer, and the second anti-corrosion layer is fixed on the front side of the sound insulation layer.

[0013] Furthermore, the thermal insulation layer is a foamed cement layer, and the sound insulation layer is a sound insulation cotton layer.

[0014] Furthermore, the second anti-corrosion layer is a ceramic anti-corrosion coating layer.

[0015] Compared with the prior art, the technical solution of this application has the following beneficial effects:

[0016] The civil air defense project protection door with an anti-corrosion structure is provided with a first anti-corrosion layer and a second anti-corrosion layer. Epoxy resin paint is selected as the material of the first anti-corrosion layer, and ceramic anti-corrosion paint is selected as the material of the second anti-corrosion layer. The excellent anti-corrosion properties of epoxy resin paint and ceramic anti-corrosion paint are utilized to improve the anti-corrosion properties of the civil air defense project protection door itself, prevent the civil air defense project protection door from being corroded during use, extend the service life of the civil air defense project protection door, improve the aesthetics of the civil air defense project protection door, and solve the problem that the protection door is mostly made of metal and the corrosion of the protection door is not taken into consideration during use. After long-term use, the protection door will be corroded, affecting the normal use and aesthetics of the protection door. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 It is a schematic diagram of the structure of the utility model;

[0018] Figure 2 This is a left view of the protective door structure of the utility model;

[0019] Figure 3 This is a left view of the anti-corrosion component of the utility model;

[0020] Figure 4 It is the left view of the thermal insulation component of the utility model.

[0021] In the figure: 1 door frame, 2 protective door body, 21 door body base layer, 22 anti-corrosion component, 221 reinforcement layer, 222 buffer layer, 223 fireproof layer, 224 first anti-corrosion layer, 23 insulation component, 231 insulation layer, 232 sound insulation layer, 233 second anti-corrosion layer, 3 door lock. DETAILED DESCRIPTION

[0022] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0023] See also Figure 1-2 In this embodiment, a civil air defense protection door with a corrosion-resistant structure includes a door frame 1 and a protection door body 2 arranged on the door frame 1, and a door lock 3 for controlling the opening and closing of the protection door body 2 is arranged on the front of the protection door body 2.

[0024] The protective door body 2 includes a door body base layer 21 , an anti-corrosion component 22 and a heat preservation component 23 . The anti-corrosion component 22 is arranged on the back side of the door body base layer 21 , and the heat preservation component 23 is arranged on the front side of the door body base layer 21 .

[0025] It should be noted that the components of the present application are all universal standard parts or components known to those skilled in the art, and their structures and principles can be known to those skilled in the art through technical manuals or conventional experimental methods.

[0026] See also Figure 3-4 In order to improve the anti-corrosion performance of the protective door of the civil air defense project, the anti-corrosion component 22 in this embodiment includes a reinforcing layer 221, a buffer layer 222, a fireproof layer 223 and a first anti-corrosion layer 224. The reinforcing layer 221 is fixed on the back of the door body base layer 21, the buffer layer 222 is fixed on the back of the reinforcing layer 221, the fireproof layer 223 is fixed on the back of the buffer layer 222, and the first anti-corrosion layer 224 is fixed on the back of the fireproof layer 223.

[0027] The reinforcing layer 221 is composed of concrete and steel mesh. After the concrete and the steel mesh are combined, the overall strength of the protective door body 2 is improved. At the same time, the concrete and the steel mesh have excellent compressive resistance and good durability after being combined, so that the protective door body 2 can maintain structural stability and strength in various environments. The buffer layer 222 is a polyurethane foam plastic layer. Polyurethane foam plastic has good elasticity and is an excellent buffer material, which improves the buffering performance of the protective door body 2 itself.

[0028] The fireproof layer 223 is a fireproof gypsum board layer, which has good fireproof performance and can also prevent the generation and spread of smoke. The first anti-corrosion layer 224 is an epoxy resin paint layer, which has excellent chemical resistance, especially alkali resistance.

[0029] The thickness of the door body base layer 21 is greater than the thickness of the reinforcement layer 221 , and the thickness of the door body base layer 21 is greater than the thickness of the first anti-corrosion layer 224 .

[0030] The insulation component 23 includes an insulation layer 231 , a sound insulation layer 232 and a second anti-corrosion layer 233 . The insulation layer 231 is fixed on the front side of the door base layer 21 , the sound insulation layer 232 is fixed on the front side of the insulation layer 231 , and the second anti-corrosion layer 233 is fixed on the front side of the sound insulation layer 232 .

[0031] The thermal insulation layer 231 is a foamed cement layer, the sound insulation layer 232 is a sound insulation cotton layer, and the second anti-corrosion layer 233 is a ceramic anti-corrosion coating layer. The ceramic anti-corrosion coating has low surface energy, high corrosion resistance, high hardness, and excellent anti-corrosion, anti-fouling, wear resistance and high temperature resistance properties, which are unmatched by traditional anti-corrosion materials.

[0032] The working principle of the above embodiment is:

[0033] (1) The reinforcing layer 221 is made of a combination of concrete and steel mesh. The combination of concrete and steel mesh improves the overall strength of the protective door body 2. At the same time, the combination of concrete and steel mesh has excellent compressive resistance and good durability, so that the protective door body 2 can maintain structural stability and strength in various environments. The buffer layer 222 is made of polyurethane foam plastic material. Polyurethane foam plastic has good elasticity and is a high-performance buffer material. It improves the buffering performance of the protective door body 2 itself, so that the protective door body 2 can withstand impact force. The fireproof layer 223 is made of fireproof gypsum board. The fireproof gypsum board has good fireproof performance and can also prevent the generation and spread of smoke.

[0034] (2) The first anti-corrosion layer 224 is made of epoxy resin paint. Epoxy resin paint has excellent chemical resistance, especially alkali resistance. At the same time, epoxy resin paint has excellent adhesion, especially on metal surfaces, which improves the anti-corrosion performance of the protective door body 2, prevents the civil air defense project protective door from being corroded, and increases the service life. The thermal insulation layer 231 is made of foamed cement material. Foamed cement has good thermal insulation, heat preservation, sound insulation and light load-bearing properties, which can improve the thermal insulation performance of the protective door body 2. The sound insulation layer 232 is made of sound insulation cotton material. The sound insulation cotton can effectively block noise and improve the sound insulation performance of the civil air defense project protective door. The second anti-corrosion layer 233 uses ceramic anti-corrosion coating. Ceramic anti-corrosion coating is a new type of anti-corrosion coating material. It adopts advanced nanotechnology and ceramic materials, utilizes network interpenetrating film-forming technology, and adds nano-silicon powder, silicon carbide, boron nitride, fine-crystalline alumina, graphite, ultrafine zinc oxide, titanium oxide, ceramic microbeads and zirconium oxide and other nano-powders. The interaction and synergistic effect working principle of the various components of the coating make the coating have low surface energy, high corrosion resistance, high hardness, and excellent anti-corrosion, anti-fouling, wear resistance and high temperature resistance. It is incomparable to traditional anti-corrosion materials and improves the anti-corrosion performance of the protective door body 2.

[0035] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the sentence "comprise a ..." do not exclude the existence of other identical elements in the process, method, article or device including the elements.

[0036] Although the embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that many changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention.

Claims

1. A civil air defense protection door with an anti-corrosion structure, comprising a door frame (1) and a protection door body (2) arranged on the door frame (1), characterized in that: A door lock (3) for controlling the opening and closing of the protective door body (2) is arranged on the front side of the protective door body (2); The protective door body (2) comprises a door body base layer (21), an anti-corrosion component (22) and a heat-insulating component (23), wherein the anti-corrosion component (22) is arranged on the back side of the door body base layer (21), and the heat-insulating component (23) is arranged on the front side of the door body base layer (21); The anti-corrosion component (22) comprises a reinforcing layer (221), a buffer layer (222), a fireproof layer (223) and a first anti-corrosion layer (224); the reinforcing layer (221) is fixed on the back side of the door body base layer (21); the buffer layer (222) is fixed on the back side of the reinforcing layer (221); the fireproof layer (223) is fixed on the back side of the buffer layer (222); and the first anti-corrosion layer (224) is fixed on the back side of the fireproof layer (223).

2. The air defense door with corrosion-resistant structure according to claim 1, characterized in that: The reinforcement layer (221) is composed of concrete and steel mesh, and the buffer layer (222) is a polyurethane foam plastic layer.

3. The air defense door with corrosion-resistant structure according to claim 1, characterized in that: The fireproof layer (223) is a fireproof gypsum board layer, and the first anti-corrosion layer (224) is an epoxy resin coating layer.

4. The air defense door with corrosion-resistant structure according to claim 1, characterized in that: The thickness of the door body base layer (21) is greater than the thickness of the reinforcement layer (221), and the thickness of the door body base layer (21) is greater than the thickness of the first anti-corrosion layer (224).

5. The air defense door with corrosion-resistant structure according to claim 1, characterized in that: The thermal insulation component (23) comprises a thermal insulation layer (231), a sound insulation layer (232) and a second anti-corrosion layer (233); the thermal insulation layer (231) is fixed on the front side of the door base layer (21); the sound insulation layer (232) is fixed on the front side of the thermal insulation layer (231); and the second anti-corrosion layer (233) is fixed on the front side of the sound insulation layer (232).

6. The air defense door with anti-corrosion structure according to claim 5, characterized in that: The thermal insulation layer (231) is a foamed cement layer, and the sound insulation layer (232) is a sound insulation cotton layer.

7. The air defense door with anti-corrosion structure according to claim 5, characterized in that: The second anti-corrosion layer (233) is a ceramic anti-corrosion coating layer.