Plastic mould for solving silk-screen bottom penetration

By partially covering tape on the surface of the plastic mold cavity to form patterns of different roughnesses, the problem of silk screen bottom-permeability is solved, the effect of silk screen bottom-permeability is achieved, and the production cost and time is reduced.

CN222022021UActive Publication Date: 2024-11-19SHENZHEN YIHENG IND TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323616169.3
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-28
Publication Date
2024-11-19
Estimated Expiration
2033-12-28

AI Technical Summary

Technical Problem

When processing plastic products, the silk screen printing area caused by the existing plastic mold is too smooth, resulting in the ink not being fully covered, resulting in the problem of silk screen printing bottoming. The existing solutions require secondary local processing of mass-produced plastic products, which is time-consuming and labor-intensive. High cost.

Method used

Design a plastic mold, wherein the mold cavity surface is partially covered with adhesive tape to form a pattern with different roughness, including one area and two areas, the roughness of the first area is smaller than the second area, and a predetermined formation is formed by sandblasting and chemical etching treatment. The pattern is made to ensure that the ink is fully covered in the silk screen printing area.

Benefits of technology

The effect of silk screen printing is achieved without bottoming, while reducing production processes and costs, avoiding secondary local processing of mass-produced plastic products, and reducing production costs and time.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222022021U_ABST
    Figure CN222022021U_ABST
Patent Text Reader

Abstract

A plastic mold for solving silk-screen bottom penetration comprises a mold cavity, the mold cavity is used for processing a plastic product, the plastic product is provided with a concave part, the concave part of the plastic product is provided with a silk-screen area, the mold cavity is provided with a convex part, the convex part corresponds to the concave part, the convex part comprises a first area and a second area, and the first area and the second area are arranged on the first area. The first area corresponds to the screen printing area, the second area surrounds the first area, the first area and the second area are located on the same horizontal plane, and the roughness of the first area is smaller than that of the second area. The silk-screen area can be independently provided with a preset pattern surface which enables the ink to completely cover, so that the plastic product cannot be integrally over a smooth surface to cause light reflection, the requirement that the silk-screen area is not transparent to the bottom is met, and the problem that the silk-screen is transparent to the bottom is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of injection mold cavities, in particular to a plastic mold for solving the problem of bottom see-through in silk screen printing. Background Art

[0002] The main surface treatments for mold cavities include sandblasting, polishing, chemical etching, etc. In order to achieve a predetermined surface effect for plastic parts, it is usually necessary to perform special process treatments on the surface of the plastic mold cavity. For example, chemical etching treatment on the surface of the mold cavity refers to corroding the cavity surface of the plastic molding mold to form a predetermined texture. After the plastic product is formed by this mold, the surface of the plastic product has the corresponding texture. Sandblasting treatment on the surface of the mold cavity refers to spraying quartz sand at high speed onto the surface of the mold cavity through air compression to form a layer of frosted surface. After the plastic product is formed by this mold, the surface of the plastic product will also have the corresponding texture.

[0003] If the overall surface of the plastic product is too smooth, it will cause excessive reflection, so the mold cavity needs to adopt a rougher texture. However, if the mold cavity adopts a rougher texture as a whole, after the plastic product is formed by this mold, the silk screen printing area of ​​the plastic product will also form a corresponding rough texture. After silk screen printing, due to the deep texture of the rough texture, the ink may not be able to completely cover the texture of the silk screen printing area, resulting in the problem of the bottom of the silk screen printing area being transparent. Usually, the way to solve this problem in the industry is to add several processes and perform secondary surface treatment on the local area of ​​the plastic products that have been mass-produced from the mold, so that the surface texture of the silk screen printing area of ​​the plastic product is smoother than the overall surface texture of the plastic product, so that the ink can completely cover the texture of the silk screen printing area, and achieve the effect of silk screen printing not being transparent. However, this treatment method requires all plastic products mass-produced from the mold to be partially surface-treated one by one, which is obviously time-consuming, labor-intensive, and costly. Therefore, a plastic mold that solves the problem of silk screen bottom transparency is urgently needed. Utility Model Content

[0004] In view of this, a plastic mold is provided which can reduce the number of processes, lower the production cost, save time and labor, and solve the problem of bottom see-through in silk screen printing.

[0005] In order to achieve the above purpose, the technical solution adopted by the utility model is:

[0006] A plastic mold for solving the problem of silk-screen bottom see-through includes a mold cavity, the mold cavity is used to process a plastic product, the plastic product has a concave portion, the concave portion of the plastic product is provided with a silk-screen area, the mold cavity has a convex portion, the convex portion corresponds to the concave portion, the convex portion includes a first area and a second area, the first area corresponds to the silk-screen area, the second area surrounds the first area, the first area and the second area are located in the same horizontal plane, and the roughness of the first area is less than the roughness of the second area.

[0007] Furthermore, the roughness of the first area and the second area is achieved by partially covering the convex surface of the mold cavity with tape and then subjecting it to surface treatment respectively, the tape comprising a first tape and a second tape, the first tape being used to cover the first area, and the second tape being used to cover the second area.

[0008] Furthermore, the industry standard surface texture model adopted in the first area is YS20043B, and the industry standard surface texture model adopted in the second area is MT11020.

[0009] Furthermore, both the first region and the second region have predetermined textures formed by secondary surface treatment.

[0010] Furthermore, the first region has a predetermined surface texture formed by two sandblasting processes.

[0011] Furthermore, the second region has a predetermined textured surface formed by chemical etching and then sandblasting.

[0012] Furthermore, the adhesive tape is a single-sided adhesive tape, and the sticky surface of the adhesive tape is in contact with the corresponding area of ​​the mold cavity.

[0013] Furthermore, when the adhesive tape is adhered, it is positioned by the outer edge of the protrusion.

[0014] Furthermore, the shape of the first adhesive tape is consistent with the outer contour shape of the first region, and the edge of the first adhesive tape is flush with the edge of the first region.

[0015] Furthermore, the outer edge of the second adhesive tape is flush with the edge of the protrusion, and a through hole is opened inside the second adhesive tape. The shape and size of the through hole are consistent with the shape and size of the first area, and the position of the through hole corresponds to the position of the first area.

[0016] Compared with the prior art, the utility model has at least the following beneficial effects:

[0017] Since the convex surface of the mold cavity is partially covered with tape, when the mold cavity surface is treated, various preset textures with different roughness can be formed on the convex surface, and the convex portion corresponds to the concave portion of the plastic product, and the first area of ​​the convex portion corresponds to the silk-screen area of ​​the concave portion. After the plastic product is formed by this mold cavity, the silk-screen area can be separately provided with a predetermined texture that is completely covered by ink, so that the plastic product will not be too glossy as a whole to cause reflection, and meet the requirement of silk-screen printing not being transparent. Compared with conventional methods in the industry, this mold that solves the problem of silk-screen printing being transparent can obtain plastic products that meet the requirements in batches after the mold is opened, and there is no need to re-perform secondary local surface treatment one by one, which will greatly reduce the production cost, and there is no need to add secondary processing steps after the mold is opened, saving time and effort. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] In the attached picture:

[0019] Figure 1 The utility model is an overall schematic diagram of a plastic mold for solving the problem of bottom see-through in silk screen printing.

[0020] Figure 2 The utility model is a partially enlarged schematic diagram of part A of a plastic mold for solving the problem of bottom see-through of silk screen printing.

[0021] in,

[0022] 1. Mold cavity; 2. Plastic product; 3. Protrusion; 4. First area; 5. Second area. DETAILED DESCRIPTION

[0023] The technical solution of the utility model will be described clearly and completely below in conjunction with the accompanying drawings. Obviously, the described embodiments are part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments of the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0024] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installation", "connection" and "connection" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0025] The present invention will be described in detail below with reference to specific embodiments and accompanying drawings.

[0026] See also Figure 1-2, showing a plastic mold for solving the problem of silk-screen bottom see-through provided by an embodiment of the utility model, comprising a mold cavity 1, wherein the mold cavity 1 is used for processing a plastic product 2, wherein the plastic product 2 has a concave portion, wherein the concave portion of the plastic product 2 is provided with a silk-screen area, and the mold cavity 1 has a convex portion 3, wherein the convex portion 3 corresponds to the concave portion, wherein the convex portion 3 comprises a first area 4 and a second area 5, wherein the first area 4 corresponds to the silk-screen area, wherein the second area 5 surrounds the first area 4, wherein the first area 4 and the second area 5 are located on the same horizontal plane, and wherein the roughness of the first area 4 is less than that of the second area 5.

[0027] Specifically, the roughness of the first area 4 and the second area 5 is achieved by partially covering the surface of the convex portion 3 of the mold cavity 1 with tape and then subjecting them to surface treatment respectively, the tape comprising a first tape and a second tape, the first tape being used to cover the first area 4, and the second tape being used to cover the second area 5.

[0028] More specifically, the industry standard surface texture model adopted in the first area 4 is YS20043B, and the industry standard surface texture model adopted in the second area 5 is MT11020.

[0029] In some specific embodiments, the texture model MT11020 will not make the overall plastic product 2 too glossy and cause reflection, and the texture model YS20043B will not make the silk-screen area too rough and cause bottom transparency. The texture models MT11020 and YS20043B are preferred, and other texture models that meet the requirements can also be selected.

[0030] More specifically, both the first region 4 and the second region 5 have predetermined textures formed by secondary surface treatment.

[0031] More specifically, the first region 4 has a predetermined surface texture formed by two sandblasting processes.

[0032] More specifically, the second region 5 has a predetermined textured surface formed by chemical etching and then sandblasting.

[0033] In some specific embodiments, the first adhesive tape is first used to cover the first area 4, and the second area 5 is not covered. At this time, chemical etching is used, that is, the second area 5 is subjected to surface chemical etching to obtain a predetermined rough surface; then, the first adhesive tape is removed, and the second adhesive tape is used to cover the second area 5, and the first area 4 is not covered. At this time, sandblasting is used, that is, the first area 4 is subjected to surface sandblasting to obtain a predetermined smooth surface; finally, the second adhesive tape is removed, and the first area 4 and the second area 5 are not covered. At this time, sandblasting is used, that is, the first area 4 and the second area 5 are subjected to surface sandblasting to make the overall surface harmonious and unified, with only different depths. Obviously, the first area 4 is subjected to two sandblasting treatments to form a predetermined surface, and the second area 5 is subjected to chemical etching and then sandblasting to form a predetermined surface. This embodiment is preferred, and the predetermined surface can also be formed by other methods.

[0034] Specifically, the adhesive tape is a single-sided adhesive tape, and the sticky surface of the adhesive tape is in contact with the corresponding area of ​​the convex portion 3 of the mold cavity 1 .

[0035] More specifically, when the adhesive tape is pasted, it is positioned by the outer edge of the protrusion 3 .

[0036] Specifically, the shape of the first adhesive tape is consistent with the outer contour of the first region 4 , and the edge of the first adhesive tape is flush with the edge of the first region 4 .

[0037] Specifically, the outer edge of the second adhesive tape is flush with the edge of the protrusion 3 , and a through hole is opened inside the second adhesive tape. The shape and size of the through hole are consistent with the shape and size of the first area 4 , and the position of the through hole corresponds to the position of the first area 4 .

[0038] In summary, since the surface of the convex portion 3 of the mold cavity 1 is partially covered with adhesive tape, when the mold cavity 1 is surface treated, the surface of the convex portion 3 can form various preset textures with different roughness, the convex portion 3 corresponds to the concave portion of the plastic product 2, and the first area 4 of the convex portion 3 corresponds to the silk-screen area of ​​the concave portion. After the plastic product 2 is formed by this mold cavity 1, the silk-screen area can be separately provided with a predetermined texture that is completely covered by ink, so that the plastic product 2 will not be too glossy as a whole to cause reflection, and meet the requirement of silk-screen printing not being transparent. Compared with conventional methods in the industry, this mold that solves the problem of silk-screen printing being transparent can obtain plastic products 2 that meet the requirements in batches after the mold is opened, and there is no need to take them one by one for secondary local surface treatment again, which will greatly reduce the production cost, and there is no need to add secondary processing steps after the mold is opened, saving time and effort.

[0039] The above embodiments are only for illustrating the technical concept and features of the utility model, and their purpose is to enable people familiar with the technology to understand the content of the utility model and implement it accordingly, and they cannot be used to limit the protection scope of the utility model. Any equivalent changes or modifications made according to the spirit of the utility model should be included in the protection scope of the utility model.

Claims

1. A plastic mold for solving the problem of bottom see-through of silk screen printing, comprising a mold cavity, the mold cavity is used to process a plastic product, the plastic product has a concave portion, the concave portion of the plastic product is provided with a silk screen printing area, characterized in that: The mold cavity has a convex portion, which corresponds to the concave portion. The convex portion includes a first area and a second area. The first area corresponds to the silk-screen printing area, and the second area surrounds the first area. The first area and the second area are located in the same horizontal plane, and the roughness of the first area is less than that of the second area.

2. A plastic mold for solving the problem of bottom see-through in silk screen printing according to claim 1, characterized in that: The roughness of the first area and the second area is achieved by partially covering the convex surface of the mold cavity with tape and then subjecting it to surface treatment respectively. The tape includes a first tape and a second tape. The first tape is used to cover the first area, and the second tape is used to cover the second area.

3. A plastic mold for solving the problem of bottom see-through in silk screen printing according to claim 1, characterized in that: The industry standard surface pattern adopted in the first area is YS20043B, and the industry standard surface pattern adopted in the second area is MT11020.

4. A plastic mold for solving the problem of bottom see-through in silk screen printing according to claim 1, characterized in that: The first region and the second region both have predetermined textures formed by secondary surface treatment.

5. A plastic mold for solving the problem of bottom see-through in silk screen printing according to claim 1, characterized in that: The first region has a predetermined surface texture formed by two sandblasting processes.

6. A plastic mold for solving the problem of bottom see-through in silk screen printing according to claim 1, characterized in that: The second area has a predetermined textured surface formed by chemical etching and then sandblasting.

7. A plastic mold for solving the problem of bottom see-through in silk screen printing according to claim 2, characterized in that: The adhesive tape is a single-sided adhesive tape, and the sticky surface of the adhesive tape is in contact with the corresponding area of ​​the mold cavity.

8. A plastic mold for solving the problem of bottom see-through in silk screen printing according to claim 7, characterized in that: When the adhesive tape is pasted, it is positioned by the outer edge of the protrusion.

9. A plastic mold for solving the problem of bottom see-through in silk screen printing according to claim 2, characterized in that: The shape of the first adhesive tape is consistent with the outer contour of the first region, and the edge of the first adhesive tape is flush with the edge of the first region.

10. A plastic mold for solving the problem of bottom see-through in silk screen printing according to claim 2, characterized in that: The outer edge of the second adhesive tape is flush with the edge of the protrusion, and a through hole is opened inside the second adhesive tape. The shape and size of the through hole are consistent with the shape and size of the first area, and the position of the through hole corresponds to the position of the first area.