Protective film for PVD (Physical Vapor Deposition) film coating

By introducing the bending-resistant part and high-temperature-resistant layer composed of unit texture into the PVD coating protective film, the problems of insufficient curling and bending resistance of the PET substrate at high temperatures are solved, and the high-temperature resistance and bonding of the protective film are improved, ensuring that Coating quality.

CN222024293UActive Publication Date: 2024-11-19JIANGYIN TONGLI OPTOELECTRONICS TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323611817.6
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-28
Publication Date
2024-11-19
Estimated Expiration
2033-12-28

AI Technical Summary

Technical Problem

In the existing PVD coating process, the commonly used PET substrate protective film is prone to curling under high temperature environments, and has insufficient bending and corrosion resistance, which cannot effectively protect the edges of the substrate surface.

Method used

A protective film for PVD coating is designed, which uses a bend-resistant part composed of unit textures. The adjacent unit textures can be reunited or separated, which enhances the tightness of the curved surface fitting with the object to be pasted, and is connected through high-temperature resistance layer and bonding. The contact area of ​​the layer increases, which improves the bonding force between layers, improves high temperature resistance and structural stability.

Benefits of technology

有效改善了基材的硬度和耐高温性,防止起翘现象,提高了保护膜的贴合力和稳定性,确保镀层品质。

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222024293U_ABST
    Figure CN222024293U_ABST
Patent Text Reader

Abstract

The utility model discloses a protective film for PVD (Physical Vapor Deposition) film coating, which comprises a base material layer provided with a first surface and a second surface which are opposite to each other along the film thickness direction; the high-temperature-resistant layer is arranged on the first surface and / or the second surface and is connected with the base material layer through an adhesive layer; the high-temperature-resistant bonding layer is connected with the base material layer or the high-temperature-resistant layer; the first surface and / or the second surface are / is provided with a bending-resistant part, the bending-resistant part comprises unit textures which extend in the first direction and are arranged side by side, and the adjacent unit textures are arranged at intervals. The protective film for PVD film coating is reasonable in structure, adjacent unit textures are close to or separated from each other through the bending-resistant part composed of the unit textures, so that the protective film is more tightly attached to the curved surface of an attached object, and the problems that a base material is not resistant to bending due to high hardness and upwarps after being heated at a high temperature are solved; the contact area between the high-temperature-resistant layer and the high-temperature-resistant bonding layer is also increased, the bonding force between the layers is improved, and the high-temperature resistance and the structural stability of the protective film are further improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of film coating, in particular to a protective film for PVD film coating. Background Art

[0002] PVD (physical vapor deposition) is a physical vapor phase reaction growth method. The physical vapor deposition process is to transfer the source material to the substrate surface to form a solid coating after "evaporation or sputtering" under vacuum or low-pressure gas discharge conditions. PVD coating is widely used and can provide corrosion protection, decoration, hardness improvement, optical effects and medical fields.

[0003] The PVD coating process usually prepares a film layer on a substrate, and a protective film is needed to protect the non-deposition surface of the substrate during this process. The PVD coating process requires a long period of high-temperature baking, and the protective film needs to meet the requirements of high temperature resistance, corrosion resistance, and no residual adhesive after peeling. The surface of the substrate can be flat or uneven, such as a curved surface. The commonly used PET (polyethylene terephthalate) as a substrate protective film has poor flexibility and is prone to warping in high temperature environments, and cannot effectively protect the edge of the substrate surface.

[0004] Therefore, it is necessary to improve the protective film for PVD coating in the prior art. Utility Model Content

[0005] The purpose of the utility model is to overcome the defects existing in the prior art and provide a protective film for PVD coating. Through the bending-resistant part composed of unit textures, adjacent unit textures are close to or separated, so as to achieve a closer fit with the curved surface of the object to be adhered, improve the problem that the substrate itself is hard and not resistant to bending and warping after high temperature heating; it also increases the contact area with the high temperature resistant layer and the high temperature resistant adhesive layer, improves the bonding strength between layers, and further improves the high temperature resistance and structural stability of the protective film.

[0006] In order to achieve the above technical effects, the technical solution of the utility model is: a protective film for PVD coating, comprising:

[0007] A substrate layer having a first surface and a second surface opposite to each other in a film thickness direction;

[0008] A high temperature resistant layer, disposed on the first surface and / or the second surface, and connected to the substrate layer via an adhesive layer;

[0009] A high temperature resistant adhesive layer connected to the substrate layer or connected to the high temperature resistant layer;

[0010] The first surface and / or the second surface is provided with a bending-resistant portion, and the bending-resistant portion includes unit textures extending along a first direction and arranged in parallel, and adjacent unit textures are arranged at intervals.

[0011] A preferred technical solution is that the cross section of the anti-bending portion along the first direction is sawtooth-shaped.

[0012] A preferred technical solution is that the high temperature resistant layer is polyimide or a composite layer containing polyimide.

[0013] A preferred technical solution is that the high temperature resistant layer is polyimide, or is a laminated structure of polyimide / thermoplastic polyimide, or polyimide / thermoplastic polyimide / polyimide, and the thermoplastic polyimide is close to the substrate layer.

[0014] A preferred technical solution is that the substrate layer is polyethylene terephthalate.

[0015] A preferred technical solution is that the adhesive layer is a high temperature resistant pressure sensitive adhesive.

[0016] A preferred technical solution is that the high temperature resistant adhesive layer is an acrylic pressure-sensitive adhesive.

[0017] A preferred technical solution is that a release film is provided on the surface of the high temperature resistant adhesive layer away from the substrate layer.

[0018] The preferred technical solution is that the thickness of the substrate layer is 15 to 30 μm, the thickness of the high temperature resistant layer is 10 to 30 μm, the thickness of the high temperature resistant adhesive layer is 5 to 10 μm, and the thickness of the glue layer is 5 to 10 μm.

[0019] The advantages and beneficial effects of the utility model are:

[0020] The protective film for PVD coating has a reasonable structure. By setting the bending-resistant part on the first surface and / or the second surface of the substrate layer, the adjacent unit textures are brought closer or separated, thereby achieving a closer fit with the curved surface of the object to be adhered, and improving the problem that the substrate itself is hard and not resistant to bending and warping after being heated at high temperature.

[0021] The bending-resistant part composed of unit textures increases the contact area with the high-temperature resistant layer and the high-temperature resistant adhesive layer, improves the bonding force between the layers, and further improves the high-temperature resistance and structural stability of the protective film. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 This is a schematic diagram of the structure of Embodiment 1 of the protective film for PVD coating of the utility model;

[0023] Figure 2 It is a schematic structural diagram of Example 2 of the protective film for PVD coating of the utility model.

[0024] In the figure: 1, substrate layer; 2, high temperature resistant layer; 3, high temperature resistant adhesive layer; 4, release film; 10, bending resistant part; 100, unit texture; 12, adhesive layer; 21, polyimide layer; 22, thermoplastic polyimide layer; 101, first surface; 102, second surface. DETAILED DESCRIPTION

[0025] The following is a further description of the specific implementation of the present invention in conjunction with the accompanying drawings and embodiments. The following embodiments are only used to more clearly illustrate the technical solution of the present invention, and cannot be used to limit the protection scope of the present invention.

[0026] “Inside” and “outside” are referenced to the normal use state of the protective film for PVD coating, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.

[0027] In addition, the terms "first", "second", etc. are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, a feature defined as "first", "second", etc. may explicitly or implicitly include one or more of the features. In the description of the invention of the utility model, unless otherwise specified, the meaning of "plurality" is two or more.

[0028] like Figures 1-2 As shown, the utility model discloses a protective film for PVD coating, comprising a substrate layer 1, a high temperature resistant layer 2 and a high temperature resistant adhesive layer 3, wherein the substrate layer 1 has a first surface 101 and a second surface 102 opposite to each other along the film thickness direction; the high temperature resistant layer 2 is arranged on the first surface 101 and / or the second surface 102, and is connected to the substrate layer 1 through a glue layer 12; the high temperature resistant adhesive layer 3 is connected to the substrate layer 1 or to the high temperature resistant layer 2.

[0029] The first surface 101 is an outer surface, and the second surface 102 is an inner surface, wherein the outer surface refers to the surface facing the outside air.

[0030] like Figure 1 As shown, in some embodiments, the protective film is a laminated structure: the high temperature resistant layer 2 is connected to the first surface 101 of the substrate layer 1 through the glue layer 12, and the high temperature resistant adhesive layer 3 is arranged on the second surface 102 of the substrate layer 1.

[0031] In some embodiments, the protective film is a stacked structure two: the high temperature resistant layer 2 is connected to the second surface 102 of the substrate layer 1 through the adhesive layer 12, and the high temperature resistant adhesive layer 3 is arranged on the surface of the high temperature resistant layer 2 away from the substrate layer 1. Compared with the stacked structure two under high temperature processing environment, the surface flatness of the protective film is more stable.

[0032] like Figure 2 As shown, in some embodiments, the protective film is a laminated structure three: the high temperature resistant layer 2 is connected to the first surface 101 and the second surface 102 of the substrate layer 1 through the adhesive layer 12, and the high temperature resistant adhesive layer 3 is arranged on the surface of the high temperature resistant layer 2 away from the substrate layer 1. The laminated structure three has many processing steps and many layers stacked, but has the best high temperature resistance and can be suitable for scenes with more stringent high temperature requirements.

[0033] The first surface 101 and / or the second surface 102 is provided with a bending-resistant portion 10, and the bending-resistant portion 10 includes unit textures 100 extending and arranged in parallel along a first direction, and adjacent unit textures 100 are arranged at intervals. Further, the cross section of the bending-resistant portion 10 along the first direction is sawtooth-shaped. The first direction is an arbitrary direction, and for the convenience of processing and production, the first direction is the horizontal or vertical direction of the substrate layer 1. Grooves are formed between adjacent unit textures 100, and the sawtooth-shaped grooves are fine and precise. The first surface 101 is provided with a bending-resistant portion 10. When the protective film is attached to a concave object, the protective film is in a bent state, and the adjacent unit textures 100 are close to each other, not squeezed but can be abutted, and the grooves are in a closed state, which overcomes the problem of micro-wrinkles when the protective film is bent due to its high hardness and poor toughness, so as not to affect the flatness of the edge of the protective film, thereby affecting the quality of the coating; similarly, when attached to a convex object, the protective film is also in a bent state, and the adjacent unit textures 100 are separated, and the grooves are in an open state, so that the protective film is more closely attached to the attached object, and can also overcome the problem of micro-wrinkles when the protective film is bent due to its high hardness and poor toughness. Similarly, the second surface 102 is provided with a bending-resistant portion 10. The first surface 101 and the second surface 102 are provided with a bending-resistant portion 10, which can improve the problem of micro-wrinkles when the protective film is bent due to its high hardness and poor toughness, and prevent the protective film from being loosely bonded and having a negative impact on the quality of the coating.

[0034] The substrate layer 1 is polyethylene terephthalate, the high temperature resistant adhesive layer 3 is an acrylic pressure sensitive adhesive, and the adhesive layer 12 is a high temperature resistant pressure sensitive adhesive. Furthermore, the adhesive layer 12 is also an acrylic pressure sensitive adhesive, and the polymeric main body of the acrylic pressure sensitive adhesive includes a soft monomer, a hard monomer, a modified monomer and a heat resistant monomer. By optimizing the formulation of the polymeric main body, an adhesive film with high adhesion and durability is obtained, and stable adhesion is formed at a high stability.

[0035] Thermosetting polymers refer to polymer materials that can solidify or have insoluble (melting) properties under heat or other conditions, have high chemical resistance and heat resistance, as well as high strength structure and are not easy to deform. Thermoplastic polymers refer to plastic polymer materials that become flexible or plastic when the temperature rises to a certain level, and solidify after cooling, usually providing the composite layer with high strength, flexibility and shrinkage resistance. Furthermore, the high temperature resistant layer 2 is polyimide or a composite layer containing polyimide.

[0036] In some embodiments, the high temperature resistant layer 2 is a single layer of polyimide.

[0037] In some embodiments, the high temperature resistant layer 2 is a laminated structure of polyimide / thermoplastic polyimide, and the thermoplastic polyimide 22 is close to the substrate layer.

[0038] like Figure 2 As shown, in some embodiments, the high temperature resistant layer 2 is a stacked structure of polyimide / thermoplastic polyimide / polyimide.

[0039] The high temperature resistant layer 2 in which the polyimide layer 21 and the thermoplastic polyimide layer 22 are alternately arranged improves the bending property and dimensional stability of the protective film.

[0040] A release film 4 is disposed on the surface of the high temperature resistant adhesive layer 3 away from the substrate layer 1 .

[0041] The thickness of the substrate layer 1 is 15-30 μm, the thickness of the high temperature resistant layer 2 is 10-30 μm, the thickness of the high temperature resistant adhesive layer 3 is 5-10 μm, and the thickness of the glue layer 12 is 5-10 μm.

[0042] Example 1

[0043] like Figure 1 As shown, the protective film includes a substrate layer 1, a high temperature resistant layer 2, a high temperature resistant adhesive layer 3 and a release film 4. The protective film is a laminated structure 1: the high temperature resistant layer 2 is connected to the first surface 101 of the substrate layer 1 through the adhesive layer 12, the high temperature resistant adhesive layer 3 is arranged on the second surface 102 of the substrate layer 1, and the first surface 101 is provided with a bending-resistant portion 10. Among them, the high temperature resistant layer 2 is a laminated structure of polyimide / thermoplastic polyimide / polyimide. The release film 4 is covered on the surface of the high temperature resistant adhesive layer 3. The layer thickness of the substrate layer 1 is 20μm, the thickness of the polyimide layer 21 is 7μm, the thickness of the thermoplastic polyimide layer 22 is 7μm, the thickness of the high temperature resistant adhesive layer 3 is 7μm, and the thickness of the adhesive layer 12 is 7μm.

[0044] Example 2

[0045] like Figure 2As shown, Example 2 is based on Example 1, except that the protective film has a laminated structure three: the high temperature resistant layer 2 is connected to the first surface 101 and the second surface 102 of the substrate layer 1 through the adhesive layer 12, and the high temperature resistant adhesive layer 3 is arranged on the surface of the high temperature resistant layer 2 away from the substrate layer 1. The first surface 101 and the second surface 102 are both provided with a bending resistant portion 10. The high temperature resistant layer 2 close to the first surface 101 has a laminated structure of polyimide / thermoplastic polyimide / polyimide; the high temperature resistant layer 2 close to the second surface 102 has a laminated structure of polyimide.

[0046] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the technical principle of the present invention. These improvements and modifications should also be regarded as the protection scope of the present invention.

Claims

1. A protective film for PVD coating, include: A substrate layer having a first surface and a second surface opposite to each other in a film thickness direction; A high temperature resistant layer, disposed on the first surface and / or the second surface, and connected to the substrate layer via an adhesive layer; A high temperature resistant adhesive layer connected to the substrate layer or connected to the high temperature resistant layer; It is characterized in that the first surface and / or the second surface is provided with a bending-resistant portion, and the bending-resistant portion includes unit textures extending along a first direction and arranged in parallel, and adjacent unit textures are arranged at intervals.

2. The protective film for PVD coating according to claim 1, It is characterized in that The cross section of the bending-resistant portion along the first direction is sawtooth-shaped.

3. The protective film for PVD coating according to claim 1, It is characterized in that The high temperature resistant layer is polyimide or a composite layer containing polyimide.

4. The protective film for PVD coating according to claim 3, It is characterized in that The high temperature resistant layer is polyimide, or is a laminated structure of polyimide / thermoplastic polyimide, or polyimide / thermoplastic polyimide / polyimide, and the thermoplastic polyimide is close to the substrate layer.

5. The protective film for PVD coating according to claim 3 or 4, It is characterized in that The substrate layer is polyethylene terephthalate.

6. The protective film for PVD coating according to claim 5, It is characterized in that The adhesive layer is a high temperature resistant pressure sensitive adhesive.

7. The protective film for PVD coating according to claim 1, It is characterized in that The high temperature resistant adhesive layer is an acrylic pressure sensitive adhesive.

8. The protective film for PVD coating according to claim 7, It is characterized in that A release film is disposed on the surface of the high temperature resistant adhesive layer away from the substrate layer.

9. The protective film for PVD coating according to claim 1, It is characterized in that The thickness of the substrate layer is 15 to 30 μm, the thickness of the high temperature resistant layer is 10 to 30 μm, the thickness of the high temperature resistant adhesive layer is 5 to 10 μm, and the thickness of the glue layer is 5 to 10 μm.