Fiber reinforced aluminum alloy structure

By adding fiber reinforced layer and structural glue layer between aluminum alloy profiles, the aluminum alloy fiber composite structure is formed, the problem of insufficient compressive strength of aluminum alloy profiles is solved, the structural strength and mechanical properties are improved, and it is suitable for lightweight new energy vehicles Quantitative design.

CN222039853UActive Publication Date: 2024-11-22WUHU HAICHENG RUBBER & PLASTIC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420538648.3
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-20
Publication Date
2024-11-22
Estimated Expiration
2034-03-20

AI Technical Summary

Technical Problem

The performance of aluminum alloy profiles is poor in compressive strength, which leads to rapid deformation of the structure after being subjected to stress, affecting structural performance. Especially in the design of beams in new energy vehicles, there is a problem of insufficient energy absorption effect.

Method used

The fiber-reinforced aluminum alloy structure is adopted. By adding an internal fiber-reinforced layer and structural glue layer between the outer layer and the inner aluminum alloy profile, an aluminum alloy fiber composite structure is formed to improve structural strength while maintaining the advantages of lightweight design.

Benefits of technology

It effectively improves the compressive strength and overall mechanical properties of the aluminum alloy structure, reduces weight gain, is suitable for lightweight automotive designs, and enhances the stability and performance of the structure.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222039853U_ABST
    Figure CN222039853U_ABST
Patent Text Reader

Abstract

The utility model discloses a fiber reinforced aluminum alloy structure, which comprises an aluminum alloy section bar and an internal fiber reinforced layer, the aluminum alloy section bar comprises a hollow outer layer aluminum alloy section bar and an inner layer aluminum alloy section bar, the inner layer aluminum alloy section bar is arranged inside the outer layer aluminum alloy section bar, and the fiber reinforced layer is arranged inside the inner layer aluminum alloy section bar. And the internal fiber reinforced layer is compounded between the outer-layer aluminum alloy section and the inner-layer aluminum alloy section. The fiber reinforced aluminum alloy is reasonable in structural design, the internal fiber reinforced layer is compounded between the outer-layer aluminum alloy profile and the inner-layer aluminum alloy profile, so that an aluminum alloy fiber composite structure is formed, the structural strength of the composite structure is effectively improved, the weight increase is relatively small, and the design of a lightweight automobile is facilitated.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of aluminum alloy profiles, in particular to a fiber-reinforced aluminum alloy structure. Background Art

[0002] At present, aluminum alloy profiles are light in weight, which is conducive to lightweight design of products. Many beams in new energy vehicles are made of aluminum alloy profiles. Aluminum alloy materials have good tensile strength, but poor mechanical properties such as compressive strength. When aluminum alloy pipes are subjected to stress, the surface deforms and the entire structure will deform rapidly, affecting the structural performance.

[0003] For example, Chinese patent CN211809482U discloses an aluminum alloy front collision beam assembly and a car to solve the problem that the aluminum alloy front collision beam assembly in the prior art has poor energy absorption effect under the conditions of optimal weight and optimal cost; the aluminum alloy front collision beam assembly comprises: a front collision beam body made of aluminum alloy material; collision energy absorption boxes respectively installed at both ends of the front collision beam body; the front collision beam body is a hollow aluminum alloy profile structure, and the surface is easily deformed when subjected to force. Utility Model Content

[0004] In view of the shortcomings of the prior art, the utility model provides a fiber-reinforced aluminum alloy structure to achieve the purpose of improving the structural strength.

[0005] In order to solve the above technical problems, the technical solution adopted by the utility model is:

[0006] The fiber-reinforced aluminum alloy structure includes an aluminum alloy profile and an internal fiber-reinforced layer. The aluminum alloy profile includes a hollow outer aluminum alloy profile and an inner aluminum alloy profile. The inner aluminum alloy profile is located inside the outer aluminum alloy profile, and the internal fiber-reinforced layer is composited between the outer aluminum alloy profile and the inner aluminum alloy profile.

[0007] Further:

[0008] It also includes an internal structural adhesive layer, and the internal fiber reinforcement layer is compounded between the outer aluminum alloy profile and the inner aluminum alloy profile through the internal structural adhesive.

[0009] The thickness of the outer aluminum alloy profile and the inner aluminum alloy profile are both in the range of 0.5-10 mm.

[0010] The inner fiber reinforcement layer is a fiber cloth layer.

[0011] Internal structural adhesive layers are provided on both the inner and outer sides of the internal fiber reinforced layer.

[0012] The thickness of the internal structural adhesive layer is in the range of 0.5-5 mm.

[0013] The thickness of the fiber cloth layer is in the range of 0.5-5 mm.

[0014] The fiber cloth layer is carbon fiber cloth, glass fiber cloth or basalt fiber cloth.

[0015] Compared with the prior art, the utility model has the following advantages:

[0016] The fiber-reinforced aluminum alloy structure is reasonably designed, with an internal fiber reinforcement layer compounded between an outer aluminum alloy profile and an inner aluminum alloy profile, thereby forming an aluminum alloy fiber composite structure, which effectively improves the structural strength of the composite structure, and the weight increase is relatively small, which is conducive to lightweight automobile design. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] The following is a brief description of the contents and symbols in the drawings of this specification:

[0018] Figure 1 It is a schematic diagram of the main structure of the utility model.

[0019] Figure 2 For along Figure 1 AA cross-sectional view.

[0020] Figure 3 for Figure 2 Enlarged schematic diagram of the aluminum alloy structure corner.

[0021] In the figure:

[0022] 1. Outer aluminum alloy profile, 2. Inner aluminum alloy profile, 3. Internal fiber reinforcement layer, 4. Internal structural adhesive layer. DETAILED DESCRIPTION

[0023] The specific implementation of the utility model will be further explained in detail below through the description of embodiments with reference to the accompanying drawings.

[0024] like Figures 1 to 3 As shown, the fiber reinforced aluminum alloy structure includes an aluminum alloy profile and an internal fiber reinforcement layer 3 and an internal structural adhesive layer 4; the aluminum alloy profile includes a hollow outer aluminum alloy profile 1 and an inner aluminum alloy profile 2, the inner aluminum alloy profile is located inside the outer aluminum alloy profile, that is, the outer aluminum alloy profile is sleeved on the inner aluminum alloy profile.

[0025] The internal fiber reinforced layer 3 is compounded between the outer aluminum alloy profile and the inner aluminum alloy profile. Further, the internal fiber reinforced layer is compounded between the outer aluminum alloy profile and the inner aluminum alloy profile through an internal structural adhesive.

[0026] In the utility model, an internal fiber reinforcement layer is compounded between the outer aluminum alloy profile and the inner aluminum alloy profile, thereby forming an aluminum alloy fiber composite structure, which effectively improves the structural strength of the composite structure, and the weight increase is relatively small, which is conducive to lightweight automobile design.

[0027] Preferably, the thickness of the outer aluminum alloy profile 1 and the inner aluminum alloy profile 2 are both in the range of 0.5-10 mm; the thickness of the internal structural adhesive layer is in the range of 0.5-5 mm.

[0028] Furthermore, internal structural adhesive layers 4 are provided on both the inner and outer sides of the internal fiber reinforced layer 3; that is, an internal structural adhesive layer is provided between the outer side of the internal fiber reinforced layer and the inner wall of the outer aluminum alloy profile, and an internal structural adhesive layer is also provided between the inner side of the internal fiber reinforced layer and the outer side of the inner aluminum alloy profile.

[0029] Preferably, the internal fiber reinforcement layer is a fiber cloth layer; the thickness of the fiber cloth layer ranges from 0.5 to 5 mm; the fiber cloth layer is carbon fiber cloth, glass fiber cloth or basalt fiber cloth.

[0030] like Figure 3 As shown, further, the corners of the outer aluminum alloy profile and the inner aluminum alloy profile are both arc transitions, which is beneficial to improving the structural strength.

[0031] The fiber-reinforced material of the utility model is compounded into the middle of the aluminum alloy, thereby enhancing the mechanical properties of the aluminum alloy and can be used for lightweight design of machinery, vehicles and the like.

[0032] The above is only an explanation of the preferred embodiments of the present invention. The above technical features can be arbitrarily combined to form multiple embodiments of the present invention.

[0033] The utility model is described above by way of example in conjunction with the accompanying drawings. It is obvious that the specific implementation of the utility model is not limited to the above-mentioned method. As long as various non-substantial improvements are made using the concept and technical solution of the utility model, or the concept and technical solution of the utility model are directly applied to other occasions without improvement, they are all within the protection scope of the utility model.

Claims

1. A fiber-reinforced aluminum alloy structure, comprising an aluminum alloy profile, characterized in that: It also includes an internal fiber reinforced layer. The aluminum alloy profile includes a hollow outer aluminum alloy profile and an inner aluminum alloy profile. The inner aluminum alloy profile is located inside the outer aluminum alloy profile, and the internal fiber reinforced layer is composited between the outer aluminum alloy profile and the inner aluminum alloy profile.

2. The fiber-reinforced aluminum alloy structure according to claim 1, characterized in that: It also includes an internal structural adhesive layer, and the internal fiber reinforcement layer is compounded between the outer aluminum alloy profile and the inner aluminum alloy profile through the internal structural adhesive.

3. The fiber-reinforced aluminum alloy structure according to claim 1, characterized in that: The thickness of the outer aluminum alloy profile and the inner aluminum alloy profile are both in the range of 0.5-10 mm.

4. The fiber-reinforced aluminum alloy structure according to claim 1, characterized in that: The inner fiber reinforcement layer is a fiber cloth layer.

5. The fiber-reinforced aluminum alloy structure according to claim 2, characterized in that: Internal structural adhesive layers are provided on both the inner and outer sides of the internal fiber reinforced layer.

6. The fiber-reinforced aluminum alloy structure according to claim 2, characterized in that: The thickness of the internal structural adhesive layer is in the range of 0.5-5 mm.

7. The fiber-reinforced aluminum alloy structure according to claim 4, characterized in that: The thickness of the fiber cloth layer is in the range of 0.5-5 mm.

8. The fiber-reinforced aluminum alloy structure according to claim 4, characterized in that: The fiber cloth layer is carbon fiber cloth, glass fiber cloth or basalt fiber cloth.