Power device with high-reliability packaging structure
By setting an epoxy adhesive encapsulation layer with a small thermal expansion coefficient on the copper-clad ceramic substrate, the warping and deformation problem caused by thermal expansion of the copper-clad ceramic substrate is solved, and the reliability of the welding layer and the service life of the power device are improved.
Patent Information
- Application Number
- CN202420685423.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-03
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2034-04-03
AI Technical Summary
The copper-clad ceramic substrate is warped and deformed during the thermal expansion, resulting in fatigue fracture of the sintered layer between the chip and the copper-clad ceramic substrate, and the welding layer between the copper-clad ceramic substrate and the radiator, reducing the reliability of the power device. and service life.
Epoxy glue with a small thermal expansion coefficient is used as the packaging layer to cover one side of the chip of the copper ceramic substrate and bond it to form a whole to resist the stress deformation caused by heat of the copper ceramic substrate and reduce the risk of fatigue and fracture of the welding layer.
It effectively reduces the warping deformation of the copper-clad ceramic substrate, improves the reliability of the welding layer, ensures the thermal conductivity of the copper-clad ceramic substrate, reduces the risk of failure of power devices, and extends the service life.
Smart Images

Figure CN222051744U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of semiconductor packaging, in particular to a power device with a high-reliability packaging structure. Background Art
[0002] As the number of chips packaged in high-power devices increases, the operating temperature of power devices also increases. The copper-clad ceramic substrate plays a key role in the heat dissipation path of the power module. The heat of the chip is first transferred to the copper-clad ceramic substrate and then to the heat sink, and finally the heat is taken away by the coolant.
[0003] Copper-clad ceramic substrate is a composite material composed of copper and ceramic. Due to the large difference in thermal expansion coefficients between the layers of material, the copper-clad ceramic substrate will generate internal stress during thermal expansion. The stress will cause the copper-clad ceramic substrate to warp and deform, and the degree of deformation will increase with the increase in temperature. The deformation of the copper-clad ceramic substrate will cause fatigue fracture in the sintering layer between the chip and the copper-clad ceramic substrate, and the welding layer between the copper-clad ceramic substrate and the heat sink, destroying the heat dissipation path of the power module, reducing the thermal conductivity of the copper-clad ceramic substrate, and increasing the risk of failure of the power device, which is not conducive to improving the reliability of the power device and reduces the service life of the power device. Utility Model Content
[0004] The utility model provides a power device with a high-reliability packaging structure, which reduces the warping deformation of the copper-clad ceramic substrate during thermal expansion, reduces the risk of fatigue fracture of the sintering layer between the chip and the copper-clad ceramic substrate, and the welding layer between the copper-clad ceramic substrate and the radiator, and improves the reliability and service life of the power device.
[0005] In order to achieve the above purpose, the utility model adopts the following technical solutions:
[0006] A power device with a high reliability packaging structure, comprising:
[0007] A copper-clad ceramic substrate, comprising an upper copper layer, an aluminum nitride ceramic layer and a lower copper layer, wherein the aluminum nitride ceramic layer is arranged between the upper copper layer and the lower copper layer, the aluminum nitride ceramic layer separates the upper copper layer and the lower copper layer, the upper copper layer is located above the lower copper layer, and a chip is arranged on one side of the upper copper layer;
[0008] The encapsulation layer has a preset thickness and is arranged on the upper surface of the copper-clad ceramic substrate. The encapsulation layer covers a side of the copper-clad ceramic substrate on which a chip is provided. The encapsulation layer and the copper-clad ceramic substrate are bonded to form a whole, wherein the thermal expansion coefficient of the encapsulation layer is lower than the thermal expansion coefficient of copper in the copper-clad ceramic substrate.
[0009] In some embodiments, the encapsulation layer is made of epoxy glue.
[0010] In some embodiments, a heat sink is further included. The heat sink is disposed on the lower surface of the copper layer under the substrate, and the heat sink is connected to the copper-clad ceramic substrate.
[0011] In some embodiments, the heat sink includes a plurality of heat dissipation columns, and a preset gap is provided between the plurality of heat dissipation columns.
[0012] In some embodiments, a plurality of circuit grooves are provided on the copper layer on the substrate, and the plurality of circuit grooves penetrate the copper layer on the substrate, and the plurality of circuit grooves divide the copper layer on the substrate into a plurality of regions.
[0013] In some embodiments, the plurality of line grooves are interconnected, and one end or both ends of the plurality of line grooves extend to the edge of the copper-clad ceramic substrate.
[0014] In some embodiments, a shell is further included, wherein the shell is connected to the heat sink, the shell is arranged along the side of the copper-clad ceramic substrate to form a packaging cavity, and the epoxy glue is arranged with the packaging cavity to form the packaging layer.
[0015] In some embodiments, a welding layer is provided between the copper-clad ceramic substrate and the heat sink, and the welding layer connects the copper layer under the substrate to the heat sink.
[0016] Compared with the prior art, the beneficial effects brought by the utility model are:
[0017] The present application sets a packaging layer with a small thermal expansion coefficient and a large modulus, sets it on the copper layer on the copper-clad ceramic substrate, covers one side of the copper-clad ceramic substrate where the chip is set, and bonds the packaging layer to the copper-clad ceramic substrate to form a whole, so that when the copper-clad ceramic substrate expands due to heat, the packaging layer resists the stress deformation generated by the heat of the copper-clad ceramic substrate, avoids fatigue fracture of the sintering layer between the chip and the copper-clad ceramic substrate, and the welding layer between the copper-clad ceramic substrate and the heat sink, improves the reliability of the solder, ensures the thermal conductivity of the copper-clad ceramic substrate, reduces the failure risk of power devices, and increases the service life of power devices.
[0018] Additional aspects and advantages of the present application will be partially given in the following description, which will become apparent from the following description, or will be understood through the practice of the present application. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 It is a cross-sectional view of a power device with a high reliability packaging structure of the utility model;
[0020] Figure 2 This is a schematic diagram of a power device packaging structure with a high reliability packaging structure of the utility model;
[0021] Figure 3 It is a partial cross-sectional view of a power device with a high reliability packaging structure of the utility model; DETAILED DESCRIPTION
[0022] The present application is further described in detail below in conjunction with specific drawings. In the description of this embodiment, unless otherwise specified, the terms "left", "right", etc. indicate directions or positional relationships based on the directions or positional relationships shown in the drawings, which are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the present application must have a specific direction, be constructed and operated in a specific direction, and therefore cannot be understood as limiting the present application.
[0023] like Figure 1 As shown, a power device with a high reliability packaging structure provided by the utility model mainly includes a copper-clad ceramic substrate 2 and a packaging layer 5. Specifically, as Figure 2 As shown, the copper-clad ceramic substrate 2 includes a copper layer 21 on the substrate, an aluminum nitride ceramic layer 22 and a copper layer 23 under the substrate, the aluminum nitride ceramic layer 22 is arranged between the copper layer 21 on the substrate and the copper layer 23 under the substrate, the aluminum nitride ceramic layer 22 separates the copper layer 21 on the substrate and the copper layer 23 under the substrate, the copper layer 21 on the substrate is located above the copper layer 23 under the substrate, and a chip 1 is provided on one side of the copper layer 21 on the substrate; the packaging layer 5 has a preset thickness, the packaging layer 5 is arranged on one side of the copper-clad ceramic substrate 2, the packaging layer 5 covers the side of the copper-clad ceramic substrate 2 on which the chip 1 is provided, and the packaging layer 5 and the copper-clad ceramic substrate 2 are bonded to form a whole, wherein the thermal expansion coefficient of the packaging layer 5 is lower than the thermal expansion coefficient of the copper-clad ceramic substrate 2. In this embodiment, by providing a packaging layer 5 with a small thermal expansion coefficient and a large modulus, a reverse force can be applied to one side of the copper-clad ceramic substrate 2, thereby preventing the welding layer 3 between the copper-clad ceramic substrate 2 and the heat sink 6 from fatigue fracture due to excessive stress during thermal expansion of the copper-clad ceramic substrate 2, thereby improving the reliability of the solder, reducing the risk of failure of the power device, and ensuring the service life of the power device.
[0024] Furthermore, the encapsulation layer 5 is made of epoxy glue. Epoxy glue has low stress, high temperature resistance (150-200°C), and high bending strength (90-150Mpa). Specifically, when making the encapsulation layer 5, liquid epoxy glue is laid on the surface of the copper-clad ceramic substrate 2. More specifically, the epoxy glue is laid on the copper-clad ceramic substrate 2 with the chip on one side to cover the chip 1. After the epoxy glue is cooled and formed, the epoxy glue and the copper-clad ceramic substrate 2 are bonded to form a whole. Since the thermal expansion coefficient of the epoxy glue is small and the bending strength is high, when the chip 1 continues to work and generates high temperature, the encapsulation layer 5 composed of epoxy glue will have a reverse force on the contact surface of the copper-clad ceramic substrate 2 to suppress the stress deformation caused by the heat of the copper-clad ceramic substrate 2. The two offset each other to avoid fatigue fracture of the sintered layer between the chip 1 and the copper-clad ceramic substrate 2, ensuring that the chip 1 can dissipate heat normally during operation, thereby improving the stability of the power device.
[0025] The packaging layer 5 composed of epoxy adhesive can suppress the warping of the copper-clad ceramic substrate 2 on the one hand, and can also cover and protect the chip 1 on the other hand to prevent it from being directly contacted with external objects and causing mechanical damage.
[0026] Furthermore, the encapsulation layer 5 can reduce the influence of the stress generated by the copper-clad ceramic substrate 2 due to heat, such as Figure 3 As shown, the circuit layout design requires that a plurality of line grooves 7 be provided on the surface of the copper layer 21 on the substrate. The line grooves 7 penetrate the copper layer 21 on the substrate of the copper-clad ceramic substrate 2, and the outlet of the line grooves 7 extends all the way to the edge of the copper-clad ceramic substrate 2. In this embodiment, the plurality of line grooves 7 divide the copper-clad ceramic substrate 2 into several areas. Since the contact area between the copper layer 23 under the substrate and the aluminum nitride ceramic layer 22 is larger than the contact area between the copper layer 21 on the substrate and the aluminum nitride ceramic layer, the stress of the copper layer 23 under the substrate on the aluminum nitride ceramic layer 22 is larger than the stress of the copper layer 21 on the substrate on the aluminum nitride ceramic layer 22. The stress difference between the two aggravates the warping deformation of the copper-clad ceramic substrate 2. When the epoxy glue is poured in and fills the gap area of the line groove 7, the copper layer 21 on the substrate and the epoxy glue form a whole. During the thermal expansion process, the stress of the copper layer 21 on the substrate and the copper layer 23 under the substrate on the aluminum nitride ceramic layer 22 can be balanced, and the overall stress of the copper-clad ceramic substrate 2 is finally reduced. Furthermore, the plurality of line grooves 7 are interconnected, wherein one end or both ends of the plurality of line grooves 7 extend to the edge of the copper-clad ceramic substrate 2. For example, when both ends of a line groove 7 extend to the edge of the copper-clad ceramic substrate 2, one end of another line groove 7 intersecting therewith extends to the edge of the copper-clad ceramic substrate 2.
[0027] Optionally, the line groove 7 can be arranged horizontally or vertically relative to the copper-clad ceramic substrate 2, or the line groove 7 can be arranged horizontally and vertically staggered. Optionally, the line groove 7 can also be arranged non-parallel and be distributed in a bending adaptive manner according to the structure of the copper-clad ceramic substrate 2.
[0028] In one embodiment, the power device further includes a heat sink 6, which is disposed on one side of the copper layer 23 under the substrate, and is connected to the copper-clad ceramic substrate 2. The heat sink 6 is mainly used to extract heat from the copper-clad ceramic substrate 2. Specifically, in this embodiment, the heat sink 6 includes a plurality of heat dissipation columns, and a preset gap is provided between the plurality of heat dissipation columns. The high temperature generated by the chip 1 can be taken away by the flow of the coolant in the preset gap, thereby reducing the temperature of the copper-clad ceramic substrate 2 and reducing the stress generated by the copper-clad ceramic substrate 2 when heated.
[0029] In one embodiment, the power device further includes a shell 4, which is connected to a heat sink 6. The shell 4 is arranged along the side of the copper-clad ceramic substrate 2. The shell 4 has a certain height relative to the copper-clad ceramic substrate 2, so as to seal and surround the copper-clad ceramic substrate 2 to form a packaging cavity. The liquid epoxy glue is arranged with the packaging cavity to form the packaging layer 5, so that the packaging layer 5 can be formed without additional auxiliary tools, and the liquid epoxy glue can be gathered together to form a structure of a certain thickness. Furthermore, in order to dissipate the heat received on the copper-clad ceramic substrate 2, as shown in FIG. Figure 2 As shown, a welding layer 3 is provided between the copper-clad ceramic substrate 2 and the radiator 6. The welding layer 3 connects the copper layer under the substrate with the radiator 6. The welding layer not only supports the connection between the copper-clad ceramic substrate 2 and the radiator 6, but also transfers the heat of the copper-clad ceramic substrate 2 to the radiator 6.
[0030] The above is only a preferred embodiment of the present invention. It should be noted that a person skilled in the art can make several improvements and modifications without departing from the principle of the present invention. These improvements and modifications should also be considered as the protection scope of the present invention.
Claims
1. A power device with a high reliability packaging structure, characterized in that: include: A copper-clad ceramic substrate, comprising an upper copper layer, an aluminum nitride ceramic layer and a lower copper layer, wherein the aluminum nitride ceramic layer is arranged between the upper copper layer and the lower copper layer, the aluminum nitride ceramic layer separates the upper copper layer and the lower copper layer, the upper copper layer is located above the lower copper layer, and a chip is arranged on one side of the upper copper layer; The encapsulation layer has a preset thickness and is arranged on the upper surface of the copper-clad ceramic substrate. The encapsulation layer covers a side of the copper-clad ceramic substrate on which a chip is provided. The encapsulation layer and the copper-clad ceramic substrate are bonded to form a whole, wherein the thermal expansion coefficient of the encapsulation layer is lower than the thermal expansion coefficient of copper in the copper-clad ceramic substrate.
2. A power device with a high reliability packaging structure according to claim 1, characterized in that: The packaging layer is made of epoxy adhesive.
3. A power device with a high reliability packaging structure according to claim 2, characterized in that: It also includes a heat sink, which is arranged on the lower surface of the copper layer under the substrate and is connected to the copper-clad ceramic substrate.
4. The power device with a high reliability packaging structure according to claim 3, characterized in that: The radiator comprises a plurality of radiating columns, and preset gaps are arranged between the plurality of radiating columns.
5. The power device with a high reliability packaging structure according to claim 1, characterized in that: A plurality of circuit grooves are arranged on the copper layer on the substrate, the plurality of circuit grooves penetrate the copper layer on the substrate, and the plurality of circuit grooves divide the copper layer on the substrate into a plurality of areas.
6. The power device with a high reliability packaging structure according to claim 5, characterized in that: The plurality of line grooves are interconnected, and one end or both ends of the plurality of line grooves extend to the edge of the copper-clad ceramic substrate.
7. The power device with a high reliability packaging structure according to claim 3, characterized in that: It also includes a shell, which is connected to the radiator. The shell is arranged along the side of the copper-clad ceramic substrate to form a packaging cavity. The epoxy glue is arranged with the packaging cavity to form the packaging layer.
8. The power device with a high reliability packaging structure according to claim 3, characterized in that: A welding layer is provided between the copper-clad ceramic substrate and the radiator, and the welding layer connects the copper layer under the substrate with the radiator.