HEMT device

By using an etching barrier layer as an etching stop layer in gallium nitride HEMT devices, and combining dry and wet etching processes, the problem of dry etching damage to the underlying structure is solved, and the damage to the etching surface is reduced. Effect.

CN222088611UActive Publication Date: 2024-11-29GANEXT (ZHUHAI) TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420843951.4
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-04-23
Publication Date
2024-11-29
Estimated Expiration
2034-04-23

AI Technical Summary

Technical Problem

When forming a depleted gallium nitride HEMT device, the dry etching process is prone to damage the underlying structure and cause damage to the etching surface.

Method used

采用刻蚀阻挡层作为第二介质层的刻蚀终止层,通过设置适当的干法刻蚀工艺参数,并利用湿法刻蚀工艺去除刻蚀阻挡层,避免干法刻蚀对下层结构的损伤 .

Benefits of technology

It effectively avoids damage to the underlying structure of depleted gallium nitride HEMT devices by dry etching process, reduces etching surface damage, and improves the overall performance of the device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222088611U_ABST
    Figure CN222088611U_ABST
Patent Text Reader

Abstract

The utility model discloses an HEMT (High Electron Mobility Transistor) device. The device comprises a gallium nitride epitaxial wafer; the first dielectric layer is positioned on one side of the gallium nitride epitaxial wafer; the source electrode and the drain electrode penetrate through the first dielectric layer and are in contact with the gallium nitride epitaxial wafer; the etching barrier layer is located on the side, away from the gallium nitride epitaxial wafer, of the first dielectric layer, and the first dielectric layer, the source electrode and the drain electrode are covered with the etching barrier layer; the second dielectric layer is positioned on one side, far away from the gallium nitride epitaxial wafer, of the etching barrier layer; the etching barrier layer is an etching stop layer of the second dielectric layer; the grid penetrates through the first dielectric layer and is in contact with the gallium nitride epitaxial wafer; the grid field plate penetrates through the second dielectric layer and the etching barrier layer to be in contact with the grid; the first contact electrode penetrates through the second dielectric layer and the etching barrier layer and is in contact with the source electrode, and the second contact electrode penetrates through the second dielectric layer and the etching barrier layer and is in contact with the drain electrode. According to the utility model, the problem of etching surface damage caused by a dry etching process is effectively avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of semiconductors, in particular to a HEMT device. Background Art

[0002] Gallium nitride high electron mobility transistor (HEMT) devices have superior device performance and broad application prospects in the fields of high frequency and high power. Gallium nitride HEMT devices are mainly divided into depletion-mode devices and enhancement-mode devices. The structure of depletion-mode GaN HEMT devices is simple, which can retain the high electron concentration and high electron mobility of GaN heterojunction to the greatest extent. At the same time, the gate of depletion-mode GaN HEMT devices is also very reliable.

[0003] Dry etching is an essential step in forming a depletion-mode GaN HEMT device. In the prior art, the dry etching process will damage the underlying structure of the depletion-mode GaN HEMT device and is also very likely to cause damage to the etching surface. Utility Model Content

[0004] The utility model provides a HEMT device to solve the problem that a dry etching process damages the lower structure of a depletion-type gallium nitride HEMT device and causes etching surface damage.

[0005] According to one aspect of the present invention, a HEMT device is provided, the device comprising:

[0006] GaN epitaxial wafers;

[0007] A first dielectric layer, located on one side of the gallium nitride epitaxial wafer;

[0008] A source electrode and a drain electrode penetrate through the first dielectric layer and contact the gallium nitride epitaxial wafer;

[0009] An etch stop layer is located on a side of the first dielectric layer away from the gallium nitride epitaxial wafer, and the etch stop layer covers the first dielectric layer, the source electrode, and the drain electrode;

[0010] A second dielectric layer is located on a side of the etching stop layer away from the gallium nitride epitaxial wafer; the etching stop layer is an etching stop layer of the second dielectric layer;

[0011] A gate, penetrating through the first dielectric layer and contacting the gallium nitride epitaxial wafer;

[0012] A gate field plate, penetrating the second dielectric layer and the etching stop layer and contacting the gate;

[0013] A first contact electrode and a second contact electrode, the first contact electrode penetrates the second dielectric layer, the etching stop layer and contacts the source electrode, and the second contact electrode penetrates the second dielectric layer, the etching stop layer and contacts the drain electrode.

[0014] Optionally, the HEMT device further comprises:

[0015] A third dielectric layer is located on a side of the second dielectric layer away from the gallium nitride epitaxial wafer, and the third dielectric layer covers the second dielectric layer and the gate field plate;

[0016] The third contact electrode penetrates the third dielectric layer and contacts the gate field plate.

[0017] Optionally, the GaN epitaxial wafer includes:

[0018] substrate;

[0019] A channel layer, located on one side of the substrate;

[0020] The barrier layer is located on the side of the channel layer away from the substrate.

[0021] Optionally, the etch stop layer is an etch stop layer of the second dielectric layer; the etch stop layer includes any one of an aluminum nitride layer and an aluminum oxide layer.

[0022] Optionally, the thickness of the etching stop layer is 5-15 nm.

[0023] Optionally, the substrate includes a silicon substrate; the channel layer includes a gallium nitride layer; and the barrier layer includes an aluminum gallium nitride layer.

[0024] Optionally, the source electrode and the drain electrode include a first layer and a second layer of a metal stack, the first layer includes a titanium layer, and the second layer includes an aluminum layer;

[0025] or a first layer, a second layer and a third layer of a metal stack, the first layer comprising a titanium layer, the second layer comprising an aluminum layer, and the third layer comprising a titanium nitride layer;

[0026] Or a first layer, a second layer, a third layer and a fourth layer of a metal stack, the first layer includes a titanium layer, the second layer includes an aluminum layer, the third layer includes a titanium layer, and the fourth layer includes a titanium nitride layer.

[0027] Optionally, the gate comprises a first layer and a second layer of a metal stack, the first layer comprises a titanium layer, and the second layer comprises an aluminum layer;

[0028] or a stacked first layer, a second layer and a third layer, the first layer comprising a titanium layer, the second layer comprising an aluminum layer, and the third layer comprising a titanium nitride layer;

[0029] The gate field plate includes a first layer and a second layer of a metal stack, the first layer includes a titanium layer, and the second layer includes an aluminum layer;

[0030] or a stacked first layer, a second layer and a third layer, the first layer comprising a titanium layer, the second layer comprising an aluminum layer, and the third layer comprising a titanium nitride layer;

[0031] The gate and the gate field plate comprise the same layer stack.

[0032] Optional,

[0033] The first contact electrode includes a first plug and a first metal layer; the second contact electrode includes a second plug and a second metal layer;

[0034] The first plug passes through the second dielectric layer and the etching stop layer and contacts the source electrode, and the first metal layer is located on a side of the second dielectric layer away from the gallium nitride epitaxial wafer and contacts the first plug;

[0035] The second plug passes through the second dielectric layer and the etching stop layer and contacts the drain. The second metal layer is located on a side of the second dielectric layer away from the gallium nitride epitaxial wafer and contacts the second plug.

[0036] Optionally, the HEMT device further includes: at least one third metal layer, at least one fourth metal layer, a third plug arranged in one-to-one correspondence with the third metal layer, a fourth plug arranged in one-to-one correspondence with the fourth metal layer, and an additional dielectric layer arranged in one-to-one correspondence with the third metal layer or the fourth metal layer;

[0037] The additional dielectric layer is located on a side of the second dielectric layer away from the gallium nitride epitaxial wafer, and covers the metal layer and the dielectric layer adjacent to the additional dielectric layer below the additional dielectric layer;

[0038] The third plug passes through the additional dielectric layer and contacts the metal layer adjacent to the additional dielectric layer below the additional dielectric layer, and is connected to the source electrode through the metal layer; the third metal layer is located on a side of the additional dielectric layer away from the gallium nitride epitaxial wafer and contacts the third plug;

[0039] The fourth plug passes through the additional dielectric layer and contacts the metal layer below and adjacent to the additional dielectric layer, and is connected to the drain through the metal layer; the fourth metal layer is located on a side of the additional dielectric layer away from the gallium nitride epitaxial wafer and contacts the fourth plug.

[0040] The technical solution of the utility model provides a HEMT device, which includes an etch barrier layer, and the etch barrier layer is used as an etch stop layer of the second dielectric layer. When the second dielectric layer is opened by dry etching, the dry etching selectivity ratio of the second dielectric layer to the etch barrier layer can be set relatively high by setting certain process parameters, and the etch barrier layer at the corresponding position is removed by wet etching process. The problem of damaging the lower structure of the depletion-type gallium nitride HEMT device and causing etching surface damage by dry etching process is effectively avoided.

[0041] It should be understood that the contents described in this section are not intended to identify the key or important features of the embodiments of the present utility model, nor are they intended to limit the scope of the present utility model. Other features of the present utility model will become easily understood through the following description. BRIEF DESCRIPTION OF THE DRAWINGS

[0042] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.

[0043] Figure 1 It is a structural schematic diagram of a HEMT device provided by an embodiment of the utility model;

[0044] Figure 2-Figure 12 It is a structural schematic diagram corresponding to each step of a method for preparing a HEMT device provided in an embodiment of the utility model;

[0045] Fig.13 It is a schematic structural diagram of another HEMT device provided in an embodiment of the utility model. DETAILED DESCRIPTION

[0046] In order to enable those skilled in the art to better understand the solution of the utility model, the technical solution in the embodiment of the utility model will be clearly and completely described below in conjunction with the drawings in the embodiment of the utility model. Obviously, the described embodiment is only a part of the embodiment of the utility model, not all of the embodiments. Based on the embodiment of the utility model, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of the utility model.

[0047] It should be noted that the terms "first", "second", etc. in the specification and claims of the utility model and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the data used in this way can be interchanged where appropriate, so that the embodiments of the utility model described here can be implemented in an order other than those illustrated or described here. In addition, the terms "including" and "having" and any of their variations are intended to cover non-exclusive inclusions, for example, a process, method, system, product or device that includes a series of steps or units is not necessarily limited to those steps or units clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products or devices.

[0048] Figure 1 Schematic diagram of the structure of a HEMT device provided by an embodiment of the utility model. Figure 1 As shown, the device includes:

[0049] A gallium nitride epitaxial wafer 1; and a first dielectric layer 2, located on one side of the gallium nitride epitaxial wafer 1.

[0050] The source electrode 3 and the drain electrode 4 penetrate the first dielectric layer 2 and contact the gallium nitride epitaxial wafer 1 .

[0051] The etching stop layer 5 is located on a side of the first dielectric layer 2 away from the gallium nitride epitaxial wafer 1 , and the etching stop layer 5 covers the first dielectric layer 2 , the source electrode 3 and the drain electrode 4 .

[0052] The second dielectric layer 6 is located on a side of the etching stop layer 5 away from the gallium nitride epitaxial wafer 1 . The etching stop layer 5 is an etching stop layer of the second dielectric layer 6 .

[0053] The gate 20 penetrates the first dielectric layer 2 and contacts the GaN epitaxial wafer 1 .

[0054] The gate field plate 9 penetrates the second dielectric layer 2 and the etching stop layer 5 and contacts the gate 20 .

[0055] The first contact electrode 7 and the second contact electrode 8 , the first contact electrode 7 penetrates the second dielectric layer 6 and the etching stop layer 5 and contacts the source electrode 3 , and the second contact electrode 8 penetrates the second dielectric layer 6 and the etching stop layer 5 and contacts the drain electrode 4 .

[0056] In the embodiment of the utility model, the gallium nitride HEMT device is a depletion-mode gallium nitride HEMT device. The gallium nitride epitaxial wafer 1 is a semiconductor material that grows one or more layers of gallium nitride thin films on a substrate by using an epitaxial method under specific conditions. The substrate includes but is not limited to a silicon carbide substrate, a sapphire substrate or a silicon substrate. The etching barrier layer 5 is an etching stop layer of the second dielectric layer 6.

[0057] Specifically, the gallium nitride HEMT device includes a gallium nitride epitaxial wafer 1 and a first dielectric layer 2, wherein the first dielectric layer 2 is disposed on one side of the gallium nitride epitaxial wafer 1. Figure 2 As shown, a first dielectric layer 2 can be formed on one side of the gallium nitride epitaxial wafer 1 by using a process such as chemical vapor deposition under specific conditions. The first dielectric layer 2 includes but is not limited to a silicon oxide layer or a silicon nitride layer.

[0058] The gallium nitride HEMT device further includes a source electrode 3 and a drain electrode 4. Both the source electrode 3 and the drain electrode 4 penetrate the first dielectric layer 2 and contact the gallium nitride epitaxial wafer 1. Figure 3 As shown, a through hole is formed in the first dielectric layer 2 by dry etching or wet etching, and a source electrode 3 and a drain electrode 4 are formed under specific conditions by physical vapor deposition or other processes. The source electrode 3 and the drain electrode 4 can be made of titanium / aluminum alloy, titanium / aluminum / titanium nitride alloy or titanium / aluminum / titanium / titanium nitride alloy, which is not specifically limited here.

[0059] The gallium nitride HEMT device further includes an etching stop layer 5, which is disposed on a side of the first dielectric layer 2 away from the gallium nitride epitaxial wafer 1, and covers the first dielectric layer 2, the source electrode 3 and the drain electrode 4. Figure 4 As shown, an etch stop layer 5 is formed on one side of the first dielectric layer 2. The etch stop layer 5 is grown by physical vapor deposition magnetron sputtering process. The process conditions are: the temperature is room temperature, the chamber pressure of the magnetron sputtering equipment is 3-4mt, and the magnetron sputtering power is 800-1000W. Selecting a lower power can reduce the surface damage of the contact surface. The etch stop layer 5 includes but is not limited to an aluminum nitride layer or an aluminum oxide layer.

[0060] The gallium nitride HEMT device further includes a second dielectric layer 6, which is disposed on a side of the etching stop layer 5 away from the gallium nitride epitaxial wafer 1. Figure 5 As shown, a second dielectric layer 6 can be formed on one side of the etch stop layer 5 by using a chemical vapor deposition process under specific conditions. The second dielectric layer 6 includes but is not limited to a silicon oxide layer or a silicon nitride layer.

[0061] like Figure 6 As shown, the second dielectric layer 6 is opened by dry etching process, and the etching stop layer 5 is the etching stop layer of the second dielectric layer 6. The process conditions of this dry etching are: etching temperature is 90°C, etching pressure is 100mT, etching power is 200W, etching gas is carbon tetrafluoride and oxygen, carbon tetrafluoride gas flow rate is 60sccm, oxygen flow rate is 10sccm. Under this process, the dry etching selectivity ratio of the second dielectric layer 6 to the etching stop layer 5 can reach 20:1. Figure 7 As shown, the etching stop layer 5 at the corresponding position is removed by wet etching. The wet etching reagent can be tetramethylammonium hydroxide, and the concentration of the tetramethylammonium hydroxide solution is 2.38%. The temperature of the wet etching is 23°C, and the etching rate of the wet etching is like Figure 8 As shown, the first dielectric layer 2 is continuously opened by dry etching or wet etching process.

[0062] The HEMT device further includes a gate 20 and a gate field plate 9. The gate 20 penetrates the first dielectric layer 2 and contacts the GaN epitaxial wafer 1. The gate field plate 9 penetrates the second dielectric layer 6 and the etching stop layer 5 and contacts the gate 20. By providing the gate field plate 9, the distribution of the electric field in the drift region can be effectively improved, thereby improving the withstand voltage performance of the HEMT device to a certain extent. Fig. 9 As shown, the gate 20 and the gate field plate 9 are formed under specific conditions by using physical vapor deposition and other processes. Fig.10 As shown, a third dielectric layer 10 can be formed on one side of the second dielectric layer 6 by using a process such as chemical vapor deposition under specific conditions.

[0063] like Fig.11As shown, the second dielectric layer 6 and the third dielectric layer 10 above the source 3 and the drain 4 are opened by dry etching process. The etching barrier layer 5 is the etching stop layer of the second dielectric layer 6. The process conditions of this dry etching are: etching temperature is 90°C, etching pressure is 100mT, etching power is 200W, etching gas is carbon tetrafluoride and oxygen, carbon tetrafluoride gas flow rate is 60sccm, oxygen flow rate is 10sccm. Under this process, the dry etching selectivity of the second dielectric layer 6 and the etching barrier layer 5 can reach 20:1. At the same time, the third dielectric layer 10 above the gate field plate 9 is opened by dry etching or wet etching process. As shown Fig.12 As shown, the etching stop layer 5 at the corresponding position is removed by wet etching. The wet etching reagent can be tetramethylammonium hydroxide, and the concentration of the tetramethylammonium hydroxide solution is 2.38%. The temperature of the wet etching is 23°C, and the etching rate of the wet etching is Finally, if Figure 1 As shown, the first contact electrode 7, the second contact electrode 8 and the third contact electrode 11 are formed under specific conditions by using chemical vapor deposition and other processes, forming a Figure 1 The structure of the GaN HEMT device is shown.

[0064] The gallium nitride HEMT device further includes a first contact electrode 7 and a second contact electrode 8. The first contact electrode 7 penetrates the second dielectric layer 6, the etch stop layer 5 and the third dielectric layer 10 and contacts the source 3. The second contact electrode 8 penetrates the second dielectric layer 6, the etch stop layer 5 and the third dielectric layer 10 and contacts the drain 4.

[0065] The technical solution of the embodiment of the utility model provides a HEMT device, which includes an etch barrier layer, and the etch barrier layer serves as an etch stop layer of the second dielectric layer. When the second dielectric layer is opened by a dry etching process, by setting certain process parameters, the dry etching selectivity ratio of the second dielectric layer to the etch barrier layer can be set relatively high, and the etch barrier layer at the corresponding position is removed by a wet etching process. The problem of the dry etching process damaging the lower structure of the depletion-type gallium nitride HEMT device and causing damage to the ohmic contact metal surface is effectively avoided.

[0066] Optional, continue to refer to Figure 1 , HEMT devices also include:

[0067] The third dielectric layer 10 is located on a side of the second dielectric layer 6 away from the gallium nitride epitaxial wafer 1 , and the third dielectric layer 10 covers the second dielectric layer 6 and the gate field plate 9 .

[0068] The third contact electrode 11 penetrates the third dielectric layer 10 and contacts the gate field plate 9 .

[0069] Specifically, the third dielectric layer 10 is disposed on a side of the second dielectric layer 6 away from the gallium nitride epitaxial wafer 1, and the third dielectric layer 10 covers the second dielectric layer 6 and the gate field plate 9. The third dielectric layer 10 includes but is not limited to a silicon oxide layer or a silicon nitride layer. Figure 1 As shown, the third contact electrode 11 penetrates the third dielectric layer 10 and contacts the gate field plate 9. The third contact electrode 11 may include a plug 111 and a metal layer 112. The plug 111 may include a tungsten plug, and the metal layer 112 may be made of an aluminum copper / titanium nitride alloy. The plug 111 penetrates the third dielectric layer 10 and contacts the gate field plate 9. The metal layer 112 is located on a side of the third dielectric layer 10 away from the gallium nitride epitaxial wafer 1 and contacts the plug 111.

[0070] Optional, continue to refer to Figure 1 The gallium nitride epitaxial wafer 1 includes: a substrate 21 ; a channel layer 22 located on one side of the substrate 21 ; and a barrier layer 23 located on a side of the channel layer 22 away from the substrate 21 .

[0071] Specifically, the gallium nitride epitaxial wafer 1 includes a substrate 21, a channel layer 22 and a barrier layer 23. The substrate 21 includes but is not limited to a silicon carbide substrate, a sapphire substrate or a silicon substrate. The barrier layer 23 is located on the side of the channel layer 22 away from the substrate 21. The source electrode 3 penetrates the first dielectric layer 2 and the barrier layer 23 and contacts the channel layer 22, and the drain electrode 4 penetrates the first dielectric layer 2 and the barrier layer 23 and contacts the channel layer 22. The gate electrode 20 penetrates the first dielectric layer 2 and contacts the barrier layer 23.

[0072] The channel layer 22 and the barrier layer 23 form a heterojunction, and a two-dimensional electron gas is formed at the interface of the heterojunction. The two-dimensional electron gas forms a channel between the source 3 and the drain 4, so that the gallium nitride HEMT device is turned on. For a depletion-type gallium nitride HEMT device, when the voltage between the gate 20 and the source 3 is zero, a two-dimensional electron gas channel already exists between the source 3 and the drain 4, and the device is turned on; when the voltage between the gate 20 and the source 3 is less than a certain threshold voltage, the two-dimensional electron gas channel between the source 3 and the drain 4 is disconnected, and the device is turned off.

[0073] Optional, continue to refer to Figure 1 The etching stop layer 5 is an etching stop layer of the second dielectric layer 6; the etching stop layer 5 includes any one of an aluminum nitride layer and an aluminum oxide layer.

[0074] Specifically, the etching stop layer 5 can be an aluminum nitride layer or an aluminum oxide layer, which is not specifically limited here. In this way, under certain processes, the dry etching selectivity ratio of the second dielectric layer 6 to the etching stop layer 5 can reach 20:1.

[0075] Optional, continue to refer to Figure 1 , the thickness of the etching stop layer 5 is 5 to 15 nm.

[0076] Specifically, the thickness of the etch stop layer 5 is set to 5-15 nm. If the thickness of the etch stop layer 5 is set to be less than 5 nm, the etch stop layer 5 may be partially opened in advance due to the problem of thickness uniformity of the etch stop layer 5 and the second dielectric layer 6, thereby damaging the underlying structure of the etch stop layer 5. The thickness of the etch stop layer 5 can be appropriately increased based on the thickness of the second dielectric layer 6.

[0077] Optional, continue to refer to Figure 1 , the substrate 21 includes a silicon substrate; the channel layer 22 includes a gallium nitride layer; and the barrier layer 23 includes an aluminum gallium nitride layer.

[0078] Specifically, the gallium nitride epitaxial wafer 1 includes a substrate 21, a channel layer 22 and a barrier layer 23. The substrate 21 may be a silicon substrate; the channel layer 22 may be a gallium nitride layer; and the barrier layer 23 may be an aluminum gallium nitride layer. The gallium nitride layer and the aluminum gallium nitride layer form a heterojunction, and a two-dimensional electron gas is formed at the interface of the heterojunction. The two-dimensional electron gas forms a channel between the source 3 and the drain 4, so that the gallium nitride HEMT device is turned on. For a depletion-type gallium nitride HEMT device, when the voltage between the gate 20 and the source 3 is zero, a two-dimensional electron gas channel already exists between the source 3 and the drain 4, and the device is turned on; when the voltage between the gate 20 and the source 3 is less than a certain threshold voltage, the two-dimensional electron gas channel between the source 3 and the drain 4 is disconnected, and the device is turned off.

[0079] Optional, continue to refer to Figure 1 The source electrode 3 and the drain electrode 4 include a first layer and a second layer of a metal stack, the first layer includes a titanium layer, and the second layer includes an aluminum layer.

[0080] Or a first layer, a second layer and a third layer of a metal stack, the first layer includes a titanium layer, the second layer includes an aluminum layer, and the third layer includes a titanium nitride layer.

[0081] Or a first layer, a second layer, a third layer and a fourth layer of a metal stack, the first layer includes a titanium layer, the second layer includes an aluminum layer, the third layer includes a titanium layer, and the fourth layer includes a titanium nitride layer.

[0082] Specifically, the source electrode 3 may include a first layer and a second layer, and the first layer may be a titanium layer, and the second layer may be an aluminum layer. The source electrode 3 may also include a first layer, a second layer, and a third layer, and the first layer may be a titanium layer, the second layer may be an aluminum layer, and the third layer may be a titanium nitride layer. The source electrode 3 may also include a first layer, a second layer, a third layer, and a fourth layer, and the first layer may be a titanium layer, the second layer may be an aluminum layer, the third layer may be a titanium layer, and the fourth layer may be a titanium nitride layer.

[0083] The drain electrode 4 may include a first layer and a second layer, and the first layer may be a titanium layer, and the second layer may be an aluminum layer. The drain electrode 4 may also include a first layer, a second layer and a third layer, and the first layer may be a titanium layer, the second layer may be an aluminum layer, and the third layer may be a titanium nitride layer. The drain electrode 4 may also include a first layer, a second layer, a third layer and a fourth layer, and the first layer may be a titanium layer, the second layer may be an aluminum layer, the third layer may be a titanium layer, and the fourth layer may be a titanium nitride layer.

[0084] Optional, continue to refer to Figure 1 The gate 20 includes a first layer and a second layer of a metal stack, the first layer includes a titanium layer, and the second layer includes an aluminum layer.

[0085] Or a first layer, a second layer and a third layer of a metal stack, the first layer includes a titanium layer, the second layer includes an aluminum layer, and the third layer includes a titanium nitride layer.

[0086] The gate field plate 9 includes a first layer and a second layer of a metal stack, wherein the first layer includes a titanium layer and the second layer includes an aluminum layer.

[0087] Or a first layer, a second layer and a third layer of a metal stack, the first layer includes a titanium layer, the second layer includes an aluminum layer, and the third layer includes a titanium nitride layer.

[0088] The gate 20 comprises the same layer stack as the gate field plate 9 .

[0089] Specifically, the gate 20 may include a first layer and a second layer, and the first layer may be a titanium layer, and the second layer may be an aluminum layer. The gate 20 may also include a first layer, a second layer and a third layer, and the first layer may be a titanium layer, the second layer may be an aluminum layer, and the third layer may be a titanium nitride layer. The gate field plate 9 may include a first layer and a second layer, and the first layer may be a titanium layer, and the second layer may be an aluminum layer. The gate field plate 9 may also include a first layer, a second layer and a third layer, and the first layer may be a titanium layer, the second layer may be an aluminum layer, and the third layer may be a titanium nitride layer. The gate 20 has the same stack as the gate field plate 9, that is, the number of metal layers and materials set for the gate 20 and the gate field plate 9 are the same and are completed in a synchronous process.

[0090] Optional, such as Figure 1 As shown, the first contact electrode 7 includes a first plug 71 and a first metal layer 72 ; the second contact electrode 8 includes a second plug 81 and a second metal layer 82 .

[0091] The first plug 71 passes through the second dielectric layer 6 and the etching stop layer 5 and contacts the source 3 . The first metal layer 72 is located on a side of the second dielectric layer 6 away from the GaN epitaxial wafer 1 and contacts the first plug 71 .

[0092] The second plug 81 passes through the second dielectric layer 6 and the etching stop layer 5 and contacts the drain 4 . The second metal layer 82 is located on a side of the second dielectric layer 6 away from the GaN epitaxial wafer 1 and contacts the second plug 81 .

[0093] Specifically, the first contact electrode 7 may include a first plug 71 and a first metal layer 72; the first plug 71 may penetrate the third dielectric layer 10, the second dielectric layer 6 and the etching stop layer 5 to contact the source electrode 3, and the first plug 71 may be formed under specific conditions by chemical vapor deposition or other processes, and illustratively, the first plug 71 may be a tungsten plug. The first metal layer 72 may be disposed on a side of the third dielectric layer 10 away from the gallium nitride epitaxial wafer 1, and contact the first plug 71. The first metal layer 72 may be formed under specific conditions by physical vapor deposition or other processes, and illustratively, the first metal layer 72 may be made of aluminum copper / titanium nitride alloy.

[0094] The second contact electrode 8 includes a second plug 81 and a second metal layer 82. The second plug 81 can penetrate the third dielectric layer 10, the second dielectric layer 6 and the etching stop layer 5 to contact the drain 4. The second plug 81 can be formed under specific conditions by chemical vapor deposition and other processes. For example, the second plug 81 can be a tungsten plug. The second metal layer 82 is arranged on the side of the third dielectric layer 10 away from the gallium nitride epitaxial wafer 1 and contacts the second plug 81. The second metal layer 82 can be formed under specific conditions by physical vapor deposition and other processes. For example, the second metal layer 82 can be made of aluminum copper / titanium nitride alloy.

[0095] Fig.13 Schematic diagram of another HEMT device provided by the embodiment of the utility model. Fig.13 As shown, the HEMT device further includes: at least one third metal layer 12, at least one fourth metal layer 13, a third plug 14 arranged in one-to-one correspondence with the third metal layer 12, a fourth plug 15 arranged in one-to-one correspondence with the fourth metal layer 13, and an additional dielectric layer 16 arranged in one-to-one correspondence with the third metal layer 12 or the fourth metal layer 13.

[0096] The additional dielectric layer 16 is located on a side of the second dielectric layer 6 away from the gallium nitride epitaxial wafer 1 , and covers the metal layer and the dielectric layer adjacent to the additional dielectric layer 16 below the additional dielectric layer 16 .

[0097] The third plug 14 passes through the additional dielectric layer 16 and contacts the metal layer adjacent to the additional dielectric layer 16 below and is connected to the source 3 through the metal layer; the third metal layer 12 is located on a side of the additional dielectric layer 16 away from the GaN epitaxial wafer 1 and contacts the third plug 14 .

[0098] The fourth plug 15 passes through the additional dielectric layer 16 and contacts the metal layer adjacent to the additional dielectric layer 16 below and is connected to the drain 4 through the metal layer; the fourth metal layer 13 is located on a side of the additional dielectric layer 16 away from the GaN epitaxial wafer 1 and contacts the fourth plug 15 .

[0099] Specifically, the gallium nitride HEMT device may further include an additional dielectric layer 16, which is disposed on a side of the second dielectric layer 6 away from the gallium nitride epitaxial wafer 1, and covers the metal layer disposed below the additional dielectric layer 16 and adjacent to the metal layer and the dielectric layer disposed adjacent to the metal layer. The additional dielectric layer 16 may be formed under specific conditions by processes such as chemical vapor deposition. The additional dielectric layer 16 includes, but is not limited to, a silicon oxide layer or a silicon nitride layer.

[0100] The gallium nitride HEMT device may further include at least one third metal layer 12, at least one fourth metal layer 13, a third plug 14 arranged in one-to-one correspondence with the third metal layer 12, and a fourth plug 15 arranged in one-to-one correspondence with the fourth metal layer 13. The number of the third metal layer 12 and the fourth metal layer 13 may be consistent. The third plug 14 passes through the additional dielectric layer 16 and contacts the metal layer arranged adjacent to the additional dielectric layer 16, and is connected to the source electrode 3 through the metal layer. The third plug 14 may be formed under specific conditions by chemical vapor deposition or other processes. For example, the third plug 14 may be a tungsten plug. The third metal layer 12 is located on a side of the additional dielectric layer 16 away from the gallium nitride epitaxial wafer 1 and contacts the third plug 14. The third metal layer 12 may be formed under specific conditions by physical vapor deposition or other processes. For example, the third metal layer 12 may be made of aluminum copper / titanium nitride alloy. The third plug 14 and the third metal layer 12 may form a contact electrode.

[0101] The fourth plug 15 passes through the additional dielectric layer 16 and contacts the metal layer disposed adjacent to the additional dielectric layer 16, and is connected to the drain 4 through the metal layer. The third plug 15 can be formed under specific conditions by using processes such as chemical vapor deposition. For example, the third plug 15 can be a tungsten plug. The fourth metal layer 13 is located on the side of the additional dielectric layer 16 away from the gallium nitride epitaxial wafer 1 and contacts the fourth plug 15. The fourth metal layer 13 can be formed under specific conditions by using processes such as physical vapor deposition. For example, the fourth metal layer 13 can be made of aluminum copper / titanium nitride alloy. The fourth plug 15 and the fourth metal layer 13 can form a contact electrode.

[0102] At least one third metal layer 12 and a third plug 14 may be provided on a side of the first contact electrode 7 away from the gallium nitride epitaxial wafer 1. The third plug 14 disposed adjacent to the first contact electrode 7 contacts the first metal layer of the first contact electrode 7 through the additional dielectric layer 16. At least one fourth metal layer 13 and a fourth plug 15 may be provided on a side of the second contact electrode 8 away from the gallium nitride epitaxial wafer 1. The fourth plug 15 disposed adjacent to the second contact electrode 8 contacts the second metal layer of the second contact electrode 8 through the additional dielectric layer 16.

[0103] By providing at least one third metal layer, at least one fourth metal layer, third plugs provided in one-to-one correspondence with the third metal layers, and fourth plugs provided in one-to-one correspondence with the fourth metal layers, a certain number of third metal layers and fourth metal layers can be provided according to actual design requirements, thereby changing the static resistance of the transistor and making the HEMT device meet the design requirements.

[0104] The gallium nitride HEMT device may further include at least one fifth metal layer 18 and a fifth plug 17 arranged in one-to-one correspondence with the fifth metal layer 18; the fifth plug 17 passes through the additional dielectric layer 16 and contacts the metal layer arranged adjacent to the additional dielectric layer 16, and is connected to the gate field plate 9 through the metal layer. The fifth plug 17 may be formed under specific conditions by chemical vapor deposition or other processes, and illustratively, the fifth plug 17 may be a tungsten plug. The fifth metal layer 18 is located on a side of the additional dielectric layer 16 away from the gallium nitride epitaxial wafer 1 and contacts the fifth plug 17. The fifth metal layer 18 may be formed under specific conditions by physical vapor deposition or other processes, and illustratively, the fifth metal layer 18 may be made of aluminum copper / titanium nitride alloy. The fifth plug 17 and the fifth metal layer 18 may form a contact electrode.

[0105] At least one fifth metal layer 18 and a fifth plug 17 may be disposed on a side of the third contact electrode 11 away from the GaN epitaxial wafer 1. The fifth plug 17 disposed adjacent to the third contact electrode 11 passes through the additional dielectric layer 16 and contacts the metal layer of the third contact electrode 11.

[0106] It should be understood that the various forms of processes shown above can be used to reorder, add or delete steps. For example, the steps described in the present invention can be performed in parallel, sequentially or in different orders, as long as the desired results of the technical solution of the present invention can be achieved, and this document does not limit this.

[0107] The above specific implementations do not constitute a limitation on the protection scope of the present utility model. It should be understood by those skilled in the art that various modifications, combinations, sub-combinations and substitutions can be made according to design requirements and other factors. Any modification, equivalent substitution and improvement made within the spirit and principle of the present utility model shall be included in the protection scope of the present utility model.

Claims

1. A HEMT device, characterized in that: include: Gallium nitride epitaxial wafers; A first dielectric layer is located on one side of the gallium nitride epitaxial wafer; a source electrode and a drain electrode, penetrating the first dielectric layer and contacting the gallium nitride epitaxial wafer; an etch stop layer, located on a side of the first dielectric layer away from the gallium nitride epitaxial wafer, the etch stop layer covering the first dielectric layer, the source electrode, and the drain electrode; A second dielectric layer is located on a side of the etch stop layer away from the gallium nitride epitaxial wafer; the etch stop layer is an etch stop layer for the second dielectric layer; a gate, penetrating the first dielectric layer and contacting the gallium nitride epitaxial wafer; a gate field plate, penetrating the second dielectric layer and the etch stop layer and contacting the gate; A first contact electrode and a second contact electrode, wherein the first contact electrode penetrates the second dielectric layer and the etch stop layer and contacts the source electrode, and the second contact electrode penetrates the second dielectric layer and the etch stop layer and contacts the drain electrode.

2. The HEMT device according to claim 1, wherein: Also includes: a third dielectric layer, located on a side of the second dielectric layer away from the gallium nitride epitaxial wafer, the third dielectric layer covering the second dielectric layer and the gate field plate; A third contact electrode penetrates the third dielectric layer and contacts the gate field plate.

3. The HEMT device according to claim 1, wherein: The gallium nitride epitaxial wafer comprises: substrate; a channel layer, located on one side of the substrate; The barrier layer is located on a side of the channel layer away from the substrate.

4. The HEMT device according to claim 1, wherein: The etch stop layer is an etch stop layer of the second dielectric layer; the etch stop layer includes any one of an aluminum nitride layer and an aluminum oxide layer.

5. The HEMT device according to claim 1, wherein: The thickness of the etching stop layer is 5-15 nm.

6. The HEMT device according to claim 3, wherein: The substrate includes a silicon substrate; the channel layer includes a gallium nitride layer; and the barrier layer includes an aluminum gallium nitride layer.

7. The HEMT device according to claim 1, wherein: The source electrode and the drain electrode include a first layer and a second layer of a metal stack, the first layer includes a titanium layer, and the second layer includes an aluminum layer; or a first layer, a second layer, and a third layer of a metal stack, wherein the first layer comprises a titanium layer, the second layer comprises an aluminum layer, and the third layer comprises a titanium nitride layer; Or a first layer, a second layer, a third layer and a fourth layer of a metal stack, the first layer includes a titanium layer, the second layer includes an aluminum layer, the third layer includes a titanium layer, and the fourth layer includes a titanium nitride layer.

8. The HEMT device according to claim 1, wherein: The gate comprises a first layer and a second layer of a metal stack, the first layer comprising a titanium layer, and the second layer comprising an aluminum layer; or a first layer, a second layer, and a third layer of a metal stack, wherein the first layer comprises a titanium layer, the second layer comprises an aluminum layer, and the third layer comprises a titanium nitride layer; The gate field plate includes a first layer and a second layer of a metal stack, the first layer includes a titanium layer, and the second layer includes an aluminum layer; or a first layer, a second layer, and a third layer of a metal stack, wherein the first layer comprises a titanium layer, the second layer comprises an aluminum layer, and the third layer comprises a titanium nitride layer; The gate and the gate field plate include the same layer stack.

9. The HEMT device according to claim 1, wherein: The first contact electrode includes a first plug and a first metal layer; the second contact electrode includes a second plug and a second metal layer; The first plug passes through the second dielectric layer and the etch stop layer and contacts the source electrode; the first metal layer is located on a side of the second dielectric layer away from the gallium nitride epitaxial wafer and contacts the first plug; The second plug passes through the second dielectric layer and the etch stop layer and contacts the drain. The second metal layer is located on a side of the second dielectric layer away from the gallium nitride epitaxial wafer and contacts the second plug.

10. The HEMT device according to claim 9, wherein: Also includes: at least one third metal layer, at least one fourth metal layer, a third plug provided in a one-to-one correspondence with the third metal layer, a fourth plug provided in a one-to-one correspondence with the fourth metal layer, and an additional dielectric layer provided in a one-to-one correspondence with the third metal layer or the fourth metal layer; The additional dielectric layer is located on a side of the second dielectric layer away from the gallium nitride epitaxial wafer, and covers the metal layer and dielectric layer adjacent to the additional dielectric layer below the additional dielectric layer; The third plug passes through the additional dielectric layer and contacts the metal layer adjacent to the additional dielectric layer below the additional dielectric layer, and is connected to the source electrode through the metal layer; The third metal layer is located on a side of the additional dielectric layer away from the gallium nitride epitaxial wafer and is in contact with the third plug; The fourth plug passes through the additional dielectric layer and contacts the metal layer below and adjacent to the additional dielectric layer, and is connected to the drain through the metal layer; the fourth metal layer is located on a side of the additional dielectric layer away from the gallium nitride epitaxial wafer and contacts the fourth plug.