Metallurgy blast furnace cooling wall surface abrasion repairing device

By designing the support side plate and limit assembly to form a slurry storage area and using scraper and drying plate to heat it, the slurry drying and covering problems during the spraying process is solved, and efficient blast furnace cooling wall surface wear repair is achieved.

CN222093737UActive Publication Date: 2024-12-03MAANSHAN RUNTONG HEAVY IND TECH CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202323581022.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-27
Publication Date
2024-12-03
Estimated Expiration
2033-12-27

AI Technical Summary

Technical Problem

During the spraying process of existing blast furnace cooling wall repair devices, sprayed slurry is difficult to dry immediately, thick-coated slurry will hang on the wall, and the movement direction of the sprayed slurry above is inaccurate, which cannot effectively cover the wear area.

Method used

A metallurgical blast furnace cooling wall surface wear repairer is designed, including support side plates, rotary plates, limiting assembly and heating blocks. The support side plates contact the blast furnace surface to limit the use distance of the repairer and use limit assembly to form slurry The storage area is stored, the scraper is scraped and the drying board is heated during spraying to achieve rapid solidification and drying of the slurry in the area.

Benefits of technology

It effectively accelerates the wear repair process of blast furnace cooling wall surface, ensures that the slurry can accurately cover the wear area and dry quickly, improving repair efficiency and stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222093737U_ABST
    Figure CN222093737U_ABST
Patent Text Reader

Abstract

The utility model discloses a metallurgical blast furnace cooling wall surface abrasion repairing device, and belongs to the technical field of blast furnace cooling wall repairing. A metallurgical blast furnace cooling wall surface abrasion repairing device comprises a supporting side plate and rotating plates, the upper end and the lower end of the supporting side plate are movably connected with the rotating plates, one end of each rotating plate is hinged to a limiting assembly, and the other end of the supporting side plate is hinged to a movable assembly. According to the repairing device, the supporting side plates are in contact with the surface of the cooling wall of the metallurgical blast furnace to limit the use distance of the repairing device, then a slurry storage area is defined by the limiting assemblies, spraying is achieved in the area, slurry hung downwards in the spraying process is upwards scraped by the scraping plate, solidification of the sprayed slurry in the area is accelerated by the drying plate, and the spraying effect is improved. And blade coating and drying treatment are carried out in the spraying process, and surface abrasion repair of the metallurgical blast furnace cooling wall can be accelerated.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of blast furnace cooling wall repair, and more specifically to a metallurgical blast furnace cooling wall surface wear repairer. Background Art

[0002] Due to the continuity and persistence of blast furnace production, the surface of the cooling wall will inevitably be worn or eroded. The Chinese patent with publication number CN219745271U discloses a blast furnace cooling wall repair device, including a connecting plate, a repair mechanism is inserted and fixedly connected to the middle of the front end of the connecting plate, and a connecting port is fixedly connected to the front end of the repair mechanism. During the spray repair process, the spraying amount of the spraying material can be easily adjusted to avoid wasting the spraying material, and at the same time, the stability of the entire device during the repair process can be improved.

[0003] This patent controls the spraying amount during the spraying process, but the sprayed slurry cannot dry immediately. The thickly coated slurry will hang on the wall, and the slurry sprayed from above will also move downward, causing the slurry to be unable to cover the worn area. Utility Model Content

[0004] The utility model aims to overcome the deficiencies in the prior art and provides a wear repairer for the surface of a metallurgical blast furnace cooling wall to solve the above deficiencies.

[0005] In order to achieve the above-mentioned purpose, the technical solution provided by the utility model is:

[0006] A metallurgical blast furnace cooling wall surface wear repairer comprises a supporting side plate and a rotating plate, wherein the upper and lower ends of the supporting side plate are movably connected to the rotating plate, one end of the rotating plate is hingedly connected to a limiting component, and the other end of the supporting side plate is hingedly connected to a movable component, wherein the movable component comprises a first side plate, a second side plate, an intermediate plate and a feed pipe, wherein the two sides of the intermediate plate are hingedly connected to the first side plate and the second side plate respectively, and the middle position of the intermediate plate is fixedly connected to the feed pipe.

[0007] Preferably, two supporting side plates are provided, a mounting plate is fixedly connected between the two supporting side plates, a threaded barrel is movably connected to the mounting plate, and the inner wall of the threaded barrel is engaged with the feed pipe.

[0008] Preferably, a driving gear is installed on the mounting plate near the threaded barrel, a driving motor is connected to the rotating shaft of the driving gear, and one end of the threaded barrel is fixedly connected to an external tooth, which meshes with the driving gear.

[0009] Preferably, the limiting assembly comprises a scraper and a drying plate, the lower end of the scraper is hingedly connected to the upper end of the drying plate, and arc-shaped notches are provided at adjacent ends of the scraper and the drying plate.

[0010] Preferably, the feed pipe passes through the arc-shaped slot, and one end of the feed pipe close to the arc-shaped slot is fixedly connected to a spray head.

[0011] Preferably, a heating block is connected to a side of the drying plate away from the middle plate, and the surface of the heating block is smooth.

[0012] Compared with the prior art, the technical solution provided by the utility model has the following beneficial effects:

[0013] The utility model supports the side plates to contact with the surface of the cooling wall of the metallurgical blast furnace, limits the use distance of the repairer, and then forms a slurry storage area through the limit assembly. Spraying is realized in the area, and the scraper scrapes upward the slurry hanging down during the spraying process, and the drying plate accelerates the solidification of the sprayed slurry in the area. The scraping and drying treatments are performed during the spraying process, which can accelerate the wear repair of the surface of the cooling wall of the metallurgical blast furnace. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 This is the overall structure diagram of the metallurgical blast furnace cooling wall surface wear repairer of the utility model;

[0015] Figure 2 This is a partial structural diagram of the metallurgical blast furnace cooling wall surface wear repairer of the utility model;

[0016] Figure 3 This is a spraying state diagram of the wear repairer on the cooling wall surface of a metallurgical blast furnace according to the utility model;

[0017] Figure 4 For the utility model Figure 3 Exploded view.

[0018] In the figure: 1. Support side plate; 11. Mounting plate; 12. Threaded cylinder; 13. Driving gear; 14. Driving motor; 2. Rotating plate; 3. Limiting assembly; 31. Scraper; 311. Arc notch; 32. Drying plate; 321. Heating block; 4. Movable assembly; 41. First side plate; 42. Second side plate; 43. Middle plate; 44. Feed pipe; 441. Spray head. DETAILED DESCRIPTION

[0019] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0020] In order to further understand the content of the utility model, the utility model is described in detail in conjunction with the accompanying drawings.

[0021] Combination Figure 1-Figure 4 , a metallurgical blast furnace cooling wall surface wear repairer, comprising a supporting side plate 1 and a rotating plate 2, the upper and lower ends of the supporting side plate 1 are movably connected with the rotating plate 2, the supporting side plate 1 limits the position of the rotating plate 2, so that the rotating plate 2 cannot move, but the rotating plate 2 can rotate on the supporting side plate 1, one end of the rotating plate 2 is hingedly connected to a limiting component 3, and the limiting component 3 extends from the end of the supporting side plate 1 close to the limiting component 3. When in use, the supporting side plate 1 contacts the surface of the metallurgical blast furnace cooling wall, the surface of the metallurgical blast furnace cooling wall, the supporting side plate 1 and the limiting component 3 form a slurry storage area, and the sprayed slurry solidifies in this area. The other end of the supporting side plate 1 is hingedly connected with a movable component 4, and the movable component 4 drives one end of the rotating plate 2 to move, thereby controlling the rotating plate 2 to rotate around the axis, and the other end of the rotating plate 2 controls the movement of the limiting component 3.

[0022] In this embodiment, two supporting side plates 1 are provided, and a mounting plate 11 is fixedly connected between the two supporting side plates 1. A threaded barrel 12 is movably connected to the mounting plate 11. The inner wall of the threaded barrel 12 is engaged with the feed pipe 44. The rotation of the threaded barrel 12 can control the relative position change of the feed pipe 44 on the mounting plate 11, and the feed pipe 44 drives the middle plate 43 to move.

[0023] In this embodiment, a driving gear 13 is installed on the mounting plate 11 near the threaded barrel 12, and a driving motor 14 is connected to the rotating shaft of the driving gear 13. One end of the threaded barrel 12 is fixedly connected with external teeth, which mesh with the driving gear 13. The driving motor 14 controls the rotation of the driving gear 13, thereby driving the threaded barrel 12 to rotate.

[0024] In this embodiment, the limiting assembly 3 includes a scraper 31 and a drying plate 32. The lower end of the scraper 31 is hingedly connected to the upper end of the drying plate 32. The adjacent ends of the scraper 31 and the drying plate 32 are each provided with an arc-shaped notch 311. During spraying, the scraper 31 and the drying plate 32 are bent into a V-shaped mouth, and the sprayed slurry is at the deepest part of the V-shaped mouth. During the spraying process, the repairer is moved up and down, and the V-shaped mouth moves up and down accordingly. The V-shaped mouth moves up, and the lower end of the scraper 31 scrapes the downward flowing slurry upward. The V-shaped mouth moves down, and the drying plate 32 is heated, thereby accelerating the drying of the slurry.

[0025] In this embodiment, a heating block 321 is connected to the side of the drying plate 32 away from the middle plate 43, and the surface of the heating block 321 is smooth. After spraying is completed, the scraper 31 and the drying plate 32 are controlled to be pulled straight to the same vertical plane. At this time, the heating block 321 protrudes from the scraper 31, and the mobile repairer can drive the heating block 321 to contact and move with the surface of the metallurgical blast furnace cooling wall after spraying, so as to dry the surface of the metallurgical blast furnace cooling wall after spraying.

[0026] In this embodiment, the movable component 4 includes a first side plate 41, a second side plate 42, an intermediate plate 43 and a feed pipe 44. The two sides of the intermediate plate 43 are hingedly connected to the first side plate 41 and the second side plate 42 respectively. The first side plate 41 and the second side plate 42 are hingedly connected to one end of the rotating plate 2 respectively. The intermediate plate 43 moves its position, driving one end of the first side plate 41 and the second side plate 42 to move, and controlling the other end of the first side plate 41 and the second side plate 42 to drive the rotating plate 2 to rotate. The middle position of the intermediate plate 43 is fixedly connected to the feed pipe 44.

[0027] In this embodiment, the feed pipe 44 passes through the arc-shaped slot 311, and the end of the feed pipe 44 close to the arc-shaped slot 311 is fixedly connected to a spray head 441. The feed pipe 44 feeds at one end close to the middle plate 43, and sprays the material onto the surface of the cooling wall of the metallurgical blast furnace through the spray head 441. The arc-shaped slot 311 provides space for the horizontal movement of the feed pipe 44. The circular hole formed by the arc-shaped slot 311 has a diameter larger than the diameter of the feed pipe 44. When the scraper 31 and the drying plate 32 are bent, the arc-shaped slot 311 can meet the needs of the feed pipe 44.

[0028] Working process: before spraying, the drive motor 14 is controlled to drive the drive gear 13 to rotate, the feed pipe 44 drives the middle plate 43 to move away from the limit component 3, the scraper 31 and the drying plate 32 are bent, the angle is fixed, and spraying begins. The feed pipe 44 sprays the slurry through the spray head 441, and the repairer moves up and down. When the repairer moves up, the lower end of the scraper 31 scrapes the downward flowing slurry upward, and when the repairer moves down, the drying plate 32 contacts the slurry to accelerate the drying of the slurry. After spraying is completed, the drive motor 14 drives the drive gear 13 to rotate, the feed pipe 44 drives the middle plate 43 to move toward the limit component 3, the scraper 31 and the drying plate 32 are straightened, and the repairer is moved up and down. The heating block 321 contacts and moves with the surface of the metallurgical blast furnace cooling wall after spraying to dry the surface of the metallurgical blast furnace cooling wall after spraying.

[0029] In summary, the supporting side plate 1 is in contact with the surface of the cooling wall of the metallurgical blast furnace to limit the use distance of the repairer, and then a slurry storage area is enclosed by the limit component 3. Spraying is realized in this area, and the scraper 31 scrapes upward the slurry hanging below during the spraying process, and the drying plate 32 accelerates the solidification of the sprayed slurry in this area. Scraping and drying treatments are performed during the spraying process, which can accelerate the repair of wear on the surface of the cooling wall of the metallurgical blast furnace.

[0030] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.

[0031] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A metallurgical blast furnace cooling wall surface wear repairer, comprising a supporting side plate (1) and a rotating plate (2), characterized in that: The upper and lower ends of the supporting side plate (1) are movably connected to a rotating plate (2); one end of the rotating plate (2) is hingedly connected to a limiting component (3); the other end of the supporting side plate (1) is hingedly connected to a movable component (4); the movable component (4) comprises a first side plate (41), a second side plate (42), an intermediate plate (43) and a feed pipe (44); two sides of the intermediate plate (43) are respectively hingedly connected to the first side plate (41) and the second side plate (42); and the middle position of the intermediate plate (43) is fixedly connected to the feed pipe (44).

2. The metallurgical blast furnace cooling wall surface wear repairer according to claim 1, characterized in that: The supporting side plates (1) are provided in two pieces, a mounting plate (11) is fixedly connected between the two supporting side plates (1), a threaded barrel (12) is movably connected to the mounting plate (11), and the inner wall of the threaded barrel (12) is meshed with the feed pipe (44).

3. The metallurgical blast furnace cooling wall surface wear repairer according to claim 2, characterized in that: A driving gear (13) is installed on the mounting plate (11) at a position close to the threaded barrel (12); a driving motor (14) is connected to the rotating shaft of the driving gear (13); one end of the threaded barrel (12) is fixedly connected to an external tooth, which meshes with the driving gear (13).

4. The metallurgical blast furnace cooling wall surface wear repairer according to claim 1, characterized in that: The limiting assembly (3) comprises a scraper (31) and a drying plate (32); the lower end of the scraper (31) is hingedly connected to the upper end of the drying plate (32); and arc-shaped notches (311) are provided at adjacent ends of the scraper (31) and the drying plate (32).

5. The wear repairer for the cooling wall surface of a metallurgical blast furnace according to claim 4, characterized in that: The feed pipe (44) passes through the arc-shaped slot (311), and one end of the feed pipe (44) close to the arc-shaped slot (311) is fixedly connected to a spray head (441).

6. The metallurgical blast furnace cooling wall surface wear repairer according to claim 4, characterized in that: A heating block (321) is connected to the side of the drying plate (32) away from the middle plate (43), and the surface of the heating block (321) is smooth.

Citation Information

Patent Citations

  • Blast furnace cooling wall repairing device

    CN219745271U