Waterproof coiled material sample preparation cutting die

By designing a combined structure including tool mold A, circular tool mold and tool mold B, the problem of manual operation time and inconvenience in the existing sample preparation process is solved, and the performance test of waterproof coils is achieved quickly and accurate support, improving sample preparation efficiency and working capacity.

CN222115362UActive Publication Date: 2024-12-06NANTONG RUILI SHANHE CONSTR ENG QUALITY CHECKING & MEASURING CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420848920.8
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-04-23
Publication Date
2024-12-06
Estimated Expiration
2034-04-23

AI Technical Summary

Technical Problem

The existing sample preparation process requires manual lines and the use of a utility knife, which consumes a lot of time and is inconvenient to make a complete set of samples, making it difficult to meet the needs of stretching, impermeable and low-temperature energy performance testing of waterproof coils.

Method used

A sample making tool mold system including knife mold A, circular knife mold and knife mold B is designed. Through the combined structure of installation block, movable block and positioning block, the tool mold is quickly fixed and used in a complete set, suitable for waterproofing. Tensile, water-impermeable and low-temperature energy performance tests of the coil.

Benefits of technology

It improves sample preparation efficiency, reduces the generation of burrs and samples that do not meet the specifications, and achieves rapid and accurate support for waterproof coil performance testing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222115362U_ABST
    Figure CN222115362U_ABST
Patent Text Reader

Abstract

The utility model discloses a waterproof coiled material sample preparation cutting die, which relates to the technical field of sample preparation cutting dies, and comprises a cutting die A, a circular cutting die and a cutting die B. The circular cutting die is arranged on one side of the cutting die A, the cutting die B is arranged on one side of the circular cutting die, and mounting blocks are arranged among the cutting die A, the circular cutting die and the cutting die B; a movable block is arranged on one side of the mounting block, positioning blocks are fixedly arranged on one side of the movable block and one side of the mounting block, a protruding block is fixedly arranged on the lower end face of the mounting block, a movable groove is formed in the protruding block, a spring A is arranged in the movable groove, and inserting rods are arranged on the two sides of the spring A; and inserting grooves are formed in one sides of the interiors of the cutting dies A. By improving the efficiency of the existing sample preparation process, burrs generated in the detection sample preparation process are reduced, the generation of samples which do not meet the normative requirement in the sample preparation process is avoided, and the working efficiency and work are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of sample making knife moulds, in particular to a sample making knife mould for waterproof coiled materials. Background Art

[0002] Waterproof membrane is mainly used for building walls, roofs, tunnels, roads, landfills, etc. It is a kind of flexible building material product that can be rolled into a roll to resist the leakage of external rainwater and groundwater. As a leakage-free connection between the engineering foundation and the building, it is the first barrier to waterproofing the entire project. It plays a vital role in the entire project. In order to improve the efficiency of the existing sample preparation process, reduce the burrs produced in the sample preparation process of the test samples, avoid the generation of samples that do not meet the regulatory requirements in the sample preparation process, improve work efficiency and work capacity, and promote the application of this application technology.

[0003] All the samples in this patent are first drawn manually with a steel ruler and then carved out with a utility knife. This takes a lot of time and requires the use of a knife die. At the same time, a set of samples is convenient for the stamping of the entire waterproof membrane. Utility Model Content

[0004] In view of the deficiencies in the prior art, the utility model provides a knife die for making sample of waterproof membrane, which solves the problem that all current sample making is first to draw lines manually with a steel ruler and then to carve them out with a utility knife, which takes a lot of time and requires the use of a knife die. At the same time, a complete set of samples can be conveniently used for stamping the entire waterproof membrane.

[0005] To achieve the above purpose, the utility model is implemented through the following technical solutions: a waterproof coiled material sample making knife die, including a knife die A, a circular knife die and a knife die B, a circular knife die is arranged on one side of the knife die A, a knife die B is arranged on one side of the circular knife die, a mounting block is arranged between the knife die A, the circular knife die and the knife die B, a movable block is arranged on one side of the mounting block, a positioning block is fixedly arranged on one side of the movable block and the mounting block, a convex block is fixedly arranged on the lower end surface of the mounting block, a movable groove is arranged inside the convex block, a spring A is arranged inside the movable groove, and plug rods are arranged on both sides of the spring A, A slot is provided on one side of the interior of the cutting die A, and the insertion rod is inserted into the slot. Limiting slots are provided on both sides of the interior of the protrusion, and movable fixing plates are provided inside the two limiting slots. A short shaft is movably connected between the movable fixing plate and the protrusion, and a spring B is provided on one side of the movable fixing plate. A triangular protrusion is provided on one side of the interior of the cutting die A, and the triangular protrusion and the movable fixing plate are clamped with each other. A positioning groove is provided on one side of the interior of the cutting die A, and the positioning block is clamped into the positioning groove. A clamping block is fixedly provided on one side of the cutting die A, and a clamping groove is provided inside the cutting die A, and the clamping block is clamped into the clamping groove.

[0006] Preferably, a movable shaft is movably connected between the movable block and the mounting block, a positioning block is fixedly provided on one side of the movable block, the positioning block is inserted into a positioning groove, and a spacing groove is provided between the two cutting dies A.

[0007] Preferably, the thickness of the blades of the cutting die A, the circular cutting die and the cutting die B is four millimeters.

[0008] Preferably, the knife die A is designed to be 300 mm long and 50 mm wide, aiming at the tensile performance of the waterproof membrane.

[0009] Preferably, the circular knife die is designed to have a diameter of fifty millimeters and a width of twenty-five millimeters, in order to achieve water-tight performance for the waterproof membrane.

[0010] Preferably, the knife die B is designed to be 50 mm in length and 25 mm in width, aiming at the low temperature and gentle performance of the waterproof membrane.

[0011] Preferably, a limiting plate is provided between the two insertion rods and the spring A, a corresponding groove is provided inside the mounting block, and the cutting die A is inserted into the corresponding groove. Beneficial Effects

[0012] The utility model provides a sample making knife die. Compared with the prior art, it has the following beneficial effects:

[0013] 1. The design length of the knife die A is 300 mm and the width is 50 mm, which is aimed at the tensile performance of the waterproof membrane; the circular knife die is designed to be 50 mm in diameter and 25 mm in width, which is aimed at the waterproof performance of the waterproof membrane; the knife die B is designed to be 50 mm in length and 25 mm in width, which is aimed at the low-temperature flexibility of the waterproof membrane. There are six tensile performance samples of the waterproof membrane, three water-impermeable samples, and ten low-temperature flexibility samples. The blade hardness and thickness of the knife die A, circular knife die and knife die B are all 4 mm.

[0014] 2. The cutting die A, the circular cutting die and the cutting die B need to be fixed by means of a mounting block so that they can be used as a set of samples as a whole. The positioning block on one side of the mounting block is inserted into the positioning groove inside the cutting die A for fixation. At the same time, the convex block on the lower end face of the mounting block is just inserted into the spacing groove between the two cutting dies A. The plug rods on both sides of the inside thereof pop out when the spring A is relaxed, so that the two plug rods are inserted into the slots inside the two cutting dies A for fixation. At this time, the triangular protrusions on one side of the inside of the two cutting dies A are just aligned with the triangular grooves on one side of the movable fixing plate to strengthen the fixation. Finally, the movable block on the other side of the mounting block and the movable shaft movably connected with the mounting block can be folded so that the positioning block on one side is just inserted into the positioning groove inside the cutting die A to complete the installation of the cutting dies. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1It is a three-dimensional structural schematic diagram of the utility model.

[0016] Figure 2 It is a schematic diagram of the cross-sectional structure of the knife die connection of the utility model.

[0017] Figure 3 For this utility model Figure 2 Schematic diagram of the local enlarged structure at cross section A.

[0018] In the figure: 1. cutting die A; 2. circular cutting die; 3. cutting die B; 4. mounting block; 5. movable shaft; 6. movable block; 7. corresponding groove; 8. positioning block; 9. positioning groove; 10. clamping groove; 11. clamping block; 12. protrusion; 13. movable groove; 14. spring A; 15. plug rod; 16. slot; 17. triangular protrusion; 18. movable fixing plate; 19. limiting groove; 20. spring B; 21. short shaft; 22. spacing groove. DETAILED DESCRIPTION

[0019] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0020] See also Figure 1-3 The utility model provides a technical solution: a waterproof coiled material sample cutting die, comprising a cutting die A1, a circular cutting die 2 and a cutting die B3, a circular cutting die 2 is arranged on one side of the cutting die A1, a cutting die B3 is arranged on one side of the circular cutting die 2, a mounting block 4 is arranged between the cutting die A1, the circular cutting die 2 and the cutting die B3, a movable block 6 is arranged on one side of the mounting block 4, a positioning block 8 is fixedly arranged on one side of the movable block 6 and the mounting block 4, a convex block 12 is fixedly arranged on the lower end surface of the mounting block 4, and the movable block 6 and the mounting block are fixedly arranged. 4 is movably connected with a movable shaft 5, a positioning block 8 is fixedly arranged on one side of the movable block 6, and the positioning block 8 is inserted into the positioning groove 9. A spacing groove 22 is arranged between the two cutting dies A1. The thickness of the blades of the cutting die A1, the circular cutting die 2 and the cutting die B3 is four millimeters. The cutting die A1, the circular cutting die 2 and the cutting die B3 need to be fixed by the mounting block 4 so that they can be used as a set of samples as a whole. Then, the positioning block 8 on one side of the mounting block 4 is inserted into the positioning groove 9 inside the cutting die A1 for fixing;

[0021] A movable groove 13 is provided inside the convex block 12, a spring A14 is provided inside the movable groove 13, and plug rods 15 are provided on both sides of the spring A14. A slot 16 is provided on one side of the inside of the cutting die A1, and the plug rod 15 is inserted into the slot 16. Limiting grooves 19 are provided on both sides of the inside of the convex block 12, and movable fixing plates 18 are provided inside the two limiting grooves 19. A short shaft 21 is movably connected between the movable fixing plate 18 and the convex block 12, and a spring B20 is provided on one side of the movable fixing plate 18. The cutting die A1 is designed to have a length of 300 mm and a width of 50 mm, aiming at the tensile performance of the waterproof coiled material. The circular cutting die 2 is designed to have a diameter of 50 mm and a width of 25 mm, aiming at the waterproof performance of the waterproof coiled material. At the same time, the convex block 12 on the lower end face of the mounting block 4 is just inserted into the spacing groove 22 between the two cutting dies A1, and the plug rods 15 on both sides of the inside thereof pop out when the spring A14 is relaxed, so that the two plug rods 15 are inserted into the slots 16 inside the two cutting dies A1 for fixing;

[0022] A triangular protrusion 17 is provided on one side of the interior of the cutting die A1, and the triangular protrusion 17 is engaged with the movable fixed plate 18. A positioning groove 9 is provided on one side of the cutting die A1, and the positioning block 8 is inserted into the positioning groove 9. A clamping block 11 is fixedly provided on one side of the cutting die A1, and a clamping groove 10 is provided on the interior of the cutting die A1, and the clamping block 11 is inserted into the clamping groove 10. The cutting die B3 is designed to be 50 mm in length and 25 mm in width. In view of the low temperature performance of the waterproof membrane, a limiting plate is provided between the two plug rods 15 and the spring A14, and a corresponding groove 7 is provided on the interior of the mounting block 4. The cutting die A1 is inserted into the corresponding groove 7. At this time, the triangular protrusion 17 on one side of the two cutting dies A1 is also just aligned with the triangular groove on one side of the movable fixed plate 18 to strengthen the fixation. Finally, the movable block 6 on the other side of the mounting block 4 and the movable shaft 5 movably connected with the mounting block 4 can be folded so that the positioning block 8 on one side is also just inserted into the positioning groove 9 inside the cutting die A1 to complete the installation set between the cutting dies.

[0023] During operation, the knife die A1 is first designed with a length of 300 mm and a width of 50 mm, which is aimed at the tensile performance of the waterproof membrane; the circular knife die 2 is designed with a diameter of 50 mm and a width of 25 mm, which is aimed at the watertight performance of the waterproof membrane; the knife die B3 is designed with a length of 50 mm and a width of 25 mm, which is aimed at the low-temperature flexibility of the waterproof membrane. There are six tensile performance samples of the waterproof membrane, one watertight sample, and ten low-temperature flexibility samples. The hardness and thickness of the blades of the knife die A1, the circular knife die 2, and the knife die B3 are all four millimeters; the knife die A1, the circular knife die 2, and the knife die B3 need to be fixed by the mounting block 4 so that they can be used as a set of samples as a whole, and the positioning block 8 on one side of the mounting block 4 is inserted into the inside of the knife die A1. The two cutting dies A1 are fixed in the positioning groove 9. At the same time, the protrusion 12 on the lower end surface of the mounting block 4 is just inserted into the spacing groove 22 between the two cutting dies A1. The insertion rods 15 on both sides of the interior thereof pop out when the spring A14 is relaxed, so that the two insertion rods 15 are inserted into the slots 16 inside the two cutting dies A1 for fixation. At this time, the triangular protrusions 17 on one side of the inside of the two cutting dies A1 are just aligned with the triangular groove on one side of the movable fixing plate 18 to strengthen the fixation. Finally, the movable shaft 5 movably connected between the movable block 6 on the other side of the mounting block 4 and the mounting block 4 can be folded, so that the positioning block 8 on one side is also just inserted into the positioning groove 9 inside the cutting die A1 to complete the installation set between the cutting dies.

[0024] Meanwhile, the contents not described in detail in this specification belong to the prior art known to those skilled in the art.

Claims

1. A cutting die for making a sample of a waterproofing coiled material, comprising a cutting die A (1), a circular cutting die (2) and a cutting die B (3), Features: A circular cutting die (2) is arranged on one side of the cutting die A (1), a cutting die B (3) is arranged on one side of the circular cutting die (2), a mounting block (4) is arranged between the cutting die A (1), the circular cutting die (2) and the cutting die B (3), a movable block (6) is arranged on one side of the mounting block (4), a positioning block (8) is fixedly arranged on one side of the movable block (6) and the mounting block (4), a convex block (12) is fixedly arranged on the lower end surface of the mounting block (4), a movable groove (13) is arranged inside the convex block (12), a spring A (14) is arranged inside the movable groove (13), an insertion rod (15) is arranged on both sides of the spring A (14), a slot (16) is arranged on one side of the interior of the cutting die A (1), and the insertion rod (15) is inserted into the slot (16) , both sides of the interior of the protrusion (12) are provided with limiting grooves (19), and both of the limiting grooves (19) are provided with movable fixing plates (18), and a short shaft (21) is movably connected between the movable fixing plate (18) and the protrusion (12), and a spring B (20) is provided on one side of the movable fixing plate (18), and a triangular protrusion (17) is provided on one side of the interior of the cutting die A (1), and the triangular protrusion (17) and the movable fixing plate (18) are mutually engaged, and a positioning groove (9) is provided on one side of the interior of the cutting die A (1), and the positioning block (8) is engaged in the positioning groove (9), and a clamping block (11) is fixedly provided on one side of the cutting die A (1), and a clamping groove (10) is provided on the interior of the cutting die A (1), and the clamping block (11) is engaged in the clamping groove (10).

2. A waterproofing coiled material sample cutting die according to claim 1, Features: A movable shaft (5) is movably connected between the movable block (6) and the mounting block (4); a positioning block (8) is fixedly provided on one side of the movable block (6); the positioning block (8) is inserted into a positioning groove (9); and a spacing groove (22) is provided between the two cutting dies A (1).

3. A waterproofing coiled material sample cutting die according to claim 1, Features: The thickness of the blades of the cutting die A (1), the circular cutting die (2) and the cutting die B (3) is four millimeters.

4. A waterproofing coiled material sample cutting die according to claim 1, Features: The knife die A (1) is designed to be 300 mm long and 50 mm wide, in order to improve the tensile performance of the waterproof membrane.

5. A waterproofing coiled material sample cutting die according to claim 1, Features: The circular knife die (2) is designed to have a diameter of fifty millimeters and a width of twenty-five millimeters, in order to achieve water-tight performance for the waterproof membrane.

6. A waterproofing coiled material sample cutting die according to claim 1, Features: The knife die B (3) is designed to be fifty millimeters in length and twenty-five millimeters in width, aiming at the low temperature performance of the waterproof membrane.

7. A waterproofing coiled material sample cutting die according to claim 1, Features: A limiting plate is provided between the two insertion rods (15) and the spring A (14), a corresponding groove (7) is provided inside the mounting block (4), and the cutting die A (1) is inserted into the corresponding groove (7).