Self-repairing automobile externally-pasted window film
By using combined technologies such as thermal curing coating, epoxy resin primer and double silver plating in automotive window films, the problem that existing automotive window films are difficult to have high light transmittance and infrared barrier rate is solved, and the self-important Repair, stain resistance and high adhesion extend the service life.
Patent Information
- Application Number
- CN202422501479.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-16
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2034-10-16
AI Technical Summary
It is difficult for existing automotive window films to have both high light transmittance and high infrared barrier rate, and their service life is short, making them prone to fading, degumming or performance degradation.
The self-repaired vehicle outer window film consisting of a heat-curing coating, a base coating, a hydrolysis-resistant polyester film layer, a composite layer, a double silver polyester film layer and an installation layer is used to form heat through PU curing thermal repair potion. The cured coating, combined with an epoxy resin primer and an acrylic composite adhesive layer, uses a double silver plating and a polyester film base to improve light transmission and infrared barrier properties, and enhance adhesion and weather resistance through epoxy resin and antioxidants.
It achieves a high infrared barrier rate while maintaining a high light transmittance, and has self-healing function, stain resistance and heat repairability, extends service life, and improves the weather resistance and adhesion of the film.
Smart Images

Figure CN222119129U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of automobile window films, in particular to a self-repairing automobile exterior window film. Background Art
[0002] Car window film is a thin film on the front and rear windshields, side windows and sunroofs of vehicles. Its main function is to block ultraviolet rays, infrared rays, heat and prevent injuries caused by sudden glass explosion. It can also reduce the damage of items and personnel in the car due to ultraviolet radiation, and save fuel consumption in some aspects. The first generation of car solar film is known as "dyed film". A dye is sprayed on a layer of polyester film to achieve the effect of light and ultraviolet isolation. This solar film is easy to install and has good light blocking, but it is not heat-resistant, easy to fade and degumming, and has a short service life; the second generation is metal reflective film, that is, "explosion-proof film". This solar film improves the explosion-proof function by spraying aluminum, titanium and other metals on the polyester layer, and the heat insulation function is also improved, but the heat insulation is low when the light transmittance is high, and the light transmittance is low when the heat insulation is high; the third generation is the "heat-absorbing film" of car solar film, which has good heat insulation and sun protection performance, and the film is still relatively thin after the explosion-proof performance is enhanced. The heat-absorbing agent is sprayed on the polyester layer to achieve a good heat insulation effect, but the life is short and the performance will decline after one or two years of use. It can be seen from this that it is difficult for automobile window films to meet both technical indicators of light transmittance and infrared blocking rate at the same time. Utility Model Content
[0003] In order to solve the above technical problems, the utility model provides a self-repairing automobile exterior window film, which can maintain a high infrared blocking rate while maintaining a high light transmittance.
[0004] The technical solution of the utility model is: a self-repairing automobile exterior window film, comprising a thermosetting coating, a primer, a hydrolysis-resistant polyester film layer, a composite layer, a double silver polyester film layer, a mounting layer and a release film layer which are arranged in sequence.
[0005] Furthermore, the thickness of the thermal curing coating is 2 to 3 μm.
[0006] Furthermore, the primer layer is an epoxy resin primer layer with a thickness of 0.5 to 1.5 μm.
[0007] Furthermore, the hydrolysis-resistant polyester film layer is colorless and transparent, and the thickness of the hydrolysis-resistant polyester film layer is 23-50 μm.
[0008] Furthermore, the composite layer and the installation layer are both acrylic composite adhesive layers, the composite layer has a thickness of 6 to 7 μm, and the installation layer has a thickness of 8 to 9 μm.
[0009] Furthermore, the double silver polyester film layer consists of a double silver plated layer and a polyester film base layer.
[0010] Furthermore, the thickness of the double silver plating layer is 250nm.
[0011] Furthermore, the double silver plating layer is provided between the polyester film base layer and the mounting layer.
[0012] Furthermore, the double silver coating consists of a first coating and a second coating with the same structure. The first coating and the second coating are composed of a titanium oxide layer, an aluminum oxide layer, a zinc oxide layer, an aluminum zinc oxide layer, a silicon oxide layer and a silver alloy layer in sequence. The titanium oxide layer of the first coating is connected to the composite layer, and the silver alloy layer of the second coating is connected to the polyester film base layer.
[0013] Furthermore, the first coating layer and the second coating layer have the same thickness.
[0014] Furthermore, the release film has a thickness of 23 um.
[0015] Compared with the prior art, the advantages of the utility model are: the self-repairing thermosetting coating is formed by coating with PU-curing thermosetting solution, the film surface has excellent thermorepairability and feel, and is resistant to stains. It can be easily wiped clean after being graffitied by an oily pen. This coating has the function of thermally repairing minor damage caused by external factors; the double silver polyester film layer is combined with a first coating and a second coating with the same structure, and has the performance of a visible light transmittance between 70% and 75% and an infrared blocking rate between 80% and 88%. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] In order to more clearly illustrate the embodiments of the utility model or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0017] Figure 1 It is a structural schematic diagram of the utility model;
[0018] Figure 2 It is a schematic diagram of the structure of the double silver polyester film layer of the utility model.
[0019] Among them: 1. thermal curing coating; 2. primer coating; 3. hydrolysis-resistant polyester film layer; 4. composite layer; 5. double silver polyester film layer; 6. mounting layer; 7. release film layer; 51. titanium oxide layer; 52. aluminum oxide layer; 53. zinc oxide layer; 54. aluminum zinc oxide layer; 55. silicon oxide layer; 56. silver alloy; 57. polyester film base layer. DETAILED DESCRIPTION
[0020] In order to further explain the technical means and effects adopted by the present invention to achieve the predetermined invention purpose, the specific implementation method, structure, characteristics and effects of the present invention are described in detail below in combination with the accompanying drawings and preferred embodiments.
[0021] like Figure 1-2 As shown, a self-repairing automobile exterior window film includes a thermosetting coating 1, a primer 2, a hydrolysis-resistant polyester film layer 3, a composite layer 4, a double silver polyester film layer 5, a mounting layer 6 and a release film layer 7 which are arranged in sequence.
[0022] The thermal curing coating 1 is also called a self-healing coating in the industry, and has a self-healing function. It is formed by coating a PU-curing thermal repair solution, and the PU-curing thermal repair solution is made of a self-healing solution, a curing agent, a propylene glycol methyl ether acetate dilution aid, and an ethyl acetate dilution aid; the thermal curing coating 1 has a thickness of 2 to 3 μm, and its main resin is a linear thermal curing resin, a modified polyurethane oligomer with a molecular weight of 500 to 3000, and a resin hydroxyl value range of 3 to 10 mgKOH / g, and the thermal curing agent is an amine curing agent and an isocyanate curing agent. The film surface of the thermosetting coating 1 has excellent thermal repairability and feel, and is resistant to stains. It can be easily wiped clean after being graffitied by an oily pen. This coating has the function of thermal repairing minor damage caused by external factors. By coating a layer of epoxy resin on the surface of the hydrolysis-resistant polyester film layer 3, a better connection between the self-repairing thermosetting coating 1 and the hydrolysis-resistant polyester film layer 3 can be achieved, and the surface adhesion can be improved. The adhesion can reach 5B. 5B is the coating peeling grade, which means that the percentage of special layer peeling is 0%. At the same time, it has the advantage of good weather resistance.
[0023] The base coating 2 is an epoxy resin base coating 2 with a thickness of 0.5 to 1.5 μm; the hydrolysis-resistant polyester film layer 3 is colorless and transparent, and the thickness of the hydrolysis-resistant polyester film layer 3 is 23 to 50 μm; the composite layer 4 and the mounting layer 6 are both acrylic composite adhesive layers, the composite layer 4 is 6 to 7 μm thick, and the mounting layer 6 is 8 to 9 μm thick;
[0024] The composite layer 4 is made of acrylic composite glue, butanone dilution aid, light stabilizer and antioxidant, and the mounting layer 6 is made of acrylic composite glue, butanone dilution aid, light stabilizer, antioxidant and ultraviolet absorber. The composite layer 4 and the mounting layer 6 both play a connecting role.
[0025] The composite layer 4 includes light stabilizers, antioxidants and ultraviolet absorbers, so that the composite layer 4 has better anti-ultraviolet aging performance, can shield, reflect ultraviolet rays or absorb ultraviolet rays and convert them into harmless heat energy, and can also capture free radicals generated by light redox, thereby preventing free radical reactions that cause aging of the vehicle film and protecting the vehicle film from ultraviolet damage.
[0026] The double silver polyester film layer 5 consists of a double silver coating and a polyester film base layer. The double silver coating has a thickness of 250 nm and is coated on the polyester film base layer by a magnetron sputtering coating machine. The double silver coating is connected to the composite layer 4 , and the polyester film base layer is connected to the mounting layer 6 .
[0027] The double silver coating is composed of a first coating and a second coating with the same structure and thickness. The first coating and the second coating are composed of a titanium oxide layer 51, an aluminum oxide layer 52, a zinc oxide layer 53, an aluminum zinc oxide layer 54, a silicon oxide layer 55 and a silver alloy 56 layer in sequence. The titanium oxide layer 51 of the first coating is connected to the composite layer 4, and the silver alloy 56 layer of the second coating is connected to the polyester film base layer. The double silver coating can be provided between the polyester film base layer and the mounting layer 6, which can further improve the light transmittance and infrared blocking rate, but the double silver coating will have certain oxidation and corrosion risks.
[0028] The release film has a thickness of 23 um.
[0029] Description of the working method of this utility model:
[0030] Embodiment 1, carry out according to the following steps in sequence:
[0031] Step 1, coating the composite glue on the double silver plated layer of the double silver polyester film layer 5, baking at a temperature of 100° C. for 1 min to form a composite layer 4;
[0032] Step 2, laminating the adhesive surface of the composite layer 4 of the double silver polyester film layer 5 to the non-coated surface of the hydrolysis-resistant polyester film layer 3;
[0033] Step 3: coating the coated surface of the hydrolysis-resistant polyester film layer 3 of the composite sample with epoxy resin, with a baking temperature of 120° C. and a baking time of 2 min to form an epoxy resin primer layer 2;
[0034] Step 4: coating the self-repairing heat-curing coating 1 on the epoxy resin base coating 2 obtained in step 3, with a baking temperature of 120° C. and a baking time of 2 min;
[0035] Step 5: Apply mounting glue on the non-plated surface of the double silver polyester film of the composite sample, with a baking temperature of 100° C. and a baking time of 1 min;
[0036] Step six, laminating the adhesive surface of the mounting layer 6 of the double silver polyester film layer 5 with the release film layer 7 to obtain a self-repairing automobile exterior window film.
[0037] Embodiment 2, carry out according to the following steps in sequence:
[0038] Step 1: coating the non-plated surface of the double silver polyester film layer 5 with mounting glue to obtain the mounting layer 6, with the baking temperature being 100° C. and the baking time being 1 min;
[0039] Step 2, laminating the adhesive surface of the mounting layer 6 of the double silver polyester film layer 5 with the release film layer 7;
[0040] Step 3, coating the double silver plated surface of the double silver polyester film layer 5 with a composite adhesive, baking at a temperature of 100° C. for 1 min to obtain a composite layer 4;
[0041] Step 4, laminating the adhesive surface of the composite layer 4 of the double silver polyester film layer 5 to the non-coated surface of the hydrolysis-resistant polyester film layer 3;
[0042] Step 5: coating the coated surface of the hydrolysis-resistant polyester film layer 3 of the composite sample with epoxy resin, with a baking temperature of 120° C. and a baking time of 2 min to obtain an epoxy resin primer layer 2;
[0043] Step six, coating the self-repairing heat-curing coating 1 on the epoxy resin primer coating 2, baking at 120° C. for 2 minutes, to obtain a self-repairing exterior window film.
[0044] The above embodiments are only used to illustrate the technical solution of the utility model, rather than to limit it. Although the utility model is described in detail with reference to the above embodiments, ordinary technicians in this field should understand that they can still modify the technical solutions recorded in the above embodiments, or replace some or all of the technical features therein with equivalents. These modifications or replacements do not make the essence of the corresponding technical solutions deviate from the scope of the technical solutions of the embodiments of the utility model.
Claims
1. A self-repairing automobile exterior window film, comprising a thermosetting coating, a primer, a hydrolysis-resistant polyester film layer, a composite layer, a double silver polyester film layer, a mounting layer and a release film layer arranged in sequence, characterized in that: The double silver polyester film layer consists of a double silver plated layer and a polyester film base layer, the double silver plated layer is connected to the composite layer, and the polyester film base layer is connected to the mounting layer.
2. The self-repairing automobile exterior window film according to claim 1, characterized in that: The thickness of the thermal curing coating is 2-3 μm.
3. The self-repairing automobile exterior window film according to claim 1, characterized in that: The primer layer is an epoxy resin primer layer with a thickness of 0.5 to 1.5 μm.
4. The self-repairing automobile exterior window film according to claim 1, characterized in that: The hydrolysis-resistant polyester film layer is colorless and transparent, and the thickness of the hydrolysis-resistant polyester film layer is 23-50 μm.
5. The self-repairing automobile exterior window film according to claim 1, characterized in that: The composite layer and the installation layer are both acrylic composite adhesive layers, the composite layer has a thickness of 6-7 μm, and the installation layer has a thickness of 8-9 μm.
6. The self-repairing automobile exterior window film according to claim 1, characterized in that: The thickness of the double silver plating layer is 250nm.
7. The self-repairing automobile exterior window film according to claim 1, characterized in that: The double silver plating layer is arranged between the polyester film base layer and the mounting layer.
8. The self-repairing automobile exterior window film according to claim 1 or 7, characterized in that: The double silver coating consists of a first coating and a second coating with the same structure. The first coating and the second coating are both composed of a titanium oxide layer, an aluminum oxide layer, a zinc oxide layer, an aluminum zinc oxide layer, a silicon oxide layer and a silver alloy layer in sequence. The titanium oxide layer of the first coating is connected to the composite layer, and the silver alloy layer of the second coating is connected to the polyester film base layer.
9. The self-repairing automobile exterior window film according to claim 8, characterized in that: The first plating layer and the second plating layer have the same thickness.
10. The self-repairing automobile exterior window film according to claim 1, characterized in that: The release film has a thickness of 23 um.