Induction coil for melting metal bar

By designing a horizontal coil group and separator structure with arithmetic decrease in diameter, combined with water cooling and insulating tape, the problem of unstable use effect and life of induction coils is solved, and uniform melting and equipment stability are improved.

CN222128335UActive Publication Date: 2024-12-06CHINA WEAPON SCI ACADEMY NINGBO BRANCH
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202422530638.8
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-10-21
Publication Date
2024-12-06
Estimated Expiration
2034-10-21

AI Technical Summary

Technical Problem

The existing induction coils have unstable usage effect and life, and it is difficult to control the heating efficiency and the dripping speed. The structure is poorly rigid and easy to deform, which affects the uniform melting and production efficiency of metal rod materials.

Method used

Design a curved induction coil group, with amorphous arithmetic decreases from top to bottom and horizontally distributed, and a partition is installed between each group of coils to improve stiffness and stability, and use water cooling technology to keep the coil stable and peripheral packages Cover the insulating tape to prevent current leakage.

Benefits of technology

A uniform and stable metal electrode melting effect is achieved, extending the service life of the coil group, improving production efficiency and equipment safety, and ensuring the shape stability and insulation performance of the coil group.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222128335U_ABST
    Figure CN222128335U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of induction coils, in particular to an induction coil for melting a metal bar, which comprises a coil group formed by bending, the diameters of coils in the coil group are in an equal difference decreasing trend from top to bottom, each coil is approximately horizontally arranged, a separation sheet is mounted in the coil group, and the upper and lower adjacent coils are supported by the separation sheet; the two ends of the coil assembly are connected with a positive electrode power connection block and a negative electrode power connection block respectively, and the positive electrode power connection block and the negative electrode power connection block are arranged on the same side of the coil. According to the scheme, each coil in the coil assembly is approximately horizontally distributed, so that the coaxiality of the coils can be better ensured, the uniform and stable metal electrode melting effect is achieved, and the electromagnetic induction loss is reduced to the maximum extent; meanwhile, as the bottom of the coil assembly is horizontal, the distance between the coil and the spraying disc can be accurately controlled during installation, and debugging parameters can be standardized.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of induction coils, and in particular to an induction coil for melting metal bars. Background Art

[0002] Electrode induction melting gas atomization (EIGA) technology is the main preparation method for titanium alloy powder in laser additive manufacturing. This method uses an induction coil to generate a high-frequency electromagnetic field to heat and melt the metal electrode. When the electrode is melted, the molten droplets fall into the gas atomization nozzle system and are dispersed into fine droplets under the impact of the inert gas flow, and finally solidified into metal powder. In order to make the molten metal droplets flow stably into the nozzle, the top of the original metal bar needs to be processed into a cone by machining or welding, and the winding method of the induction coil also needs to be designed to match the shape of the metal bar. The diameter of each circle is different and the overall shape is conical.

[0003] Key parameters in induction coil design: (1) Number of windings. The number of coils will affect the heating efficiency and the superheat of the molten droplet. The more coils there are, the faster the heating will be. However, the molten droplet will also drip faster and be more difficult to control. (2) Coil spacing. The spacing will affect the heating range of the bar. The smaller the spacing, the more concentrated the heat will be. The risk of sparks between coils will also be higher. Too small a spacing will easily affect the service life of the induction coil. (3) Coaxiality of the coil. Coaxiality is a very critical parameter that can directly affect the uniformity of bar melting and the location of molten droplets. If the coil coaxiality is poor due to improper production, transportation and installation, the melting rates at different locations on the periphery of the bar will be different, and the molten droplets will easily deviate from the axis when dripping. In severe cases, the molten droplet will be blocked on the nozzle of the spray plate below, reducing production efficiency and affecting the service life of the spray plate. In addition, when installing the coil, the distance between the bottom of the coil group and the spray plate determines the travel of the molten droplet. If the distance is too large, the superheat of the molten droplet will decrease, the viscosity of the molten droplet will increase, and the production rate of fine powder will decrease; if the distance is too small, sparks are likely to be generated between the induction coil and the spray plate, and the sparks may penetrate the coil copper tube, causing the coil to be scrapped.

[0004] At present, the induction coil used in EIGA is spirally wound, similar to a spring. Its advantages are good coil continuity, simple structure, and easy production; its disadvantages are poor rigidity, easy deformation, and difficult control of coil spacing and coaxiality. The service life of the coil is unstable, ranging from one day to several months. In addition, the bottom of the spirally wound coil is not horizontal. During installation, the distance control between the induction coil and the spray disc depends on the operator's operating experience, which is not conducive to standardized production and still has room for optimization. Utility Model Content

[0005] In order to solve the problem of unstable use effect and life of induction coils in the prior art, the present application provides an induction coil for melting metal bars.

[0006] The induction coil for melting metal bars provided in the present application adopts the following technical solution:

[0007] An induction coil for melting metal bars, comprising a coil group formed by bending, wherein the diameter of the coils in the coil group decreases arithmetically from top to bottom, and each circle of coils is arranged horizontally; the two ends of the coil group are respectively connected to a positive electrode connection block and a negative electrode connection block, and the positive electrode connection block and the negative electrode connection block are arranged on the same side of the coil group; a separator is installed in the coil group, and grooves for coil clamping are provided at the upper and lower ends of the separator, and the separator is arranged on a side away from the positive electrode connection block, and the separator is installed between each group of upper and lower adjacent coils.

[0008] By adopting the above technical scheme, the winding method of the existing spiral induction coil is different. In the present application, each circle of the coil in the coil group is horizontally distributed, which can better ensure the coaxiality of the coil, so as to obtain a uniform and stable metal electrode melting effect and minimize the electromagnetic induction loss; the design also makes the bottom of the coil group horizontal, which is more conducive to accurately controlling the distance between the coil group and the spray plate during installation, and the debugging parameters can be standardized; using a separator to support the coil can effectively improve the stiffness of the coil, making the coil less likely to deform, and the coil spacing and coaxiality are more stable, which can extend the service life of the coil group; and the separator and the coil can be produced separately, and the combination and installation are flexible, and the circular coil can be fixed in the groove of the separator by its own gravity and interference fit.

[0009] Optionally, the separator is a ceramic separator, and the thickness of the separator is 1-5 mm.

[0010] By adopting the above technical solution, the ceramic separator is light and thin, will not cause excessive load burden on the coil, and does not require additional fixation.

[0011] Optionally, the separator is a porous separator.

[0012] By adopting the above technical solution and porous design, the weight of the separator is further reduced.

[0013] Optionally, the number of coils in the coil group is N, and the total number of separators is N-1.

[0014] By adopting the above technical solution, it is ensured that there is a separator between every two coils to fix them, thereby improving the overall stability of the coil group, while limiting the number of separators to avoid causing load burden on the coils.

[0015] Optionally, all the separators are aligned vertically.

[0016] By adopting the above technical solution, the separators are aligned up and down, which can effectively enhance the overall rigidity of the coil group and ensure that the shape of the coil group remains unchanged during operation.

[0017] Optionally, a water inlet is provided on the plate surface of the positive electrode connection block, a water outlet is provided on the plate surface of the negative electrode connection block, a cooling water channel is provided in the coil assembly, and both ends of the cooling water channel are respectively connected to the water inlet and the water outlet.

[0018] By adopting the above technical solution, when the induction coil is working, water cooling is used to keep the coil in stable physical properties, thereby extending the service life of the equipment.

[0019] Optionally, the outer periphery of the coil assembly is coated with insulating tape.

[0020] By adopting the above technical solution, the outer periphery of the coil group is covered with insulating tape, which enhances the insulation performance between the coil and the external environment, helps prevent current leakage, avoids sparking, improves the overall safety of the equipment, and reduces the frequency of maintenance and overhaul. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1 It is a schematic diagram of the overall structure of the induction coil used for melting metal bars in an embodiment of the present application.

[0022] Figure 2 is a top view of an induction coil for melting metal bars according to an embodiment of the present application.

[0023] Figure 3 is a side view of an induction coil for melting a metal bar according to an embodiment of the present application.

[0024] Explanation of the reference numerals: 1. coil assembly; 11. insulating tape; 12. cooling water channel; 2. positive electrode connection block; 21. water inlet; 3. negative electrode connection block; 31. water outlet; 4. threaded hole; 5. separator; 51. groove. DETAILED DESCRIPTION

[0025] The following will be combined with the attached Figure 1-3 The technical solution of the utility model is described clearly and completely. Obviously, the described embodiments are part of the embodiments of the utility model, not all of them. Based on the embodiments of the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0026] The present application embodiment discloses an induction coil for melting a metal bar. Figures 1 to 3The induction coil for melting the metal bar comprises a coil group 1 formed by bending a round copper tube, a positive electrode connection block 2 and a negative electrode connection block 3 are welded at both ends of the coil group 1, the positive electrode connection block 2 and the negative electrode connection block 3 are placed on the same side of the coil group 1, and the plate surfaces of the positive electrode connection block 2 and the negative electrode connection block 3 are both provided with threaded holes 4 for fixing.

[0027] The diameter of the coil in the coil group 1 decreases arithmetically from top to bottom. Each coil is horizontal and wound downward near the power connection block, so that multiple coils are connected and the direction of the current vortex field formed by the coils is consistent. In order to reduce the risk of electric sparks between coils, between coils and metal bars, and between coils and spray plates, the outer periphery of the coil group 1 is coated with insulating tape 11.

[0028] A water inlet 21 is provided in the middle of the plate surface of the positive electrode connection block 2, a water outlet 31 is provided in the middle of the plate surface of the negative electrode connection block 3, a cooling water channel 12 is provided inside the coil assembly 1, and both ends of the cooling water channel 12 are respectively connected to the water inlet 21 and the water outlet 31. When the induction coil is working, cooling water flows into the coil assembly 1 through the water inlet 21 to cool the coil assembly 1, and then flows out through the water outlet 31. The outflowing cooling water can be recycled or directly discharged. This application takes recycling as an example, and the specific circulation principle is consistent with the existing circulating water system.

[0029] A separator 5 is also clamped between the upper and lower adjacent coils. The separator 5 is shown as a ceramic material. The thickness of the separator 5 of this material can be 1-5 mm. In this application, 2 mm is shown as an example. In order to further reduce weight, holes are punched on the separator 5 to form a porous separator 5.

[0030] The upper and lower ends of the separator 5 are provided with grooves 51 for coil clamping, so that the separator 5 can be clamped between the coils away from the positive electrode connection block 2, and the circular coil can be fixed in the groove 51 by its own gravity and interference fit.

[0031] A separator 5 is installed between each group of upper and lower adjacent coils. During production, the number of coils in the coil group 1 is related to actual needs, and the number of coils is assumed to be N. For lightweight considerations, the total number of separators is N-1, that is, a separator 5 is installed between each group of upper and lower adjacent coils, and multiple separators 5 are aligned up and down. This application takes a total of three coils and two separators 5 as an example.

[0032] The implementation principle of the induction coil for melting metal bars in the embodiment of the present application is as follows: by adopting a horizontally arranged coil group 1 with equidistantly decreasing diameters, the uniformity of the electromagnetic field is ensured, so that the melting process of the metal bar is more stable, and the horizontal bottom of the coil group 1 is also conducive to accurately controlling the distance between the coil group 1 and the spray plate.

[0033] When in use, first put the conical metal bar into the coil group 1, the induction coil generates a uniform electromagnetic field, the metal bar gradually melts, and forms a molten droplet. During the working process, the coil is continuously cooled by water cooling to ensure its stable operation.

[0034] The above are all preferred embodiments of the present application, and the protection scope of the present application is not limited thereto. Therefore, any equivalent changes made according to the structure, shape, and principle of the present application should be included in the protection scope of the present application.

Claims

1. An induction coil for melting a metal bar, characterized in that: The invention comprises a coil group (1) formed by bending, wherein the diameter of the coil inside the coil group (1) decreases arithmetically from top to bottom, and each coil is arranged horizontally; the two ends of the coil group (1) are respectively connected to a positive pole connection block (2) and a negative pole connection block (3), and the positive pole connection block (2) and the negative pole connection block (3) are arranged on the same side of the coil group (1); a separator (5) is installed inside the coil group (1), and grooves (51) for coil clamping are provided at both upper and lower ends of the separator (5), and the separator (5) is arranged on a side away from the positive pole connection block (2), and the separator (5) is installed between each group of upper and lower adjacent coils.

2. An induction coil for melting metal bars according to claim 1, characterized in that: The separator (5) is a ceramic separator, and the thickness of the separator (5) is 1-5 mm.

3. An induction coil for melting metal bars according to claim 2, characterized in that: The separator (5) is a porous separator.

4. An induction coil for melting metal bars according to claim 1, characterized in that: The number of coils in the coil group (1) is N, and the total number of separators (5) is N-1.

5. The induction coil for melting metal bars according to claim 1, characterized in that: All the separators (5) are aligned vertically.

6. An induction coil for melting metal bars according to claim 1, characterized in that: The plate surface of the positive electrode connection block (2) is provided with a water inlet (21), the plate surface of the negative electrode connection block (3) is provided with a water outlet (31), and a cooling water channel (12) is provided in the coil assembly (1), with two ends of the cooling water channel (12) respectively connected to the water inlet (21) and the water outlet (31).

7. An induction coil for melting metal bars according to claim 1, characterized in that: The outer periphery of the coil assembly (1) is coated with an insulating tape (11).

Citation Information

Cited By

  • Induction coil

    CN223987195U