Improved power generation paint coating

By adding a protective layer to the power generation paint coating and optimizing the structure of the electrode film layer, the problems of insufficient environmentally friendly power generation, poor durability and difficulty in power storage of the power generation paint coating in the prior art are solved, and better power supply and lasting and charge and discharge energy density.

CN222282078UActive Publication Date: 2024-12-31GUANGZHOU HELI PAINT TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420482223.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-13
Publication Date
2024-12-31
Estimated Expiration
2034-03-13

AI Technical Summary

Technical Problem

The existing power generation paint coatings have problems such as insufficient environmentally friendly power generation, poor durability and difficulty in power storage, and the lack of protection of the negative electrode film affects the durability of power generation and poor carrier collection.

Method used

An improved power generation paint coating is designed, including a protective layer, a negative current collector, a negative electrode film layer, a solid electrolyte conductive layer, a positive electrode film layer, a positive current collector, an adhesion insulating layer and a base. The stability of the electrode and carrier collection are ensured by adding protective layer and optimizing the thickness and position of the electrode film layer.

Benefits of technology

It effectively improves the power supply durability and charge and discharge energy density of the coating, ensuring the stability of the electrode and carrier collection effect.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222282078U_ABST
    Figure CN222282078U_ABST
Patent Text Reader

Abstract

The utility model relates to an improved power generation paint coating which sequentially comprises a protective layer, a negative current collector, a negative electrode film layer, a solid electrolyte conducting layer, a positive electrode film layer, a positive current collector, an adhesive force insulating layer and a base material from top to bottom, and the thickness of the improved power generation paint coating is 30-80 microns. According to the utility model, by adding the protective layer on the surface, the power supply durability of the functional coating is effectively protected. Meanwhile, the negative current collector is arranged between the protective layer and the negative electrode film layer, and the positive current collector is arranged between the positive electrode film layer and the adhesive force insulating layer, so that carriers formed on the surfaces of the positive electrode and the negative electrode can be better collected in the charging and discharging process.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the field of paint coatings, in particular to an improved power generation paint coating. Background Art

[0002] Power-generating coatings are a special type of functional coating that has emerged in recent years. By coating the surface of a substrate that is not conductive, it gives the object a certain ability to conduct and eliminate static electricity, while also preventing electromagnetic radiation. However, in actual applications, conductive coatings have problems such as insufficient environmentally friendly power generation, poor durability, and difficulty in storing electricity, and have not attracted much attention.

[0003] A Chinese patent with patent number CN202210071333.8 discloses a power generation paint coating and a preparation method thereof, in which the negative electrode film layer is directly located on the surface of the conductive coating, so that the negative electrode film lacks direct protection, which will directly affect the durability of power generation. At the same time, in the prior art, the current collectors are respectively located in the upper and lower parts of the solid electrolyte layer. Such a design does not better collect the carriers formed on the positive and negative electrode surfaces during the charging and discharging process. Utility Model Content

[0004] In view of the above-mentioned technical deficiencies, the purpose of the utility model is to provide an improved power generation paint coating to solve the problems raised in the background technology.

[0005] In order to solve the above technical problems, the utility model adopts the following technical solutions:

[0006] The utility model provides an improved power generation paint coating, which comprises, from top to bottom, a protective layer, a negative current collector, a negative electrode film layer, a solid electrolyte conductive layer, a positive electrode film layer, a positive current collector, an adhesion insulating layer, and a substrate, wherein the adhesion insulating layer is attached to the substrate, the positive current collector is attached to the adhesion insulating layer, the positive electrode film layer is attached to the positive current collector, the solid electrolyte conductive layer is attached to the positive electrode film layer, the negative electrode film layer is attached to the solid electrolyte conductive layer, the negative current collector is attached to the negative electrode film layer, the protective layer is attached to the negative current collector, the negative current collector and the positive current collector are respectively connected to a frequency converter through conductive wires, and the thickness of the improved power generation paint coating is 30-80um.

[0007] Preferably, the protective layer has a thickness of 3-10 um.

[0008] Preferably, the protective layer is a weather-resistant water-based acrylic coating or a weather-resistant water-based fluorocarbon coating, wherein the volume solid content of the protective coating is 52-56%.

[0009] Preferably, the thickness of the negative electrode thin film layer is 8-25 um, the thickness of the solid electrolyte conductive layer is 1-5 um, and the thickness of the positive electrode thin film layer is 8-25 um.

[0010] Compared with the prior art, the beneficial effects of the utility model are:

[0011] The utility model effectively protects the power supply durability of the functional coating by adding a protective layer on the surface. At the same time, the negative current collector is arranged between the protective layer and the negative electrode film layer, and the positive current collector is arranged between the positive electrode film layer and the adhesion insulating layer, so as to better collect the carriers formed on the positive and negative electrode surfaces during the charging and discharging process. BRIEF DESCRIPTION OF THE DRAWINGS

[0012] Figure 1 Schematic diagram of the overall structure of the utility model;

[0013] Explanation of the reference numerals in the figure: negative current collector 11; negative electrode film layer 2; solid electrolyte conductive layer 3; positive electrode film layer 4; positive current collector 12, adhesion insulating bottom layer 5, substrate 6; protective layer 7; DETAILED DESCRIPTION

[0014] The technical solution in one embodiment of the utility model will be clearly and completely described below in conjunction with the accompanying drawings in the embodiments of the present invention.

[0015] See also Figure 1 :The utility model provides an improved power generation paint coating, an environmentally friendly power supply paint coating, which includes a protective layer 7, a negative current collector 11, a negative electrode film layer 2, a solid electrolyte conductive layer 3, a positive electrode film layer 4, a positive current collector 12, an adhesion insulating layer 5, and a substrate 6 from top to bottom, wherein the adhesion insulating layer 5 is attached to the substrate 6, the positive current collector 12 is attached to the adhesion insulating layer 5, the positive electrode film layer 4 is attached to the positive current collector 12, the solid electrolyte conductive layer 3 is attached to the positive electrode film layer 4, the negative electrode film layer 2 is attached to the solid electrolyte conductive layer 3, the negative current collector 11 is attached to the negative electrode film layer 2, the protective layer 7 is attached to the negative current collector 11, the negative current collector 11 and the positive current collector 12 are respectively connected to the inverter through conductive wires, and the thickness of the environmentally friendly power supply paint coating is 30-80um. The utility model will add a protective layer to the environmentally friendly power supply paint coating, which is conducive to the effective protection of the power supply durability of the functional coating. At the same time, the negative current collector 1 is arranged between the protective layer 7 and the negative electrode film layer 2, and the positive current collector is arranged between the positive electrode film layer 4 and the adhesion insulating layer 5, which is conducive to better collection of carriers formed on the positive and negative electrode surfaces during the charge and discharge process.

[0016] In this embodiment, preferably, the thickness of the protective layer is 3-10 um.

[0017] In this embodiment, preferably, the protective layer is a weather-resistant water-based fluorocarbon coating, wherein the volume solid content of the protective coating is 52-56%.

[0018] Weather-resistant water-based fluorocarbon coating is used as a protective layer. Due to the anti-UV and aging properties of the weather-resistant water-based fluorocarbon coating, it is beneficial to improve the long-term stability of the thin film coating.

[0019] In this embodiment, preferably, the thickness of the negative electrode thin film layer is 8-25 um, the thickness of the solid electrolyte conductive layer is 1-5 um, and the thickness of the positive electrode thin film layer is 8-25 um.

[0020] The utility model increases the thickness of the solid electrolyte conductive layer and the thickness ratio of the positive electrode film layer and the negative electrode film layer in the entire coating, so that the electrolyte is not easy to rupture, so as to prevent the positive and negative electrodes from directly contacting each other due to the electrolyte rupture, thereby improving the stability of the electrolyte. At the same time, the thickening of the positive and negative electrode coatings can fully carry out the redox reaction, form more carriers, and thus improve the charge and discharge energy density.

[0021] The above description is only an embodiment of the present invention, and does not limit the patent scope of the present invention. Any equivalent structure or equivalent process transformation made by using the contents of the specification and drawings of the present invention, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the present invention.

Claims

1. An improved power generation paint coating, characterized in that: The improved power generation paint coating comprises, from top to bottom, a protective layer, a negative current collector, a negative electrode film layer, a solid electrolyte conductive layer, a positive electrode film layer, a positive current collector, an adhesion insulating layer, and a substrate. The adhesion insulating layer is attached to the substrate, the positive current collector is attached to the adhesion insulating layer, the positive electrode film layer is attached to the positive current collector, the solid electrolyte conductive layer is attached to the positive electrode film layer, the negative electrode film layer is attached to the solid electrolyte conductive layer, the negative current collector is attached to the negative electrode film layer, the protective layer is attached to the negative current collector, the negative current collector and the positive current collector are respectively connected to the inverter through conductive wires, and the thickness of the improved power generation paint coating is 30-80um.

2. An improved power generation paint coating as claimed in claim 1, characterized in that: The thickness of the protective layer is 3-10 um.

3. An improved power generation paint coating as claimed in claim 1, characterized in that: The protective layer is a weather-resistant water-based acrylic coating or a weather-resistant water-based fluorocarbon coating, wherein the volume solid content of the protective coating is 52-56%.

4. An improved power generation paint coating as claimed in claim 1, characterized in that: The negative electrode film layer has a thickness of 8 to 25 um, the solid electrolyte conductive layer has a thickness of 1 to 5 um, and the positive electrode film layer has a thickness of 8 to 25 um.